scholarly journals Analysis of the Effects of Ageing on the Cohesive Strength of Polymer-Modified Bitumen at Low Temperatures

2018 ◽  
Vol 13 (2) ◽  
pp. 156-164 ◽  
Author(s):  
Chuanfeng Zheng ◽  
Genze Li ◽  
Yazhi Xu ◽  
Danni Wang ◽  
Dan Lv

The decay law on the ageing process of the cohesive strength of styrene-butadiene-styrene(SBS)- and polyethylene(PE)-modified bitumens at low temperatures was investigated. The rotated-thin-film oven test was used to age the two types of polymer-modified bitumens. The cohesive strengths at different low-temperature conditions were tested quantitatively according to technology for testing the low-temperature cohesive strength of bitumen. The decay curve of bitumen low-temperature cohesive strengths was drawn, and the embrittlement time of bitumen at different ageing states was obtained according to the decay curve. Results showed that ageing time definitely influenced the attenuation degree of the low-temperature cohesive strength of the two types of polymer-modified bitumens and influenced the appearance of the low-temperature cohesive strength peak, i.e., the bitumen embrittlement time, which advanced after ageing. The lightweight components of polymer-modified bitumen were lost after ageing. The bitumen embrittlement time was advanced, and the sharp attenuation of the low-temperature cohesive strength of bitumen appeared. In the future, bitumen antiageing technology and lighter part pre-supplement technology should be studied in-depth.

Materials ◽  
2019 ◽  
Vol 12 (15) ◽  
pp. 2345 ◽  
Author(s):  
Yangsheng Ye ◽  
Gang Xu ◽  
Liangwei Lou ◽  
Xianhua Chen ◽  
Degou Cai ◽  
...  

In this study, a new type of composite modified bitumen was developed by blending styrene-butadiene-styrene (SBS) and crumb rubber (CR) with a chemical method to satisfy the durability requirements of waterproofing material in the waterproofing layer of high-speed railway subgrade. A pressure-aging-vessel test for 20, 40 and 80 h were conducted to obtain bitumen samples in different long-term aging conditions. Multiple stress creep recovery (MSCR) tests, linear amplitude scanning tests and bending beam rheometer tests were conducted on three kinds of asphalt binders (SBS modified asphalt, CR modified asphalt and SBS/CR composite modified asphalt) after different long-term aging processes, including high temperature permanent deformation performance, resistance to low temperature thermal and fatigue crack. Meanwhile, aging sensitivities were compared by different rheological indices. Results showed that SBS/CR composite modified asphalt possessed the best properties before and after aging. The elastic property of CR in SBS/CR composite modified asphalt improved the ability to resist low temperature thermal and fatigue cracks at a range of low and middle temperatures. Simultaneously, the copolymer network of SBS and CR significantly improved the elastic response of the asphalt SBS/CR modified asphalt at a range of high temperatures. Furthermore, all test results indicated that the SBS/CR modified asphalt possesses the outstanding ability to anti-aging. SBS/CR is an ideal kind of asphalt to satisfy the demand of 60 years of service life in the subgrade of high speed railway.


Materials ◽  
2021 ◽  
Vol 14 (11) ◽  
pp. 2888
Author(s):  
Sylwia Dziadosz ◽  
Mieczysław Słowik ◽  
Filip Niwczyk ◽  
Marcin Bilski

The paper presents the results of laboratory investigation on asphalt binders relaxation at low temperature, carried out in a ductilometer using the tensile test with continuous force measurement. Polymer modified asphalt binder samples consisting of a 50/70 penetration grade bitumen mixed with a concentrate of styrene-butadiene-styrene (SBS) modified bitumen—a 160/220 penetration grade bitumen modified with a SBS copolymer in the amount of 9%—were tested. Therefore, polymer modified binders containing 3%, 4.5%, 6% and 7.5% SBS, respectively, were obtained and investigated. Tensile tests were performed at −16 °C on samples before aging and subjected to short-term aging (RTFOT). Test results in the form of relaxation curves have been mathematically described using a modified generalized Maxwell model. Based on the acquired results, it was shown that the increase of the SBS copolymer content in asphalt binder precipitates the relaxation process, while aging slows down this phenomenon. It has also been proven that with increased content of SBS elastomer in asphalt binder, the effect of short-term aging on binder’s stress relaxation ability at low temperatures is reduced.


Author(s):  
Yuliya A. Urcheva ◽  
◽  
Vladislav A. Kholodnov ◽  
Alexander M. Syroezhko ◽  
Valentin V. Vasiliev ◽  
...  

The influence of structure of styrene-butadiene-styrene rubber on the quality characteristics of polymer-modified bitumen – produced on its basis – was identified. A program for a compromise assessment of the preference of such polymers using fuzzy sets was developed. A mathematical model was obtained that is recommended for use to optimize production and reduce costs in the industrial production of polymer-modified bitumen.


Polymers ◽  
2021 ◽  
Vol 13 (14) ◽  
pp. 2249
Author(s):  
Bei Chen ◽  
Fuqiang Dong ◽  
Xin Yu ◽  
Changjiang Zheng

In order to solve the problems caused by asphalt diseases and prolong the life cycle of asphalt pavement, many studies on the properties of modified asphalt have been conducted, especially polyurethane (PU) modified asphalt. This study is to replace part of the styrene-butadiene-styrene (SBS) modifier with waste polyurethane (WP), for preparing WP/SBS composite modified asphalt, as well as exploring its properties and microstructure. On this basis, this paper studied the basic performance of WP/SBS composite modified asphalt with a conventional performance test, to analyze the high- and low-temperature rheological properties, permanent deformation resistance and storage stability of WP/SBS composite modified asphalt by dynamic shear rheometer (DSR) and bending beam rheometer (BBR) tests. The microstructure of WP/SBS composite modified asphalt was also observed by fluorescence microscope (FM) and Fourier transform infrared spectroscopy (FTIR), as well as the reaction between WP and asphalt. According to the results of this study, WP can replace SBS as a modifier to prepare WP/SBS composite modified asphalt with good low-temperature resistance, whose high-temperature performance will be lower than that of SBS modified asphalt. After comprehensive consideration, 4% SBS content and 15% WPU content (4 S/15 W) are determined as the suitable types of WPU/SBS composite modified asphalt.


2017 ◽  
Vol 50 (3) ◽  
pp. 241-255 ◽  
Author(s):  
Seyfullah Keyf

In this article, 50/70 penetration grade TUPRAS bitumen was modified. Reactive elastomeric terpolymer (Elvaloy RET; DuPont Company), ethylene vinyl acetate (EVA) and styrene–butadiene–styrene (SBS) polymers were used in bitumen modification. Set hours of the tests were applied to samples taken from the obtained modified bitumen mixture. Varying amount of reactive ethylene terpolymer with weight ratios of 0.5%, 1.0%, 1.5%, 2.0% and 2.5% were introduced to the mixture of raw bitumen with 1.0% SBS and 1.0% EVA. Penetration, penetration index, softening point, ductility and elastic recovery tests were performed with these modified bitumen and raw bitumen. The samples of raw bitumen and modified bitumens of 2.0% Elvaloy RET, 1.0% SBS and 1.0% EVA were investigated by means of IR spectroscopy. The raw bitumen was modified with SBS, EVA and RET, and it was determined that penetration and ductility values were decreased while penetration index, softening point and elastic recovery were increased. The purpose of this study is to research the improving properties of 50/70 penetration grade–modified bitumen used in highways of Turkey. The most important characteristics (such as softening point, penetration and % elastic recovery) of new polymer-modified bitumen (NPMB) containing 2.5% EVA, 1% RET and 1% SBS were compared with eight different types of polymer-modified bitumens in Turkey (TPMB). NPMB provided all required parameters (softening point, penetration and % elastic recovery) for five different types of TPMBs (TPMB 70-16, TPMB 70-22, TPMB 76-16, TPMB 76-22 and TPMB 82-16).