creep exposure
Recently Published Documents


TOTAL DOCUMENTS

37
(FIVE YEARS 10)

H-INDEX

9
(FIVE YEARS 1)

2021 ◽  
Vol 2101 (1) ◽  
pp. 012071
Author(s):  
Soban Muddassir Dar ◽  
Yutao Zhao ◽  
Hengcheng Liao ◽  
Xizhou Kai

Abstract This paper describes the microstructure evolution in a creep aged Al-Cu-Mn alloy using optical microscopy (OM), scanning electron microscopy (SEM) and transmission electron microscopy (TEM). Results show the sub-grains formation and accelerated coarsening of θ′ precipitates in creep aged samples. It is observed that at an applied stress of 50MPa, as the creep temperature increases the average length of θ′ precipitates increases and their aspect ratio first increases then decreases. It is also found that after 100h of creep exposure at 200°C/50MPa, θ′ precipitates have grown to an average length of 279nm; at 225°C/50MPa to an average length of 425nm and at 250°C/50MPa they have grown to an average length of 844nm. Coarsening/growth rate of the precipitates is described by Lifshitz-Slyozov-Wagner (LSW) model.


Author(s):  
Kazuhiro Kimura ◽  
Kota Sawada

Abstract Creep deformation behavior, creep strength property and microstructural evolution during creep exposure were investigated on Super 304H steel for boiler tube. In the high stress and lower temperature regime, creep rupture strength of Super 304H steel is higher than that of SUS304H steel. The slope of stress vs. time to rupture curve of Super 304H steel, however, becomes steeper with increase in creep exposure time and temperature, and the creep rupture strength of Super 304H steel becomes closer to that of SUS304H steel after the tens of thousands of hours at 700°C and above. In the short-term, at 600°C, creep rupture ductility increases with increase in creep rupture life. However, it tends to decrease after showing the maximum value and the creep rupture ductility decreases with increase in temperature. The complex shape of creep rate vs. time curves, with two minima in creep rate, was observed at 600°C. Several type precipitates of niobium carbonitride (Nb(C,N)), Z phase (NbCrN), and copper were observed in Super 304H steel, as well as M23C6 carbide and sigma phase observed in SUS304H steel. The change in slope of stress vs. time to rupture curve is caused by disappearance of precipitation strengthening effect during creep exposure. Accuracy of creep rupture life evaluation was improved by stress range splitting method which takes into accounts of the change in slope of stress vs. time to rupture curves was demonstrated.


Author(s):  
Kazuhiro Kimura ◽  
Kota Sawada

Abstract Creep deformation behavior, creep strength property and microstructural evolution during creep exposure were investigated on Super 304H steel for boiler tube. In the high stress and lower temperature regime, creep rupture strength of Super 304H steel is higher than that of SUS304H steel. The slope of stress vs. time to rupture curve of Super 304H steel, however, becomes steeper with increases in creep exposure time and temperature, and the creep rupture strength of Super 304H steel becomes closer to that of SUS304H steel after the tens of thousands of hours at 700°C (1292°F) and above. In the short-term, at 600°C (1112°F), creep rupture ductility increases with increase in creep rupture life. However, it tends to decrease after showing this maximum value and the creep rupture ductility decreases with increase in temperature. The complex shape of creep rate vs. time curves, with two minima in creep rate, was observed at 600°C (1112°F). Several type precipitates of niobium carbonitride (Nb(C,N)), Z phase (NbCrN), and copper were observed in Super 304H steel, as well as M23C6 carbide and sigma phase observed in SUS304H steel. The change in slope of stress vs. time to rupture curve is caused by disappearance of precipitation strengthening effect during creep exposure. Accuracy of creep rupture life evaluation was improved by stress range splitting method which takes into account the change in slope of stress vs. time to rupture curves was demonstrated.


Metals ◽  
2019 ◽  
Vol 9 (7) ◽  
pp. 800 ◽  
Author(s):  
G. N. Haidemenopoulos ◽  
K. Polychronopoulou ◽  
A. D. Zervaki ◽  
H. Kamoutsi ◽  
S. I. Alkhoori ◽  
...  

An investigation of aging phenomena during creep exposure has been conducted for HP-Nb cast reformer tubes for several exposure conditions. Aging was manifested by carbide precipitation, carbide coarsening, and carbide transformation. The transformation of primary M7C3 to the more stable M23C6 carbide takes place at high exposure temperature (910 °C and above). The primary MC carbides transform to the Ni-Nb silicide or G-phase during creep exposure. The presence of Ti in the steel prevented the transformation of MC carbides to the G-phase. Morphological changes like needle to globular transitions, rounding of carbide edges, and carbide coarsening take place during creep exposure. The room-temperature tensile elongation and ultimate tensile strength are significantly reduced during creep exposure. The above aging phenomena are precursors to creep damage.


2019 ◽  
Vol 28 (5) ◽  
pp. 3076-3093
Author(s):  
Arya Chatterjee ◽  
P. Modak ◽  
K. Barat ◽  
D. Chakrabarti ◽  
R. Mitra