Origin and mechanism of torsion fracture in cold-drawn pearlitic steel wires

2013 ◽  
Vol 48 (16) ◽  
pp. 5528-5535 ◽  
Author(s):  
Xianjun Hu ◽  
Lei Wang ◽  
Feng Fang ◽  
Zhongquan Ma ◽  
Zong-han Xie ◽  
...  
2008 ◽  
Vol 33-37 ◽  
pp. 41-46 ◽  
Author(s):  
Zhi Jia Wang ◽  
Xiao Lei Wu ◽  
You Shi Hong

In this paper, torsion fracture behavior of drawn pearlitic steel wires with different heat treatments was investigated. Samples with different heat treatment conditions were subjected to torsion and tensile tests. The shear strain along the torsion sample after fracture was measured. Fracture surface of wires was examined by Scanning Electron Microscopy. In addition, the method of Differential Scanning Calorimetry was used to characterize the thermodynamic process in the heat treatment. A numerical simulation via finite element method on temperature field evolution for the wire during heat treatment process was performed. The results show that both strain aging and recovery process occur in the material within the temperature range between room temperature and 435 °C. It was shown that the ductility measured by the number of twists drops at short heating times and recovers after further heating in the lead bath of 435 °C. On the other hand, the strength of the wire increases at short heating times and decreases after further heating. The microstructure inhomogeneity due to short period of heat treatment, coupled with the gradient characteristics of shear deformation during torsion, results in localized shear deformation of the wire. In this situation, shear cracks nucleate between lamella and the wire breaks with low number of twists.


Metals ◽  
2021 ◽  
Vol 11 (2) ◽  
pp. 178
Author(s):  
Jin Young Jung ◽  
Kang Suk An ◽  
Pyeong Yeol Park ◽  
Won Jong Nam

The relationship between microstructures and ductility parameters, including reduction of area, elongation to failure, occurrence of delamination, and number of turns to failure in torsion, in hypereutectoid pearlitic steel wires was investigated. The transformed steel wires at 620 °C were successively dry-drawn to drawing strains from 0.40 to 2.38. To examine the effects of hot-dip galvanizing conditions, post-deformation annealing was performed on cold drawn steel wires (ε = 0.99, 1.59, and 2.38) with a different heating time of 30–3600 s at 500 °C in a salt bath. In cold drawn wires, elongation to failure dropped due to the formation of dislocation substructures, decreased slowly due to the increase of dislocation density, and saturated with drawing strain. During annealing, elongation to failure increased due to recovery, and saturated with annealing time. The variation of elongation to failure in cold drawn and annealed steel wires would depend on the distribution of dislocations in lamellar ferrite. The orientation of lamellar cementite and the shape of cementite particles would become an effective factor controlling number of turns to failure in torsion of cold drawn and annealed steel wires. The orientation and shape of lamellar cementite would become microstructural features controlling reduction of area of cold drawn and annealed steel wires. The density of dislocations contributed to reduction of area to some extent.


1997 ◽  
Vol 45 (3) ◽  
pp. 1201-1212 ◽  
Author(s):  
J. Languillaume ◽  
G. Kapelski ◽  
B. Baudelet

2013 ◽  
Vol 132 ◽  
pp. 233-238 ◽  
Author(s):  
Y.J. Li ◽  
P. Choi ◽  
S. Goto ◽  
C. Borchers ◽  
D. Raabe ◽  
...  

Metals ◽  
2020 ◽  
Vol 10 (1) ◽  
pp. 114
Author(s):  
Jesús Toribio ◽  
Viktor Kharin ◽  
Francisco-Javier Ayaso ◽  
Miguel Lorenzo ◽  
Beatriz González ◽  
...  

Prestressing steel wires usually undergo cyclic loading in service. Therefore, it is of interest to analyse certain features of their mechanical behaviour under this type of loading, such as the Bauschinger effect (BE) or the hardening rule, that fit the real mechanical behaviour appropriately. In this study, different samples of high strength pearlitic steel wires were subjected to cyclic tension-compression load exceeding the material yield strength, thus generating plastic strains. From the experimental results, various parameters were obtained revealing that analysed steels exhibited the so-called Masing type BE. In addition, the variation of the BE characteristics (of the effective and internal stresses) with the applied plastic pre-strain indicated that the studied materials followed a mixed strain hardening rule with the domination of the kinematic component.


2011 ◽  
Vol 211 (1) ◽  
pp. 103-112 ◽  
Author(s):  
T. Massé ◽  
Y. Chastel ◽  
P. Montmitonnet ◽  
C. Bobadilla ◽  
N. Persem ◽  
...  