Colouration mechanism of underglaze copper-red decoration porcelain (AD 13th–14th century), China

2014 ◽  
Vol 21 (4) ◽  
pp. 751-755 ◽  
Author(s):  
Jian Zhu ◽  
Huiping Duan ◽  
Yimin Yang ◽  
Li Guan ◽  
Wei Xu ◽  
...  

Underglaze copper-red decoration,i.e.the copper colourant used to paint diversified patterns on the surface of a body and then covered by transparent glaze and fired at high temperature in a reductive firing environment, is famous all over the world. However, the red colouration mechanism generated by underglaze copper remains unclear. In particular, the fact that the edges of the red patterns are orange has been ignored in previous research. Here, non-destructive analysis has been carried out on a precious fragment of early underglaze red porcelain using synchrotron radiation X-ray fluorescence, X-ray absorption near-edge spectroscopy (XANES) and reflection spectrometry techniques. The results suggest that the copper content in the red region is higher than that in the orange region, and other colour generation elements do not have obvious content difference, indicating that the colour generation effect of the underglaze red product is related to the copper content. XANES analysis shows that the valence states of copper in the red and orange regions are similar and metal copper contributes to their hues. The results of reflection spectrometry demonstrate that tiny orange hues could be attributed to the Mie scatting effect. Therefore, light-scattering effects should be considered when researching the colouration mechanism of underglaze red.

1991 ◽  
Vol 240 ◽  
Author(s):  
F. Uchida ◽  
J. Shigeta ◽  
Y. SUZUKI

ABSTRACTA non-destructive characterization technique featuring a hard X-ray Microprobe is demonstrated for lll-V semiconductor device structures. A GaAs FET with a 2 μm gate length is measured as a model sample of a thin film structure. X-ray scanning microscopic images of the FET are obtained by diffracted X-ray and fluorescence X-ray detection. Diffracted X-ray detection measures the difference in gate material and source or drain material as a gray level difference on the image due to the X-ray absorption ratio. Ni Ka fluorescence detection, on the other hand, provides imaging of 500 Å thick Ni layers, which are contained only in the source and drain metals, through non-destructive observation.


1990 ◽  
Vol 187 ◽  
Author(s):  
H. Watabe ◽  
M. Iwami ◽  
M. Hirai ◽  
M. Kusaka ◽  
M. Kubota ◽  
...  

AbstractSpectra obtained by a new soft x-ray emission spectroscopy(SXES) apparatus again exhibited clear differences among Si-compounds and Si crystal. A non-destructive analysis of an annealed transition metal(TMSi:film)/Si(111) contact system was carried out using either the distinct differences of Si L2, 3 SXES spectra between TMSi's and Si single crystals or the fad that the soft x-ray production depth increases in a solid with the energy of the primary electron, Ep. It was shown that the apparatus was capable of exploring electronic and atomic structures of a multi-layered contact system grown on a Si(111) substrate.


2012 ◽  
Vol 512-515 ◽  
pp. 1434-1437
Author(s):  
Xing Ao Li ◽  
Peng Li ◽  
Yong Tao Li ◽  
Jian Ping Yang ◽  
Qiu Fei Bai ◽  
...  

Bi0.95Eu0.05Fe0.95Co0.05O3 Nanoparticles sample was prepared by sol-gel process. The microstructure of samples was analysised by X-ray diffraction(XRD), the result indicated that it was the single phase rhombohedral perovskite structure. The morphology of samples was measured by scanning electron microsopy(SEM), the SEM photograph of samples indicated that the nanoparticles of Bi0.95Eu0.05Fe0.95Co0.05O3 sample were small than that of BiFeO3. The valence states of Fe ions in the samples was analysised by the X-ray absorption spectroscopy(XAS). The XAS of Fe2p showed that it was the mixed valence states (Fe2+ and Fe3+) of Fe ions in samples, and the binding energy of Bi0.95Eu0.05Fe0.95Co0.05O3 was bigger than that of BiFeO3.The magnetic characteristics of the samples were measured by vibrating sample magnetometer (VSM),the results showed that the weak metamagnetism were obtained from clear hysteresis loop and the magnetic saturation reached 0.408emu/g,compared with BiFeO3 sample, the magnetic properties were significantly enhanced.


1987 ◽  
Vol 36 (12) ◽  
pp. 6426-6433 ◽  
Author(s):  
A. Bianconi ◽  
A. Di Cicco ◽  
N. V. Pavel ◽  
M. Benfatto ◽  
A. Marcelli ◽  
...  

Sign in / Sign up

Export Citation Format

Share Document