A Simple Method For The Determination of Thickness and Grain Size of Deposited Films as Used On Non-Conductive Specimens For Scanning Electron Microscopy

1978 ◽  
Vol 112 (3) ◽  
pp. 359-364 ◽  
Author(s):  
Jakob Røli ◽  
Per R. Flood
2021 ◽  
Author(s):  
Rowan Mclachlan ◽  
Ashruti Patel ◽  
Andrea G Grottoli

Coral morphology is influenced by genetics, the environment, or the interaction of both, and thus is highly variable. This protocol outlines a non-destructive and relatively simple method for measuring Scleractinian coral sub-corallite skeletal structures (such as the septa length, theca thickness, and corallite diameter, etc.) using digital images produced as a result of digital microscopy or from scanning electron microscopy. This method uses X and Y coordinates of points placed onto photomicrographs to automatically calculate the length and/or diameter of a variety of sub-corallite skeletal structures in the Scleractinian coral Porites lobata. However, this protocol can be easily adapted for other coral species - the only difference may be the specific skeletal structures that are measured (for example, not all coral species have a pronounced columella or pali, or even circular corallites). This protocol is adapted from the methods described in Forsman et al. (2015) & Tisthammer et al. (2018). There are 4 steps to this protocol: 1) Removal of Organic Tissue from Coral Skeletons 2) Imaging of Coral Skeletons 3) Photomicrograph Image Analysis 4) Calculation of Corallite Microstructure Size This protocol was written by Dr. Rowan McLachlan and was reviewed by Ashruti Patel and Dr. Andréa Grottoli. Acknowledgments Leica DMS 1000 and Scanning Electron Microscopy photomicrographs used in this protocol were acquired at the Subsurface Energy Materials Characterization and Analysis Laboratory (SEMCAL), School of Earth Sciences at The Ohio State University, Ohio, USA. I would like to thank Dr. Julie Sheets, Dr. Sue Welch, and Dr. David Cole for training me on the use of these instruments.


2012 ◽  
Vol 496 ◽  
pp. 379-382
Author(s):  
Rui Song Yang ◽  
Ming Tian Li ◽  
Chun Hai Liu ◽  
Xue Jun Cui ◽  
Yong Zhong Jin

The Cu0.81Ni0.19 has been synthesized directly from elemental powder of nickel and copper by mechanical alloying. The alloyed Cu0.81Ni0.19 alloy powders are prepared by milling of 8h. The grain size calculated by Scherrer equation of the NiCu alloy decreased with the increasing of milling time. The end-product was analyzed by X-ray diffraction (XRD), scanning electron microscopy (SEM)


2013 ◽  
Vol 12 (4) ◽  
pp. 095-105
Author(s):  
Beata Klimek

One of the main tasks in the study of historic buildings is the need to identify the original materials and extensions, which often have historic character. The next task concerns the determination of the composition and structure of the historical, diagnosis technique to develop original paint. The article presents the preliminary results of paintings. Methods were used with the scanning electron microscope was equipped with an energy dispersive X-ray spectrometer (SEM-EDS).


2019 ◽  
Vol 64 (3) ◽  
pp. 418-421 ◽  
Author(s):  
A. I. Lihachev ◽  
A. V. Nashchekin ◽  
R. V. Sokolov ◽  
S. G. Konnikov

2018 ◽  
Vol 281 ◽  
pp. 156-162
Author(s):  
Wang Nian Zhang ◽  
Xi Tang Wang ◽  
Zhou Fu Wang

The influence of the light burning temperature on the sintering property of nature dolomite has been investigated by two-step sintering process in the temperature range 1500 °C to 1600 °C. The resulting bulk densities and apparent porosities of the sintered dolomite samples were examined, and analyzing the sintered dolomite by scanning electron microscopy and X-ray diffraction were performed. The results showed light burned at 850 °C for 3 h, the main phases of the dolomite with 3-5 grain size were MgO, CaO and little CaCO3, and then fired at 1600 °C,the density of sintering dolomite reached to 3.38 g/cm3, the apparent property was 1.2 %, the size of MgO grain up to 3.75 μm . However when dolomite light burned at 1050 °C for 3 h, the main phases were MgO and CaO, and then fired at 1600 °C,the density of sintering dolomite only was 3.30 g/cm3, the apparent property was 2.3 %, the size of MgO only was 3.05 μm .


2013 ◽  
Vol 850-851 ◽  
pp. 1309-1312
Author(s):  
Yu Zhou ◽  
Quan Yu ◽  
Wei Hang ◽  
Yu Zhong Wang ◽  
Hui Pin Wang ◽  
...  

In order to investigate the diatom distribution in the five lakes along the Yangtze River, and discuss the significance for the diagnosis of drowning. 6 water samples were collected in the five lakes along Yangtze River in June, 2012. Subsequently, The genus and the quantity of the diatoms in the water samples were investigated using scanning electron microscopy (SEM). The result showed us that there was significant difference between the waters sampled from the different sites . These data on diatom distribution are helpful to the diagnosis of the cause of the death as well as to the determination of the drowning site in cases of drowning. Therefore, it is necessary to develop the database of diatoms in more extensive water bodies for the forensic diagnosis of drowning in the future.


2011 ◽  
Vol 686 ◽  
pp. 348-354 ◽  
Author(s):  
Shu Tao Xiong ◽  
Fu Sheng Pan ◽  
Bin Jiang ◽  
Xiao Ke Li

In the present work, Al-Ca metallic compound was prepared in Mg-Ca alloys and the effects of Al-Ca metallic compound and different Al/Ca values on the grain refinement of Mg-Ca alloys were investigated by scanning electron microscopy and X-ray diffraction, and the mechanism of grain refinement of Mg-Ca alloys was discussed. The results showed that the grain size of Mg-0.5Ca alloy was obviously reduced from 550μm to 230μm due to the addition of Al. Al2Ca phase existed in these alloys and its morphology evolved from granular to rod-like. It is regarded as the main factor for the grain refinement.