Development of a combined processing technology for low-sulfide gold-bearing ores

2021 ◽  
pp. 3-8
Author(s):  
A. K. Koyzhanova ◽  
B. K. Kenzhaliev ◽  
D. R. Magomedov ◽  
N. N. Abdyldaev

This paper presents the results of laboratory dressability studies for low-sulfide gold-bearing ores using combined processing and subsequent oxidation leaching of the resulting combined concentrate. According to the current raw materials processing circuit used at the Sekisovskoye deposit, gravity concentration experiments were first carried out using the following laboratory equipment: a Knelson KSMD 3 centrifugal concentrator, an SKO-05 concentration table, and a two-chamber diaphragm jigging machine (i.e., OML by TsNIGRI). A significant portion (0.5 to 1.0 g/t) of the gold remains in the gravity concentration tailings. Subsequent flotation experiments for the tailings suggest that additional gold recovery is possible. The gold content in the final flotation tailings was in the range of 0.15–0.25 g/t. The final gold recovery in the combined process was therefore 93.7–96.5 %. The subsequent sorption cyanidation of the concentrate according to the current processing circuit allows depositing an average of 75.0–80.0 % Au on the coal. At the same time, the residual gold content in the sorption leaching tailings is significant and amounts to 3.6–7.5 g/t. The preliminary oxidation experiments for the concentrate slurry indicate the possibility of a more complete gold recovery with subsequent leaching, including sorption leaching. The residual gold content in the cakes was measured at 0.7–1.5 g/t, which ultimately yielded 95–96 % recovery at the leaching stage. The research was completed with the financial support of the Science Committee of the Ministry of Education and Science of the Republic of Kazakhstan under grant No. АР05130143.

Author(s):  
P. K. Fedotov ◽  
A. E. Senchenko ◽  
K. V. Fedotov ◽  
A. E. Burdonov

The paper focuses on the study of the gold-bearing ore dressability. According to technological research, the average gold content is 11.88 g/t. The silver content is insignificant – 2.43 g/t. Main ore minerals in the sample are pyrite and pyrrhotite. According to mineralogical and X-ray structural analysis, the average content of these minerals in the ore is about 6 % (in total). Main rock-forming minerals of the original ore are: quartz (60.1 %), quartz-chlorite-mica aggregates (3.8 %), carbonates (7.1 %). According to the study results, it was found that the gold recovery in the GRG test was 72.75 % with a total concentrate yield of 1.34 % and a content of 664.78 g/t. At the same time, the gold content in tailings was 3.29 g/t. A stage test showed that it is advisable to use a two-stage scheme for ore processing by gravity technology only. The first stage is in the grinding cycle with the 60–70 % ore size, and the second stage is with the final classifier overflow size of 90 % –0.071 mm. Centrifugal separation has high performance as a free gold recovery operation in the grinding cycle. A concentrate with a gold content of 2426 g/t was obtained with a yield of 0.31 % and a recovery of 63.74 %. The beneficiation of first stage tailings ground to 90 % –0.071 mm at the KC-CVD concentrator (modeling) made it possible to extract gold into a total gravity concentrate (KC-MD + KC-CVD) of 87.25 % with a concentrate yield of 22.63 %. The gold content in tailings was 1.97 g/t. The results of gravity and flotation concentration of the original ore indicate the feasibility of using a combined gravity-flotation technological scheme. In a closed experiment of the initial ore beneficiation according to the gravity-flotation scheme at a natural pH of the pulp (without adding acid), the following products were obtained: gravity concentrate with a gold content of 2426 g/t at a yield of 0.31 % and recovery of 64.06 %; flotation concentrate (after the II cleaning) with a gold content of 122 g/t at a yield of 2.90 % and recovery of 33.01 %; the total gold recovery in the gravity-flotation concentrate was 94.07 % with a yield of 3.21 % and an Au content of 345.87 g/t, the gold content in the flotation tailings was 0.72 g/t.


2021 ◽  
Vol 27 (4) ◽  
pp. 45-54
Author(s):  
G. Yurgenson ◽  
◽  
L. Shumilova ◽  
А. Khatkova ◽  
◽  
...  

The relevance of the research is the need to recultivate the waste from the enrichment of gold-bearing ores that lie in the immediate vicinity of the residential areas of Baley city, which have a negative impact on the environmental situation in it, as well as to develop a technological approach to the extraction of gold and silver. The purpose of the study is to study the material composition and develop a technology for extracting precious metals. The object of the study is the stale tailings of the ZIF-1 plant “Baleizoloto”. The subject of the study is mineral composition of stale tailings, content of useful components and their extraction technology, the method and methodology presented by mineralogical and chemical analyses of enrichment tailings. Results. The analysis of the tailings dumps’ state of the gold recovery factories of the Baleizoloto plant was carried out. The contents of gold and other chemical elements, among which arsenic, zinc, copper, antimony, and lead predominate, were determined. The gold content prevails in the stale tailings of the ZIF-1 factory, which processed the ores of the Baley deposit, and is in the range of 1.09-1.37 g / t, on average – 1.17 g/t. This determines the prospects for their primary processing. The gold in the clay-sand fraction of the stale tailings is mainly found in thin accretions with quartz, carbonates, pyrite, arsenopyrite, sulfosols, and tellurides. The field of application is processing of technogenic raw materials. Conclusions. It was determined that the sizes of gold inclusions are in the range of 0.7-0.03 mm, the gold penetration varies from 63 to 91.15, and on average is 82.13; the main impurity in gold is silver with a content of 8.85-37%; the average silver content in the tailings of the ZIF-1 factory is 1.85 g/t; the recommended technological scheme for processing stale tailings of ZIF-1 of the Baleizoloto plant has been developed, including the following operations: photoelectron-activation preparation, pelletizing with active solution, heap leaching, two-stage sorption with bubbling with ozone


2021 ◽  
pp. 24-28
Author(s):  
Зоя Алиевна Яралиева

Климатические условия на большей части территории Российской Федерации не позволяют выращивать виноград в открытом грунте, поэтому его завозят из южных районов страны. Производство виноградных напитков обычно сосредоточено в местах выращивания винограда, так как доставка готовой продукции в северные регионы сопряжена со значительными финансовыми затратами. В Республике Дагестан выращивают около 30% винограда в масштабах всей страны, а площадь плодоносящих виноградников занимает более 20 тыс. га. Возникла необходимость переработать виноград таким образом, чтобы полуфабрикат для изготовления напитков выдерживал длительные сроки хранения и транспортировку, отличался высоким качеством и имел небольшую массу. Разработана технология получения виноградных криопорошков, которые можно использовать в качестве пищевых добавок, для изготовления восстановленных соков и напитков. Целью исследования было создание инновационной технологии производства криопорошков для получения безалкогольных напитков. Объектом исследования стал виноград дагестанских технических, столовых и изюмных сортов. Алгоритм получения криопорошков соответствовал предложенной автором схеме: доставка винограда, отделение гребней, инспекция, мойка, дробление, замораживание жидким азотом, обезвоживание в вакуумной СВЧ-установке, криоизмельчение и фасовка. При выполнении работы определяли качественный состав сырья и криопорошков с использованием аналитических приборов и лабораторного оборудования кафедры технологии продуктов питания и учреждений Дагестанского научного Центра РАН. Определен химический состав криопорошков, полученных из винограда, выращенного в горно-долинной зоне Дагестана. Приведены физико-химические показатели напитка из криопорошка винограда. Органолептические показатели изготовленных виноградных напитков подтвердили их высокие качественные показатели. Climatic conditions in most of the Russian Federation do not allow growing grapes in the open field, therefore they are imported from the southern regions of the country. The production of grape drinks is usually concentrated in places where grapes are grown, since the delivery of finished products to the northern regions is associated with significant financial costs. Winegrowers of the Republic of Dagestan grow about 30% of grapes throughout the country, and the area of fruit-bearing vineyards occupies more than 20 thousand hectares. There was a problem to process grapes in such a way that the semi-finished product for the production of drinks withstands long storage and transportation periods, is of high quality and has a small weight. A technology has been developed for producing grape cryopowders, which can be used as food additives, for the production of reconstituted juices and drinks. The aim of the study was to create an innovative technology for the production of cryopowders for the production of soft drinks. The objects of the study were Dagestan common and raisin grapes. The algorithm for obtaining cryopowders corresponded to the scheme proposed by the author: delivery of grapes, separation of ridges, inspection, washing, crushing, freezing with liquid nitrogen, dehydration in a vacuum microwave unit, cryo-grinding and packaging. When performing the work, the qualitative composition of raw materials and cryopowders was determined using analytical instruments and laboratory equipment of the Department of Food Technology and institutions of the Dagestan Scientific Center of the Russian Academy of Sciences. The chemical composition of cryopowders obtained from grapes grown in the mountain-valley zone of Dagestan has been determined. The physical and chemical parameters of a wine drink made from grape cryopowder are given. The organoleptic characteristics of the produced wine drinks confirmed their high quality indicators.


2021 ◽  
Vol 43 (4) ◽  
pp. 458-466
Author(s):  
S. A. Prokopiev ◽  
E. S. Prokopiev ◽  
I. V. Kadesnikov ◽  
N. A. Cherimichkina

The purpose of this article is to conduct industrial tests of spiral separation technology on technogenic refractory raw materials. The object of the study is the Yurskoye gold placer deposit in the Republic of Sakha (Yakutia). An OKV-100 benefication complex with the productive capacity of 100 m3 /h by initial sands was set up in order to conduct pilot mining of the fine-grained tailings dumps of the Yurskoye deposit with the maximum extraction of small size gold. Sands supplied from the different sections of the technogenic deposit had different gold content, granulometric characteristics, and mineralogical composition. The study included experiments carried out at different initial feed; equipment was adjusted for specific raw material depending on productive capacity, liquid/solid ratio, product yield of the small size gold recovery module. The complex productivity was from 90 to 150 m3 /h. The yield and extraction of gold-bearing concentrate, as well as its gold content were determined. The pilot washing with the use of small size gold recovery technology resulted in the average additional gold recovery from sluice tailings of 19.07 %, which is a high indicator, given the low content of gold in technogenic placers. The technology under consideration can be used for the development of both technogenic and operated gold placer deposits.


2021 ◽  
Vol 13 (1) ◽  
pp. 84-93
Author(s):  
Sergey EVDOKIMOV ◽  
◽  
Tatyana GERASIMENKO ◽  
Azamat MARZOEV ◽  
◽  
...  

Increasing the economic efficiency of enrichment of refractory gold-bearing ores is possible by reducing the cost of opening sulphide gold-bearing concentrates by reducing the yield of flotation concentrate sent to pyro- or hydrometallurgical processing. It is important to maintain the achieved level of gold recovery into concentrate with a lower concentrate yield. In order to achieve this goal, the gold content in the main flotation operation is increased by mixing the rough concentrate separated from ½ part of the ore feed with another ½ part of it. Mixing in the flotation operation of products with a high level of wash ability (ability to separate) – initial feed and rough concentrate – is identical to an increase in the content of the extractable component in the original ore. In accordance with the new regime of flotation, the process is carried out in cold slurry with bubbles filled with hot steam. The physical basis of the new flotation regime is the dependence of the surface properties of air bubbles and surface forces that determine the stability of the liquid film separating the bubble and the particle on the temperature, which increases due to the heat of the vapor-liquid phase transition. Radial oscillations of the bubble surface as a result of pressure pulsations during condensation and vapor evaporation and surface thermal flows of liquid in the wetting film are factors that provide an increase in the completeness of gold recovery and the selectivity of flotation adhesion obtained in ore flotation experiments. In laboratory conditions, a comparison was made of the indicators obtained during the dressing of gold-bearing ores according to the factory and new schemes. It was revealed that the use of the developed technology allows, with a lower concentrate yield, to obtain an increase of 7.06% abs. extraction of gold into a concentrate of the best quality. A decrease in gold losses with flotation tailings is a consequence of an increase in the number of particles reaching the bubble surface due to radial oscillations of its surface and a weakening of the stability of the wetting film by the thermo-capillary mechanism. An increase in adhesion selectivity can be interpreted using the concept of surface forces of structural origin – an increase in the forces of hydrophobic attraction and hydrophilic repulsion with increasing temperature. The interaction of vapor bubbles with nanobubbles on the surface of the solid phase (wetting by the Cassie-Baxter mechanism) ensures efficient particle recovery by the coalescence mechanism of flotation.


2020 ◽  
Vol 168 ◽  
pp. 00004
Author(s):  
Gulzhan Askarova ◽  
Mels Shautenov ◽  
Kulzhamal Nogaeva

The aim of the research is the selection and justification of the combined gravity method of enrichment of refractory gold-bearing raw materials and the hydro and pyrometallurgical method of processing enrichment products based on the study of the technological properties of the feedstock and enrichment products in the mineral and raw materials complex of the deposit located on the territory of the Republic of Kazakhstan. There is a tendency to increase the imbalance between mining and also the increase in off-balance reserves of gold-bearing ores, which ultimately poses a serious problem for the development of the country’s economy. Research on the development of technology for the extraction of gold from refractory ores has been performed on three samples of the Vasilkovsky stockwork deposit. The ores are persistent in the presence of arsenic (arsenopyrite) and finely divided gold, a significant part of which is in the form associated with both sulfides (mainly arsenopyrite) and rockforming minerals.


2020 ◽  
pp. 25-30
Author(s):  
Ye. K. Yessengarayev ◽  
B. S. Baimbetov ◽  
B. N. Surimbayev

One of the cheapest methods of extracting gold is heap leaching. However, the recovery of gold by this method is relatively low, compared with cyanidation of the crushed material, so the search for the ways to intensify leaching and increase gold recovery is an urgent task. Investigations on heap leaching of gold from the gold-bearing ore of the Sari Gunay deposit were conducted using a promising reagent sodium acetate to intensify the heap leaching process. The results of assay-gravimetric, chemical, mineralogical and granulometric analyses of oxidized ore are presented. The average gold content in the ore was 2.90 g/t. According to the electron probe analysis, gold in the ore is present in the form of fine (micron) inclusions in minerals and ore rocks. Comparative studies on heap leaching of gold from the crushed ore with a grain size of –20 + 0 mm with the addition of sodium acetate and without that were carried out. The degree of gold recovery with sodium acetate at a flow rate of 0.5 kg/t was 58.74%, that without sodium acetate was 54.69%, i.e. the addition of the reagent provides an increase in recovery of more than 4%. Leaching with the addition of the reagent also reduces sodium cyanide consumption from 0.65 to 0.59 kg/t. The research results have shown that sodium acetate can be used to intensify the process of heap leaching of gold when the ore size is –20+0 mm.


Author(s):  
Гаруш Александрович Самвелян ◽  
Агнесса Гарушевна Самвелян ◽  
Арман Эмилевич Манукян ◽  
Нуне Рубеновна Симонян ◽  
Гор Маркосович Аветисян ◽  
...  

Возросший интерес к винам из стран, считающихся родиной виноделия (Армения, Грузия, Греция, Румыния), связан со своеобразием ароматов и вкусов, обусловленных местными традиционными сортами винограда. Однако сортовой состав автохтонного винограда, используемый в производстве вин в Армении, весьма ограничен. Нами поставлена цель выявить и изучить перспективность малораспространенных, забытых аборигенных армянских сортов винограда для производства высококачественных вин. Актуальность работы связана с увеличением сырьевых ресурсов виноградовинодельческой отрасли республики. Для исследования были выбраны аборигенные красные сорта Тозот, Кохбени, Арени (контроль) из двух регионов Армении. Опытные виноматериалы были приготовлены в условиях микровиноделия. Двухлетние изучения технохимических показателей и органолептическая оценка опытных образцов выявили перспективность использования красных (Тозот и Кохбени) сортов автохтонного винограда в качестве сырья для производства вин высокого качества в разных регионах Армении. Recent years the increased interest in wines from countries considered to be the birthplace of winemaking (Armenia, Georgia, Greece, Romania) is associated with the uniqueness of aroma and flavor of the local traditional grape varieties. However, the variety assortment of autochthonous grapes used in wine production in Armenia is very limited. Our goal is to find out and study the prospects of less common autochthonous Armenian grape varieties for the high quality wine production. The relevance of this work is associated with the increase in the amount of raw materials of the viticultural and winemaking industry of the Republic. Red autochthonous grape varieties 'Tozot', 'Koghbeni', 'Areni' (as the control) from two regions of Armenia were selected for the research. Experimental base wines were produced in the conditions of microvinification. A two-year research of technochemical indicators and organoleptic assessment of experimental samples revealed the potential of using local red varieties ('Tozot' and 'Koghbeni') as raw materials for the high quality wine production in different regions of Armenia. The research was carried out with the financial support of State Science Committee of the Ministry of Education and Science of the Republic of Armenia within the framework of scientific project No. 18T-2K024.


2018 ◽  
pp. 33-37 ◽  
Author(s):  
N. K. Algebraistova ◽  
◽  
P. N. Samorodskiy ◽  
D. M. Kolotushkin ◽  
I. V. Prokopyev ◽  
...  

2021 ◽  
Vol 1 (7) ◽  
pp. 35-44
Author(s):  
Sergei I. Evdokimov ◽  
◽  
Tatiana E. Gerasimenko ◽  

Research objective is to address an up to date task of developing the technology of associated gold recovery from complex ore. Object of research is the gold-bearing copper-pyrite ore. Gold was recovered in laboratory conditions with the use of gravity methods of mineral separation. Research tools. Rational modes of machinery operation have been determined through mathematical planning of experiments including the obtained results processing by mathematical and statistical methods. Methods of research. Gold was recovered in the grinding-classification circuit based on a seriesinstalled short-cone hydrocyclone, a jigging machine and a shaking table. Research results. The developed jig mode differs from the existing ones by the closed-circuit of jig machine chambers: from the feed of the second (in the direction of the light fraction travel) jig chamber, the light fraction (tailings) and undersize product – fraction with the increased content of accessory minerals (rough concentrate) are separated. The rough concentrate in the second chamber is directed to the first chamber of the machine, where the finished jig concentrate is obtained in the form of an undersize product. The light fraction moves from the first chamber to the second and is removed from the machine through the tail board. When fine-tuning the heavy fraction of jigging on a shaking table, it is recommended to mix 1/2 part of the initial feed of the tables with the rough concentrate isolated from the other 1/2 of the original feed. The new jigging mode and the scheme of concentration on the tables provide an increase in the gold content in the initial feed of the apparatus, which is the reason for a decrease in gold losses with the tails of the gravity circuit. Research relevance. Gold recovery increment by 4.77% was obtained due to the use of all three recommended scientific and technical measures, namely sands concentration in a short head cone crusher on a jig, switching the jig chambers to a closed circuit, and jet motion of concentrates on shaking tables. Scope of the results. The results should be applied when concentrating ore containing free (amalgamable) gold, as well as gold-bearing pyrite.