scholarly journals Five-year Clinical Evaluation of a Nanofilled and a Nanohybrid Composite in Class IV Cavities

2018 ◽  
Vol 43 (3) ◽  
pp. 261-271 ◽  
Author(s):  
M Demirci ◽  
S Tuncer ◽  
HS Sancakli ◽  
N Tekçe ◽  
C Baydemir

SUMMARY The purpose of this study was to evaluate a nanofilled and a nanohybrid composite, in combination with manufacturer-recommended etch-and-rinse adhesives, in class IV cavities. Thirty-four patients aged 14-46 years (mean age, 27.1 years) comprised the study group. Twenty-six patients received two class IV restorations and eight patients received four class IV restorations. For each patient, half the number of restorations were performed using a nanohybrid composite (Ceram X duo) and the remaining half used a nanofilled resin composite (Filtek Supreme XT), with two- (XP Bond) and three-step (Scotchbond Multipurpose) etch-and-rinse adhesives, respectively. Two experienced examiners evaluated the restorations for retention, color match, marginal discoloration, wear/loss of anatomic form, caries formation, marginal adaptation, and surface texture to compare the baseline (after placement) and annual recalls over 5 years. The cumulative success rates for the Filtek Supreme XT and Ceram X duo restorations after five years were 86.2% and 89.7%, respectively. Four Filtek Supreme XT and three Ceram X duo restorations failed. There was no statistically significant difference between the nanofilled and nanohybrid composites at any of the evaluation periods for any of the parameters evaluated. Despite the limited number of restorations, all restorations were clinically acceptable regarding retention, color match, marginal discoloration, wear or loss of anatomic form, the formation of caries, marginal adaptation, and surface texture, except the failed restorations. Fracture was the main cause of restoration failure.

2020 ◽  
Vol 45 (5) ◽  
pp. 473-483 ◽  
Author(s):  
CAGA Costa ◽  
NLG Albuquerque ◽  
JS Mendonça ◽  
AD Loguercio ◽  
VPA Saboia ◽  
...  

Clinical Relevance At 24 months, the dentin pretreatment with epigallocatechin-3-gallate did not impair the clinical performance of the adhesive Single Bond Universal regardless of the bonding strategy used. SUMMARY Purpose: To evaluate the two-year effect of dentin pretreatment with epigallocatechin-3-gallate (EGCG) on the clinical performance of restorations of noncarious cervical lesions (NCCLs) with Single Bond Universal, applied in two different modes (self-etch and etch-and-rinse). Methods and Materials: In this randomized clinical trial, 33 volunteers were selected, and 156 NCCLs were assigned to four groups: ER, etch-and-rinse; ER-EGCG, 0.1% EGCG dentin pretreatment + etch-and-rinse; SE, self-etch; and SE-EGCG, 0.1% EGCG dentin pretreatment + self-etch. The NCCLs were restored with a nanofilled resin composite and evaluated at baseline and at six, 12, 18, and 24 months using FDI criteria for retention, marginal staining, marginal adaptation, caries, and postoperative sensitivity. Two evaluators were blinded to the treatments performed, and impressions were taken for resin replicas to allow indirect observations. Statistical analyses were performed with Kruskal-Wallis and McNemar tests with a significance level of 5%. Results: Six restorations (one from ER, two from SE, one from ER-EGCG, and two from SEEGCG) were lost at 24 months with no significant differences (p>0.05). The retention rates were 97.0% (ER and ER-EGCG), 94.1% (SE), and 94.2% (SE-EGCG). For marginal adaptation, a significant difference was detected between the baseline and 24 months for the SE group (p=0.0313). There were no statistical differences among all other evaluated criteria at 24 months, neither for each group at baseline nor for 24-month comparisons (p>0.05). Conclusions: The pretreatment with EGCG provided no benefit in the clinical performance of the adhesive regardless of the bonding strategy used. In addition, it adds an additional required step to the restorative procedure.


2020 ◽  
Author(s):  
Sumer M Alaki ◽  
Bashaer S Abdulhadi ◽  
Medhat A AbdelBaki ◽  
Najla M Al-Alamoudi

Abstract Background: Providing restorations to anterior teeth in children is a challenging task due to the need for high esthetics, strength, and durability. This study was done to compare prefabricated primary zirconia with resin composite strip crowns on primary maxillary central and lateral incisors with regards to gingival health, plaque accumulation, recurrent caries, restoration failure, and opposing teeth wear over a period of 3, 6 and 12 months. Methods: Children attending the King Abdulaziz University, Faculty of Dentistry (KAUFD) clinics who needed restorations were screened for inclusion criteria. A total of 120 teeth were treated; 60 with zirconia and 60 with strip crowns. Randomization was done by simple random allocation using SPSS software version 20.0 (Armonk, NY; IBM Corp.). A simple descriptive statistic was used for analysis by Wilcoxon Signed-Rank test and Chi-square test. Level of significance was set at (α = 0.05) and level of confidence at (95%). The presented research was registered retrospectively at ClinicalTrials.gov in 6th of August 2017, under registration number NCT03184012.Results: Zirconia crowns showed significantly less gingival bleeding at the 3- and 6-months follow up periods (p<0.006, p<0.001; respectively), less plaque accumulation at all follow up visits (p<0.001), no restoration failure (p<0.001), but more wear to opposing teeth (p<0.02). No significant difference was found between the two crowns with regards to recurrent caries (p<0.135).Conclusion: Based on our data we conclude that overtime teeth covered with zirconia crowns show better gingival health and less bleeding, plaque accumulation as well as less loss of material. On the other hand, zirconia can cause more loss of opposing tooth structure.


2009 ◽  
Vol 10 (4) ◽  
pp. 17-25 ◽  
Author(s):  
Andre Figueiredo Reis ◽  
Flávio Henrique Baggio Aguiar ◽  
Marcelo Giannini ◽  
Patricia Nóbrega Rodrigues Pereira

Abstract Aim The aim of this study was to assess the influence of surface texture and etching technique on surface roughness (Ra) and bond strength (BS) to enamel and to determine if a correlation exists between them. Methods and Materials Fifty enamel blocks were either roughened with 600-grit SiC paper or polished with diamond pastes. After establishing ten test groups (n=5), the initial Ra measurements, rough (R) and smooth (S) enamel surfaces were etched according to the following protocols: Group 1(R)/Group 2(S)- 35% phosphoric acid gel (H3PO4) for 15 seconds; Group 3(R)/Group 4(S)- 35% H3PO4 for 60 seconds; Group 5(R)/Group 6(S)- Clearfil SE Bond primer for 20 seconds; Group 7(R)/Group 8(S)- self-etching primer (SEP) for 60 seconds; Group 9(R)/ Group 10(S)- 35% H3PO4 for 15 seconds + SEP for 20 seconds. After treatments, a new Ra measurement was performed and enamel surfaces were bonded with either Single Bond (Group 1 to Group 4) or Clearfil SE Bond (Group 5 to Group 10). Afterwards, specimens were prepared for the microtensile test. Ra values were analyzed using repeated-measures analysis of variance (ANOVA) and the BS values were analyzed using a two-way ANOVA and Tukey test (5%). Correlation between BS and Ra values was assessed using the Pearson's test. Results The application of SEP produced the lowest Ra values. No significant difference was detected between the BS values of polished and rough surfaces. No correlation was observed between Ra and BS values. Even though etching enamel with the SEP resulted in a surface with less roughness, similar BS values were observed for both self-etching and etch-and-rinse techniques. Conclusion Within the limits of this study increasing the etching time or combining both etching techniques failed to improve the BS using SEP or etch-and-rinse systems. Clinical Significance Based on the findings of this study, there is no clinical justification for increasing the etching time or for combining the use of a SEP following the use of a 35% H3PO4 etchant to achieve a greater BS to ground enamel. Citation Reis AF, Aguiar FHB, Pereira PNR, Giannini M. Effects of Surface Texture and Etching Time on Roughness and Bond Strength to Ground Enamel. J Contemp Dent Pract 2009 July; (10)4:017-025.


2021 ◽  
Vol 20 ◽  
pp. e213981
Author(s):  
Fariba Motevasselian ◽  
Hamid Kermanshah ◽  
Ebrahim Rasoulkhani ◽  
Mutlu Özcan

Aim: To compare the microleakage of Cention N, a subgroup of composite resins with a resin-modified glass ionomer (RMGI) and a composite resin. Methods: Class V cavities were prepared on the buccal and lingual surfaces of 46 extracted human molars. The teeth were randomly assigned to four groups. Group A: Tetric N-Bond etch-and-rinse adhesive and Tetric N-Ceram nanohybrid composite resin, group B: Cention N without adhesive, group C: Cention N with adhesive, and group D: Fuji II LC RMGI. The teeth were thermocycled between 5°-55°C (×10,000). The teeth were coated with two layers of nail vanish except for 1 mm around the restoration margins, and immersed in 2% methylene blue (37°C, 24 h) before buccolingual sectioning to evaluate dye penetration under a stereomicroscope (×20). The data were analyzed by the Kruskal-Wallis and Wilcoxon tests (α=0.05). Results: Type of material and restoration margin had significant effects on the microleakage (p<0.05). Dentin margins showed a higher leakage score in all groups. Cention N and RMGI groups showed significant differences at the enamel margin (p=0.025, p=0.011), and for the latter group the scores were higher. No significant difference was found at the dentin margins between the materials except between Cention N with adhesive and RMGI (p=0.031). Conclusion: Microleakage was evident in all three restorative materials. Cention N groups showed similar microleakage scores to the composite resin and displayed lower microleakage scores compared with RMGI.


2021 ◽  
Author(s):  
TP Matos ◽  
TA Hanzen ◽  
R Almeida ◽  
C Tardem ◽  
MC Bandeca ◽  
...  

SUMMARY Objectives: To evaluate the 5-year clinical performance of two-step etch-and-rinse adhesives in noncarious cervical lesions (NCCL). Methods and Materials: The sample comprised 35 adults with at least two similar-sized NCCL. Seventy restorations were placed, according to one of the following groups: Adper Single Bond 2 (SB) and Ambar (AM). The restorations were placed incrementally using a resin composite (Opallis). The restorations were evaluated at baseline and after 6 and 18 months and 5 years using some items of the FDI criteria. The differences in the ratings of the two materials after 6 months, 18 months, and 5 years were performed with Friedman repeated measures ANOVA by rank and McNemar test for significance in each pair (α=0.05). Results: Five patients did not attend the 60-month recall. No significant differences were observed between the materials for any criteria evaluated. Twenty-one restorations failed (12 for SB and 9 for AM) after 60 months. Thus, the retention rate for SB at 60 months were 55.6% for SB and 71% for AM (p=0.32). After 60 months, 12 restorations (6 for SB and 6 AM) showed some loss of marginal adaptation (p=1.0). Slight marginal discoloration was observed in 10 restorations (6 for SB and 4 AM; p=0.91). Five restorations (2 for SB and 3 for AM) showed recurrences of caries (p=1.0). Conclusions: Both two-step etch-and-rinse adhesives—Adper Single Bond 2, a polyalkenoic acid-containing adhesive, and Ambar, a 10-methacryloyloxydecyl dihydrogen phosphate (MDP)-containing adhesive—showed acceptable clinical performance after 60 months.


2020 ◽  
Vol 2020 ◽  
pp. 1-7
Author(s):  
Ruba M. Mustafa ◽  
Suhad J. Al-Nasrawi ◽  
Abtesam I. Aljdaimi

Biodentine is a calcium silicate cement (CSC) that has been broadly applied in vital pulp therapy. The quality of the Biodentine-composite bond has a significant effect on the longevity of the definitive restoration. The aim of this study is to investigate the shear bond strength (SBS) between Biodentine and composite restoration at different maturation times of Biodentine aged in artificial saliva. Fifteen Biodentine discs were allocated into three groups (n = 5) based on the timeframe of performance of composite restoration: immediate (after 12  min), after 14 days, and after 28 days of Biodentine maturation. Total etch and rinse adhesive system and bulk-fill regular resin composite were used. The shear bond strength and the failure pattern were assessed. One-way ANOVA with the Bonferroni post hoc test was applied for statistical analysis at p < 0.05 . The highest (32.47 ± 8.18 MPa) and the lowest (4.08 ± 0.81 MPa) SBS values were recorded for 14 days and 12 min groups, respectively. Significant statistical differences were reported among the groups, and a high statistically significant difference was found between the immediate group and the other groups. Adhesive failure patterns were evident in all groups. More clinically acceptable bond strength between the Biodentine and overlaid composite restoration is at 14 days after Biodentine maturation. Delaying the coverage of Biodentine later than 14 days may significantly reduce the SBS. Using the artificial saliva as an aging medium may affect the SBS between Biodentine and composite material.


2012 ◽  
Vol 37 (6) ◽  
pp. 610-616 ◽  
Author(s):  
RL Quock ◽  
JA Barros ◽  
SW Yang ◽  
SA Patel

SUMMARY The aim of this in vitro study was to investigate the effect of the cariostatic and preventive agent silver diamine fluoride (SDF) on the microtensile bond strength of resin composite to dentin. Forty-two caries-free, extracted molars were flattened occlusally and apically using a diamond saw, and the exposed occlusal dentin was polished with a series of silicon carbide papers, all under water irrigation. The teeth were then randomly divided into six groups of seven teeth each that were treated as follows: 1) Peak SE self-etch bonding agent; 2) 12% SDF + Peak SE; 3) 38% SDF + Peak SE; 4) Peak LC etch-and-rinse bonding agent; 5) 12% SDF + Peak LC; and 6) 38% SDF + Peak LC. Four-millimeter buildups of Amelogen Plus were incrementally placed on all teeth; after a 24-hour storage period in distilled water, the specimens were sectioned perpendicular to the adhesive interface to produce beams of cross-sectional surface area measuring approximately 1 mm2. The beams were placed on a microtensile testing machine, which utilized a single-speed pump motor and force gauge at 20 kgf × 0.01 second to record maximum tensile force before failure occurred. Two-way analysis of variance and post hoc Tukey tests were performed to compare the effects of the SDF on microtensile bond strength, with statistical significance set at α = 0.05. None of the experimental groups treated with different concentrations of SDF showed a significant difference in bond strength compared to the control groups, and there was no significant difference in bond strength between self-etch and etch-and-rinse groups. However, the effect of SDF on self-etch bonded teeth compared to etch-and-rinse bonded teeth was statistically significant (p=0.0363), specifically at the 12% concentration. SDF does not adversely affect the bond strength of resin composite to noncarious dentin.


2016 ◽  
Vol 2016 ◽  
pp. 1-11 ◽  
Author(s):  
Secil Bektaş Donmez ◽  
Melek D. Turgut ◽  
Serdar Uysal ◽  
Pinar Ozdemir ◽  
Meryem Tekcicek ◽  
...  

The purpose of this study was to assess the clinical performance of composite restorations placed with different adhesive systems in primary teeth. In 32 patients, 128 composite restorations were placed using a split-mouth design as follows (4 groups/patient): three-step etch-and-rinse (Group 1), two-step etch-and-rinse (Group 2), two-step self-etch (Group 3), and one-step self-etch (Group 4). The restorations were clinically evaluated at baseline and at 6, 18, and 36 months according to the FDI criteria. There was no significant difference between the adhesive systems in retention of the restorations (p>0.05). Over time, there was a statistically significant decrease in marginal adaptation in all groups, whereas surface and marginal staining significantly increased in Groups 3 and 4 (p<0.05). The etch-and-rinse adhesive systems resulted in better marginal adaptation than the self-etch adhesive systems (p<0.05). It was concluded that preetching of the primary enamel might help improve the clinical performance of the self-etch adhesive systems in primary teeth.


2020 ◽  
Vol 19 ◽  
pp. e201662
Author(s):  
Maria Luísa de Alencar e Silva Leite ◽  
Caroline de Farias Charamba ◽  
Renally Bezerra Wanderley e Lima ◽  
Sônia Saeger Meireles ◽  
Rosângela Marques Duarte ◽  
...  

Aim: This study evaluated the influence of dentin wettability on the immediate and extended microtensile bond strength (mTBS) of a universal adhesive system used in the etch-and-rinse strategy. Methods: Twenty human third molars were selected and divided into four groups according to the adhesive system and dentin wettability. The mTBS values of each group were registered 24 h and one year after adhesive system application and resin composite block build-up (n=30). Data were analyzed by the t-test (p<0.05). Results: When both adhesive systems were compared, there was no statistically significant difference when they were applied following wet bonding (p>0.05). However, the dry bonding reduced μTBS values of the Adper Single Bond 2 adhesive (p<0.05). Regarding storage time, both groups presented similar μTBS values at 24 h and one year (p>0.05). Conclusions: Therefore, the Scotchbond Universal Adhesive can be applied to dry or wet dentin without compromising the etch-and-rinse bonding quality and the durability of the restorations.


Author(s):  
Omnia M. Sami ◽  
Essam A. Naguib ◽  
Rasha H. Afifi ◽  
Shaymaa M. Nagi

Abstract Objective Bonding to different dentin substrates influences resin composite restoration outcomes. This study investigated the influence of different adhesion protocols on the shear bond strength of universal adhesive systems to sound and artificial caries-affected dentin (CAD). Materials and Methods Occlusal enamel of 80 premolars were wet grinded to obtain flat midcoronal dentin. Specimens were equally divided according to the substrate condition: sound and CAD by subjecting to pH-cycling for 14 days. Each dentin substrate was bonded with the adhesive systems used in this study: Single Bond universal adhesive or Prime&Bond universal (applied either in etch-and-rinse or self-etch adhesion protocol). Adhesive systems were utilized according to manufacturers’ instructions, then resin composite was built up. Specimens were tested for shear bond strength. The data were analyzed by three-way analysis of variance, and failure modes were determined using stereomicroscope. Results There was no statistically significant difference between the two tested adhesive systems on artificially created CAD with different adhesion protocols. On sound dentin, Single Bond universal, either in the etch-and-rinse or self-etch adhesion protocols, revealed higher statistically significant shear bond strength mean values compared with CAD. Conclusion Single Bond universal adhesive in an etch-and-rinse adhesion protocol improved only bonding to sound dentin, while no added positive effect for the etching step with Prime&Bond universal adhesive was found when bonded to both sound and CAD substrates. The influence of CAD on the performance of the universal adhesives was material-dependent.