scholarly journals Durability of Structural Recycled Aggregate Concrete Subjected to Freeze-Thaw Cycles

2020 ◽  
Vol 12 (16) ◽  
pp. 6475 ◽  
Author(s):  
Caroline Santana Rangel ◽  
Mayara Amario ◽  
Marco Pepe ◽  
Enzo Martinelli ◽  
Romildo Dias Toledo Filho

The increasing global demand for natural resources and the extensive production of construction and demolition waste (CDW) raise concerns for both the economic and environmental consequences that they can induce. Several efforts are being made with the aim to promote sustainable practices in the construction industry. In this context, one of the most relevant options refers to reusing CDW in new construction: specifically, the use of recycled concrete aggregate (RCA) is attracting a growing interest. Unfortunately, although the behavior of recycled aggregate concrete (RAC) has been widely investigated in the last few years, there are still knowledge gaps to fill on various aspects of the RAC performance, such as its durability in extreme conditions. The present study deals with the freeze-thaw performance of normal- (C35) and high-strength (C60) RAC produced with RCAs derived from different sources. Specifically, ten concrete mixtures were subjected to a different number of freeze-thaw cycles (namely, 0, 150 and 300), with the aim of analyzing the degradation of key physical and mechanical properties, such density, compressive strength, elastic modulus and tensile strength. Based on the obtained experimental results, a novel degradation law for freeze-thaw cycles is proposed: it unveils a relationship between open porosity of concrete, which is directly correlated to the peculiar properties of RCAs, and the corresponding damage level determined on RAC specimens.

2014 ◽  
Vol 5 (2) ◽  
Author(s):  
Mirjana Malešev ◽  
Vlastimir Radonjanin ◽  
Gordana Broćeta

Following an example of the world's great powers that developed the recycling industry after natural disasters and wars, the paper points to the possibility of using large quantities of construction and demolition waste, generated as a result of the recent floods in the BiH and Serbia. Based on the years of extensive experimental research, and the research conducted by eminent experts, an overview is provided of the most basic properties and application of recycled aggregate concrete. It has been shown that the application of coarse recycled concrete aggregate, as the component materials in the concrete mixtures, it is possible to produce structural concrete that can be satisfactory and even with high quality, which primarily depends on the characteristics of crushed demolished concrete.


2021 ◽  
Vol 11 (21) ◽  
pp. 10063
Author(s):  
Caroline Santana Rangel ◽  
Marco Pepe ◽  
Mayara Amario ◽  
Lucas Caon Menegatti ◽  
Enzo Martinelli ◽  
...  

In the last several decades, the growth of Construction and Demolition Waste (CDW) production and the increased consumption of natural resources have led to promoting the use of secondary raw materials for a more sustainable construction. Specifically, the use of Recycled Concrete Aggregate (RCA), derived from waste concrete, for the production of Recycled Aggregate Concrete (RAC) has attracted a significant interest both in industry and in academia. However, the use of RAC in field applications still finds some barriers. In this context, the present study investigates experimentally the effects of freeze-thaw and wet-dry cycles on the stress transfer mechanisms of reinforced RAC elements through tension stiffening tests. First of all, the paper presents a detailed analysis of the degradation due to the aging process of RAC with RCAs obtained from different sources. Particularly, the results of tension stiffening tests are analyzed in terms of crack formation and propagation, matrix tensile strength contribution and steel-to-concrete bond. The results highlight that the pre-cracking elastic modulus, the first crack strength as well as the maximum concrete strength are strongly influenced by the presence of the Attached Mortar (AM) in RCA, as the former affects the concrete’s open porosity. Therefore, the amount of AM is identified as the key parameter for the evaluation of durability of reinforced RAC members: a degradation-law is also proposed which correlates the initial concrete open porosity with the damage observed in reinforced RAC elements.


2018 ◽  
Vol 760 ◽  
pp. 193-198 ◽  
Author(s):  
Kristina Fořtová ◽  
Tereza Pavlů

This paper presents research results of recycled fine aggregate concrete testing. The main aim of this contribution is verification of properties of fine aggregate concrete with partial replacement of fine natural aggregate by recycled masonry aggregate originated from construction and demolition waste. The influence of partial replacement of natural sand to mechanical properties and freeze-thaw resistance is described. The compressive strength and flexural strength were tested at the age of 28 and 60 days and after 25, 50, 75 and 100 freeze-thaw cycles. Partial replacement of natural sand was 0, 25 and 50 % for all these tests. Prismatic specimens were examined.


Materials ◽  
2020 ◽  
Vol 13 (24) ◽  
pp. 5675
Author(s):  
Caroline S. Rangel ◽  
Mayara Amario ◽  
Marco Pepe ◽  
Enzo Martinelli ◽  
Romildo D. Toledo Filho

Recently, concerns have been rising about the impact of increasing the depletion of natural resources and the relevant generation of construction and demolition waste, on the environment and economy. Therefore, several efforts have been made to promote sustainable efficiency in the construction industry and the use of recycled aggregates derived from concrete debris for new concrete mixtures (leading to so-called recycled aggregate concrete, RAC) is one of the most promising solutions. Unfortunately, there are still gaps in knowledge regarding the durability performances of RAC. In this study, we investigate durability of structural RAC subjected to wet-dry cycles. We analyze the results of an experimental campaign aimed at evaluating the degradation process induced by wetting and drying cycles on the key physical and mechanical properties of normal- and high-strength concrete, produced with coarse recycled concrete aggregates (RCAs) of different sizes and origins. On the basis of the results we propose a degradation law for wetting and drying cycles, which explicitly makes a possible correlation between the initial concrete porosity, directly related to the specific properties of the RCAs and the resulting level of damage obtained in RAC samples.


2014 ◽  
Vol 1054 ◽  
pp. 221-226 ◽  
Author(s):  
Tereza Pavlů ◽  
Magdaléna Šefflová

The main aim of this contribution is description of the static and the dynamic modulus of elasticity of concrete containing recycled aggregate. Recycled construction and demolition waste, especially recycled concrete, is able to use as an aggregate for concrete, but using of recycled aggregate has a negative impact of concrete characteristic. This paper presents results of non-destructive measurement of recycled aggregate concrete properties. Series of concrete samples with 100% replacement ratios of coarse natural aggregate by coarse recycled aggregate from different sources were prepared for this study. The static and the dynamic modulus of elasticity were investigated on specimens 100 x 100 x 400 mm. All tested mixtures were also tested on compressive strength.


2009 ◽  
Vol 620-622 ◽  
pp. 255-258 ◽  
Author(s):  
Cheol Woo Park

As the amount of waste concrete has been increased and recycling technique advances, this study investigates the applicability of recycled concrete aggregate for concrete structures. In addition fly ash, the industrial by-product, was considered in the concrete mix. Experimental program performed compressive strength and chloride penetration resistance tests with various replacement levels of fine recycled concrete aggregate and fly ash. In most case, the design strength, 40MPa, was obtained. It was known that the replacement of the fine aggregate with fine RCA may have greater influence on the strength development rather than the addition of fly ash. It is recommended that when complete coarse aggregate is replaced with RCA the fine RCA replacement should be less than 60%. The recycled aggregate concrete can achieve sufficient resistance to the chloride ion penetration and the resistance can be more effectively controlled by adding fly ash. It I finally conclude that the recycled concrete aggregate can be successfully used in the construction field and the recycling rate of waste concrete and flay ash should be increased without causing significant engineering problems.


Materials ◽  
2021 ◽  
Vol 14 (16) ◽  
pp. 4620
Author(s):  
Fan You ◽  
Surong Luo ◽  
Jianlan Zheng ◽  
Kaibin Lin

Using recycled aggregate in concrete is effective in recycling construction and demolition waste. It is of critical significance to understand the fatigue properties of recycled aggregate concrete (RAC) to implement it safely in structures subjected to repeated or fatigue load. In this study, a series of fatigue tests was performed to investigate the compressive fatigue behavior of RAC. The performance of interfacial transition zones (ITZs) was analyzed by nanoindentation. Moreover, the influence of ITZs on the fatigue life of RAC was discussed. The results showed that the fatigue life of RAC obeyed the Weibull distribution, and the S-N-p equation could be obtained based on the fitting of Weibull parameters. In the high cycle fatigue zone (N≥104), the fatigue life of RAC was lower than that of natural aggregate concrete (NAC) under the same stress level. The fatigue deformation of RAC presented a three-stage deformation regularity, and the maximum deformation at the point of fatigue failure closely matched the monotonic stress-strain envelope. The multiple ITZs matched the weak areas of RAC, and the negative effect of ITZs on the fatigue life of RAC in the high cycle fatigue zone was found to be greater than that of NAC.


2019 ◽  
Vol 12 (1) ◽  
pp. 250 ◽  
Author(s):  
Debora Acosta Álvarez ◽  
Anadelys Alonso Aenlle ◽  
Antonio José Tenza-Abril ◽  
Salvador Ivorra

The main objective of this work is to evaluate the properties of hot asphalt mixtures that have been manufactured with different recycled concrete aggregate (RCA) percentages (0%, 20%, 40%, 60% and 80% of the fraction 5–13 mm) and asphalt (4%, 4.5% and 5%). Dense asphalt mixtures were made; partially replacing the natural aggregate (NA) fraction between 5 and 13 mm. Marshall specimens were manufactured to determine the main properties of the asphalt concrete (AC) in terms of density, voids, stability and deformation. Additionally, the optimal asphalt content (OAC) was determined, and measured the water sensibility, the stiffness modulus and the permanent deformation. The results corroborate the potential for using these sources of construction and demolition waste (CDW) as a RCA in asphalt concrete and show that the hot asphalt mixtures with up to 40% substitution of natural aggregate by recycled aggregate in the fraction 5–13 mm present good behavior.


2013 ◽  
Vol 811 ◽  
pp. 249-253 ◽  
Author(s):  
Wei Li ◽  
Hai Ying Zhang

Experiments on influence of species of aggregate and mixing method on interfacial zone in recycled aggregate concrete were investigated. SEM observations revealed that a recycle normal-strength concrete aggregate consist of loose and porous interfacial structure, whereas a recycled high performance concrete (HPC) aggregate and a triple mixing (TM) consist mainly of dense hydrates. Various admixtures on ITZ was produced that consumed CH in the pore, modified attached cement mortar. Strength of recycled concrete was explained by interaction between cements paste and recycled aggregate. The result verified that the relatively dense pore structure of the recycled concrete benefit to development of mechanical properties.


2017 ◽  
Vol 11 (1) ◽  
pp. 270-280 ◽  
Author(s):  
Haicheng Niu ◽  
Yonggui Wang ◽  
Xianggang Zhang ◽  
Xiaojing Yin

Introduction: Freeze-thaw resistance of recycled aggregate concrete with partial or total replacement of recycled aggregate compared with that of natural aggregate concrete was investigated in this paper. Method: Ninety specimens were fabricated to study the influence of different recycled aggregate replacement ratios on the surface scaling, mass loss, and residual compressive strength after 100 freeze-thaw cycles. Results: The experiment results indicate that the type of recycled aggregate and its replacement ratio have significant effects on the freeze-thaw performance. The cubic compressive strength of recycled aggregate concrete is overall slightly lower than that of normal concrete. After 100 freeze-thaw cycles, the compressive strength decreases and the reduction extent increases with increasing replacement rate of recycled aggregate. The surface scaling of reinforced recycled concrete prisms tends to be more severe with the increase of freeze-thaw cycles. Conclusion: Furthermore, a notable rise in mass loss and the bearing capacity loss is also found as the substitution ratio increases. Under the same replacement rate, recycled fine aggregate causes more negative effects on the freeze-thaw resistance than recycled coarse aggregate.


Sign in / Sign up

Export Citation Format

Share Document