Development of ternary iron vanadium oxide semiconductors for applications in photoelectrochemical water oxidation

RSC Advances ◽  
2016 ◽  
Vol 6 (6) ◽  
pp. 4992-4999 ◽  
Author(s):  
Harahari Mandal ◽  
Sanjib Shyamal ◽  
Paramita Hajra ◽  
Aparajita Bera ◽  
Debasis Sariket ◽  
...  

Herein, we report the synthesis and photoelectrochemical characterizations of n-type Fe–V-oxide semiconductors thin film via drop cast method in different proportions onto indium tin oxide coated glass followed by annealing in air at 500 °C for 3 h.

2011 ◽  
Vol 287-290 ◽  
pp. 2271-2274 ◽  
Author(s):  
Jian Du ◽  
Jun Wei Di

A simple one-step method was developed to electrodeposit gold thin film from HAuCl4solution with cyclic voltammetric mode on indium tin oxide (ITO) coated glass. The color of as-prepared gold film can vary from red to blue due to different particle-particle interaction. The Au thin film comprised of isolated gold nanoparticles (GNPs) were red color, while blue gold thin films were obtained by electrodeposition in high HAuCl4concentration and the increasing deposition cycles.


2014 ◽  
Vol 2 (43) ◽  
pp. 9132-9140 ◽  
Author(s):  
Tsofnat Safrani ◽  
Tatipamula Arun Kumar ◽  
Matvey Klebanov ◽  
Neta Arad-Vosk ◽  
Rotem Beach ◽  
...  

Lead sulfide semiconducting thin films were chemically deposited on indium tin oxide coated glass plates for use as photoreceptor layers in conjugation with optically addressed spatial light modulators (OASLMs).


2014 ◽  
Vol 43 (9) ◽  
pp. 3177-3183 ◽  
Author(s):  
T. W. Seo ◽  
Hyun-Suk Kim ◽  
Kwang-Ho Lee ◽  
Kwun-Bum Chung ◽  
Jin-Seong Park

2016 ◽  
Vol 2016 ◽  
pp. 1-12 ◽  
Author(s):  
Li Lin ◽  
Chin-Pao Cheng ◽  
Tun-Ping Teng

In this study, tungsten trioxide (WO3) thin films were electrodeposited on indium tin oxide (ITO) glass to form WO3-coated glass. The electrodeposition (ED) time (tED) and ED current (IED) were varied to control the film thickness and morphology. Furthermore, the crystallization of the thin films was controlled by annealing them at 250°C, 500°C, and 700°C. The results showed that the thickness of the WO3thin films increased withtEDandIED. The as-deposited thin films and those annealed at 250°C were amorphous, whereas the WO3thin films annealed at 500 and 700°C were in the anorthic phase. Moreover, the amorphous WO3-coated glass exhibited high transmittance in visible light and low transmittance in near-infrared light, whereas the anorthic WO3-coated glass had high transmittance in near-infrared light. An empirical formula for determining the thickness of WO3thin films was derived through multiple regressions of the ED process parameters.


2018 ◽  
Vol 122 (29) ◽  
pp. 16510-16518 ◽  
Author(s):  
Mandana Amiri ◽  
Maryam Fallahi ◽  
Abolfazl Bezaatpour ◽  
Roxana Jijie ◽  
Mehran Nozari-asbmarz ◽  
...  

1994 ◽  
Vol 33 (Part 1, No. 12B) ◽  
pp. 7057-7060 ◽  
Author(s):  
Meiso Yokoyama ◽  
Jiin Wen Li ◽  
Shui Hsiang Su ◽  
Yan Kuin Su

Nanoscale ◽  
2015 ◽  
Vol 7 (28) ◽  
pp. 12226-12226 ◽  
Author(s):  
Isvar A. Cordova ◽  
Qing Peng ◽  
Isa L. Ferrall ◽  
Adam J. Rieth ◽  
Paul G. Hoertz ◽  
...  

2011 ◽  
Vol 6 (8) ◽  
pp. 592 ◽  
Author(s):  
O.I. Kuntyi ◽  
P.Y. Stakhira ◽  
V.V. Cherpak ◽  
O.I. Bilan ◽  
Ye.V. Okhremchuk ◽  
...  

Sign in / Sign up

Export Citation Format

Share Document