Epitaxial BaTiO3 Thin Films on Different Substrates for Optical Waveguide Applications

1999 ◽  
Vol 597 ◽  
Author(s):  
M. Siegert ◽  
Judit G. Lisoni ◽  
C. H. Lei ◽  
A. Eckau ◽  
W. Zander ◽  
...  

AbstractIn the process of developing thin film electro-optical waveguides we investigated the influence of different substrates on the optical and structural properties of epitaxial BaTiO3 thin films. These films are grown by on-axis pulsed laser deposition (PLD) on MgO(100), MgAl2O4(100), SrTiO3(100) and MgO buffered A12O3(1102) substrates. The waveguide losses and the refractive indices were measured with a prism coupling setup. The optical data are correlated to the results of Rutherford backscattering spectrometry/ion channeling (RBS/C). X-ray diffraction (XRD), atomic force microscopy (AFM) and transmission electron microscopy (TEM). BaTiO3 films on MgO(100) substrates show planar waveguide losses of 3 dB/cm and ridge waveguide losses of 5 dB/cm at a wavelength of 633 nm.

2001 ◽  
Vol 696 ◽  
Author(s):  
Ravi Bathe ◽  
R.D. Vispute ◽  
Daniel Habersat ◽  
R. P. Sharma ◽  
T. Venkatesan ◽  
...  

AbstractWe have investigated the epitaxy, surfaces, interfaces, and defects in AlN thin films grown on SiC by pulsed laser deposition. The stress origin, evolution, and relaxation in these films is reported. The crystalline structure and surface morphology of the epitaxially grown AlN thin films on SiC (0001) substrates have been studied using x-ray diffraction (θ–2θ, ω, and Ψ scans) and atomic force microscopy, respectively. The defect analysis has been carried out by using Rutherford backscattering spectrometry and ion channeling technique. The films were grown at various substrate temperatures ranging from room temperature to 1100 °C. X-ray diffraction measurements show highly oriented AlN films when grown at temperatures of 750- 800 °C, and single crystals above 800 °C. The films grown in the temperature range of 950 °C to 1000 °C have been found to be highly strained, whereas the films grown above 1000 °C were found to be cracked along the crystallographic axes. The results of stress as a function of growth temperature, thermal mismatch, growth mode, and buffer layer thickness will be presented, and the implications of these results for wide band gap power electronics will be discussed.


2015 ◽  
Vol 821-823 ◽  
pp. 213-216
Author(s):  
S.M. Ryndya ◽  
N.I. Kargin ◽  
A.S. Gusev ◽  
E.P. Pavlova

Silicon carbide thin films were obtained on Si (100) and (111) substrates by means of vacuum laser ablation of α-SiC ceramic target. The influence of substrate temperature on composition, structure and surface morphology of experimental samples was examined using Rutherford backscattering spectrometry (RBS), Fourier transform infrared spectroscopy (FTIR), scanning electron microscopy (SEM), conventional and high-resolution transmission electron microscopy (TEM/HRTEM), atomic force microscopy (AFM), selected area electron diffraction (SAED) and X-ray diffraction (XRD) methods.


1995 ◽  
Vol 10 (3) ◽  
pp. 680-691 ◽  
Author(s):  
Andreas Seifert ◽  
Fred F. Lange ◽  
James S. Speck

A mixed alkoxide liquid precursor was used to form epitaxial PbTiO3 thin films by spin-coating on cubic (001) SrTiO3 substrates. The films were heat-treated at temperatures between 380 °C/1 h and 800 °C/1 h. X-ray diffraction, atomic force microscopy, scanning and transmission electron microscopy were used to characterize the microstructure of the films and to evaluate the epitaxial phenomena. At ∼400 °C/1 h, a polycrystalline, metastable Pb-Ti fluorite crystallizes from the pyrolyzed amorphous precursor. At slightly higher temperatures (∼420 °C/1 h), the thermodynamically stable phase with the perovskite structure epitaxially nucleates at the film/substrate interface. A small number of epitaxial grains grow through the film toward the surface and consume the nanocrystalline fluorite grains. Coarsening of the perovskite grains leads to a reduction in mosaic spread during further heating. Pores, which concurrently coarsen with grain growth, produce a pitted surface as they disappear from within the film. At 800 °C/1 ha dense epitaxial PbTiO3 film with a smooth surface is observed. Parameters governing the formation of a- and c-domains are discussed as well as the small tilts of the domain axes away from the substrate normal.


2005 ◽  
Vol 872 ◽  
Author(s):  
Yuebing Zheng ◽  
Shijie Wang ◽  
Cheng Hon A. Huan

AbstractThe effect of dopants on the band structure and crystal structure of Ba0.5Sr0.5TiO3thin films on (100) LaAlO3 substrates has been investigated. The dopants include Ti, Mg and Al. The band-gap energies of the thin films were determined from the transmission spectra measured by UVVIS spectrophotometer and increased with the increase of dopant concentration regardless of the type of dopants. The crystal structure was studied by using transmission electron microscopy, atomic force microscopy, x-ray diffraction and micro-Raman spectroscopy. The relation between band structure and crystal structure was discussed.


1996 ◽  
Vol 441 ◽  
Author(s):  
P. Fons ◽  
S. Niki ◽  
A. Yamada ◽  
D. J. Tweet

AbstractDue to its high near bandedge absorption, CuInSe2 is considered to be one of the most promising solar cell materials. As CuInSe2 films are usually grown by metastable processes, the Cu/In ratio often deviates from the ideal ratio of unity. To investigate the structural and morphological changes induced by such stoichiometric variations we have grown a series of epitaxial CuInSe2 epitaxial thin films with varying Cu/In ratios by molecular beam epitaxy on GaAs(001) substrates from elemental sources at a growth temperature of 450° C. Overall structural, microstructural and surface morphological changes were observed by X-ray diffraction, transmission electron microscopy, and atomic force microscopy, respectively. It was observed that as films deviated from stoichiometry, twinning occurred preferentially on the anion {1 · 1 · 2} planes.


2009 ◽  
Vol 24 (1) ◽  
pp. 212-216
Author(s):  
Srinivas Sathiraju ◽  
Paul N. Barnes ◽  
Robert A. Wheeler

We report the systematic substitution of Nb at the Cu1 site of YBa2Cu3Oy in thin films to form a new phase of YBa2Cu2NbO8. These films were deposited on SrTiO3(100) crystals using pulsed laser deposition and deposited at an optimal temperature of 850 °C. Films were characterized using x-ray diffraction (XRD), atomic force microscopy, x-ray photoelectron spectroscopy (XPS), micro-Raman spectroscopy, and transmission electron microscopy. XRD of these films indicate c-axis oriented YBa2Cu2NbOy formation. XPS and micro-Raman spectroscopy analysis suggests Cu exists in the +2 state.


1995 ◽  
Vol 382 ◽  
Author(s):  
Martin Pehnt ◽  
Douglas L. Schulz ◽  
Calvin J. Curtis ◽  
Helio R. Moutinho ◽  
Amy Swartzlander ◽  
...  

ABSTRACTIn this article we report the first nanoparticle-derived route to smooth, dense, phase-pure CdTe thin films. Capped CdTe nanoparticles were prepared by injection of a mixture of Cd(CH3)2, (n-C8H17)3 PTe and (n-C8H17)3P into (n-C8H17)3PO at elevated temperatures. The resultant nanoparticles 32-45 Å in diameter were characterized by x-ray diffraction, UV-Vis spectroscopy, transmission electron microscopy, thermogravimetric analysis and energy dispersive x-ray spectroscopy. CdTe thin film deposition was accomplished by dissolving CdTe nanoparticles in butanol and then spraying the solution onto SnO2-coated glass substrates at variable susceptor temperatures. Smooth and dense CdTe thin films were obtained using growth temperatures approximately 200 °C less than conventional spray pyrolysis approaches. CdTe films were characterized by x-ray diffraction, UV-Vis spectroscopy, atomic force microscopy, and Auger electron spectroscopy. An increase in crystallinity and average grain size as determined by x-ray diffraction was noted as growth temperature was increased from 240 to 300 °C. This temperature dependence of film grain size was further confirmed by atomic force microscopy with no remnant nanocrystalline morphological features detected. UV-Vis characterization of the CdTe thin films revealed a gradual decrease of the band gap (i.e., elimination of nanocrystalline CdTe phase) as the growth temperature was increased with bulk CdTe optical properties observed for films grown at 300 °C.


Cerâmica ◽  
2002 ◽  
Vol 48 (305) ◽  
pp. 38-42 ◽  
Author(s):  
M. I. B. Bernardi ◽  
E. J. H. Lee ◽  
P. N. Lisboa-Filho ◽  
E. R. Leite ◽  
E. Longo ◽  
...  

The synthesis of TiO2 thin films was carried out by the Organometallic Chemical Vapor Deposition (MOCVD) method. The influence of deposition parameters used during growth on the final structural characteristics was studied. A combination of the following experimental parameters was studied: temperature of the organometallic bath, deposition time, and temperature and substrate type. The high influence of those parameters on the final thin film microstructure was analyzed by scanning electron microscopy with electron dispersive X-ray spectroscopy, atomic force microscopy and X-ray diffraction.


2001 ◽  
Vol 688 ◽  
Author(s):  
J. Rodríguez Contreras ◽  
J. Schubert ◽  
U. Poppe ◽  
O. Trithaveesak ◽  
K. Szot ◽  
...  

AbstractWe have prepared single crystalline epitaxial PbZr0.52Ti0.48O3 (PZT) and BaTiO3 (BTO) thin films on single crystalline epitaxial SrRuO3 (SRO) thin films grown on SrTiO3 (100) (STO) substrates. PZT and SRO thin films were grown using high-pressure on-axis sputtering and BTO using pulsed laser deposition (PLD). The film thickness ranged between 12 to 165 nm. Their excellent structural properties, surface smoothness and interface sharpness were demonstrated by X-Ray Diffraction measurements (XRD), High Resolution Transmission Electron Microscopy (HRTEM) and Atomic Force Microscopy (AFM). Rutherford Backscattering Spectrometry and Channeling measurements (RBS/C) were used to analyze stoichiometry and crystalline quality. Ferroelectric hysteresis loops were obtained for all films of a thickness down to 12 nm showing a decrease in the remanent polarization Pr and an increase in the coercive field Ec towards thinner film thicknesses. Furthermore we have prepared tunneling junctions with a PZT or BTO barrier thickness of 3-6 nm. Reproducible bi-stable I-V-curves and bias dependence of the conductance were obtained suggesting an influence of the ferroelectric properties of the barrier material on the tunnel current.


2020 ◽  
Vol 98 (5) ◽  
pp. 365-375
Author(s):  
Andrea Quintero ◽  
Patrice Gergaud ◽  
Jean-Michel Hartmann ◽  
Vincent Delaye ◽  
Nicolas Bernier ◽  
...  