scholarly journals Liquid butadiene rubber as safe process-aid in natural rubber product : A substitute for carcinogenic aromatic oils

IJIREEICE ◽  
2021 ◽  
Vol 9 (10) ◽  
Author(s):  
Chandresh Mysore Parameshwaraiah ◽  
Roopa S ◽  
Bhavana M
2020 ◽  
Vol 26 (2) ◽  
pp. 62-69
Author(s):  
Farida Ali ◽  
Tuti I. Sari ◽  
Andi A. Siahaan ◽  
Al-Kautsar D. Arya ◽  
Tri Susanto

Penelitian ini untuk mengetahui pengaruh penambahan Natural Rubber (NR) dan Epoxidation Natural Rubber (ENR-46) dengan kompatibiliser Chlorprene Rubber (CR) pada aplikasi kompon termoplastik Poly Vinyl Chloride (PVC) dan Nitrile Butadiene Rubber (NBR), variabel penelitian meliputi ENR-46/PVC/NBR/CR, NR/PVC/NBR/CR dan CR-NR/PVC/NBR, CR-ENR-46/PVC/NBR. Parameter pengujian sifat fisik-mekanik : Hardness (Shore A), Tensile Strength (Mpa), Elongation at Break (%) dan ketahanan terhadap pelarut minyak (n-Pentane, Toluene, Hexane dan Pertalite). Hasil penelitian didapatkan untuk sifat fisik-mekanik, semakin banyak penambahan NR Kekerasan kompon termoplastik akan menurun, Tensile Strength dan Elongation at Break kompon akan meningkat begitu juga dengan CR-NR. Tetapi berbanding terbalik hasilnya untuk ENR-46 dan CR-ENR-46. Pengujian Ketahanan terhadap pelarut minyak semakin banyak penambahan ENR-46 Ketahanan kompon termoplastik terhadap pelarut akan meningkat, hasil yang sama juga pada CR-ENR-46. Tetapi berbanding terbalik hasilnya dengan penambahan NR dan CR-NR pada kompon termoplastik.


2020 ◽  
Vol 391 (1) ◽  
pp. 1900175
Author(s):  
Dewi K. Arti ◽  
Ade S. Hidayat ◽  
Ika M. Ulfah ◽  
Herri Susanto ◽  
Lies A. Wisojodharmo ◽  
...  

1999 ◽  
Vol 72 (4) ◽  
pp. 721-730 ◽  
Author(s):  
G. R. Hamed ◽  
J. Zhao

Abstract Typical sulfur-cured vulcanizates of styrene-butadiene rubber (SBR) and natural rubber (NR) were prepared, and subjected to air-oven aging at 100 °C. Gum specimens exhibited an initial aging period in which stiffness was unchanged, while tensile strength and strain-to-break were significantly reduced. In contrast, black-filled vulcanizates stiffened during early aging. After intermediate aging times, NR specimens softened, while SBR stiffened. With prolonged aging, all compositions became hard and inextensible.


Polymers ◽  
2018 ◽  
Vol 10 (6) ◽  
pp. 658 ◽  
Author(s):  
Byungwoo Moon ◽  
Jongmin Lee ◽  
Soo Park ◽  
Chang-Sung Seok

2017 ◽  
Vol 44 (5) ◽  
pp. 25-28 ◽  
Author(s):  
A.A. Zuev ◽  
L.R. Lyusova ◽  
N.P. Boreiko

Now there is not a single area of industry that can do without adhesive elastomer materials. Composites based on synthetic rubbers comprise 75% of the total volume of adhesive materials produced, which is due to the combination of unique properties typical of the elastomer base of the adhesive. The base of many imported adhesives for the bonding of rubber to metal is chlorinated natural rubber. As an alternative, chlorinated synthetic isoprene rubber has been proposed, developed at the Scientific Research Institute for Synthetic Rubber in St Petersburg. The chlorinated isoprene rubber was compared with imported chlorinated natural rubber in adhesive composites, and the physicomechanical properties of mixes based on a blend of chlorinated rubber and nitrile butadiene rubber were investigated. The investigation was conducted on chlorinated natural rubber of grade Pergut S20, chlorinated isoprene rubber SKI-3, and nitrile butadiene rubbers of grades BNKS-28AMN and SKN-26S. The influence of the ratio of chlorinated rubber to nitrile butadiene rubber and the technological factors of mix preparation on the properties of films produced from them was established. It was shown that, in terms of the level of properties, home-produced chlorinated rubber can be used as the base for adhesives for hot bonding of rubber to metal instead of imported Pergut S20.