scholarly journals Effect of Minor Alloying Substitution on Glass-Forming Ability and Crystallization Behavior of a Ni57Zr22X8Nb8Al5 (X = Ti, Cu) Alloy Synthesized by Mechanical Alloying

2013 ◽  
Vol 54 (9) ◽  
pp. 1844-1850 ◽  
Author(s):  
Chao Yang ◽  
Jin Zeng ◽  
Hao Guo ◽  
ShengGuan Qu ◽  
XiaoQiang Li
Materials ◽  
2019 ◽  
Vol 12 (3) ◽  
pp. 383 ◽  
Author(s):  
Xuan Liu ◽  
Xingfu Wang ◽  
Yongli Si ◽  
Xiaokang Zhong ◽  
Fusheng Han

In this study, the formation and crystallization of the Al70Fe12.5V12.5Nb5 amorphous alloys has been investigated. The addition of Nb enhances the supercooled liquid region and glass forming ability of the Al-Fe-V amorphous alloys. The Al70Fe12.5V12.5Nb5 amorphous alloy exhibits two distinct crystallization steps and a large supercooled liquid region at more than 100 K. Kissinger and Ozawa analyses showed that the two activation energies for crystallization (Ex) were estimated to be 366.3 ± 23.9 and 380.5 ± 23.9 kJ/mol. Large supercooled liquid regions are expected to gain an application field of Al-based amorphous alloys.


2008 ◽  
Vol 01 (02) ◽  
pp. 145-149 ◽  
Author(s):  
JUNG MIN NAM ◽  
YONG HEE LEE ◽  
TAE HYUN NAM ◽  
YEON WOOK KIM ◽  
JUNG MOO LEE

Amorphous Ti 50 Ni (50-x) Cu x (at.%) (x = 15, 20 and 25) alloy ribbons were prepared by melt spinning, and then their crystallization behavior was investigated by optical microscopy, transmission electron microscopy, X-ray diffraction and differential scanning calorimetry. Wavenumber (Qp) decreased from 29.40 nm-1 to 29.29 nm-1 and ΔT(T g - T x ) increased from 31 K to 36 K with increasing Cu content from 15 at.% to 25 at.%, suggesting that glass forming ability of Ti – Ni – Cu alloy ribbons increased with increasing Cu content. Activation energy for crystallization decreased from 211.5 kJ/mol to 136.4 kJ/mol with increasing Cu content from 15 at.% to 25 at.%, suggesting that a stability of Ti – Ni – Cu amorphous decreased with increasing Cu content.


2007 ◽  
Vol 22 (2) ◽  
pp. 471-477 ◽  
Author(s):  
Dong Ho Kim ◽  
Jin Man Park ◽  
Do Hyang Kim ◽  
Won Tae Kim

The effects of niobium (Nb) addition on the glass-forming ability (GFA), crystallization behavior, and compressive mechanical property of iron (Fe)–boron (B)–yttrium (Y) alloys have been investigated. Among the (Fe71.2B24Y4.8)100−xNbx (x = 0, 2, 4, 6, 8) alloys investigated, (Fe71.2B24Y4.8)96Nb4 exhibits the highest GFA, enabling the formation of glassy rods with a maximum diameter of 7 mm, which is the largest among quaternary Fe-based alloys. The comparison of the crystallization behavior of the alloys shows that the formation of metastable Fe23B6 phase during crystallization in the (Fe71.2B24Y4.8)96Nb4 alloy can suppress the formation of other stable crystalline phases such as α-Fe, enhancing the stability of the glass phase. The present results show that the attainment of a significantly high GFA is possible even in a quaternary Fe-based alloy system by properly tailoring the competing crystalline phase by the modification of liquid chemistry.


Materials ◽  
2020 ◽  
Vol 13 (1) ◽  
pp. 223 ◽  
Author(s):  
Pan Gong ◽  
Fangwei Li ◽  
Junsong Jin

We developed novel Ti-Zr-Be-Co bulk metallic glasses through Co addition based on a ternary Ti45Zr20Be35 alloy. By altering the alloying routes and alloying contents, the influence of Co alloying on glass-forming ability, thermal stability, thermoplastic formability, crystallization behavior, and corrosion resistance has been investigated systematically. It was found that the best alloying route for enhancing the glass-forming ability, thermoplastic formability, compressive plasticity, and corrosion resistance is to replace Be by Co. Ti45Zr20Be23Co12 possesses the largest critical diameter of 15 mm for glass formation. Ti45Zr20Be27Co8 possesses the highest thermoplastic formability which is comparable to that of Vitreloy alloys. Ti45Zr20Be25Co10 exhibits the largest room temperature plasticity of 15.7% together with a high specific strength of 3.90 × 105 Nm/kg. The addition of Co also strongly affects the crystallization behavior of the base alloy, resulting in a more complex crystallization process. The corrosion resistance of Ti-Zr-Be alloy in 1 mol/L HCl solution can also be enhanced by Co alloying. The related mechanisms have been explained in detail, which provide guidance for the composition design of Ti-based metallic glasses with improved properties.


2022 ◽  
Vol 580 ◽  
pp. 121391
Author(s):  
Liqiao Yue ◽  
Qijing Sun ◽  
Yihao Wang ◽  
Yin Wang ◽  
Rongjie Xue ◽  
...  

Sign in / Sign up

Export Citation Format

Share Document