scholarly journals Al0.5CoCrFeNi2 High Entropy Alloy Particle Reinforced AZ91 Magnesium Alloy-Based Composite Processed by Spark Plasma Sintering

Materials ◽  
2021 ◽  
Vol 14 (21) ◽  
pp. 6520
Author(s):  
Chun Chiu ◽  
Hsun-Hsiang Chang

In this study, AZ91 magnesium-alloy-based metal matrix composites (MMCs) reinforced with 10 wt% of Al0.5CoCrFeNi2 high-entropy alloy (HEA) particles and SiC particles were prepared by a spark plasma sintering (SPS) process at 300 °C. The effects of reinforcements on the microstructure and mechanical properties of AZ91-based MMCs were studied. The results showed that AZ91–HEA composite consisted of α-Mg, Mg17Al12 and FCC phases. No interfacial reaction layer was observed between HEA particles and the Mg matrix. After adding HEA into AZ91, the compressive yield strength (C.Y.S) of the AZ91–HEA composite increased by 17% without degradation of failure strain. In addition, the increment in C.Y.S brought by HEA was comparable to that contributed by commonly used SiC reinforcement (15%). A relatively low porosity in the composite and enhanced interfacial bonding between the α-Mg matrix and HEA particles make HEA a potential reinforcement material in MMCs.

2020 ◽  
Vol 842 ◽  
pp. 83-89
Author(s):  
Dai Hong Xiao ◽  
Min Dong Wu

TiB2/AlFeNiCoCr high-entropy-alloy-matrix composites were fabricated by spark plasma sintering. Effects of SPS process on microstructure and mechanical properties of 0.5 vol.% TiB2/AlFeNiCoCr composites were studied using X-ray diffraction, density testing, scanning electron microscopy, mechanical property testing. It is shown that increasing of sintering temperature and pressure can improve the relative density and compressive properties of 5 vol. %TiB2/AlCoCrFeNi composites. During the spark plasma sintering, there is phase evolution in the composites. The 5 vol. % TiB2/AlCoCrFeNi composite after sintering at 1200 °C and 30 ~ 45 MPa is composed of phases BCC, B2, FCC, σ and TiB2.


Materia Japan ◽  
2018 ◽  
Vol 57 (7) ◽  
pp. 333-337
Author(s):  
Soo-Hyun Joo ◽  
Takeshi Wada ◽  
Hidemi Kato ◽  
Soon-Jik Hong ◽  
Hyoung Seop Kim

Metals ◽  
2020 ◽  
Vol 10 (9) ◽  
pp. 1268 ◽  
Author(s):  
Natalia Shkodich ◽  
Alexey Sedegov ◽  
Kirill Kuskov ◽  
Sergey Busurin ◽  
Yury Scheck ◽  
...  

For the first time, a powder of refractory body-centered cubic (bcc) HfTaTiNbZr-based high-entropy alloy (RHEA) was prepared by short-term (90 min) high-energy ball milling (HEBM) followed by spark plasma sintering (SPS) at 1300 °C for 10 min and the resultant bulk material was characterized by XRD and SEM/EDX. The material showed ultra-high Vickers hardness (10.7 GPa) and a density of 9.87 ± 0.18 g/cm³ (98.7%). Our alloy was found to consist of HfZrTiTaNb-based solid solution with bcc structure as a main phase, a hexagonal closest packed (hcp) Hf/Zr-based solid solution, and Me2Fe phases (Me = Hf, Zr) as minor admixtures. Principal elements of the HEA phase were uniformly distributed over the bulk of HfTaTiNbZr-based alloy. Similar alloys synthesized without milling or in the case of low-energy ball milling (LEBM, 10 h) consisted of a bcc HEA and a Hf/Zr-rich hcp solid solution; in this case, the Vickers hardness of such alloys was found to have a value of 6.4 GPa and 5.8 GPa, respectively.