Demineralized bone matrix (DBM)-calcium phosphate cement (CPC) composites were subjected to cellular test of osteogenic potentials and implantation in animal model. The expression of osteogenic marker gene from mouse preosteoblast cell line MC3T3-E1 adhered to the DBM-CPC composite was much higher than plain CPC. In addition, the DBM-CPC composite implanted nude mice revealed osteoinduction between the implanted composite and adjacent tissues, whereas the plain CPC induced osteoconduction.


2005 ◽  
Vol 288-289 ◽  
pp. 63-66 ◽  
Author(s):  
Lei Cui ◽  
Dong Li ◽  
Xiang Dong Liu ◽  
Fanfan Chen ◽  
Wei Liu ◽  
...  

Objective The purpose of this study is to explore the growth, differentiation and osteogeneration of bone marrow stromal cells (BMSCs) on partially demineralized bone matrix (pDBM) and to generate bone tissue by tissue engineering approach in vivo. Methods Demineralized bone was processed from femur head of Shanghai white swine. Calcium content, porosity and pore size was measured respectively. In vitro osteogenic differentiated human BMSCs of passage 3 were seeded in pDBM. Adhesive rate of cells to pDBM was calculated 24hours after seeding. Distribution, growth and proliferation of BMSCs on pDBM were observed with fluorescent DiI labeling. Matrix disposition was analyzed with SEM observation. Cell-material complex was implanted subcutaneously in nude mice. The implants were harvested at 8, 12 weeks post surgery and samples were observed by H&E staining. Results BMSCs adhered well on the material and the distribution of cells was uniform. The adhesive rate is 99.1%±1%. New bone formation was observed in implant of 8, 12 weeks respectively. The newly formed bone was generated on the surface of the residual material and a layer of cells with typical characteristic of osteoblast was observed to adhere on the surface of the new bone. Conclusion With good biocompatibility to hBMSCs, pDBM could serve as ideal scaffold for bone tissue engineering both in vitro and in vivo.


2021 ◽  
Vol 25 (1) ◽  
Author(s):  
Thakoon Thitiset ◽  
Siriporn Damrongsakkul ◽  
Supansa Yodmuang ◽  
Wilairat Leeanansaksiri ◽  
Jirun Apinun ◽  
...  

Abstract Background A novel biodegradable scaffold including gelatin (G), chitooligosaccharide (COS), and demineralized bone matrix (DBM) could play a significant part in bone tissue engineering. The present study aimed to investigate the biological characteristics of composite scaffolds in combination of G, COS, and DBM for in vitro cell culture and in vivo animal bioassays. Methods Three-dimensional scaffolds from the mixture of G, COS, and DBM were fabricated into 3 groups, namely, G, GC, and GCD using a lyophilization technique. The scaffolds were cultured with mesenchymal stem cells (MSCs) for 4 weeks to determine biological responses such as cell attachment and cell proliferation, alkaline phosphatase (ALP) activity, calcium deposition, cell morphology, and cell surface elemental composition. For the in vivo bioassay, G, GC, and GCD, acellular scaffolds were implanted subcutaneously in 8-week-old male Wistar rats for 4 weeks and 8 weeks. The explants were assessed for new bone formation using hematoxylin and eosin (H&E) staining and von Kossa staining. Results The MSCs could attach and proliferate on all three groups of scaffolds. Interestingly, the ALP activity of MSCs reached the greatest value on day 7 after cultured on the scaffolds, whereas the calcium assay displayed the highest level of calcium in MSCs on day 28. Furthermore, weight percentages of calcium and phosphorus on the surface of MSCs after cultivation on the GCD scaffolds increased when compared to those on other scaffolds. The scanning electron microscopy images showed that MSCs attached and proliferated on the scaffold surface thoroughly over the cultivation time. Mineral crystal aggregation was evident in GC and greatly in GCD scaffolds. H&E staining illustrated that G, GC, and GCD scaffolds displayed osteoid after 4 weeks of implantation and von Kossa staining confirmed the mineralization at 8 weeks in G, GC, and GCD scaffolds. Conclusion The MSCs cultured in GCD scaffolds revealed greater osteogenic differentiation than those cultured in G and GC scaffolds. Additionally, the G, GC, and GCD scaffolds could promote in vivo ectopic bone formation in rat model. The GCD scaffolds exhibited maximum osteoinductive capability compared with others and may be potentially used for bone regeneration.


2012 ◽  
Vol 1417 ◽  
Author(s):  
Titilayo Moloye ◽  
Christopher Batich

ABSTRACTCylindrical porous polycaprolactone (PCL) scaffolds containing 25, 35, and 50 wt% demineralized bone matrix (DBM) were fabricated using a salt-leaching method for application in bone engineering. In the present work, PCL-DBM scaffolds were monitored for calcium and phosphorus deposition in both deionized (DI) water and simulated body fluid (SBF) for time periods of 5, 10, 15, and 20 days at 37°C under constant rotation. An in vitro assessment of the bioactivity of synthetic materials using SBF under physiological conditions can be used as a barometer of scaffold behavior in vivo. DBM, an osteoinductive material, was used to gauge if there was a correlation between the concentration of DBM within a scaffold and the apatite formation on its surface. Biochemical assays, alizarin red S staining, and scanning electron microscopy (SEM) with elemental analysis of calcium and phosphorus were consistent in that they confirmed that PCL scaffolds containing 35 wt% DBM in SBF at 14 days post-immersion showed signs of early apatite formation.


2013 ◽  
Vol 24 (6) ◽  
pp. 2135-2140 ◽  
Author(s):  
Shima Tavakol ◽  
Ahad Khoshzaban ◽  
Mahmoud Azami ◽  
Iraj Ragerdi Kashani ◽  
Hani Tavakol ◽  
...  

2018 ◽  
Vol 33 (2) ◽  
pp. 182-195 ◽  
Author(s):  
Qiannan Li ◽  
Wenjie Zhang ◽  
Guangdong Zhou ◽  
Yilin Cao ◽  
Wei Liu ◽  
...  

Insufficient neo-vascularization of in vivo implanted cell-seeded scaffold remains a major bottleneck for clinical translation of engineered bone formation. Demineralized bone matrix is an ideal bone scaffold for bone engineering due to its structural and biochemical components similar to those of native bone. We hypothesized that the microcarrier form of demineralized bone matrix favors ingrowth of vessels and bone regeneration upon in vivo implantation. In this study, a rat model of femoral vessel pedicle-based bone engineering was employed by filling the demineralized bone matrix scaffolds inside a silicone chamber that surrounded the vessel pedicles, and to compare the efficiency of vascularized bone regeneration between microcarrier demineralized bone matrix and block demineralized bone matrix. The results showed that bone marrow stem cells better adhered to microcarrier demineralized bone matrix and produced more extracellular matrices during in vitro culture. After in vivo implantation, microcarrier demineralized bone matrix seeded with bone marrow stem cells formed relatively more bone tissue than block demineralized bone matrix counterpart at three months upon histological examination. Furthermore, micro-computed tomography three-dimensional reconstruction showed that microcarrier demineralized bone matrix group regenerate significantly better and more bone tissues than block demineralized bone matrix both qualitatively and quantitatively (p < 0.05). Moreover, micro-computed tomography reconstructed angiographic images also demonstrated significantly enhanced tissue vascularization in microcarrier demineralized bone matrix group than in block demineralized bone matrix group both qualitatively and quantitatively (p < 0.05). Anti-CD31 immunohistochemical staining of (micro-) vessels and semi-quantitative analysis also evidenced enhanced vascularization of regenerated bone in microcarrier demineralized bone matrix group than in block demineralized bone matrix group (p < 0.05). In conclusion, the microcarrier form of demineralized bone matrix is an ideal bone regenerative scaffold due to its advantages of osteoinductivity and vascular induction, two essentials for in vivo bone regeneration.


1989 ◽  
Vol 7 (1) ◽  
pp. 22-27 ◽  
Author(s):  
Zachary B. Friedenberg ◽  
Carl T. Brighton ◽  
James D. Michelson ◽  
John Bednar ◽  
Richard Schmidt ◽  
...  

Sign in / Sign up

Export Citation Format

Share Document