This paper performs analytical and experimental investigation on the section properties of locally produced cold-formed steel sections. Effective width method given by BS EN1993-1-3 is used to calculate the section properties for two slender cold-formed steel channel sections, namely KS200C20 and KS250C20. Local buckling and distortional buckling are taken into account in the calculation. Effective width method has significantly reduced the full sectional area and thus gives a relative lower value for the sectional resistance of cold-formed steel channel sections. The analytical results is compared to manufacturer’s data and differences of not more than 3.37% is recorded. Experimental study on the flexural behaviour on the two types of cold-formed steel channel sections is carried out. The results show that BS EN1993-1-3 has good agreement with experimental results for flexural resistance that included local and distortional buckling consideration. It is concluded that effective width method by BS EN1993-1-3 is suitable to calculate the section properties of of locally produced cold-formed steel channel sections.

1984 ◽  
Vol 11 (1) ◽  
pp. 1-7 ◽  
Author(s):  
Robert Loov

Load tests were carried out on 36 stub column samples of cold-formed steel studs having 38.1 mm wide × 44.5 mm long holes punched through their webs, steel thicknesses of 1.21–2.01 mm, and overall section depths of 63–204 mm. Based on these tests a best-fit equation for the effective width of the unstiffened portion of the web beside the holes has been developed. Suggested design equations have been proposed. The test results support the present equation for the average yield stress [Formula: see text] in Canadian Standards Association Standard S136-1974 but the present code equations for unstiffened plates are unduly conservative when applied to the design of the web adjacent to openings of the size considered.


2010 ◽  
Vol 163-167 ◽  
pp. 651-654
Author(s):  
Tian Hua Zhou ◽  
Shao Feng Nie ◽  
Xiang Bin Liu ◽  
Guang Yi Li

18 specimens of cold-formed steel three limbs built-up section members are tested under axial compression load in this paper. The section forms are divided into two categories: A and B. Load-displacement (P-Δ) curves and failure characteristics of specimens are obtained. The results show that: As to section A members, the failure characteristics of LC, MC and SC series of specimens are flexural-torsional buckling, torsional buckling and distortional buckling, local buckling and distortional buckling. As to section B members, the failure characteristics of LC, MC series of specimens are flexural buckling, while local buckling and distortional buckling for members of SC series.


2021 ◽  
Vol 2021 ◽  
pp. 1-21
Author(s):  
Xingyou Yao

The cold-formed steel (CFS) lipped channel section with circular holes has been widely used in low-rise and multistory building structures as the column. However, the circular hole in the web makes the lipped channel column become susceptible to buckle. A total of 54 CFS lipped channel axial compression columns with and without circular holes were used to study the buckling behavior and the effective width design method. The interaction of the local buckling and the distortional buckling were observed for the short and intermediate columns, while the slender columns were controlled by the interaction of the local buckling, distortional buckling, and flexural buckling or flexural-torsional buckling. The experimental failure loads were gradually decreased with the increase in the diameter of the circular hole for the specimens with the same section. The failure loads of the specimens with two holes were lower than those of the specimens with one hole with same section and same diameter of holes. Then, the experimental results were used to validate a nonlinear finite element model (FEM) previously developed by the authors. The validated FEM was subsequently used to obtain additional 36 numerical failure results concerning the effects of the length, the section, and the diameter and the number of the circular holes. Furthermore, the proposal to calculate the distortional buckling coefficient of the CFS lipped channel section with circular holes were put forward based on numerical analysis considering the reduction of effect of holes. Finally, a proposal to improve the effective width method (EWM) design approach for CFS lipped channel sections with circular holes under axial compression was presented. The comparisons between experimental and numerical capacities and their calculations provided by the proposed EWM design method illustrate a great application of the proposed approach.


1992 ◽  
Vol 19 (1) ◽  
pp. 39-50 ◽  
Author(s):  
Aaron S. Dinovitzer

The lip dimension of cold formed steel C-sections (channels) is optimized according to the provisions of CSA Standard CAN/CSA-S136-M89 "Cold formed steel structural members." The provisions in the 1989 edition of S136 are compared with those of the 1984 edition. Due to changes in design criteria, previously optimal sections are no longer optimal. The interaction of many of the elements is described and the manner in which the design standard takes the interaction into account is discussed. The lip sizes of C-sections are optimized in order to maximize flexural resistance and minimize cross-sectional area. An optimal C-section is one in which the flange is nearest to being fully effective. The optimal geometry generally has a lip-to-flange ratio of 3/8, which is restricted by a maximum lip flat width of 14 times the steel thickness. An optimal section based on the 1989 edition of S136 has a lower flexural resistance and a longer lip than an optimal C-section based on the 1984 edition of S136. Due to certain changes in the 1989 edition of S136, cold work of forming is now applicable in fewer cases than previously allowed by the 1984 edition of S136. Key words: cold formed steel, effective width, stiffener, lip, C-section, channel, optimization.


2011 ◽  
Vol 201-203 ◽  
pp. 2900-2903 ◽  
Author(s):  
Chui Huon Tina Ting ◽  
Hieng Ho Lau

Built-up sections are used to resist load induced in a structure when a single section is not sufficient to carry the design load for example roof trusses. In current North American Specification, the provision has been substantially taken from research in hot-rolled built-up members connected with bolts or welds [1]. The aim of this paper is to investigate on built-up back-to-back channels stub columns experimentally and theoretically using Effective Width Method and Direct Strength Method. Compression test was performed on 5 lipped channel and 5 back-to-back channels stub columns fabricated from cold-formed steel sheets of 1.2mm thicknesses. The test results indicated that local buckling is the dominant failure modes of stub columns. Therefore, Effective Width Method predicts the capacity of stub columns compared to Direct Strength Method. When compared to the average test results, results based on EWM are 5% higher while results based on DSM are 12% higher for stub column.


Author(s):  
Majahar M. Baraskar ◽  
Pranil Shetake ◽  
Prof. V. M Bogar ◽  
Dr. Y. M Ghugal

Steel is used in construction industry due to its hardness and tensile strength. Cold formed steel is type of steel which is manufactured at lower temperature. Cold form steel became more popular in twentieth century in construction industry due to its high strength to weight ratio and post-buckling strength. The purpose of this study is to study the behavior of cold-formed steel sections of different shapes but of same cross sectional area for compressive loading. Effect of lips within same cross sectional area, effect of perforation and shape stiffener is evaluated on different sections as channel section, Z section and hat section. Eigen value buckling analysis was carried out to on twelve different models to obtain the buckling load and failure pattern. ANSYS WORKBENCH software was used for numerical simulation of sections. I.S. 801:1975 has been taken under consideration wherever required. Based upon the results, optimum section in each of cases as with lips, without lips and perforated amongst all three sections is suggested. Effect of shape stiffeners provided by previous researcher P. Manikandan on solid sections is evaluated to check its suitability with perforated sections.


2011 ◽  
Vol 473 ◽  
pp. 343-351 ◽  
Author(s):  
Iveta Georgieva ◽  
Luc Schueremans ◽  
Guido De Roeck ◽  
Lincy Pyl

The construction industry uses cold-formed steel (CFS) sheets in the form of galvanised thin-walled profiles and corrugated sheets. In the past decade, CFS profiles have been competing with their hot-rolled counterparts as primary structural members of industrial halls, office buildings and residential housing of up to 3-4 storeys. The spans and column heights achieved with CFS profiles are ever larger. Due to the large slenderness of these members, adequate strength and stability are necessary, as well as reliability in design. Thin-walled members go through buckling during all stages of their working life. Local buckling appears at loads sometimes much lower than the design load. Distortional buckling seriously reduces the member resistance. It interacts with warping and lateral-torsional buckling, being significant for these asymmetric open sections. To restrict these effects, builders employ double sections - usually two standard cold-formed shapes bolted together to form a built-up section. These sections have the advantages of symmetry, higher stability and strength. The design of built-up members involves many uncertainties - although the European standard includes guidelines on the prediction of local, distortional and global buckling, the partial integrity and interaction between the parts of the composed members is still not studied. To study the actual behaviour, built-up members are tested in bending. An optical device for 3D motion analysis measures the displacement of points of interest on the specimen. Two interacting cameras use parallax to obtain the position of an arbitrary number of reflective markers glued to the specimen. The device tracks the movement of the markers in a 3D coordinate system without any contact with the specimen. Standard displacement transducers measure vertical displacements to validate the results. The paper gives an appraisal of the applicability of the method, a summary of the difficulties faced and the outcome of the test campaign.