Modulation of bactericidal action in polymer nanocomposites: light-tuned Ag+ release from electrospun PMMA fibers

RSC Advances ◽  
2016 ◽  
Vol 6 (81) ◽  
pp. 78036-78042 ◽  
Author(s):  
I. Moreno ◽  
N. Navascues ◽  
S. Irusta ◽  
J. Santamaria

Silver rate release from electrospun PMMA fibers tuned by combination of silver ions and silver nanoparticles produced by UV irradiation.

Chemosphere ◽  
2020 ◽  
Vol 247 ◽  
pp. 125937 ◽  
Author(s):  
Min Liu ◽  
Xinyu Gao ◽  
Fei Pan ◽  
Yuwei Deng ◽  
Dongsheng Xia ◽  
...  

Author(s):  
Vidyasagar G M ◽  
Shankaravva B ◽  
R Begum ◽  
Imrose ◽  
Sagar R ◽  
...  

Microorganisms like fungi, actinomycetes and bacteria are considered nanofactories and are helpful in the production of nanoparticles useful in the welfare of human beings. In the present study, we investigated the production of silver nanoparticles from Streptomyces species JF714876. Extracellular synthesis of silver nanoparticles by Streptomyces species was carried out using two different media. Silver nanoparticles were examined using UV-visible, IR and atomic force microscopy. The size of silver nanoparticles was in the range of 80-100 nm. Antimicrobial activity of silver nanoparticle against bacteria such as E. coli, S. aureus, and dermatophytes like T. rubrum and T. tonsurans was determined. Thus, this study suggests that the Streptomyces sp. JF741876 can produce silver ions that can be used as an antimicrobial substance.


2021 ◽  
pp. 1-14
Author(s):  
N.U.H. Altaf ◽  
M.Y. Naz ◽  
S. Shukrullah ◽  
H.N. Bhatti

In this study, silver nanoparticles (AgNPs) were produced through an atmospheric pressure plasma reduction reaction and tested for photodegradation of methyl blue (MB) under sunlight exposure. The argon plasma born reactive species were used to reduce silver ions to AgNPs in the solution. Glucose, fructose and sucrose were also added in the solution to stabilize the growth process. The glucose stabilized reaction produced the smallest nanoparticles of 12 nm, while sucrose stabilized reaction produced relatively larger nanoparticles (14 nm). The nanoparticles exhibited rough morphology and narrow diameter distribution regardless of stabilizer type. The narrow diameter distribution and small band gap helped activating majority of nanoparticles at a single wavelength of light spectrum. The band gap energy of AgNPs varied from 2.22 eV to 2.41 eV, depending on the saccharide type. The photoluminescence spectroscopy of AgNPs produced emission peaks at 413 nm, 415 nm, and 418 nm. The photocatalytic potential of AgNP samples was checked by degrading MB dye under sunlight. The degradation reaction reached a saturation level of 98% after 60 min of light exposure.


2021 ◽  
Vol 359 ◽  
pp. 129859
Author(s):  
Li Wang ◽  
Govindasami Periyasami ◽  
Ali Aldalbahi ◽  
Vincenzo Fogliano

Materials ◽  
2019 ◽  
Vol 12 (15) ◽  
pp. 2382 ◽  
Author(s):  
Muhammad Jamshed Khan ◽  
Suriya Kumari ◽  
Kamyar Shameli ◽  
Jinap Selamat ◽  
Awis Qurni Sazili

Nanoparticles (NPs) are, frequently, being utilized in multi-dimensional enterprises. Silver nanoparticles (AgNPs) have attracted researchers in the last decade due to their exceptional efficacy at very low volume and stability at higher temperatures. Due to certain limitations of the chemical method of synthesis, AgNPs can be obtained by physical methods including sun rays, microwaves and ultraviolet (UV) radiation. In the current study, the synthesis of pullulan mediated silver nanoparticles (P-AgNPs) was achieved through ultraviolet (UV) irradiation, with a wavelength of 365 nm, for 96 h. P-AgNPs were formed after 24 h of UV-irradiation time and expressed spectra maxima as 415 nm, after 96 h, in UV-vis spectroscopy. The crystallographic structure was “face centered cubic (fcc)” as confirmed by powder X-ray diffraction (PXRD). Furthermore, high resolution transmission electron microscopy (HRTEM) proved that P-AgNPs were covered with a thin layer of pullulan, with a mean crystalline size of 6.02 ± 2.37. The average lattice fringe spacing of nanoparticles was confirmed as 0.235 nm with quasi-spherical characteristics, by selected area electron diffraction (SAED) analysis. These green synthesized P-AgNPs can be utilized efficiently, as an active food and meat preservative, when incorporated into the edible films.


2017 ◽  
Vol 137 ◽  
pp. 18-28 ◽  
Author(s):  
Petra Cvjetko ◽  
Anita Milošić ◽  
Ana-Marija Domijan ◽  
Ivana Vinković Vrček ◽  
Sonja Tolić ◽  
...  

2014 ◽  
Vol 2014 ◽  
pp. 1-11 ◽  
Author(s):  
M. A. El-Sheikh

The water soluble photoinitiator (PI) 4-(trimethyl ammonium methyl) benzophenone chloride is used for the first time in the synthesis of silver nanoparticles (AgNPs). A new green synthesis method involves using PI/UV system, carboxymethyl starch (CMS), silver nitrate, and water. A mechanism of the reduction of silver ions to AgNPs by PI/UV system as well as by the newly born aldehydic groups was proposed. The synthesis process was assessed by UV-vis spectra and TEM of AgNPs colloidal solution. The highest absorbance was obtained using CMS, PI and AgNO3concentrations of 10 g/L, 1 g/L, and 1 g/L, respectively; 40°C; 60 min; pH 7; and a material : liquor ratio 1 : 20. AgNPs so-obtained were stable in aqueous solution over a period of three weeks at room temperature (~25°C) and have round shape morphology. The sizes of synthesized AgNPs were in the range of 1–21 nm and the highest counts % of these particles were for particles of 6–10 and 1–3 nm, respectively.


2021 ◽  
Vol 892 ◽  
pp. 36-42
Author(s):  
Muhammad Iqbal Hidayat ◽  
Muhammad Adlim ◽  
Ilham Maulana ◽  
Muhammad Zulfajri

Silver nanoparticles (Ag0) have attracted the most attention due to their broad antimicrobial application and outstanding activity. The silver nanoparticles are usually in colloidal form, then immobilization the colloid onto solid support is still interesting to explore. In this work, a new method for silver colloidal nanoparticle immobilization on silica gel beads (SiG), which was then symbolized as Ag0-[chi-SiG] was conducted and characterized successfully. The finding proved that SiG must be coated with three chitosan film layers to give stable support for silver nanoparticles. This coating method caused the chitosan completely covered SiG, and the chitosan film provides coordination bonding for silver ions. The most appropriate solvent for silver ion impregnation on the surface of chi-SiG is methanol compared to other solvents. Tungsten lamp as the photo-irradiation, which is low cost and environmentally friendly has been proven effective for silver ion reduction, as shown by silver metal colloid UV-Vis surface plasmon resonance at 400-700 nm. Ag0-[chi-SiG] showed the antibacterial properties of inhibiting the growth Staphylococcus aureus and Escherichia coli; then it provides the potential application for antibacterial filter material. According to the weight comparison between antibacterial standard and Ag content, then Ag0-[chi-SiG] has two and five times higher of exhibiting zone for each bacteria.