scholarly journals Polymerization Shrinkage of Bulk Fill Composites and its Correlation with Bond Strength

2018 ◽  
Vol 29 (3) ◽  
pp. 261-267 ◽  
Author(s):  
Lauber Jose dos Santos Almeida Junior ◽  
Estevam Carlos de Oliveira Lula ◽  
Karla Janilee de Souza Penha ◽  
Vinicius Souza Correia ◽  
Fernando Augusto Cintra Magalhães ◽  
...  

Abstract The present study aimed to evaluates polymerization shrinkage (PS) using microcomputed tomography (μCT) and microtensile bond strength (μTBS) in bulk fill composites (BFC) and conventional class I restorations as well as the correlation between these factors. Class I cavities (4 x 5 x 4 mm), factor-C = 4.2, were created in third molars that were free of caries, which were randomly divided in 4 groups (n = 6): XTI (Filtek Supreme XTE: incremental technique); XTB (Filtek Supreme XTE: single fill technique); TBF (Tetric Bulk Fill); and SF (SonicFill). Each tooth was scanned twice in μCT: T0 was after filling the cavity with composite, and T1 was after light curing. The data were analyzed by subtracting the composite volume for each time (T1 - T0). After 1 week, the teeth were sectioned crosswise in the buccolingual and mesiodistal directions to obtain specimens with approximately 1 mm² thickness and fixed in a universal testing machine to perform μTBS. The Kruskal-Wallis and Dunn tests showed a statistically significant difference for shrinkage in µCT among the XTI and XTB and between the SF and XTB. Regarding the μTBS, all the groups differed from XTB. Bulk fill composites type presents a PS similar to that of the conventional nanoparticulate composite inserted using the incremental technique, but the bond strength was higher for the incremental group, which presented a lower number of pre-test failures when compared to BFC. No correlation was observed between the polymerization shrinkage and bond strength in the studied composites.

2017 ◽  
Vol 16 ◽  
pp. 1-7
Author(s):  
Bruna Genari ◽  
Vicente Castelo Branco Leitune ◽  
João Henrique Macedo Saucedo ◽  
Susana Maria Werner Samuel ◽  
Fabrício Mezzomo Collares

Self-adhesive, dual-polymerizing resin cements require no treatment to the prepared tooth surfaces before cementation. Aim: The aim of this study was to evaluate the influence of curing mode on bond strength (BS) of three cementing systems to bovine dentin. Methods: The buccal enamel surfaces of 50 bovine incisors were removed to expose dentin and to flat the surface. The teeth were divided into five groups (n=10), which consisted of two resin cements (Multilink and Clearfil SA Cement) that were tested in dual- (halogen light for 40 s) and self-cured modes, and a control (RelyX ARC). Two cylinders of resin cements (1.0 mm X 0.75 mm) were prepared on each bonded dentin surface. After 24h at 37oC, resin cylinders were subjected to micro-shear testing in a universal testing machine (4411/Instron - 0.5 mm/min). Data were statistically analyzed by two-way ANOVA, Tukey and Dunnett`s test (5%). Results: Multilink showed higher BS than those observed on Clearfil SA. Light-curing resulted in higher BS for both Multilink and Clearfil SA. When Multilink was light-cured, no significant difference on BS was demonstrated between it and RelyX ARC. Conclusions: The highest BS values were obtained in control group and light-cured Multilink resin cement.


2020 ◽  
Vol 49 ◽  
Author(s):  
Raquel Devisate BORGHI ◽  
Erick Kamiya COPPINI ◽  
Josué Junior Araújo PIEROTE ◽  
João Victor Frazão CÂMARA ◽  
Luis Alexandre Maffei Sartini PAULILLO

Abstract Introduction To prevent the shrinkage stresses produced during polymerization, composite resins of low polymerization shrinkage were developed. Objective To evaluate the microtensile bond strength in class I cavities restored by acid-etching the cavosurface angle and with composite resins indicated for posterior teeth. Material and method 48 healthy molars were selected and divided into six groups (n = 8), considering that the cavosurface enamel of three groups was etched with 35% phosphoric acid. The teeth were restored with the Clearfil SE Bond adhesive system and Filtek Z350 XT, Empress Direct, and Charisma Diamond composite resins, which were light-cured for 40 seconds. After 24 hours, the teeth were taken to a cutting machine, which produced sections in the buccolingual and mesiodistal directions. This resulted in toothpicks of 0.9×0.9 mm that were taken to the universal testing machine for the microtensile bond strength test. Statistical analysis was performed with ANOVA and Tukey’s test (p < 0.05). Result There was no statistically significant difference between the groups evaluated. Conclusion Acid-etching the cavosurface angle did not affect the performance of restorations, probably due to the adhesive system used.


2011 ◽  
Vol 22 (6) ◽  
pp. 468-472 ◽  
Author(s):  
Klíssia Romero Felizardo ◽  
Letícia Vargas Freire Martins Lemos ◽  
Rodrigo Varella de Carvalho ◽  
Alcides Gonini Junior ◽  
Murilo Baena Lopes ◽  
...  

This study analyzed the bond strength (BS) of HEMA versus HEMA-free self-etch adhesive systems to dentin. The occlusal surface of 20 third molars was removed and the dentin was abraded with 600-grit silicon carbide paper. The teeth were randomly assigned to 4 groups (n=5) and restored with GO, Adper SE Plus, OptiBond All-In-One, and Clearfil 3S Bond adhesive systems and Filtek Z350 composite. After light curing (600 mW/cm²), the teeth were stored in distilled water at 37ºC for 24 h and were sectioned in the mesiodistal and buccolingual directions to obtain sticks (0.8 mm²). The sticks were subjected to tensile force using a universal testing machine (0.5 mm/min), and the modes of failure were analyzed by scanning electron microscopy and classified as adhesive, cohesive, or mixed. The BS data (in MPa) were treated using one-way ANOVA and Tukey’s tests at 5% significance. GO presented the lowest mean bond strength value (10.57 ± 3.72) and differed significantly from the other materials (p=0.001), which, in turn, presented statistically similar results (p>0.05) among themselves: Adper SE Plus (29.08 ± 8.93), OptiBond All-In-One (28.36 ± 6.49), and Clearfil 3S Bond (28.62 ± 6.97). Mixed fractures were the most prevalent. It was concluded that the influence of HEMA on BS to dentin was material dependent.


2009 ◽  
Vol 03 (03) ◽  
pp. 173-177 ◽  
Author(s):  
Ahmet Yalcin Gungor ◽  
Hakan Turkkahraman ◽  
Necdet Adanir ◽  
Huseyin Alkis

ABSTRACTObjectives: To evaluate the effects fluorosis and self etching primers (SEP) on shear bond strengths (SBS) of orthodontic brackets.Methods: A total of 48 (24 fluorosed and 24 non-fluorosed) non-carious freshly extracted human permanent premolar teeth were used in this study. Fluorosed teeth were selected according to the modified Thylstrup and Fejerskov index (TFI), which is based on the clinical changes in fluorosed teeth. Fluorosed and non-fluorosed teeth were randomly assigned to 4 groups of 12 each. In groups I (non-fluorosed teeth) and II (fluorosed teeth), standard etching protocol was used and brackets were bonded with Light Bond. In groups III (non-fluorosed teeth) and IV (fluorosed teeth), Transbond Plus SEP was used and brackets were bonded with Transbond XT Light Cure Adhesive. All specimens were cured with a halogen light. After bonding, SBS of the brackets were tested with Universal testing machine. After debonding, all teeth and brackets in the test groups were examined under 10x magnifications. Any adhesive remained after debonding was assessed and scored according to the modified Adhesive Remnant Index (ARI).Results: ANOVA indicated a significant difference between groups (P<.001). SBS in group II (Light Bond+Fluorosis) were significantly lower than other groups. ARI scores of the groups were also significantly different (P<.001). There was a greater frequency of ARI scores of 1,2 and 3 in group II (Light Bond+Fluorosis).Conclusions: When standard etching protocol was used enamel fluorosis significantly decreased the bond strength of orthodontic brackets. Satisfactory bond strengths were obtained when SEP was used for bonding brackets to the fluorosed teeth. (Eur J Dent 2009;3:173-177)


2017 ◽  
Vol 15 (4) ◽  
pp. 258
Author(s):  
Marcelo Giannini ◽  
Andreia Assis Carvalho ◽  
Ariovaldo Stefani ◽  
Wladimir Franco de Sá Barbosa ◽  
Lawrence Gonzaga Lopes

Self-adhesive, dual-polymerizing resin cements require no treatment to the prepared tooth surfaces before cementation. Aim: The aim of this study was to evaluate the influence of curing mode on bond strength (BS) of three cementing systems to bovine dentin. Methods: The buccal enamel surfaces of 50 bovine incisors were removed to expose dentin and to flat the surface. The teeth were divided into five groups (n=10), which consisted of two resin cements (Multilink and Clearfil SA Cement) that were tested in dual- (halogen light for 40 s) and self-cured modes, and a control (RelyX ARC). Two cylinders of resin cements (1.0 mm X 0.75 mm) were prepared on each bonded dentin surface. After 24h at 37oC, resin cylinders were subjected to micro-shear testing in a universal testing machine (4411/Instron - 0.5 mm/min). Data were statistically analyzed by two-way ANOVA, Tukey and Dunnett`s test (5%). Results: Multilink showed higher BS than those observed on Clearfil SA. Light-curing resulted in higher BS for both Multilink and Clearfil SA. When Multilink was light-cured, no significant difference on BS was demonstrated between it and RelyX ARC. Conclusions: The highest BS values were obtained in control group and light-cured Multilink resin cement.


2015 ◽  
Vol 2015 ◽  
pp. 1-6 ◽  
Author(s):  
Baraba Anja ◽  
Dukić Walter ◽  
Chieffi Nicoletta ◽  
Ferrari Marco ◽  
Sonja Pezelj Ribarić ◽  
...  

The purpose of thisin vitrostudy was to evaluate the microtensile bond strength of one-step self-etch adhesive to human dentin surface modified with air abrasion and sonic technique and to assess the morphological characteristics of the pretreated dentin surface. The occlusal enamel was removed to obtain a flat dentin surface for thirty-six human molar teeth. The teeth were randomly divided into three experimental groups (n= 12 per group), according to the pretreatment of the dentin: (1) control group, (2) air abrasion group, and (3) sonic preparation group. Microtensile bond strength test was performed on a universal testing machine. Two specimens from each experimental group were subjected to SEM examination. There was no statistically significant difference in bond strength between the three experimental groups (P> 0.05). Mean microtensile bond strength (MPa) values were 35.3 ± 12.8 for control group, 35.8 ± 13.5 for air abrasion group, and 37.7 ± 12.0 for sonic preparation group. The use of air abrasion and sonic preparation with one-step self-etch adhesive does not appear to enhance or impair microtensile bond strength in dentin.


2011 ◽  
Vol 82 (1) ◽  
pp. 158-164 ◽  
Author(s):  
Maria Francesca Sfondrini ◽  
Esmeralda Xheka ◽  
Andrea Scribante ◽  
Paola Gandini ◽  
Giuseppe Sfondrini

Abstract Objective: To test the null hypothesis that there is no significant difference in the shear bond strength (SBS) and Adhesive Remnant Index (ARI) scores of new vs reconditioned self-ligating brackets. Materials and Methods: One hundred and twenty permanent extracted bovine teeth were embedded in resin blocks. Three different new and reconditioned self-ligating orthodontic brackets (Smart Clip [3M Unitek]; Quick [Forestadent]; and Damon3MX [Ormco]) were tested. Scanning electron microphotographs of the different new (groups 1, 3, and 5) and reconditioned (groups 2, 4, and 6) bracket bases were taken before starting the experiments. Brackets were then bonded to the teeth using an orthodontic adhesive and were then tested in shear mode using an Instron Universal Testing Machine. ARI scores were then recorded. Statistical analysis was performed to determine significant differences in SBS and ARI Scores. Results: Smart Clip and Damon3MX reconditioned brackets showed significantly lower SBS than did new ones. On the contrary, Quick reconditioned brackets showed significantly higher SBS than did new ones. No significant differences in ARI scores were found after the reconditioning process for the three different brackets tested. Conclusion: The in-office reconditioning procedure alters the SBS of self-ligating brackets, although SBS values still remain clinically acceptable.


2001 ◽  
Vol 25 (1) ◽  
pp. 57-63 ◽  
Author(s):  
Azza El-Housseiny ◽  
Hana Jamjoum

This study was undertaken to evaluate the effect of caries detector dyes and/or cavity cleanser on composite bonding and etching patterns of enamel and dentin. One hundred and eight non-carious premolars were divided into six groups according to the enamel and dentin pretreatment investigated. The different pretreatment were as follows: Group I: teeth with prophylaxis only, Group II: Sable seek caries detector dye,Groups III: chlorhexidine cavity cleanser,Group IV: the caries detectors dye followed by prophylaxis, Group V: the cavity cleanser followed by the caries detector dye, and Group IV: Snoop caries detector dye. The shear bond strength of composite resin bonded to enamel and dentin was evaluated by the Instron Universal testing machine while, the topographic details of enamel and dentin were examined by the SEM following the different pretreatment and acid etching. Results of the shear bond strength showed no statistically significant difference among the six groups, with no substantial differences in SEM results. It is concluded that using the caries detector dyes and/or chlorhexidine cavity cleanser before acid etching does not significantly affect composite bonding to enamel and dentin.


2004 ◽  
Vol 12 (4) ◽  
pp. 280-284 ◽  
Author(s):  
Mariana Pretti ◽  
Edson Hilgert ◽  
Marco Antônio Bottino ◽  
Rander Pereira Avelar

INTRODUCTION: Based on the importance of the integrity of the metal/ceramic interface, the purpose of this work was to evaluate the shear bond strength of the metal-ceramic union of two Co-Cr alloys (Wirobond C, Bego; Remanium 2000, Dentaurum) combined with Omega 900 ceramic (Vita Zahnfabrik). MATERIAL AND METHOD: Eleven cylindrical matrixes were made for each alloy, and the metallic portion was obtained with the lost wax casting technique with standardized waxing of 4mm of height and of 4mm of diameter. The ceramic was applied according to the manufacturer's recommendations with the aid of a teflon matrix that allowed its dimension to be standardized in the same size as the metallic portion. The specimens were submitted to the shear bond test in an universal testing machine (EMIC), with the aid of a device developed for such intention, and constant speed of 0.5mm/min. RESULTS AND CONCLUSIONS: The mean resistance was 48.387MPa for Wirobond C alloy, with standard deviation of 17.718, and 55.956MPa for Remanium 2000, with standard deviation of 17.198. No statistically significant difference was observed between the shear strength of the two metal-ceramic alloys.


2021 ◽  
pp. 030157422110044
Author(s):  
I Ranganayakulu ◽  
D Praveen Kumar Varma ◽  
Padma Priya CV ◽  
RSVM Raghu Ram ◽  
K Anand Viswanadh ◽  
...  

Objectives: To evaluate and compare the effect of adhesion boosters on shear bond strength (SBS) of orthodontic brackets on bleached teeth. Materials and Methods: A sample of 90 extracted maxillary premolars was equally divided into 2 groups of bleached and non-bleached teeth. Twenty-two percent carbamide peroxide gel was used as an agent for bleaching. Each group was further divided equally into 3 subgroups depending on the type of adhesive booster used (Enhance LC, All-bond 2, and no adhesive booster [control]) and maxillary premolars brackets were bonded. Debonding was done with a universal testing machine, and the SBS was recorded. Results: The SBS of non-bleached teeth was highest for All-bond 2 (14.78 ± 2.47 MPa) followed by Enhance LC (13.15 ± 3.49 MPa) and control (10.30 ± 1.06 MPa). The SBS of bleached teeth was highest for All bond 2 (12.23 ± 1.41 MPa) followed by Enhance LC (11.76 ± 1.71 MPa) and control (9.63 ± 1.06 MPa). All subgroups showed a significant difference in SBS (P = .000) on bleached and non-bleached teeth. The SBS showed a significant difference between the bleached and non-bleached teeth in All-bond 2 group (P = .019). Conclusion: Adhesive boosters increased the SBS of both bleached and non-bleached teeth significantly. Among the two adhesive boosters used, All-bond 2 showed more SBS values.