scholarly journals Bi2Te3 and Sb2Te3 Thin Films with Enhanced Thermoelectric Properties for Flexible Thermal Sensors

Proceedings ◽  
2018 ◽  
Vol 2 (13) ◽  
pp. 815
Author(s):  
Eliana Vieira ◽  
Joana Figueira ◽  
Ana Lucia Pires ◽  
José Grilo ◽  
Manuel Fernando Silva ◽  
...  

The influence of substrate type in boosting thermoelectric properties of co-evaporated Bi2Te3 and Sb2Te3 films (with 400 nm-thick) is here reported. Optimized power factor values are 2.7 × 10−3 W K−2 m−1 and 1.4 × 10−3 W K−2 m−1 for flexible Bi2Te3 and Sb2Te3 films, respectively. This is an important result as it is at least 2 times higher than the power factor found in the literature for flexible Bi2Te3 and Sb2Te3 films. A flexible infrared thermopile sensor was developed with high detectivity (2.50 × 107 cm √HzW−1).

2013 ◽  
Vol 2013 ◽  
pp. 1-6 ◽  
Author(s):  
Jyun-Min Lin ◽  
Ying-Chung Chen ◽  
Chi-Pi Lin

Bismuth telluride-based compounds are known to be the best thermoelectric materials within room temperature region, which exhibit potential applications in cooler or power generation. In this paper, thermal evaporation processes were adopted to fabricate the n-type Bi2Te3thin films on SiO2/Si substrates. The influence of thermal annealing on the microstructures and thermoelectric properties of Bi2Te3thin films was investigated in temperature range 100–250°C. The crystalline structures and morphologies were characterized by X-ray diffraction and field emission scanning electron microscope analyses. The Seebeck coefficients, electrical conductivity, and power factor were measured at room temperature. The experimental results showed that both the Seebeck coefficient and power factor were enhanced as the annealing temperature increased. When the annealing temperature increased to 250°C for 30 min, the Seebeck coefficient and power factor of n-type Bi2Te3-based thin films were found to be about −132.02 μV/K and 6.05 μW/cm·K2, respectively.


2020 ◽  
Vol 10 ◽  
Author(s):  
Harsha Sharma ◽  
Yogesh Chandra Sharma

Background: Thermoelectric material with high performance and low cost is the basic need of today. Bismuth selenide is a thermoelectric material. A set of bismuth selenide thin films having different stoichiometry ratio varying Bi/Se ratio from 0.123 to 0.309 have been prepared. Objective: Present work deals with the synthesis and characterization of various thin films of bismuth selenide. Thermoe-lectric properties of thin films were also investigated. Aim of this work is to investigate the effect of composition ratio on the structural and thermoelectric properties and to find out the best stoichiometry ratio of bismuth selenide thin films which can be used in application of thermoelectric devices. Method: The set of bismuth selenide thin films having different elemental compositions were prepared by employing thermal evaporation technique. Crystal structure and elemental composition of thin films were investigated by XRD and EDAX respectively. Roughness of films were analysed by AFM. Thermoelectric properties of various thin films were al-so measured. Results: XRD spectrum confirms the formation of phases formed in thin films which slightly matched with standard data. AFM results indicate that surface of films are smooth and nanoparticles are generated on surface. AFM results indicate that the surfaces of annealed thin films are smoother than as-deposited thin films. Seebeck coefficient found negative throughout the temperature rang. Power factor is also calculated by Seebeck coefficient and results reveal effect of com-position ratio on Seebeck coefficient , electrical conductivity and power factor. Thin films having the composition ratio of 0.182 exhibited the highest power factor. Conclusion: This study provides relevant basic information of the thermoelectric property of thin films. As well as pre-sents the effect of compositional variation on thermoelectric measurements. From the application point of view in the thermoelectric devices the best stoichiometric thin films out of four prepared thin films have been presented.


RSC Advances ◽  
2019 ◽  
Vol 9 (62) ◽  
pp. 36113-36122 ◽  
Author(s):  
Anha Masarrat ◽  
Anuradha Bhogra ◽  
Ramcharan Meena ◽  
Manju Bala ◽  
Ranveer Singh ◽  
...  

The power factor for the Fe ion-implanted samples is greater than that of the pristine sample with a value of 700 mW m−1 K−2 at 420 K for the I1E15A sample.


2012 ◽  
Vol 538-541 ◽  
pp. 154-157
Author(s):  
Peng Juan Liu ◽  
Ping Fan ◽  
Zhuang Hao Zheng ◽  
Dong Ping Zhang ◽  
Xing Min Cai ◽  
...  

Antimony (Sb) and zinc (Zn) bilayer was sputter-deposited at room temperature with various Zn contents by ion-beam sputtering and transformed into Antimony zinc after post thermal annealed at 573K for 60 min. A power factor of 6.18×10-4 W/mK2 at 473 K has been obtained when the sputtering time of the Zn was 20 minutes. The maximum Seebeck coefficient is 42.0 μVK-1. Composition analysis shows that the compound of SbZn is achieved and the small Seebeck coefficient is due to the deviation of stoichiometric.


2015 ◽  
Author(s):  
Ewa Kowalska ◽  
Elżbieta Czerwosz ◽  
Miroslaw Kozłowski ◽  
Piotr Firek

2014 ◽  
Vol 1043 ◽  
pp. 40-44 ◽  
Author(s):  
Ghenadii Korotcenkov ◽  
V. Brinzari ◽  
L. Trakhtenberg ◽  
B.K. Cho

Structural, electrophysical and thermoelectric properties of nanoscaled In2O3films doped by Sn and Zn were studied. Thin films based on In2O3-SnO2and In2O3-SnO2-ZnO systems were prepared by spray pyrolysis method from water solutions of metal chlorides. It was confirmed that In2O3-based films, especially the In2O3:Sn ones, are promising material for applications related to thermoelectricity. The power factor of obtained films was found to be on the level of the best samples prepared on the base of ITO system.


2016 ◽  
Vol 42 (2) ◽  
pp. 3028-3032 ◽  
Author(s):  
Ke Sun ◽  
Yue Dai ◽  
Yan Yang ◽  
Zhong Yu ◽  
Hai Liu ◽  
...  

2013 ◽  
Vol 1543 ◽  
Author(s):  
P. Mele ◽  
S. Saini ◽  
H. Abe ◽  
H. Honda ◽  
K. Matsumoto ◽  
...  

ABSTRACTWe have prepared 2% Al doped ZnO (AZO) thin films on SrTiO3 and Al2O3 substrates by Pulsed Laser Deposition (PLD) technique at various deposition temperatures (Tdep = 300 °C – 600 °C). Transport and thermoelectric properties of AZO thin films were studied in low temperature range (300 K - 600 K). AZO/STO films present superior performance respect to AZO/Al2O3 films deposited at the same temperature, except for films deposited at 400 °C. Best film is the fully c-axis oriented AZO/STO deposited at 300 °C, with electrical conductivity 310 S/cm, Seebeck coefficient -65 μV/K and power factor 0.13 × 10-3 Wm-1K-2 at 300 K. Its performance increases with temperature. For instance, power factor is enhanced up to × 10-3 Wm-1K-2 at 600 K, surpassing the best AZO film previously reported in literature.