scholarly journals DEVELOPMENT OF A BIODEGRADABLE COMPOSITE FILM FROM CHITOSAN, AGAR AND GLYCEROL BASED ON OPTIMIZATION PROCESS BY RESPONSE SURFACE METHODOLOGY

2021 ◽  
Vol 55 (7-8) ◽  
pp. 849-865
Author(s):  
PARTHIBAN FATHIRAJA ◽  
SUGUMAR GOPALRAJAN ◽  
MASILAN KARUNANITHI ◽  
MURALIDHARAN NAGARAJAN ◽  
MOHAN CHITRADURGA OBAIAH ◽  
...  

The aim of the study has been to develop a biodegradable film from marine polysaccharides. The optimization of polysaccharides quantity for the composite film was sought by empirical response surface methodology. The Box–Behnken Model Design was applied to optimize the concentration of chitosan (1.0-2.0% (w/v), agar (1.0-2.0% (w/v) and glycerol (0.1-0.5% (w/v) as independent variables to achieve the goal. The overall desirability function fits with the quadratic model (0.862043) at a significant level (p < 0.05) for the optimum concentration of chitosan (1.5% (w/v), agar (2.0% (w/v) and glycerol (0.41% (w/v) to obtain the minimum water vapor permeability (7.25 10-10g m m-2 Pa-1 s-1) and maximum tensile strength (12.21 Ma P), elongation at break (7.32%) and puncture resistance (16.18 N) in the optimized composite film. The absolute residual errors of experimental and predicted responses were between 1.24 and 3.56% acceptable levels. Attenuated total reflection–Fourier transform infrared spectroscopy confirmed the intermolecular non-covalent hydrogen bond between the hydroxyl groups of agar and glycerol with the amino group of chitosan. 3D atomic force microscopy images revealed that the chitosan, agar and glycerol film has layer-by-layer smooth surface properties due to homogenous interaction among the polysaccharides; this provides the film with good mechanical properties and with functional application. Chitosan was found to be responsible for the lower level of water vapor permeability and higher puncture resistance of the film. Tensile strength and elongation at break were influenced by agar and glycerol. The whiteness of the film was negatively affected with the concentration of chitosan.

2000 ◽  
Vol 9 (1) ◽  
pp. 23-35 ◽  
Author(s):  
P. TANADA-PALMU ◽  
H. HELÉN ◽  
L. HYVÖNEN

Edible films from wheat gluten were prepared with various amounts of glycerol as a plasticizer. Water vapor permeability, oxygen permeability, tensile strength and percentage elongation at break at different water activities ( aw ) were measured. Films with low amounts of glycerol had lower water vapor and oxygen permeabilities, higher tensile strength and lower elongation at break. Wheat gluten coatings reduced weight loss during two weeks of storage for cherry tomatoes and sharon fruits compared to uncoated controls. A bilayer film of wheat gluten and beeswax significantly lowered weight loss from coated cheese cubes compared to single layer coating of wheat gluten.;


2011 ◽  
Vol 233-235 ◽  
pp. 1162-1166 ◽  
Author(s):  
Feng Jun Wang ◽  
Jian Qing Wang ◽  
Mei Xu

Cellulose-based composites packaging films containing various amounts of modified nano-SiO2 were prepared by utilizing hardwood pulps as natural cellulose resource through NMMO-technology to improve the mechanical properties, permeability for oxygen and water vapor etc. The tensile strength, elongation at break, thermal stability and permeability of the cellulose composites films as a function of the content of modified nano-SiO2 were studied. The investigation suggested that the capabilities of composites films with 2 wt.% modified nano-SiO2 added were improved largely, compared to pure cellulose films, when the diameter of particles is 30nm. The tensile strength was increased from 8.95 to 17.37 MPa and the elongation at break of the cellulose composites films was improved from 41.11% to 58.34%. The composites films with rational mechanical properties have adjustable oxygen permeability (7.90×10-15-72.18×10-15 cm3·cm/cm2·s·Pa) and water vapor permeability (7.12×10-13-5.32×10-13g·cm/cm2·s·Pa). And thermal stability of the composites films was advanced through adding modified nano-SiO2.


Materials ◽  
2018 ◽  
Vol 11 (9) ◽  
pp. 1589 ◽  
Author(s):  
Xinxin Liu ◽  
Xiaofeng Chen ◽  
Junli Ren ◽  
Chunhui Zhang

In order to improve the strength of polyvinyl alcohol (PVA)/xylan composite films and endow them with ultraviolet (UV) shielding ability, TiO2-KH550 nanoparticles was synthesized and added into the PVA/xylan matrix. The TiO2-KH550 nanoparticle dispersed well in the 0.04% sodium hexametaphosphate (SHMP) solution under ultrasonic and stirring treatments. Investigations on the properties of the films showed that TiO2-KH550 had the positive impact on improving the strength, moisture, and oxygen barrier properties of the composite films. The maximum tensile strength (27.3 MPa), the minimum water vapor permeability (2.75 × 10−11 g·m−1·s−1·Pa−1), and oxygen permeability (4.013 cm3·m−2·24 h−1·0.1MPa−1) were obtained under the addition of 1.5% TiO2-KH550. The tensile strength of TiO2-KH550 reinforced composite film was increased by 70% than that of the pure PVA/xylan composite film, and the water vapor and oxygen permeability were decreased by 31% and 41%, respectively. Moreover, the UV transmittance of the film at the wavelength of 400 nm was almost zero when adding ≈1.5~2.5% (weight ratio, based on the total weight of PVA and xylan) of TiO2-KH550, which indicated the PVA/xylan composite films were endowed with an excellent UV light shielding ability.


Author(s):  
Xinxin Liu ◽  
Xiaofeng Chen ◽  
Junli Ren ◽  
Chunhui Zhang

In order to improve the strength of PVA/xylan composite films and endow them with ultraviolet (UV) shielding ability, TiO2-KH550 nanoparticle was synthesized and added into the PVA/xylan matrix. The TiO2-KH550 nanoparticle dispersed well in the 0.04% sodium hexametaphosphate (SHMP) solution under ultrasonic and stirring treatments. Investigations on the properties of films showed that TiO2-KH550 had the positive impact on improving the strength, moisture and oxygen barrier properties of the composite films. The maximum tensile strength (27.3 MPa), the minimum water vapor permeability (2.75&times;10-11 g&bull;m-1&bull;s-1&bull;Pa-1) and oxygen permeability (4.013 cm3&bull;m-2&bull;24h-1&bull;0.1MPa-1) were obtained under the addition of 1.5% TiO2-KH550. The tensile strength of TiO2-KH550 reinforced composite film was increased by 70% than that of the pure PVA/xylan composite film, and the water vapor and oxygen permeability were decreased by 31% and 41%, respectively. Moreover, the UV transmittance of film at the wavelength of 400 nm was almost zero when adding 1.5~2.5% of TiO2-KH550, which indicated the PVA/xylan composite films were endowed with excellent UV light shielding ability.


2021 ◽  
Vol 60 (1) ◽  
Author(s):  
Gema Morales-Olán ◽  
María Antonieta Ríos-Corripio ◽  
Aleida Selene Hernández-Cázares ◽  
Placido Zaca-Morán ◽  
Silvia Luna-Suárez ◽  
...  

Research background. Amaranth flour (Amaranthus hypochondriacus) produces films with excellent barrier properties against water vapor, allowing food preservation, but the mechanical properties are poor versus to synthetic films. One strategy to improve these properties is the incorporation of nanoparticles. The particles can also serve as a vehicle for the addition of antioxidants agents into the films. The objective of this work was to optimize the formulation for preparation of amaranth flour films treated with antioxidant chia (Salvia hispanica L.) extract-loaded chitosan particles using RSM. Experimental approach. Chitosan nanoparticles with the extract were synthesized by ionic gelation, and the films were made by the casting method. Three independent variables were assigned: amaranth flour (4-6 %), glycerol (25-35 %), and chitosan nanoparticles loaded with the chia extract (0-0.75 %). We then evaluated the physical (thickness), mechanical (tensile strength, Young´s modulus, and elongation), barrier (water vapor permeability, moisture, and water solubility), and antioxidant properties of the films. The experimental results of the properties were analyzed using a Box-Behnken experimental design generating 15 runs with three replicates at the central point. Results and conclusions. Second and third order polynomial models were obtained from the ANOVA analysis of the evaluated responses, and high coefficients of determination were found (0.91-1.0). The films presented a water vapor permeability of 0.82-2.39·10-7 (g·mm)/(Pa·s·m2), a tensile strength of 0.33-1.63 MPa, and antioxidant activity of 2.24-5.65 %. The variables had different effects on the films: The glycerol negatively affected their properties, and the permeability values increased with amaranth flour concentration. The nanoparticles improved the mechanical, barrier, and antioxidant properties of the films versus films without nanosystems. The optimal formulation was 4 % amaranth flour, 25 % of glycerol, and 0.36 % of chitosan nanoparticles. The optimized films had better mechanical (1.62 MPa) properties, a low water vapor permeability value (0.91·10-7 (g·mm)/(Pa·s·m2)), and moderate antioxidant activity (6.43 %). Novelty and scientific contribution. The results show the effect of chitosan nanoparticles on the properties of amaranth flour films for the first time. The resulting equations are useful in the design of food packaging.


Author(s):  
Jie Liu ◽  
Yanchun Liu ◽  
Eleanor M. Brown ◽  
Zhengxin Ma ◽  
Cheng-Kung Liu

The leather industry generates considerable amounts of solid waste and raises many environmental concerns during its disposal. The presence of collagen in these wastes provides a potential protein source for the fabrication of bio-based value-added products. Herein, a novel composite film was fabricated by incorporating vegetable-tanned collagen fiber (VCF), a mechanically ground powder-like leather waste, into a chitosan matrix and crosslinked with genipin. The obtained composite film showed a compact structure and the hydrogen bonding interactions were confirmed by FTIR analysis, indicating a good compatibility between chitosan and VCF. The optical properties, water absorption capacity, thermal stability, water vapor permeability and mechanical properties of the composite films were characterized. The incorporation of VCF into chitosan led to significant decreases in opacity and solubility of the films. At the same time, the mechanical properties, water vapor permeability and thermal stability of the films were improved. The composite film exhibited antibacterial activity against food-borne pathogens. Results from this research indicated the potential of the genipin-crosslinked chitosan/VCF composites for applications in antimicrobial packaging. 


Coatings ◽  
2018 ◽  
Vol 8 (11) ◽  
pp. 384
Author(s):  
Juan Tirado-Gallegos ◽  
Paul Zamudio-Flores ◽  
José Ornelas-Paz ◽  
Claudio Rios-Velasco ◽  
Guadalupe Olivas Orozco ◽  
...  

Apple starch films were obtained from apples harvested at 60, 70, 80 and 90 days after full bloom (DAFB). Mechanical properties and water vapor permeability (WVP) were evaluated. The apple starch films at 70 DAFB presented higher values in the variables of tensile strength (8.12 MPa), elastic modulus (3.10 MPa) and lower values of water vapor permeability (6.77 × 10−11 g m−1 s−1 Pa−1) than apple starch films from apples harvested at 60, 80 and 90 DAFB. Therefore, these films were chosen to continue the study incorporating ellagic acid (EA). The EA was added at three concentrations [0.02% (FILM-EA0.02%), 0.05% (FILM-EA0.05%) and 0.1% (FILM-EA0.1%) w/w] and compared with the apple starch films without EA (FILM-Control). The films were characterized by their physicochemical, optical, morphological and mechanical properties. Their thermal stability and antioxidant capacity were also evaluated. The FILM-Control and FILM-EA0.02% showed a uniform surface, while FILM-EA0.05% and FILM-EA0.1% showed a rough surface and insoluble EA particles. Compared to FILM-Control, EA modified the values of tensile strength, elasticity modulus and elongation at break. The antioxidant capacity increased as EA concentration did. EA incorporation allowed obtaining films with higher antioxidant capacity, capable of blocking UV light with better mechanical properties than film without EA.


2014 ◽  
Vol 884-885 ◽  
pp. 481-484 ◽  
Author(s):  
Yan Wu ◽  
Ming Wei Yuan ◽  
Ji Yi Yang ◽  
Yu Yue Qin ◽  
Ming Long Yuan ◽  
...  

Thymol (TH), which has antimicrobial effect on many food pathogens, was incorporated as antimicrobial agent into composite poly (lactic acid)/poly (trimethylene carbonate)(PLA-PTMC) films. Antimicrobial active films based on PLA-PTMC were prepared by incorporating thymol at five different concentrations: 0, 3, 6, 9 and 12 %(w/w). The mechanical characterization, water vapor permeability (WVP), and antimicrobial activity of all formulations composite film were carried out. A decrease in elastic modulus was obtained for the active composite film compared with neat PLA-PTMC film. The presence of thymol decreased water vapor permeability, with a significant antimicrobial activity. Antimicrobial activities of films were tested against Escherichia coli, Staphylococcus aurous, Listeria, Bacillus subtilis, and Salmonella. Increasing amount of the thymol in the film caused a significant increase in inhibitory zones. These results suggest that thymol incorporated PLA-PTMC films have a prospectively potential in antimicrobial food packaging.