Sol-Gel Derived Li2O Doped BNT-BKT-BT Ceramics: Microstructure and Piezoelectric Properties

2012 ◽  
Vol 512-515 ◽  
pp. 1355-1358 ◽  
Author(s):  
Tao Sun ◽  
Ye Jing Dai ◽  
Hong Qiang Wang

The introduction of lithium ion into BNT-BKT-BT ceramics with sol-gel method allows the development of high-performance lead-free piezoelectric ceramics. Nanoscale precursor powders were synthesized through calcination of amorphous gels, and densified ceramics with single perovskite structure were prepared at a relatively low sintering temperature 1110 °C. Crystal grain growth was fully developed with the Li+ addition through scanning electron microscope observation. Enhanced electrical properties, piezoelectric constant d33~184 pC/N and planar electromechanical coupling factor kp~0.30, were obtained for the ceramics.

2014 ◽  
Vol 602-603 ◽  
pp. 822-825
Author(s):  
Ling Peng ◽  
Min Hong Jiang ◽  
Zheng Fei Gu ◽  
Gang Cheng

Lead-free piezoelectric 0.97 K0.5Na0.5NbO3-0.03 AlFeO3(KNN-AF) ceramics were prepared at low temperature of 980 °C to 1020 °C by the conventional ceramic process. The effect of sintering temperature on the crystal structure, density and electrical properties of the ceramics was investigated. The results indicate that KNN-AF ceramics sintered at an low temperature of 1000 °C exhibit high electrical and piezoelectric properties, with piezoelectric constantd33=116ρC/N, and electromechanical coupling factorkp= 32.9%, polarization (Pr) wasPr=21.8 μC/cm2and curie temperatureTC=382°C. This also indicates that KNN-AF ceramics are promising candidate materials for lead-free piezoelectric applications.


2011 ◽  
Vol 287-290 ◽  
pp. 801-804 ◽  
Author(s):  
Man Soon Yoon ◽  
Neamul Hayet Khansur ◽  
Woong Jae Lee ◽  
Young Geun Lee ◽  
Soon Chul Ur

The effect of AgSbO3on the piezoelectric properties of (K0.5Na0.5)0.95Li0.05NbO3was examined. The AgSbO3doped KNLN samples sintered at 1050°C showed the maximum values of the sintering density of 4.56 g/cm3compared to un-doped KNLN samples sintered at same temperature with 4.25 g/cm3. Moreover, the addition of AgSbO3enhanced the piezoelectric and dielectric properties. Piezoelectric constant (d33), the planar electromechanical coupling factor (kp) and the relative dielectric permittivity (K33T) increased up to 230pC/N, 43.5%, 1080, respectively, with addition of AgSbO3.


Materials ◽  
2018 ◽  
Vol 11 (11) ◽  
pp. 2247 ◽  
Author(s):  
Jinhwan Kim ◽  
Sanghyun Yoon ◽  
Jae-Hoon Ji ◽  
Young-Ho Ko ◽  
Kyung-Ho Cho ◽  
...  

The pyrochlore phase in ferroelectric and piezoelectric materials is the main obstacle device application due to its poor electrical properties. Especially, the pyrochlore phase is frequently observed in the perovskite-based metal-oxide materials including piezoelectric and ferroelectric ceramics, which are based on solid-state reaction methods for fabrication. To overcome these problems, advanced innovative methods such as partial oxalate process will be investigated. In this method, crystalized magnesium niobite (MN) and lead titanate (PT) powders will be coated with a certain amount of lead oxalate and, then, the calcination process can be carried out to form the PMN-PT without pyrochlore phase. In this study, (1−x)PMN-xPT ceramics near the morphotropic phase boundary (MPB), with compositions of x = 0.25–0.40, have been prepared employing the partial oxalate method at various temperatures. The crystalline, microstructure, and piezoelectric properties of (1−x)PMN-xPT ceramics depending on the sintering temperature were intensively investigated and discussed. By optimizing the sintering temperature and compositions from the PMN-PT ceramics, the maximum value of the piezoelectric charge coefficient (d33) of 665pC/N, planar electromechanical coupling factor (kp) of 77.8%, dielectric constant (εr) of 3230, and remanent polarization (Pr) of 31.67 μC/cm2 were obtained.


2006 ◽  
Vol 301 ◽  
pp. 19-22 ◽  
Author(s):  
Takeru Yoshida ◽  
Hajime Nagata ◽  
Tadashi Takenaka

Doping a small quantity of additive Bi2O3 is effective in suppressing the deliquescence of KNbO3 ceramics. When an optimized ball-milling process was included, dense and nondeliquescent KNbO3 ceramics were obtained by a conventional firing process. However, the presence of Bi prevented grain growth (<0.2 μm) and it was one of the causes of low ferroelectricity. Moreover, the insufficient resistivity made the poling treatment difficult. In order to improve the electric properties, a small quantity of additive MnCO3 was also doped into KNbO3 with 0.5 mass% Bi2O3. Codoping of KNbO3 with MnCO3 and Bi2O3 (abbreviated to KNBixMny; x = 0~1.0, y = 0~1.0 in mass%) improved the ferroelectricity of samples, and it also had an effect on the resistivity and densification of sintered bodies. Well-saturated P-E hysteresis loops were observed with any amount of Mn and the largest remanent polarization Pr was about 16 μC/cm2. The piezoelectric properties of KNBi0.5Mn0.3, which had the highest piezoelectricity in this study, are an electromechanical coupling factor k33 and piezoelectric constant d33 of 0.30 and 101 pC/N, respectively.


2011 ◽  
Vol 284-286 ◽  
pp. 1375-1380 ◽  
Author(s):  
Ming Cheng Chure ◽  
Ping Cheng Chen ◽  
Long Wu ◽  
Bing Huei Chen ◽  
King Kung Wu

In the poling process of PZT ceramics, the poling temperature is a critical condition. When the poling temperature is too low, no matter how high is the poling field and how long is the poling time, the planar electromechanical coupling factor kpis lower. When the poling temperature is higher enough, the kpcan reach to a saturated value with a lower poling field and short poling time. The variation of dielectric constant with the poling conditions is the same as that of planar electromechanical coupling factor. When poling with a low temperature, the dielectric constant after poling is lower than 1400. When poling with higher temperature, no matter how high is the poling field and how long is the poling time, the dielectric constant after poling is higher than 1500.


2017 ◽  
Vol 732 ◽  
pp. 69-75
Author(s):  
Tai Kuang Lee ◽  
Jyun Hung Chen ◽  
Ying Chieh Lee

(Na0.5Bi0.5)0.94Ba0.06TiO3 (NBBT) ceramics doped with 0.1∼2.0 mol.% Ba (Zr0.05Ti0.95)O3 were investigated in terms of the sintering, microstructure, phase transition, and piezoelectric properties. BZT doping has no remarkable effect on the microstructure and densification within the studied doping content. Up to 2 mol.% BZT can dissolve into the lattice of NBBT ceramics, and the structure symmetry is not changed. However, a significant change in the piezoelectric properties took place. The piezoelectric coefficient d33 for the 0.1 wt.% BZT-doped NBBT ceramics sintered at 1150 °C was found to be 120 pC/N and the electromechanical coupling factor kp = 0.24.


2014 ◽  
Vol 887-888 ◽  
pp. 289-293
Author(s):  
Jing Chang Zhao ◽  
Zhen Lai Zhou

(Na,Bi)TiO3-BaTiO3lead free piezoelectric ceramics were fabricated with modification of CaCu3Ti4O12additives. The phase structure, morphology, dielectric and piezoelectric properties of prepared samples were investigated, respectively. It was found that CaCu3Ti4O12additives evidently improve the polarization properties of (Na,Bi)TiO3-BaTiO3lead free ceramics and the obtained samples exhibit an excellent piezoelectric properties (electromechanical coupling factorKp=31%, mechanical quality factorQm=151 and piezoelectric constantd33=160pC/N). According to results, the effect of CaCu3Ti4O12additives on electrical properties of (Na,Bi)TiO3-BaTiO3lead free piezoelectric ceramics is discussed.


2021 ◽  
Vol 11 (1) ◽  
pp. 57-65
Author(s):  
Cong Luo ◽  
Tomoaki Karaki ◽  
Zhuangkai Wang ◽  
Yiqin Sun ◽  
Yohachi Yamashita ◽  
...  

AbstractAfter field cooling (FC) alternating current poling (ACP), we investigated the dielectric and piezoelectric properties of [001]pc-oriented 0.24Pb(In1/2Nb1/2)O3 (PIN)-0.46Pb(Mg1/3Nb2/3)O3 (PMN)-0.30PbTiO3 (PT) (PIMN-0.30PT) single crystals (SCs), which were manufactured by continuous-feeding Bridgman (CF BM) within morphotropic phase boundary (MPB) region. By ACP with 4 kVrms/cm from 100 to 70 °C, the PIMN-0.30PT SC attained high dielectric permittivity (ε33T/ε0) of 8330, piezoelectric coefficient (d33) of 2750 pC/N, bar mode electromechanical coupling factor k33 of 0.96 with higher phase change temperature (Tpc) of 103 °C, and high Curie temperature (TC) of 180 °C. These values are the highest ever reported as PIMN-xPT SC system with Tpc > 100 °C. The enhancement of these properties is attributed to the induced low symmetry multi-phase supported by phase analysis. This work indicates that FC ACP is a smart and promising method to enhance piezoelectric properties of relaxor-PT ferroelectric SCs including PIMN-xPT, and provides a route to a wide range of piezoelectric device applications.


2021 ◽  
Author(s):  
Cong Luo ◽  
Tomoaki Karaki ◽  
Zhuangkai Wang ◽  
Yiqin Sun ◽  
Yohachi Yamashita ◽  
...  

Abstract We investigated the dielectric and piezoelectric properties of [001]-oriented 0.24Pb(In1/2Nb1/2)O3-0.46Pb(Mg1/3Nb2/3)O3-0.30PbTiO3 (PIMN-0.30PT) single crystals (SCs) manufactured by continuous-feeding Bridgman (CF BM) within morphotropic phase boundary (MPB) region after field cooling alternating current poling (FC ACP). By optimized the FC ACP conditions of 4 kVrms/cm from 100 to 70 oC, the PIMN-0.30PT SC process attained ultrahigh dielectric permittivity (εT 33/ε0) of 8330 and piezoelectric coefficient (d33) of 2750 pC/N, and bar mode electromechanical coupling factor k33 of 0.96 with higher phase change temperature (Tpc) of 103 oC, respectively. These values are the highest ever reported as PIMN-xPT system SCs with Tpc > 100 oC. The enhancement of these properties of the PIMN-0.30PT SC is attributed to the induced low symmetry multi-phase supported by phase analysis. This work indicates that FC ACP is a smart and promising method to enhance piezoelectric properties of relaxor-PT ferroelectric SCs including PIMNT, which provide a route to a wide range of piezoelectric device applications.