High temperature rheological properties of crumb rubber modified asphalt binders with various modifiers

2016 ◽  
Vol 112 ◽  
pp. 49-58 ◽  
Author(s):  
Ouming Xu ◽  
Feipeng Xiao ◽  
Sen Han ◽  
Serji N. Amirkhanian ◽  
Zhenjun Wang
2021 ◽  
Vol 13 (18) ◽  
pp. 10271
Author(s):  
Yuchen Guo ◽  
Xuancang Wang ◽  
Guanyu Ji ◽  
Yi Zhang ◽  
Hao Su ◽  
...  

The deteriorating ecological environment and the concept of sustainable development have highlighted the importance of waste reuse. This article investigates the performance changes resulting from the incorporation of shellac into asphalt binders. Seashell powder-modified asphalt was prepared with 5%, 10%, and 15% admixture using the high-speed shear method. The microstructure of the seashell powder was observed by scanning electron microscope test (SEM); the physical-phase analysis of the seashell powder was carried out using an X-ray diffraction (XRD) test; the surface characteristics and pore structure of shellac were analyzed by the specific surface area Brunauer-Emmett-Teller (BET) test; and Fourier infrared spectroscopy (FTIR) qualitatively analyzed the composition and changes of functional groups of seashell powder-modified asphalt. The conventional performance index of seashell powder asphalt was analyzed by penetration, softening point, and ductility (5 °C) tests; the effect of seashell powder on asphalt binder was studied using a dynamic shear rheometer (DSR) and bending beam rheometer (BBR) at high and low temperatures, respectively. The results indicate the following: seashell powder is a coarse, porous, and angular CaCO3 bio-material; seashell powder and the asphalt binder represent a stable physical mixture of modified properties; seashell powder improves the consistency, hardness, and high-temperature performance of the asphalt binder but weakens the low-temperature performance of it; seashell powder enhances the elasticity, recovery performance, and permanent deformation resistance of asphalt binders and improves high-temperature rheological properties; finally, seashell powder has a minimal effect on the crack resistance of asphalt binders at very low temperatures. In summary, the use of waste seashells for recycling as bio-modifiers for asphalt binders is a practical approach.


Author(s):  
Haopeng Wang ◽  
Xueyan Liu ◽  
Panos Apostolidis ◽  
Tom Scarpas

The microstructure and chemical composition of asphalt binders have a significant effect on their rheological properties and, therefore, their performance as road paving binders. This study aims to investigate the effects of warm-mix asphalt (WMA) additives, organic type and chemical type, on the rheological properties and chemical internal structure of base asphalt and crumb rubber modified asphalt (CRMA). A set of dynamic shear rheometer (DSR) tests was conducted to obtain the rheological parameters (e.g., complex viscosity, complex modulus, phase angle) of asphalt binders. The flow activation energy was calculated from Arrhenius equation based on viscosity data to rank the thermal susceptibility. Black diagrams and master curves of complex modulus and phase angle were utilized to analyze the rheological properties. The molecular weight distributions of asphalt binders were inverted from the phase angle master curve to evaluate the molecular weight characteristics. It was found that the the addition of crumb rubber into base asphalt improves the rheological properties of enhanced modulus and elasticity. Organic and chemical types of WMA additives have different chemo-physical effects on both base asphalt and CRMA. Phase angle inversion method provides a powerful tool to monitor the molecular structure change and, therefore, the chemo-physical interactions of asphalt binders induced by modifications. Finally, there is a good correlation between flow activation energy and molecular weight.


Materials ◽  
2021 ◽  
Vol 14 (14) ◽  
pp. 3780
Author(s):  
Jingyao Yang ◽  
Gang Xu ◽  
Peipei Kong ◽  
Xianhua Chen

With the growing interest in bituminous construction materials, desulfurized crumb rubber (CR)/styrene–butadiene–styrene (SBS) modified asphalts have been investigated by many researchers as low-cost environmental-friendly road construction materials. This study aimed to investigate the rheological properties of desulfurized CR/SBS composite modified asphalt within various temperature ranges. Bending beam rheometer (BBR), linear amplitude sweep (LAS), and multiple stress creep recovery (MSCR) tests were performed on conventional CR/SBS composite modified asphalt and five types of desulfurized CR/SBS modified asphalts. Meanwhile, Burgers’ model and the Kelvin–Voigt model were used to derive nonlinear viscoelastic parameters and analyze the viscoelastic mechanical behavior of the asphalts. The experimental results indicate that both the desulfurized CR/SBS composite modifier and force chemical reactor technique can enhance the crosslinking of CR and SBS copolymer, resulting in an improved high-, intermediate-, and low-temperature performance of desulfurized CR/SBS composite modified asphalt. Burgers’ model was found to be apposite in simulating the creep stages obtained from MSCR tests for CR/SBS composite modified asphalts. The superior high-temperature performance of desulfurized CR/SBS modified asphalt prepared with 4% SBS, 20% desulfurized rubber, and a force chemical reactor time of 45 min contributes to the good high-temperature elastic properties of the asphalt. Therefore, this combination is recommended as an optimal preparation process. In summary, the desulfurization of crumb rubber and using the force chemical reactor technique are beneficial to composite asphalt performance and can provide a new way of utilizing waste tire rubber.


Materials ◽  
2021 ◽  
Vol 14 (14) ◽  
pp. 3986
Author(s):  
Huan-Yun Zhou ◽  
Huai-Bing Dou ◽  
Xian-Hua Chen

Aiming to improve the comprehensive road performance of asphalt binders, especially the high-temperature performance, a novel asphalt binder was prepared by compounding high-quality and low-cost polyethylene (PE) with graphene (GNPs) using a high-speed shearing machine. The rheological properties and interaction mechanism of PE/GNPs composite modified asphalt were investigated using temperature sweep (TeS), multiple stress creep recovery (MSCR), linear amplitude sweep (LAS) and Fourier transform infrared spectroscopy (FT-IR) and field emission scanning electron microscopy (FESEM). The experimental results demonstrated that GNPs and PE can synergistically improve the high-temperature performance of asphalt binders and enhance the rutting resistance of pavements; the pre-blended PE/GNPs masterbatch has good medium-temperature fatigue and low-temperature cracking resistance. Meanwhile, PE/GNPs dispersed uniformly in the asphalt matrix, and the microstructure and dispersion of premixed PE/GNPs masterbatch facilitated the asphalt modification. No new absorption peaks appeared in the FT-IR spectra of the composite modified asphalt, indicating that asphalt binders were physically modified with GNPs and PE. These findings may cast light on the feasibility of polyethylene/graphene composite for asphalt modification.


Author(s):  
Ovidijus Šernas ◽  
Donatas Čygas ◽  
Audrius Vaitkus ◽  
Vytautė Gumauskaitė

Rubber derived from grinding of recycled cars and trucks tyres may be successfully used as a bitumen modifier. Number of researches reported sufficient characteristics of rubber modified asphalt binders or modified asphalt mixes in terms of improved permanent deformation and fatigue cracking. The behavior of crumb rubber asphalt binders depends on several factors, such as modification method, rubber content and size, modification temperature, mixing speed and time applied during the digestion process. The aim of this study is to evaluate the effect of crumb rubber amount and type on modified bitumen low and high temperature properties. This paper presents results of unmodified bitumen, crumb rubber crumb rubber and polymer modified bitumen. Low and high temperature properties have been evaluated using bending beam rheometer and dynamic shear rheometer. Moreover, softening point and viscosity tests have been performed. The study results revealed that crumb rubber modified bitumen performed better than pure bitumen and similarly to polymer modified bitumen.


Environments ◽  
2021 ◽  
Vol 8 (6) ◽  
pp. 47
Author(s):  
Lim Min Khiong ◽  
Md. Safiuddin ◽  
Mohammad Abdul Mannan ◽  
Resdiansyah

This paper presents the results of a laboratory-based experimental investigation on the properties of asphalt binder and hot-mix asphalt (HMA) mixes modified by locally available crumb rubber, which was used as a partial replacement of asphalt by weight. In this study, fine crumb rubber with a particle size in the range of 0.3–0.6 mm, obtained from scrap tires, was added to the asphalt binder through the wet process. Crumb rubber contents of 5%, 10%, 15%, and 19% by weight of asphalt were added to the virgin binder in order to prepare the modified asphalt binder samples, while the unmodified asphalt binder was used as the control sample. The crumb rubber modified binder samples were examined for measuring viscosity indirectly using the penetration test, and temperature resistance using the softening point test. Later, both the modified and unmodified asphalt binders were used to produce HMA mixes. Two categories of HMA mix commonly used in Malaysia—namely, AC 14 (dense-graded) and SMA 14 (gap-graded)—were produced using the modified asphalt binders containing 5%, 10%, 15%, and 19% crumb rubber. Two AC 14 and SMA 14 control mixes were also produced, incorporating the unmodified asphalt binder (0% crumb rubber). All of the AC 14 and SMA 14 asphalt mixes were examined in order to determine their volumetric properties, such as bulk density, voids in total mix (VTM), voids in mineral aggregate (VMA), and voids filled with asphalt (VFA). In addition, the Marshall stability, Marshall flow, and stiffness of all of the AC 14 and SMA 14 mixes were determined. Test results indicated that the modified asphalt binders possessed higher viscosity and temperature resistance than the unmodified asphalt binder. The viscosity and temperature resistance of the asphalt binders increased with the increase in their crumb rubber content. The increased crumb rubber content also led to improvements in the volumetric properties (bulk density, VTM, VMA, and VFA) of the AC 14 and SMA 14 mixes. In addition, the performance characteristics of the AC 14 and SMA 14 mixes—such as Marshall stability, Marshall flow, and stiffness—increased with the increase in crumb rubber content. However, the AC 14 mixes performed much better than the SMA 14 mixes. The overall research findings suggest that crumb rubber can be used to produce durable and sustainable HMA mixes, with manifold environmental benefits, for use in flexible pavements carrying the heavy traffic load of highways.


Materials ◽  
2021 ◽  
Vol 14 (5) ◽  
pp. 1145
Author(s):  
Wei Li ◽  
Sen Han ◽  
Xiaokang Fu ◽  
Ke Huang

The aims of this paper are to prepare disintegrated high volume crumb rubber asphalt (DHVRA) with low viscosity, good workability and low-temperature performance by adding disintegrating agent (DA) in the preparation process, and to further analyze the disintegrating mechanism and evaluated high-temperature and low-temperature rheological properties. To obtain DHVRA with excellent comprehensive performance, the optimum DA dosage was determined. Based on long-term disintegrating tests and the Fluorescence Microscopy (FM) method, the correlations between key indexes and crumb rubber (CR) particle diameter was analyzed, and the evaluation indicator and disintegrating stage division standard were put forward. Furthermore, Fourier transform infrared spectroscopy (FT-IR) and Gel Permeation Chromatography (GPC) was used to reveal the reaction mechanism, and the contact angle test method was adopted to evaluate the surface free energy (SFE). In addition, the high-temperature and low-temperature rheological properties were measured, and the optimum CR content was proposed. Results indicated that the optimum DA dosage was 7.5‰, and the addition of DA promoted the melt decomposition of CR, reduced the viscosity and improved the storage stability. The 135 °C rotational viscosity (RV) of DHVRA from mixing for 3 h could be reduced to 1.475 Pa·s, and the softening point difference was even less than 2 °C. The linear correlation between 135 °C RV and the diameter of CR particle in rubber asphalt system was as high as 0.968, and the viscosity decay rate (VDR) was used as the standard to divide the disintegrating process into a fast disintegrating stage, stable disintegrating stage and slight disintegrating stage. Compared to common rubber asphalt (CRA), DHVRA has an absorption peak at 960 cm−1 caused by trans olefin = C-H, and higher molecular weight and polar component of surface energy. Compared with CRA, although the high-temperature performance of DHVRA decreases slightly, the low-temperature relaxation ability can be greatly improved.