Enhanced thermal stability and lifetime of epoxy nanocomposites using covalently functionalized clay: experimental and modelling

2015 ◽  
Vol 39 (3) ◽  
pp. 2269-2278 ◽  
Author(s):  
Omid Zabihi ◽  
Hamid Khayyam ◽  
Bronwyn L. Fox ◽  
Minoo Naebe

Relationship between thermal degradation model of epoxy nanocomposites containing different types of modified nanoclay and their structural changes is explained.

Author(s):  
Lijie Qu ◽  
Zhenyu Wang ◽  
Jing Qian ◽  
Zhengbin He ◽  
Songlin Yi

Abstract Acidic aluminum sulfate hydrolysis solutions can be used to catalyze the thermal degradation of wood in a mild temperature environment, and thus reduce the temperature required for heat treatment process. To improve the dimensional and thermal stability of Chinese fir during heat treatment at 120 °C, 140 °C and 160 °C, this study investigated the effects of soaking pretreatment with 5%, 10% and 15% aluminum sulfate on the chemical and structural changes of the heat-treated Chinese fir. The results indicated that the samples treated at 15% aluminum sulfate concentration and 160 °C heat treatment achieved the best dimensional and thermal stability. Chemical analyses by Fourier transform infrared spectroscopy (FTIR) and X-ray diffraction (XRD) indicated that the catalysis of aluminum sulfate resulted in degradation of hemicelluloses during the heat treatment, and an increase in the soaking concentration and heat treatment temperature also affected the thermal degradation of celluloses. The scanning electron microscope (SEM) and mass changes test results proved that the hydrolyzed aluminum flocs mainly adhered to the inner wall of the wood tracheid as spherical precipitates, and when the soaking concentration reached 10% and 15%, a uniform soaking effect could be achieved. The thermogravimetric (TG) analysis revealed the soaking pretreatment effectively improved the thermal stability of the heat-treated wood by physically wrapping and promoting the formation of a carbon layer on the wood surface during heat treatment. Thus, aluminum sulfate soaking pretreatment exerted a great effect on the dimensional and thermal stability of wood, allowing heat treatment to be performed at a lower temperature.


2018 ◽  
Vol 69 (5) ◽  
pp. 1139-1144
Author(s):  
Iosif Lingvay ◽  
Adriana Mariana Bors ◽  
Livia Carmen Ungureanu ◽  
Valerica Stanoi ◽  
Traian Rus

For the purpose of using three different types of painting materials for the inner protection of the transformer vats, their behavior was studied under actual conditions of operation in the transformer (thermal stress in electro-insulating fluid based on the natural ester in contact with copper for electro-technical use and electro-insulating paper). By comparing determination of the content in furans products (HPLC technique) and gases formed (by gas-chromatography) in the electro-insulating fluid (natural ester with high oleic content) thermally aged at 130 �C to 1000 hours in closed glass vessels, it have been found that the presence the investigated painting materials lead to a change in the mechanism and kinetics of the thermo-oxidation processes. These changes are supported by oxygen dissolved in oil, what leads to decrease both to gases formation CO2, CO, H2, CH4, C2H4 and C2H6) and furans products (5-HMF, 2-FOL, 2 -FAL and 2-ACF). The painting materials investigated during the heat treatment applied did not suffer any remarkable structural changes affecting their functionality in the electro-insulating fluid based on vegetable esters.


2014 ◽  
Vol 28 (2) ◽  
pp. 313-330 ◽  
Author(s):  
R. David Plumlee ◽  
Philip M. J. Reckers

SYNOPSIS: In 2005, an ad hoc committee appointed by the American Accounting Association (AAA) documented a crisis-level shortage of accounting Ph.D.s and recommended significant structural changes to doctoral programs (Kachelmeier, Madeo, Plumlee, Pratt, and Krull 2005). However, subsequent studies show that the shortage continues and the cumulative costs grow (e.g., Fogarty and Holder 2012; Brink, Glasscock, and Wier 2012). The Association to Advance Collegiate Schools of Business (AACSB) recently called for renewed attention to the problem (AACSB 2013b). We contribute to the literature by providing updated information regarding responses by doctoral programs and, from the eyes of potential candidates, of continuing impediments to solving the doctoral shortage. In this paper, we present information gathered through surveys of program administrators and master's and Accounting Doctoral Scholars Program (ADS) students. We explore (1) the cumulative impact of the Ph.D. shortage as of 2013, including its impact on accounting faculty composition, across different types of institutions, (2) negative student perceptions of Ph.D. programs and academic accounting careers, which discourage applicants from pursuing Ph.D. programs, and (3) impediments facing institutions in expanding doctoral programs.


2021 ◽  
pp. 002199832110082
Author(s):  
Azzeddine Gharsallah ◽  
Abdelheq Layachi ◽  
Ali Louaer ◽  
Hamid Satha

This paper reports the effect of lignocellulosic flour and talc powder on the thermal degradation behavior of poly (lactic acid) (PLA) by thermogravimetric analysis (TGA). Lignocellulosic flour was obtained by grinding Opuntia Ficus Indica cladodes. PLA/talc/ Opuntia Ficus Indica flour (OFI-F) biocomposites were prepared by melt processing and characterized using Wide-angle X-ray scattering (WAXS) and Scanning Electron Microscope (SEM). The thermal degradation of neat PLA and its biocomposites can be identified quantitatively by solid-state kinetics models. Thermal degradation results on biocomposites compared to neat PLA show that talc particles at 10 wt % into the PLA matrix have a minor impact on the thermal stability of biocomposites. Loading OFI-F and Talc/OFI-F mixture into the PLA matrix results in a decrease in the maximum degradation temperature, which means that the biocomposites have lower thermal stability. The activation energies (Ea) calculated by the Flynn Wall Ozawa (FWO) and Kissinger Akahira Sunose (KAS) model-free approaches and by model-fitting (Kissinger method and Coats-Redfern method) are in good agreement with one another. In addition, in this work, the degradation mechanism of biocomposites is proposed using Coats-Redfern and Criado methods.


Molecules ◽  
2021 ◽  
Vol 26 (6) ◽  
pp. 1597
Author(s):  
Iman Jafari ◽  
Mohamadreza Shakiba ◽  
Fatemeh Khosravi ◽  
Seeram Ramakrishna ◽  
Ehsan Abasi ◽  
...  

The incorporation of nanofillers such as graphene into polymers has shown significant improvements in mechanical characteristics, thermal stability, and conductivity of resulting polymeric nanocomposites. To this aim, the influence of incorporation of graphene nanosheets into ultra-high molecular weight polyethylene (UHMWPE) on the thermal behavior and degradation kinetics of UHMWPE/graphene nanocomposites was investigated. Scanning electron microscopy (SEM) analysis revealed that graphene nanosheets were uniformly spread throughout the UHMWPE’s molecular chains. X-Ray Diffraction (XRD) data posited that the morphology of dispersed graphene sheets in UHMWPE was exfoliated. Non-isothermal differential scanning calorimetry (DSC) studies identified a more pronounced increase in melting temperatures and latent heat of fusions in nanocomposites compared to UHMWPE at lower concentrations of graphene. Thermogravimetric analysis (TGA) and derivative thermogravimetric (DTG) revealed that UHMWPE’s thermal stability has been improved via incorporating graphene nanosheets. Further, degradation kinetics of neat polymer and nanocomposites have been modeled using equations such as Friedman, Ozawa–Flynn–Wall (OFW), Kissinger, and Augis and Bennett’s. The "Model-Fitting Method” showed that the auto-catalytic nth-order mechanism provided a highly consistent and appropriate fit to describe the degradation mechanism of UHMWPE and its graphene nanocomposites. In addition, the calculated activation energy (Ea) of thermal degradation was enhanced by an increase in graphene concentration up to 2.1 wt.%, followed by a decrease in higher graphene content.


2014 ◽  
Vol 1053 ◽  
pp. 263-267 ◽  
Author(s):  
Xiu Juan Tian

Thermal stability and thermal degradation kinetics of epoxy resins with 2-(Diphenylphosphinyl)-1, 4-benzenediol were investegated by thermogravimetric analysis (TGA) at different heating rates of 5 K/min, 10 K/min, 20 K/min and 40 K/min. The thermal degradation kinetic mechanism and models of the modified epoxy resins were determined by Coast Redfern method.The results showed that epoxy resins modified with the flame retardant had more thermal stability than pure epoxy resin. The solid-state decomposition mechanism of epoxy resin and the modified epoxy resin corresponded to the controlled decelerating ځ˽̈́˰̵̳͂͆ͅ˼˰̴̱̾˰̸̵̈́˰̵̸̳̱̹̽̾̓̽˰̶̳̹̾̈́̿̾̓ͅ˰̶˸ځ˹˰̵̵͇͂˰̃˸́˽ځ˹2/3. The introduction of phosphorus-containing flame retardant reduced thermal degradation rate of epoxy resins in the primary stage, and promote the formation of carbon layer.


2013 ◽  
Vol 820 ◽  
pp. 84-87
Author(s):  
Zheng Zhou Wang ◽  
Charles A. Wilkie

Cadmin sulfate nanoparticles, hollow sphere (CdS-HS) and rode (CdS-NR) were synthesized by ultrasonic and solvothermal process, respectively. The effect of the two kinds of nanoparticles on flammability of polystyrene was investigated using cone calorimeter (Cone) and microscale combustion calorimeter (MCC). Cone data indicate that the incorporation of 1% CdS nanoparticles leads to a about 20% reduction in the peak heat release rate (PHRR) compared to the pure PS; CdS-NR is more efficient in reducing the PHRR proved by both Cone and MCC results. The TG results show that the addition of the nanoparticles mainly increases thermal stability of PS at high temepratures.


Sign in / Sign up

Export Citation Format

Share Document