Proposed Compaction Procedure for Dry Process Crumb Rubber Modified Asphalt Mixtures Using Air Void Content and Expansion Ratio

2014 ◽  
Vol 42 (2) ◽  
pp. 20120337 ◽  
Author(s):  
Miao Yu ◽  
Guoxiong Wu ◽  
Jinchuan Zhou ◽  
Said Easa
2021 ◽  
Vol 13 (13) ◽  
pp. 2613
Author(s):  
Nectaria Diamanti ◽  
A. Peter Annan ◽  
Steven R. Jackson ◽  
Dylan Klazinga

Density is one of the most important parameters in the construction of asphalt mixtures and pavement engineering. When a mixture is properly designed and compacted, it will contain enough air voids to prevent plastic deformation but will have low enough air void content to prevent water ingress and moisture damage. By mapping asphalt pavement density, areas with air void content outside of the acceptable range can be identified to predict its future life and performance. We describe a new instrument, the pavement density profiler (PDP) that has evolved from many years of making measurements of asphalt pavement properties. This instrument measures the electromagnetic (EM) wave impedance to infer the asphalt pavement density (or air void content) locally and over profiles.


2015 ◽  
Vol 2507 (1) ◽  
pp. 108-119 ◽  
Author(s):  
Jong-Sub Lee ◽  
Nelson Gibson ◽  
Y. Richard Kim

Effects of design air void contents, design voids in mineral aggregate (VMA), and in-place air voids on the fatigue performance of asphalt mixtures were investigated with mechanistic analyses based on the viscoelastic continuum damage (VECD) analyses and the mechanistic–empirical pavement analysis using the AASHTOWare Pavement ME Design program. The VECD analyses included the simplified viscoelastic continuum damage model at the material level and two structural models: ( a) layered viscoelastic analysis and ( b) layered viscoelastic pavement analysis for critical distresses. The mix design of a 2013 accelerated loading facility test lane was selected to develop the volumetric mix designs with the design air voids of 3%, 4%, and 5%, design VMAs of 13%, 14%, and 15%, and in-place air void contents of 5%, 7%, and 9% with the Bailey method. Dynamic modulus and direct tension cyclic fatigue tests were performed in accordance with the AASHTO TP 107 procedure. The test results showed that the linear viscoelastic property was affected by the design VMA, design air void content, and in-place air void content in order of sensitivity. Also, the damage states at failure determined from the damage characteristic curves and the mechanistic fatigue predictions had consistent trends as observed for the design VMA, in-place air void, and design air void content in rank of sensitivity. Finally, the design VMA, in-place air void, and design air void parameters were found to be sensitive in the mechanistic analyses, whereas the parameter that was most sensitive in the pavement mechanistic–empirical analysis was the in-place air void content.


Author(s):  
Pajtim Sulejmani ◽  
Safwat Said ◽  
Sven Agardh ◽  
Abubeker Ahmed

One of the major causes of premature failure in asphalt pavements is moisture damage. Asphalt mixtures designed without considering climate impacts may suffer from durability problems caused by movement of water inside the asphalt mixture. Rolling traffic over wet pavement builds up pore pressure in the mixture, which will consequently accelerate deterioration. The objective of the study was to assess the moisture damage to asphalt concrete mixtures by means of complex modulus testing of dry and moisture-conditioned asphalt specimens with various mixture compositions. The asphalt mixtures were conditioned with the Moisture Induced Sensitivity Tester (MIST), which aims to replicate pore pressure in field conditions. The results showed a decline in stiffness modulus and a reduction in elastic properties after MIST conditioning. In addition, the results indicated that binder content and air void content had a significant influence on the reduction in stiffness. To capture the relationship between air void content, binder content, and the reduction in stiffness, a relationship was developed and validated with measurements on cores extracted in the field.


Author(s):  
A. Varveri ◽  
S. Avgerinopoulos ◽  
C. Kasbergen ◽  
A. Scarpas ◽  
A. Collop

2021 ◽  
Author(s):  
Ovidijus Šernas ◽  
Audrius Vaitkus ◽  
Deimantė Kilaitė

The use of crumb rubber made from end of life tyres for asphalt mixtures modification in order to improve their properties or just utilize waste products may be considered as potential solution. Crumb rubber can be used as a bitumen modifier (wet process) or supplementary component of the asphalt mixture (dry process). Dry modification process has more potential due relatively unsophisticated technology and higher possible to use amount of crumb rubber comparing to the wet process. The performance of asphalt mixtures modified by dry process mainly depends on several factors as crumb rubber type, content and size. However, limited number of publications reported the results of dry method crumb rubber modified asphalt mixtures performance. This paper summarizes the latest findings from literature review on the modification technologies and specifications related to dry modification process, the effect of crumb rubber type and amount on modified asphalt mixture performance in terms of stiffness, rutting resistance, water sensitivity, resistance to fatigue and low temperature cracking. The algorithm of crumb rubber modified asphalt mix design was introduced.


Author(s):  
Salih Kocak ◽  
M. Emin Kutay

Three major methods are used to produce crumb rubber modified asphalt pavement: the dry process (CRDry), the terminal blend process (CRTB), and the wet process (CRWet). Although the CRDry process replaces the portion of fine aggregate in the asphalt mixture with crumb rubber (CR) particles, the CRWet process incorporates CR particles into hot liquid asphalt before it is mixed with aggregates. CRTB is known as a special type of CRWet process in which the CR is blended with asphalt binder at the asphalt terminal. In general, the CRWet process can integrate 15% to 22% CR by weight of the binder. This amount ranges from 10% to 12% in the CRTB process as a result of the limitations associated with transportation and pumping. This study investigated the feasibility of increasing the CR content of CRTB modified asphalt mixtures. The addition to the mixture of about 0.5% CR (by weight of the mix) through the CRDry process doubled the amount of rubber to be found in a conventional CRTB mix. The relative performances of the CRTB and the CRTB+CRDry processes [i.e., crumb rubber hybrid (CRHY)] were investigated with respect to their linear viscoelastic properties, rutting susceptibility, moisture damage, resistance to fatigue, and low temperature cracking. It was shown that it was possible to increase the amount of CR in the mixture through the use of the CRHY method proposed here, without adverse effect on the performance of the mixture.


Materials ◽  
2021 ◽  
Vol 14 (10) ◽  
pp. 2649
Author(s):  
Wladyslaw Gardziejczyk ◽  
Piotr Jaskula ◽  
Jerzy A. Ejsmont ◽  
Marek Motylewicz ◽  
Marcin Stienss ◽  
...  

Measures for the improvement of acoustic conditions in the vicinity of roads include the construction of pavement structures with low-noise surfaces with optimal macrotexture and the highest possible sound absorption coefficient. Laboratory evaluation of acoustic properties of a designed asphalt mixture before its placement in the pavement is a good solution. Currently, the most popular method for the determination of the sound absorption coefficient of various construction materials under laboratory conditions is the Kundt’s tube test. Sound absorption coefficient can also be assessed based on field and laboratory measurements performed using a Spectronics ACUPAVE System. Other parameters characterising the acoustic properties of road pavement courses include air void content and water drainability or permeability. The article presents an analysis of results of sound absorption coefficient obtained using a Spectronics ACUPAVE System and water drainability and permeability of poroelastic mixtures obtained both in laboratory and on test sections, in relation to air void content and grading of the mixtures. It was established that poroelastic mixtures containing an aggregate of maximum particle size of 5 mm are characterised by better acoustic properties than mixtures with a maximum aggregate particle size of 8 mm. Changes of crumb rubber aggregate grading and bitumen type (within the tested range of values) as well as the addition of lime have shown no evident influence on the sound absorption coefficient. Noise level values at the speed of 30 km/h according to the CPX method were measured as well. Relationships between sound absorption coefficient, water drainability/permeability, and air void content were determined. The performed analyses confirmed that Spectronics ACUPAVE System may be applied for evaluation of acoustic properties of asphalt mixtures in laboratory conditions, but further research is needed to reduce the uncertainty of the results.