scholarly journals OPTIMIZING THE USE OF ROCK ASH AS FINE AGGREGATES WITH THE ADDITION OF ADDITIVES TO THE CONCRETE MIXTURE WITH A COMPRESSIVE STRENGTH OF 350 Kg/cm2

CI-TECH ◽  
2020 ◽  
Vol 1 (01) ◽  
pp. 45-48
Author(s):  
Triaswati ◽  
Srie Subekti ◽  
Sulchan Arifin ◽  
Febri Aditya

Stone dust nowadays is a side product of the stone crushing industry, the quality of which is quite a lot that it becomes a waste that needs to be handled. This study is intended to find out the composition of stone dust by adding some additive substance type D and type F to reach a compressive strength of 350 kg/cm2. The variation of percentage of stone dust on the composition of concrete mixture is 0%, 20%, 40%, 60%, 80%, 100%. The design of concrete mixture composition refers to the procedure of making preparation of the normal concrete mixture. SNI 03-2384-1993. The size of the cylinder test object is 15 cm in diameter and 30 cm in height. The result of this research shows that the mixture using stone dust has quite an effect on the compressive strength of concrete. From the result of the experiment, it is shown that for compressive strength of 350 kg/cm2, we can use 100% of stone dust with a resulted compressive strength of 445 kg/cm2.

Jurnal Tekno ◽  
2021 ◽  
Vol 18 (2) ◽  
pp. 11-20
Author(s):  
Ahmad Junaidi ◽  
R Dewo Hiraliyamaesa Hariyanto

Perumpung (Eulalia japonica) is a wild plant that usually grows on the banks of river. The locals consider this plant as a waste/pest, but the authors are interested in researching perumpung because they are similar to bamboo, sugarcane and other fibrous plants. In this study, the authors aims to compare the compressive strength of normal concrete with the compressive strength of concrete added with Perumpung ash at 28-days-old K-300. The study used a cube-shaped test object (15 x 15 x 15 cm) with 6 samples for each condition. The total number of test objects is 48, which consists of 8 conditions, namely normal conditions and 5%, 7.5%, 10%, 12.5%, 15%, 17.5% and 20% addition of perumpung ash by cement weight. The results obtained that the compressive strength of 28-days-old concrete under normal conditions was 316,060 kg/cm2 and the addition of 5% ash was 331.583 kg/cm2, 7.5% was 337.181 kg/cm2, 10% was 341.813 kg/cm2, 12 ,5% is 347,045 kg/cm2, 15% is 353,889 kg/cm2, 17.5% is 311,160 kg/cm2 and 20% is 298.44 kg/cm2. From the results above it can be concluded that the addition of 15% Perumpung Ash to the concrete mixture increases the maximum characteristic concrete compressive strength by 353.889 kg/cm2.


Author(s):  
Sudirman Kimi ◽  
Abdullah Abuzar Alghafari

In the development of concrete technology (Concrete Technology) today which is increasingly unceasingly, along with the development of the era hence the quality of concrete selection as the main raw material of building construction is very important. This research writer take silica fume and glenium sky as added concrete mixture to know the influence of the addition of silica fume and glenium sky to the compressive strength of concrete. The research is divided into three stages : material testing, test object making and test object. This research uses cube-shaped specimen with size 15x15x15 cm, with 5 variations, they are normal concrete, silica fume 5%, silica fume 5% + glenium sky 2%, silica fume 5% + glenium sky 4%, and silica fume 5% + glenium sky 6%, which every variations has 3 test specimens with 3 days, 7 days, and 28 days. From laboratorium testing, the characteristics of compressive strength of concrete at age 28 days of normal concrete is 407,2 Kg/Cm2, normal concrete with silica fume 5% is 418,5 Kg/Cm2, normal concrete with silica fume 5% + glenium sky 2% is 435,9 Kg/Cm2, normal concrete with silica fume 5% + glenium sky 4% is 451,9 Kg/Cm2, normal concrete with silica fume 5% + glenium sky 6% is 484,1 Kg/Cm2.


2020 ◽  
Vol 8 (1) ◽  
pp. 36-41
Author(s):  
Whendy Trissan ◽  
Yongki Pratomo

In general, concrete fillers are made from materials that are easily obtained, easily processed, and have the durability and strength that is very much needed in particular construction of coarse and fine aggregates, each region would have different aggregates as the main ingredients in making concrete. The research conducted aims to determine how the optimum compressive strength value of the concrete produced from the addition of Kapuas Sand to the concrete mixture. In this research, Kapuas Sand is used as a fine aggregate enhancer. The percentage variation of Kapuas red sand used in this study varies, namely 0%, 25%, 50%, 75%, and 100%. Concrete mixture planning using SNI 03-2834-2000. The test uses cylindrical specimens with a height of 30 cm, a diameter of 15 cm with a total sample of 10 cylinders for each addition of Kapuas Sand so that the total specimens are 50 cylinders. Testing is carried out at the age of 14 and 28 days in the Laboratory of Building Engineering Education Study Program, Faculty of Teacher Training and Education, University of Palangka Raya. The results of the compressive strength of concrete using a mixture of Kapuas Sand at 28 days 0% 25%, 50%, 75% and, 100% respectively were 24.71 MPa, 21.79 MPa, 25.36 MPa, 23 .3 MPa, and .22.62 MPa. This result shows the compressive strength value of concrete in the concrete mix with a percentage of 50% that is equal to 25.36 MPa while the compressive strength of normal concrete is 24.71 MPa so that the compressive strength of concrete is 2.66% of normal concrete compressive strength with age concrete compressive strength 28 days.


2020 ◽  
Vol 2 (1) ◽  
pp. 31-57
Author(s):  
Ni Ketut Sri Astati Sukawati

Concrete with various variants is a basic requirement in building a building. The concrete mixture is diverse depending on the planning made beforehand. The cement mixture is usually in the form of a mixture of artificial stone, cement, water and fine aggregates and coarse aggregates. Aggregates (fine aggregates and coarse aggregates) function as fillers in concrete mixtures. (Subakti, A., 1994). However, in building construction, additives are often added, but there is still a sense of uncertainty at the time of dismantling the mold and the reference before the concrete reaches sufficient strength to carry its own weight and the carrying loads acting on it. To overcome the time of carrying out work related to concrete, it is necessary to find an alternative solution, for example by looking for alternative ingredients of concrete mixture on the basis of consideration without reducing the quality of the concrete. From the results of previous studies it was stated that due to the partial replacement of cement with Fly Ash, the strength of the pressure and tensile strength of the concrete had increased (Budhi Saputro, A., 2008). Based on the description above, the author seeks to examine how the compressive strength of concrete characteristics that occur by adding additives Addition H.E in the concrete mixture and is there any additive Additon H.E effect on the increase in the compressive strength characteristic of the concrete. From the results of the study, it was found that the compressive strength of the concrete with the addition of additives HE was that after the compressive strength test of the concrete cube was carried out and the analysis of concrete compressive strength of 10 specimens, in each experiment a cube specimen was made with the addition of additons. HE with a dose of 80 cc, 120 cc, and 200 cc can accelerate and increase the compressive strength of concrete characteristics.


2019 ◽  
Vol 14 (2) ◽  
Author(s):  
Syifa Fauziah ◽  
Anisah Anisah ◽  
Sittati Musalamah

This research aims to determine the maximum compressive strength value of concrete speedcrete using naphthalene additive additive at each test age and compare with normal concrete 28 days. This research used cylindrical test object with diameter 15 cm and height 30 cm. Speedcrete concrete does not undergo the treatment process while the normal concrete test object through the treatment process. Testing compressive strength of concrete speedcrete using Crushing Test Machine tool. In this research the compressive strength was produced by using superplasticizer type naphthalene and compared with normal concrete without using additive. The target quality plan is fc '35 MPa with the use of additive dose of 1.7% of the weight of cement. The results of this research showed an increase in the value of compressive strength of concrete speedcrete with aadditive materials added naphthalene increased with increasing age of concrete. The results showed that the compressive strength of concrete speedcrete with naphthalene additive materials of 12 hours, 18 hours, 28 hours and 48 hours was 0.5 MPa, 17,81 MPa, 31,14 MPa and 45,77 MPa. Normal strength concrete strength with the addition of 20% water age 28 days that is equal to 54.76 MPa.


Author(s):  
N. Sharma ◽  
M. Singh Thakur ◽  
P.L. Goel ◽  
P. Sihag

Purpose: Over the years, various experiments have been performed to investigate the impact of marble powder within the concrete mixture. In the present study, a review has been done to check the persistence of marble dirt as the substitute for concrete constituents. Design/methodology/approach: Furthermore, the impact of marble powder as a replacement of cement and aggregates were reviewed. By reviewing previous studies, the result indicates that the use of waste marble powder in cement and aggregate was adequate to a certain range. Findings: By replacing cement with marble powder in a range between 5% to 10% by weight, it increases the compressive strength of concrete mix by 11.30% to 24.56%, compared to the nominal mix. According to the study, any further increase in the amount of marble powder in place of cement i.e, 12.5% to 20% replacement by weight, results in the reduction of compressive strength of concrete mix by 7.5% to 26.01%. Replacement of aggregates from 5% to 75% with marble powder increases the compressive strength of about 3.22% to 23.91% as compared to the nominal mix. Research limitations/implications: It was also concluded from the current study that, to obtain higher compressive strength, it is advantageous to replace fine aggregates with marble powder than the replacement of cement with the marble powder.


2021 ◽  
Vol 2 (1) ◽  
pp. 46-54
Author(s):  
Neti Rahmawati ◽  
Irwan Lakawa ◽  
Sulaiman Sulaiman

Concrete is one of the most widely used building materials today interms of physical construction. Concrete is made from a mixture offine, coarse aggregate, cement, and water with a certain ratio, aswell as materials that are usually added to the concrete mixtureduring or during mixing, to changing the properties of concrete tomake it more suitable in certain jobs and more economical, can alsobe added with certain other mixed materials as needed if deemednecessary. Seashells can be used to mix concrete. This study aims todetermine whether the addition of shells aggregate shells in aconcrete mixture can affect the mechanical properties of concrete.The specimens used are in the form of cubes with a size of 15cm x 15cm x 15 cm, consisting of additional concrete coarse and fineaggregate with shell substitution percentage of 0%, 15%, 20% with atotal sample of 45, with the planned concrete quality of K225. Theuse of sea shells in increasing the compressive strength of concrete isbetter used as fine aggregate than coarse aggregate. The use of seashells as a substitute for fine aggregates achieves maximum resultsat 20% composition.


2017 ◽  
Vol 6 (1) ◽  
pp. 30-40
Author(s):  
Fauzi Rahman ◽  
Fathurrahman Fathurrahman

In 2015 the total area of oil palm plantations in Kalimantan reached 3.47 million Ha with a production of 8.12 million tons per year. Solid waste is in the form of fresh fruit bunches and palm shells. The result of combustion of oil palm shell waste in the form of boiler crust ash is a waste that has chemical elements SiO2, Al2O3, and CaO, with the content of these compounds can affect the strength of the concrete and can increase its strength. In this study, the quality of the concrete mix planned at 28 days is 23 MPa. Concrete testing included compressive strength tests carried out at 3 days, 7 days, 14 days, 28 days, 42 days and 56 days. Before making concrete samples, the mortar compressive strength is tested first by varying the boiler crust ash content by 0%, 15%, 25%, 35%, and 50% to obtain the optimum mixture. Based on the results of the analysis of compressive strength mortar obtained the optimum mixture of 15% for the manufacture of concrete that will be compared with normal concrete. The compressive strength of concrete with the optimum mixture at 28 days is 24.44 Mpa more than the compressive strength of the 23 Mpa plan. Concrete that has the highest compressive strength occurs at the age of 56 days is concrete with the normal mixture with a compressive strength of 34.44 Mpa higher than the compressive strength of concrete with an optimum mixture of 15% boiler crust ash which is 28.51 MPa.


2020 ◽  
Vol 3 (1) ◽  
pp. 12
Author(s):  
Moh. Abdul Basit Minanulloh ◽  
Yosef Cahyo ◽  
Ahmad Ridwan

K-300 concrete is concrete that has a characteristic compressive strength of 300 kg/cm2.  Many studies that use plantation and mining waste materials are simply wasted. These wastes are in the form of kemiri shell ash, rice husk ash, and others. in this study, kemiri shell ash as a cement additive, with variations in the addition of 5%, 10%, and 15% of the weight of cement to the quality of K-300 concrete. Concrete compressive tests carried out at the age of 7 and 28 days. The purpose of this study was to determine the compressive strength of concrete, the highest pressure strength, and the optimum percentage. Strong concrete pressure characteristics obtained at 28 days at a normal concrete variation 304.127 kg / cm, normal concrete variations with the addition of 5% “Abu Cangkang kemiri” 421,551 kg / cm, normal concrete variations with the addition of 10% “Abu Cangkang kemiri” 426,863 kg / cm2, and variations  normal concrete with the addition of 15% “Abu Cangkang kemiri” 428,210 kg / cm.  The results show that the optimum percentage of the addition of kemiri shell ash is 15% of the weight of cement with a maximum compressive strength of 428,210 kg/cm.  Beton K-300 adalah beton yang mempunyai kuat tekan karakteristik sebesar 300 kg/cm². Banyak penelitian yang menggunakan bahan – bahan limbah perkebunan dan tambang yang terbuang begitu saja. Limbah tersebut berupa abu cangkang kemiri, abu sekam Padi, dan lain- lain. Pada penelitian ini menggunakan abu cangkang Kemiri sebagai bahan tambah semen, dengan variasi penambahan 5%, 10%, dan 15%  dari berat semen terhadap mutu beton K-300. Uji tekan beton dilaksanakan pada umur 7 dan 28 hari. Tujuan penelitian ini adalah untuk mengetahui kuat tekan beton dan  kuat tekan tertinggi. Kuat tekan karakteristik yang diperoleh pada umur 28 hari pada variasi beton normal 304,127 kg/cm², variasi beton normal dengan penambahan 5% abu cangkang  Kemiri 421,551 kg/cm², variasi beton normal dengan penambahan10% abu cangkang Kemiri 426,863kg/cm², dan variasi beton normal dengan penambahan 15% abu cangkang Kemiri 428,210 kg/cm². Hasil penelitian menunjukkan bahwa presentase optimum dari penambahan abu cangang Kemiri  adalah sebesar15% dari berat semen dengan kuat tekan maksimum sebesar 428,210 kg/cm².


2020 ◽  
Vol 2 (1) ◽  
pp. 1-12
Author(s):  
Rafki Imani ◽  
Widiawati Purba ◽  
Rainaldi S Nainggolan

AbstractConcrete is composed of three main constituent materials, namely cement, aggregate and water. The development of concrete technology in the trial of adding a mixture of materials continues to be done to achieve the desired strength and quality. In this experiment, the addition of gypsum waste was used as a concrete mixture to determine its effect on the compressive strength of concrete. The variation in the percentage of the addition of gypsum waste is 5%, 10%, and 15% with the age of treatment observed at 14 days and 28 days. The results showed that the normal compressive strength value at 14 days was 186.87 kg/cm2, while with the addition of gypsum waste mixture the concrete compressive strength at 5%, 10% and 15% were obtained 178.45 kg respectively /cm2, 101, 01 kg/cm2, 70.71 kg/cm2. Meanwhile the compressive strength value of normal concrete at 28 days is 164.44 kg/cm2, and the compressive strength value of concrete after mixed with gypsum waste at 28 days is obtained 157.04 kg/cm2, 88.89 kg/cm2, 62.22 kg/cm2. Based on the results it can be concluded that the addition of gypsum waste as a concrete mixture material can reduce the compressive strength values of normal concrete.Keywords : Concrete, compressive strength, and gypsum waste.AbstrakBahan beton terdiri dari semen, pasir, kerikil dan air. Perkembangan teknologi beton dalam uji coba penambahan bahan campuran terus dilakukan untuk mendapatkan kekuatan dan mutu beton yang diinginkan. Dalam penelitian ini, penambahan limbah gipsum dimaksudkan sebagai campuran beton untuk melihat pengaruhnya pada nilai kuat tekan beton. Variasi persentase penambahan limbah gipsum ini adalah sebesar 5%, 10%, dan 15% dengan umur perawatan diamati pada umur 14 hari dan 28 hari. Hasil penelitian menunjukkan bahwa nilai kuat tekan beton normal pada umur 14 hari diperoleh sebesar 186,87 kg/cm2, sementara dengan penambahan campuran limbah gipsum nilai kuat tekan beton pada persentase 5%, 10% dan 15% secara berurutan diperoleh sebesar 178,45 kg/cm2, 101, 01 kg/cm2, 70,71 kg/cm2. Sementara nilai kuat tekan beton normal pada umur 28 hari adalah sebesar 164,44 kg/cm2, dan nilai kuat tekan beton setelah dicampur limbah gipsum pada umur 28 hari secara berurutan diperoleh sebesar 157,04 kg/cm2, 88,89 kg/cm2, 62,22 kg/cm2. Hasil penelitian menyimpulkan bahwa penambahan limbah gipsum sebagai bahan campuran beton dapat mengurangi nilai kuat tekan beton dibandingkan dengan kuat tekan beton normal. Kata kunci : Beton, kuat tekan dan limbah gipsum.