scholarly journals Experimental Investigation of Porous and Mechanical Characteristics of Single-Crack Rock-like Material under Freeze-Thaw Weathering

Minerals ◽  
2021 ◽  
Vol 11 (12) ◽  
pp. 1318
Author(s):  
Songtao Yu ◽  
Yuxian Ke ◽  
Hongwei Deng ◽  
Guanglin Tian ◽  
Junren Deng

Freeze-thaw weathering changes the pore structure, permeability, and groundwater transportation of rock material. Meanwhile, the change in rock material structure deduced by frost heaving deteriorates mechanical properties of rock material, leading to instability and insecurity of mine slopes in cold regions. In this paper, rock-like specimens containing prefabricated cracks at different angles and having undergone various freeze-thaw cycles are used as the object. Their pore structure, compressive mechanical properties, strain energies, failure characteristics, and the connection between pore structure and mechanical properties are analyzed. Results show that the porosity, spectrum area of mesopores, and spectrum area of macropores increase with the increase in freeze-thaw cycles, while crack angle shows no obvious influence on pore structure. Peak stress and elastic modulus drop with the increase in freeze-thaw cycles, while peak strain shows an increasing trend. Peak stress and elastic modulus decrease in the beginning, and then increase with the increase in crack angle, while peak strain shows a reverse trend. Elastic strain energy and pre-peak strain energy drop with the increase in freeze-thaw cycles. Elastic strain energy decreases first, and then increases with the increase in crack angle. The correlation between the spectrum area of macropores and elastic modulus is the strongest among different pores. Elastic modulus and peak stress decrease with the increase in macropore spectrum area, and peak strain increases with the increase in macropore spectrum area.

2020 ◽  
Vol 2020 ◽  
pp. 1-8
Author(s):  
Guoliang Yang ◽  
Jingjiu Bi ◽  
Xuguang Li ◽  
Jie Liu ◽  
Yanjie Feng

Shale gas is the most important new energy source in the field of energy, and its exploitation is very important. The research on the dynamic mechanical properties of shale is the premise of exploitation. To study the dynamic mechanical properties of shale from the Changning-Weiyuan area of Sichuan Province, China, under confining pressure, we used a split Hopkinson pressure bar (SHPB) test system with an active containment device to carry out dynamic compression tests on shale with different bedding angles. (1) With active confining pressure, the shale experiences a high strain rate, and its stress-strain curve exhibits obvious plastic deformation. (2) For the same impact pressure, the peak stress of shale describes a U-shaped curve with an increasing bedding angle; besides, the peak stress of shale with different bedding angles increases linearly with rising confining pressure. The strain rate shows a significant confining pressure enhancement effect. With active confining pressure, the peak strain gradually decreases as the bedding angle increases. (3) As a result of the influence of different bedding angles, the dynamic elastic modulus of shale has obvious anisotropic characteristics. Shale with different bedding angles exhibits different rates of increase in the dynamic elastic modulus with rising confining pressure, which may be related to differences in the development of planes of weakness in the shale. The results of this study improve our understanding of the behavior of bedded shale under stress.


Geofluids ◽  
2021 ◽  
Vol 2021 ◽  
pp. 1-15
Author(s):  
Xiaoxiao Cao ◽  
Meimei Feng ◽  
Kangsheng Yuan

During the construction of geotechnical engineering in cold regions, the stability of rock is inevitably affected by freeze-thaw cycles and hydrochemical corrosion. In order to study the effect of hydrochemical corrosion on dynamic mechanical properties of freeze-thaw rocks, dynamic compression tests were carried out on sandstone samples corroded by four different concentrations of HCl solutions with the same number of freeze-thaw cycles using split-Hopkinson pressure bar (SHPB) test system. The coupling effects of freeze-thaw cycles with different concentrations of HCl solutions and strain rate on mechanical properties of sandstones were explored. The results showed that strain rate could enhance the dynamic compressive strength and peak strain but had no significant effect on the elastic modulus. The coupling effect of freeze-thaw cycles and acid corrosion weakened the dynamic compressive strength, and elastic modulus but enhanced the peak strain. In addition, X-ray diffractometer (XRD) and scanning electron microscope (SEM) were used to analyze the changes of mineral composition and microstructure damage of sandstone samples under the coupling effect of acid corrosion and freeze-thaw cycles. The analysis results were basically consistent with the damage characteristics of macro mechanical properties. The research results can provide reference for open pit coal mining in cold regions.


2014 ◽  
Vol 1014 ◽  
pp. 49-52
Author(s):  
Xiao Ping Su

With the wide application of high strength concrete in the building construction,the risk making concrete subject to high temperatures during a fire is increasing. Comparison tests on the mechanical properties of high strength concrete (HSC) and normal strength concrete (NSC) after the action of high temperature were made in this article, which were compared from the following aspects: the peak stress, the peak strain, elasticity modulus, and stress-strain curve after high temperature. Results show that the laws of the mechanical properties of HSC and NSC changing with the temperature are the same. With the increase of heating temperature, the peak stress and elasticity modulus decreases, while the peak strain grows rapidly. HSC shows greater brittleness and worse fire-resistant performance than NSC, and destroys suddenly. The research and evaluation on the fire-resistant performance of HSC should be strengthened during the structural design and construction on the HSC buildings.


2021 ◽  
Vol 28 (1) ◽  
pp. 516-527
Author(s):  
Jiangwei Bian ◽  
Wenbing Zhang ◽  
Zhenzhong Shen ◽  
Song Li ◽  
Zhanglan Chen

Abstract The most significant difference between recycled and natural concretes lies in aggregates. The performance of recycled coarse aggregates directly affects the characteristics of recycled concrete. Therefore, an in-depth study of aggregate characteristics is of great significance for improving the quality of recycled concrete. Based on the coarse aggregate content, maximum aggregate size, and aggregate shape, this study uses experiments, theoretical analysis, and numerical simulation to reveal the impact of aggregate characteristics on the mechanical properties of recycled concrete. In this study, we selected the coarse aggregate content, maximum aggregate size, and the aggregate shape as design variables to establish the regression equations of the peak stress and elastic modulus of recycled concrete using the response surface methodology. The results showed that the peak stress and elastic modulus of recycled concrete reach the best when the coarse aggregate content is 45%, the maximum coarse aggregate size is 16 mm, and the regular round coarse aggregates occupy 75%. Such results provide a theoretical basis for the resource utilization and engineering design of recycled aggregates.


2020 ◽  
Vol 10 (10) ◽  
pp. 3351
Author(s):  
Bo Ke ◽  
Jian Zhang ◽  
Hongwei Deng ◽  
Xiangru Yang

The effect of temperature fluctuation on rocks needs to be considered in many civil engineering applications. Up to date the dynamic characteristics of rock under freeze-thaw cycles are still not quite clearly understood. In this study, the dynamic mechanical properties of sandstone under pre-compression stress and freeze-thaw cycles were investigated. At the same number of freeze-thaw cycles, with increasing axial pre-compression stress, the dynamic Young’s modulus and peak stress first increase and then decrease, whereas the dynamic peak strain first decreases and then increases. At the same pre-compression stress, with increasing number of freeze-thaw cycles, the peak stress decreases while the peak strain increases, and the peak strain and peak stress show an inverse correlation before or after the pre-compression stress reaches the densification load of the static stress–strain curve. The peak stress and strain both increase under the static load near the yielding stage threshold of the static stress–strain curve. The failure mode is mainly shear failure, and with increasing axial pre-compression stress, the degree of shear failure increases, the energy absorption rate of the specimen increases first and then decreases. With increasing number of freeze-thaw cycles, the number of fragments increases and the size diminishes, and the energy absorption rates of the sandstone increase.


2019 ◽  
Vol 2019 ◽  
pp. 1-12
Author(s):  
Ruijun Wang ◽  
Yan Li ◽  
Yang Li ◽  
Fan Xu ◽  
Xiaotong Li ◽  
...  

This study aims at determining the effect of water pressure on the mechanical properties of concrete subjected to freeze-thaw (F-T) attack under the dynamic triaxial compression state. Two specimens were used: (1) a 100 mm × 100 mm × 400 mm prism for testing the loss of mass and relative dynamic modulus of elasticity (RDME) after F-T cycles and (2) cylinders with a diameter of 100 mm and a height of 200 mm for testing the dynamic mechanical properties of concrete. Strain rates ranged from 10−5·s−1 to 10−3·s−1, and F-T cycles ranged from 0 to 100. Three levels of water pressure (0, 5, and 10 MPa) were applied to concrete. Results showed that as the number of F-T cycles increased, the mass loss rate of the concrete specimen initially decreased and then increased, but the RDME decreased. Under 5 MPa of water pressure and at the same strain rate, the ultimate compressive strength decreased, whereas the peak strain increased with the increase in the number of F-T cycles. This result is contrary to the variation law of ultimate compressive strength and peak strain with the increase in strain rate under the same number of F-T times. With the increase in F-T cycles or water pressure, the strain sensitivity of the dynamic increase factor of ultimate compressive strength and peak strain decreased, respectively. After 100 F-T cycles, the dynamic compressive strength under all water pressure levels tended to increase as the strain rate increased, whereas the peak strain decreased gradually.


2013 ◽  
Vol 843 ◽  
pp. 66-69 ◽  
Author(s):  
Hui Jing Zhao ◽  
Guo Li Zhou ◽  
Zhi Qing Yuan

Biomaterials used for vascular prostheses should possess certain strength that can keep the normal blood fluidity, as well as certain flexibility and elasticity that can resist blood pulsation pressure. In order to fabricate small diameter vascular prostheses (SDVP) that possess matchable mechanical properties with natural blood vessels, a bi-layered tubular structure composed of electrospinning blended nanofiber and silk fiber was designed and prepared in this study. The inner layer of the structure, prepared through electrospinning, was composed of Poly (L-lactide-co-ε-caprolactone) (PLCL) and silk fibroin (SF) blended nanofibers. Braided silk tube was used as the outer layer of the structure. Morphological, structural and mechanical properties including peak stress, peak strain, and Youngs modulus of the prototype bi-layered SDVP were characterized initially. Results showed that the diameter range of the blended nanofiber was between 100 and 900 nm, and the fiber diameter increased with the content increase of PLCL. Through blending PLCL together with SF, peak stress and peak strain of the electrospun inner layer were improved, and that of the Youngs modulus decreased. Meanwhile, the outer layer of SDVP was stronger and had higher Youngs modulus. Those mechanical performances of the prototype bi-layered SDVP fabricated in this study are similar to natural blood vessels, which provide a promising biomaterial that could be applied on tubular tissue engineering scaffolds.


2013 ◽  
Vol 690-693 ◽  
pp. 1737-1740
Author(s):  
Lin Bu ◽  
Tao Xu ◽  
Yun Jie Zhang

The mechanical properties of granite experiencing high temperatures under uniaxial compression condition were simulated in this paper. Numerically simulated stress-strain curve, peak stress, peak strain and the tangent elastic modulus were compared with the corresponding physical tests. Simulated results agree well with physical tests results, it is shown that Abaqus is suitable for the analysis of the temperature effect on rock fracture.


Geofluids ◽  
2021 ◽  
Vol 2021 ◽  
pp. 1-14
Author(s):  
Peng Wu ◽  
Lianying Zhang ◽  
Xianbiao Mao ◽  
Yanlong Chen ◽  
Ming Li ◽  
...  

Strain rate is not only an important influence factor for deformation property but also an important parameter for analyzing the dynamic mechanical behavior of rock material. In this study, the dynamic compressive mechanical properties of saturated yellow sandstone at four strain rates and six freeze-thaw temperatures are investigated by using the SHPB test system. The coupling effect of strain rate and freeze-thaw temperatures on the mechanical parameters of rock material are discussed in detail, and the relationship formula of peak strain and dissipated energy with strain rate and freeze-thaw temperature are also established. Finally, the fractal dimension characteristic of fracture specimens with the strain rate and temperature are analyzed by using the fractal dimension method. The research results indicate that (1) with the increase of strain rate, the increase speed of peak strain, peak strength, and dissipated energy at medium strain rate level was obviously higher than that at high strain rate level, indicating that the strain rate effect weakened at high strain rate. (2) Freeze-thaw temperature can improve the brittleness-ductile transformation rate of saturated specimens. (3) According to the strain rate sensitivity coefficient, at room temperature, the strain rate effects on peak strain and peak strength are weakest, while at -20°C ~ -30°C, they are most significant. In addition, the strain rate effect on dissipated energy is significant at room temperature, while weakest at -30°C. (4) The fractal dimension gradually increases with strain rate increasing or freeze-thaw temperature decreasing, indicating that the freeze-thaw environment has a positive function for increasing the damage and fracture degree of specimens for saturated specimen. Our research results can provide an extremely important theoretical basis for the dynamic disaster prevention and structural design of rock engineering in cold regions.