Basic Mechanics Characters of Recycled Fine Aggregate Concrete

2012 ◽  
Vol 446-449 ◽  
pp. 2028-2032 ◽  
Author(s):  
Jian Geng ◽  
Yong Yong Chen ◽  
Jia Ying Sun ◽  
Wei Chen

In this article, the basic mechanical characters of recycled fine aggregate concrete (RFAC) are studied, and the relationships of recycled fine aggregate (RFA) content, minimum particle size and water content with them are also discussed according to results of cubic compressive strength (f¬¬cu), flexural strength (ff), splitting tensile strength(fts), axial compressive strength(fc)and Yang’s modulus (Ec). The results indicate that the use of RFA will induce mechanical properties of RFAC to deteriorate, and the deteriorated trend of it become more obviously with RFA content increased and minimum particle size reduced, in addition to, the early compressive strength of RFA develop slowly. The RFAC elastic modulus is significantly lower than ordinary concrete, besides, RFA on elastic modulus was significantly affected than other mechanical properties.

Geofluids ◽  
2021 ◽  
Vol 2021 ◽  
pp. 1-13
Author(s):  
Yanlin Huang ◽  
An Zhou

In recent years, with the rapid development of the construction industry, the demand for natural river sand has become increasingly prominent. Development of alternatives to river sand has become an interesting direction for concrete research. In this paper, coal gangue was proposed to replace part of the river sand to produce coal gangue fine aggregate concrete, while waste polyethene terephthalate (PET) bottles were used as raw materials to make PET fibers to improve the mechanical properties of coal gangue fine aggregate concrete. There were two parts of the test conducted. In the first part, the compressive strength of the gangue fine aggregate concrete cube, splitting tensile strength, axial compressive strength, and static elastic modulus were studied when the substitution rate of coal gangue increased from 0% to 50%. Referring to the equation of the full stress-strain curve of plain concrete, the stress-strain constitutive equation of coal gangue fine aggregate concrete was analyzed and studied. By comparing with plain concrete, it was found that the coal gangue concrete with a replacement rate of 50% had higher compressive strength and tensile strength, but its brittleness was significantly greater than that of plain concrete in the later stage. In the second part, by studying the effect of different PET fiber content on the mechanical properties of coal gangue fine aggregate concrete with a replacement rate of 50%, it was found that when the addition of PET fiber was 0.1% and 0.3%, not only were compressive strength, splitting tensile strength, static elastic modulus, and flexural strength of the gangue fine aggregate concrete effectively improved but also the brittleness of concrete can be significantly reduced. The study found that after adding 0.3% PET fiber, the coal gangue fine aggregate concrete with a replacement rate of 50% has better mechanical properties and less brittleness.


Energies ◽  
2021 ◽  
Vol 14 (8) ◽  
pp. 2303
Author(s):  
Congyu Zhong ◽  
Liwen Cao ◽  
Jishi Geng ◽  
Zhihao Jiang ◽  
Shuai Zhang

Because of its weak cementation and abundant pores and cracks, it is difficult to obtain suitable samples of tectonic coal to test its mechanical properties. Therefore, the research and development of coalbed methane drilling and mining technology are restricted. In this study, tectonic coal samples are remodeled with different particle sizes to test the mechanical parameters and loading resistivity. The research results show that the particle size and gradation of tectonic coal significantly impact its uniaxial compressive strength and elastic modulus and affect changes in resistivity. As the converted particle size increases, the uniaxial compressive strength and elastic modulus decrease first and then tend to remain unchanged. The strength of the single-particle gradation coal sample decreases from 0.867 to 0.433 MPa and the elastic modulus decreases from 59.28 to 41.63 MPa with increasing particle size. The change in resistivity of the coal sample increases with increasing particle size, and the degree of resistivity variation decreases during the coal sample failure stage. In composite-particle gradation, the proportion of fine particles in the tectonic coal sample increases from 33% to 80%. Its strength and elastic modulus increase from 0.996 to 1.31 MPa and 83.96 to 125.4 MPa, respectively, and the resistivity change degree decreases. The proportion of medium particles or coarse particles increases, and the sample strength, elastic modulus, and resistivity changes all decrease.


2010 ◽  
Vol 168-170 ◽  
pp. 2200-2203 ◽  
Author(s):  
Shun Bo Zhao ◽  
Na Liang ◽  
Li Xin Liu ◽  
Li Sun ◽  
Su Yang

The validity of the wet-sieving concrete technique for building the reinforced composite concrete wall are demonstrated in the paper. The fine aggregate concrete made by ordinary concrete passing the sieve with square mash of 15 mm was cast for the surface layer, the recomposed concrete mixed by the residual concrete stayed on the sieve with the ordinary concrete was cast for the reinforced concrete structural wall. The mechanical properties such as the cubic and compressive strengths, the elastic modulus and the splitting and flexural tensile strengths of the fine aggregate concrete, the recomposed concrete and the ordinary concrete were tested and analyzed. The results show that the elastic modulus and splitting tensile strength of fine aggregate concrete reduce in some extent compared with that of ordinary concrete, the mechanical properties of recomposed concrete are almost the same as that of ordinary concrete.


2011 ◽  
Vol 418-420 ◽  
pp. 441-444 ◽  
Author(s):  
Feng Lan Li ◽  
Yan Zeng ◽  
Chang Yong Li

Due to many different characteristics such as irregular polygon particle with pointed edges, rough surface and larger content of stone powder, machine-made sand has ignorable effects on the properties of concrete. As the basis for the design of concrete structures, the relations among the basic mechanical properties of concrete such as compressive strength, tensile strength, flexural strength and elastic modulus should be clearly understood. This paper summarizes the test data from the published references, and discusses the relations among these properties by statistical analyses compared with those of ordinary concrete. The results show that the axial compressive strength and the tensile strength can be prospected by the same formulas of ordinary concrete specified in current Chinese design code, but the prospected tensile strength should multiply a reducing coefficient when the strength grade of concrete is lower than C30. The elastic modulus of concrete with machine-made sand is larger than that of ordinary concrete, which should be prospect by the formula in this paper. Meanwhile, the formula of flexural strength is suggested.


2013 ◽  
Vol 438-439 ◽  
pp. 15-19
Author(s):  
Chun Jie Liu ◽  
Chun Yan Jia ◽  
Chang Yong Li

Although the machine-made sand was widely used for concrete in recent years in China, it was short of studies on the relations among the basic mechanical properties of fly-ash concrete with machine-made sand (MSFAC). However, these relations such as the compressive strength, the tensile strength and the elastic modulus with the cubic compressive strength (i.e. strength grade) are the basis of design for concrete structures. This paper summarizes the test data from the published references, and discusses the relations among these properties by statistical analyses compared with those of ordinary concrete. The results show that only the tensile strength of MSFAC can be safely forecasted by the same formula of ordinary concrete specified in current Chinese design code. When the strength grade is higher than C45, the axial compressive strength of MSFAC is largely forecasted by the formula of ordinary concrete. The elastic modulus of MSFAC is larger than that of ordinary concrete, which should be prospect by the formula in this paper. This work gives out some cautions for the proper use of the MSFAC in concrete structures.


2014 ◽  
Vol 548-549 ◽  
pp. 1663-1666
Author(s):  
Fu Xing Wang ◽  
Guo Zhong Li ◽  
Juan Chen

The effect of admixtures on the mechanical properties of recycled fine aggregate cement mortar was studied. The result indicated that compared with blank samples the 28d flexural strength, the compressive strength and osmotic pressure of cement mortar were increased by 15.6%, 35.5%, 41.1% respectively when adding silicone waterproofing agent 0.2wt%, naphdalin series water reducer 1.0wt%, polycarboxylate superplasticizer 0.8wt%. The micro-morphology and hydration products of mortar specimens was observed by SEM, XRD respectively.


Materials ◽  
2021 ◽  
Vol 14 (19) ◽  
pp. 5581
Author(s):  
Xuhang Zang ◽  
Pinghua Zhu ◽  
Chunhong Chen ◽  
Xiancui Yan ◽  
Xinjie Wang

In this study, the shrinkage performance of recycled aggregate thermal insulation concrete (RATIC) with added glazed hollow beads (GHB) was investigated and a time-dependent shrinkage model was proposed. Two types of recycled fine aggregate (RFA) were used to replace natural fine aggregate in RATIC: RFA from waste concrete (RFA1) and waste clay brick (RFA2). Besides, the mechanical properties and thermal insulation performance of RATIC were also studied. Results showed that the pozzolanic reaction caused by RFA2 effectively improved the mechanical properties of RATIC; 75% was the optimal replacement ratio of RATIC prepared by RFA2. Added RFA decreased the thermal conductivity of thermal insulation concrete (TIC). The total shrinkage strain of RATIC increased with the increase of the replacement ratio of RFA. The 150d total shrinkage of RATIC prepared by RFA1 was 1.46 times that of TIC and the 150d total shrinkage of RATIC prepared by RFA2 was 1.23 times. The addition of GHBs led to the increase of early total shrinkage strain of concrete. Under the combined action of the higher elastic modulus of RFA2 and the pozzolanic components contained in RFA2, the total shrinkage strain of RATIC prepared by RFA2 with the same replacement ratio was smaller than that of RATIC prepared by RFA1. For example, the final total shrinkage strain of RATIC prepared by RFA2 at 100% replacement ratio was about 18.6% less than that of RATIC prepared by RFA1. A time-dependent shrinkage model considering the influence of the elastic modulus of RFA and the addition of GHB on the total shrinkage of RATIC was proposed and validated by the experimental results.


2013 ◽  
Vol 357-360 ◽  
pp. 1102-1105 ◽  
Author(s):  
Shun Bo Zhao ◽  
Qi Guo ◽  
Guang Xin Li ◽  
Yan Feng Su

Experimental study was carried out on the concrete mixed with machine-made sand and recycled coarse aggregate (MSRAC), three strength grades of concrete were designed by changing the water to cement ratio as 0.36, 0.45 and 0.55, while the sand ratio varied in a range of 32%~38%, 32%~42% and 38%~44% successively. The workability and the mechanical properties such as compressive and splitting tensile strengths and elastic modulus of MSRAC were tested. The results show that although the mechanical properties of MSRAC were influenced by sand ratio, they were still controlled by the water to cement ratio. The ratio of axial compressive strength to cubic compressive strength and the elastic modulus of MSRAC basically satisfy the specifications of the current design code for concrete structures. It should be noticed that the tensile strength of MSRAC is lower than current specification, and tends to reduce with the increase of water to cement ratio.


2019 ◽  
Vol 11 (2) ◽  
pp. 216-238
Author(s):  
Faezeh Nejati ◽  
S.A. Edalatpanah

Purpose The purpose of this paper is to investigate the effect of steel and carbon fibers on the mechanical properties of light concrete in terms of tension strength, compressive strength and elastic modulus under completely dry and wet conditions. Design/methodology/approach In this study, the lightweight concrete made of Light Expanded Clay Aggregate (LECA) as coarse aggregate and sand as fine aggregate was used. To achieve a compressive strength of at least 20 MPa, microsilica was used 10 percent by weight of cement. In order to compensate for the reduction of tension strength of concrete, steel and carbon fibers were used with three volume ratio of 0.5, 1 and 1.5 percent in concrete. The results of concrete specimens were studied at the age of 7, 28, 42 and 90 days under controlled dry and wet conditions. Findings The results showed that the addition of steel and carbon fibers to the concrete mixture would reduce the drop in slump. Also, the use of steel and carbon fibers plays a significant role in increasing the tension strength of the specimens. Furthermore, the highest increase in tension strength of steel and carbon fiber samples was 83.3 and 50 percent, respectively, than the non-fibrous specimen when evaluated at 90 days of age. Moreover, the steel and carbon fiber increased the water absorption of the samples. Adding steel and carbon fibers to a lightweight concretes mixture containing LECA aggregates plays a significant role in increasing the modulus of elasticity of the samples. The highest increase in the elastic modulus of steel and carbon fibers was 18.9 and 35.4 percent, respectively, than the non-fibrous specimen at 28 days of age. Originality/value In this paper, the authors investigated the mechanical properties of steel fiber and carbon reinforced concrete. Also, according to the conditions of storage of samples and the age of concrete (day), the experiments were carried out on samples.


Sign in / Sign up

Export Citation Format

Share Document