AEM of reaction-bonded SiC

Author(s):  
K Das Chowdhury ◽  
R. W. Carpenter ◽  
W. Braue

Research on reaction-bonded SiC (RBSiC) is aimed at developing a reliable structural ceramic with improved mechanical properties. The starting materials for RBSiC were Si,C and α-SiC powder. The formation of the complex microstructure of RBSiC involves (i) solution of carbon in liquid silicon, (ii) nucleation and epitaxial growth of secondary β-SiC on the original α-SiC grains followed by (iii) β>α-SiC phase transformation of newly formed SiC. Due to their coherent nature, epitaxial SiC/SiC interfaces are considered to be segregation-free and “strong” with respect to their effect on the mechanical properties of RBSiC. But the “weak” Si/SiC interface limits its use in high temperature situations. However, few data exist on the structure and chemistry of these interfaces. Microanalytical results obtained by parallel EELS and HREM imaging are reported here.

2010 ◽  
Vol 13 (1) ◽  
pp. 32-38
Author(s):  
Thong Duy Nguyen ◽  
Du Vinh Nguyen

This paper presents the effect of Cadium in Aluminium alloys on mechanical property and phase transformation in the alloys. The Aluminium 4,8Cu 0,6Mn 0,2Ti alloys that contain between 0,150 and 0,288 Cadmium not only enhanced strength but also stabilized physical-mechanical properties. These characteristics are particularly shown on high temperature conditions. Although Cadmium does not participate in the resistance phases of the alloys, it still can maintain and dispose the vacancies in Al-Cu-Mn alloys after tempering. That's reason why Cadmium can control the precipitation of the resistance phase - CuAl2- in the tempering process.


2019 ◽  
Vol 9 (23) ◽  
pp. 5094
Author(s):  
Dayu Chen ◽  
Heng Cui ◽  
Rudong Wang

The high-temperature mechanical properties of a 4.5% Al-containing δ-transformation-induced plasticity (TRIP) steel were studied by using the Gleeble 3500 thermomechanical simulator. The zero ductility temperature (ZDT) and the zero strength temperature (ZST) were measured, and the brittle zones were divided. The phase transformation zone was determined by differential scanning calorimetry (DSC). The temperature of the phase transformation and the proportion of the phase were calculated by the Thermo-Calc software. The ZDT and the ZST of the 4.5% Al-containing δ-TRIP steel are 1355 and 1405 °C, respectively. The first brittle zone and the third brittle zone of the steel are 1300–1350 °C and 800–975 °C, respectively. The reason for the embrittlement of the third brittle zone of the 4.5% Al-containing δ-TRIP steel is that the α-ferrite formed at the austenite grain boundary causes the sample to crack along the grain boundary under stress. The ductility of the 4.5% Al-containing δ-TRIP steel decreases first and then increases with the increase of the α-ferrite. When the proportion of the α-ferrite reaches 37%, the reduction of area (RA) of the 4.5% Al-containing δ-TRIP steel is reduced to 44%. The 4.5% Al-containing δ-TRIP steel has good resistance to the high-temperature cracking.


2004 ◽  
Vol 120 ◽  
pp. 161-168
Author(s):  
Y. Vincent ◽  
J.-M. Bergheau ◽  
J.-B. Leblond ◽  
J.-F.Jullien

In most numerical simulations of welding, due to the very short times involved, viscoplastic effects are neglected. However an experimental mock-up developed at INSA has evidenced the possible importance of such effects, which must therefore be incorporated in a more refined description of the material behaviour. This paper presents such a description; an extension of Leblond’s model for transformation plasticity, accounting for the dependence of mechanical properties upon strain rate, is proposed. Finite element analyses using elastic-plastic or elastic-viscoplastic constitutive laws are compared with experiments, and it is found that incorporation of viscoplastic effects significantly improves the quality of the agreement between numerical and experimental results.


Author(s):  
D. R. Clarke ◽  
G. Thomas

Grain boundaries have long held a special significance to ceramicists. In part, this has been because it has been impossible until now to actually observe the boundaries themselves. Just as important, however, is the fact that the grain boundaries and their environs have a determing influence on both the mechanisms by which powder compaction occurs during fabrication, and on the overall mechanical properties of the material. One area where the grain boundary plays a particularly important role is in the high temperature strength of hot-pressed ceramics. This is a subject of current interest as extensive efforts are being made to develop ceramics, such as silicon nitride alloys, for high temperature structural applications. In this presentation we describe how the techniques of lattice fringe imaging have made it possible to study the grain boundaries in a number of refractory ceramics, and illustrate some of the findings.


Author(s):  
H.-J. Kleebe ◽  
J.S. Vetrano ◽  
J. Bruley ◽  
M. Rühle

It is expected that silicon nitride based ceramics will be used as high-temperature structural components. Though much progress has been made in both processing techniques and microstructural control, the mechanical properties required have not yet been achieved. It is thought that the high-temperature mechanical properties of Si3N4 are limited largely by the secondary glassy phases present at triple points. These are due to various oxide additives used to promote liquid-phase sintering. Therefore, many attempts have been performed to crystallize these second phase glassy pockets in order to improve high temperature properties. In addition to the glassy or crystallized second phases at triple points a thin amorphous film exists at two-grain junctions. This thin film is found even in silicon nitride formed by hot isostatic pressing (HIPing) without additives. It has been proposed by Clarke that an amorphous film can exist at two-grain junctions with an equilibrium thickness.


Author(s):  
H. Kung ◽  
T. R. Jervis ◽  
J.-P. Hirvonen ◽  
M. Nastasi ◽  
T. E. Mitchell ◽  
...  

MoSi2 is a potential matrix material for high temperature structural composites due to its high melting temperature and good oxidation resistance at elevated temperatures. The two major drawbacksfor structural applications are inadequate high temperature strength and poor low temperature ductility. The search for appropriate composite additions has been the focus of extensive investigations in recent years. The addition of SiC in a nanolayered configuration was shown to exhibit superior oxidation resistance and significant hardness increase through annealing at 500°C. One potential application of MoSi2- SiC multilayers is for high temperature coatings, where structural stability ofthe layering is of major concern. In this study, we have systematically investigated both the evolution of phases and the stability of layers by varying the heat treating conditions.Alternating layers of MoSi2 and SiC were synthesized by DC-magnetron and rf-diode sputtering respectively. Cross-sectional transmission electron microscopy (XTEM) was used to examine three distinct reactions in the specimens when exposed to different annealing conditions: crystallization and phase transformation of MoSi2, crystallization of SiC, and spheroidization of the layer structures.