Mechanical behaviour in shear and compression of polyurethane foam at elevated temperature

2021 ◽  
pp. 109963622110509
Author(s):  
Pietro Mazzuca ◽  
João P Firmo ◽  
João R Correia ◽  
Mário Garrido

This paper presents an experimental investigation about the effect of elevated temperature on the mechanical properties of two polyurethane (PUR) foams, with densities of 40 kg/m3 and 93 kg/m3. The experimental campaign included shear and compressive tests over a temperature range of 20°C–200°C, performed to assess the degradation of the mechanical properties of the PUR foams with temperature. To validate the diagonal tension shear test method adopted in this investigation, a numerical study was also performed, namely to assess the (shear) stress state developed within the foam. The results obtained validated the adopted test procedures, showing that the compressive and shear responses are strongly affected by elevated temperature, due to the softening of the polymeric material when it undergoes the glass transition process. For the temperature range considered in this study, both strength and modulus in shear and compression present an approximately linear reduction with temperature.

2006 ◽  
Vol 15-17 ◽  
pp. 240-245 ◽  
Author(s):  
Hua Min Kou ◽  
Yu Bai Pan ◽  
Jing Kun Guo

Al/Al2O3 cermet composites were fabricated by hot-pressing at the temperature range of 1350~1450oC from commercial γ - Al2O3 reinforced by Al/Al2O3 core-shell particles, which were synthesized via calcining the Al/AlOOH·nH2O core-shell particles prepared by wet-chemical based method. This newly designed aluminum coated with alumina composite structure can not only reduce or resist the oxidization of Al at elevated temperature but also make it possible to control inter-particle and particle-matrix interactions, and this predesigned structure is expected to improve the following sintering ability and therefore the properties of final products.


Polymers ◽  
2021 ◽  
Vol 13 (13) ◽  
pp. 2038
Author(s):  
Maria Pia Falaschetti ◽  
Matteo Scafé ◽  
Nicola Zavatta ◽  
Enrico Troiani

Composite materials usage in several industrial fields is now widespread, and this leads to the necessity of overcoming issues that are still currently open. In the aeronautic industry, this is especially true for Barely Visible Impact Damage (BVID) and humidity uptake issues. BVID is the most insidious kind of impact damage, being rather common and not easily detectable. These, along with the ageing that a composite structure could face during its operative life, could be a cause of fatal failures. In this paper, the influence of water absorption on impacted specimens compressive residual strength was studied. Specimens were impacted using a modified Charpy pendulum. Two different locations were chosen for comparison: Near-Edge (NE) and Central (CI). Accelerated hygrothermal ageing was conducted on impacted and reference nonimpacted coupons, placing them in a water-filled jar at 70 °C. Compressive tests were performed in accordance with the Combined Loading Compression (CLC) test method. A Dynamic Mechanical Analysis (DMA) was performed as well. The results showed the influence of hygrothermal ageing, as expected. Nevertheless, the influence of impact location on compressive residual strength is not clearly noticeable in aged specimens, leading to the conclusion that hygrothermal ageing may have a greater effect on composite compressive strength than the analysed BVI damage.


Polymers ◽  
2021 ◽  
Vol 13 (9) ◽  
pp. 1473
Author(s):  
Jun Zhao ◽  
Kang Wang ◽  
Shuaibin Wang ◽  
Zike Wang ◽  
Zhaohui Yang ◽  
...  

This paper presents results from experimental work on mechanical properties of geopolymer concrete, mortar and paste prepared using fly ash and blended slag. Compressive strength, splitting tensile strength and flexural strength tests were conducted on large sets of geopolymer and ordinary concrete, mortar and paste after exposure to elevated temperatures. From Thermogravimetric analyzer (TGA), X-ray diffraction (XRD), Scanning electron microscope (SEM) test results, the geopolymer exhibits excellent resistance to elevated temperature. Compressive strengths of C30, C40 and C50 geopolymer concrete, mortar and paste show incremental improvement then followed by a gradual reduction, and finally reach a relatively consistent value with an increase in exposure temperature. The higher slag content in the geopolymer reduces residual strength and the lower exposure temperature corresponding to peak residual strength. Resistance to elevated temperature of C40 geopolymer concrete, mortar and paste is better than that of ordinary concrete, mortar and paste at the same grade. XRD, TGA and SEM analysis suggests that the heat resistance of C–S–H produced using slag is lower than that of sulphoaluminate gel (quartz and mullite, etc.) produced using fly ash. This facilitates degradation of C30, C40 and C50 geopolymer after exposure to elevated temperatures.


2021 ◽  
Vol 8 (5) ◽  
pp. 70
Author(s):  
Marco Ferroni ◽  
Beatrice Belgio ◽  
Giuseppe M. Peretti ◽  
Alessia Di Giancamillo ◽  
Federica Boschetti

The menisci of the knee are complex fibro-cartilaginous tissues that play important roles in load bearing, shock absorption, joint lubrication, and stabilization. The objective of this study was to evaluate the interaction between the different meniscal tissue components (i.e., the solid matrix constituents and the fluid phase) and the mechanical response according to the developmental stage of the tissue. Menisci derived from partially and fully developed pigs were analyzed. We carried out biochemical analyses to quantify glycosaminoglycan (GAG) and DNA content according to the developmental stage. These values were related to tissue mechanical properties that were measured in vitro by performing compression and tension tests on meniscal specimens. Both compression and tension protocols consisted of multi-ramp stress–relaxation tests comprised of increasing strains followed by stress–relaxation to equilibrium. To better understand the mechanical response to different directions of mechanical stimulus and to relate it to the tissue structural composition and development, we performed numerical simulations that implemented different constitutive models (poro-elasticity, viscoelasticity, transversal isotropy, or combinations of the above) using the commercial software COMSOL Multiphysics. The numerical models also allowed us to determine several mechanical parameters that cannot be directly measured by experimental tests. The results of our investigation showed that the meniscus is a non-linear, anisotropic, non-homogeneous material: mechanical parameters increase with strain, depend on the direction of load, and vary among regions (anterior, central, and posterior). Preliminary numerical results showed the predominant role of the different tissue components depending on the mechanical stimulus. The outcomes of biochemical analyses related to mechanical properties confirmed the findings of the numerical models, suggesting a specific response of meniscal cells to the regional mechanical stimuli in the knee joint. During maturation, the increase in compressive moduli could be explained by cell differentiation from fibroblasts to metabolically active chondrocytes, as indicated by the found increase in GAG/DNA ratio. The changes of tensile mechanical response during development could be related to collagen II accumulation during growth. This study provides new information on the changes of tissue structural components during maturation and the relationship between tissue composition and mechanical response.