Effect of composition and grain size on electrical discharge machining of BN–TiB2 composites

1991 ◽  
Vol 6 (11) ◽  
pp. 2457-2462 ◽  
Author(s):  
A.M. Gadalla ◽  
H.S. Bedi

TiB2 conducts the current and forms a liquid phase at the interface with BN. Neighboring crystals of BN and some TiB2 spall due to thermal shock. During pause periods parts of the liquid and fragments are flushed out by the dielectric. Composites rich in TiB2 or with fine TiB2 grains gave high material removal rates. Increasing the amount of the conducting phase by 10% is as effective as decreasing the grain size from 11 to 7 μm. Coarse TiB2 could withstand high pulse durations before wire breaks. Material removal rate increases with pulse duration, frequency, and current. For the same composition and grain size, increasing the pulse duration or current increased the crater depth (the roughness) up to a certain value, beyond which increasing these parameters yielded a smoother surface. The conductivity of the dielectric was effective only for compositions rich in TiB2 content. In such cases, higher water conductivity lowered the energy required for material removal.

Author(s):  
Qingyu Liu ◽  
Qinhe Zhang ◽  
Min Zhang ◽  
Jianhua Zhang

The material removal process of micro electrical discharge machining is based on the instantaneous ultra-high temperature generated by a series of repetitive discharge pulses. Due to the size effects, the polycrystal cannot be considered as continuous and homogeneous material when machining is in micron scale, and the effects of material microstructure should not be neglected. In this article, the thermoelectric characteristics of grain and grain boundary are discussed, and the influence of grain size on the machining performances in micro electrical discharge machining is researched. Two kinds of austenitic stainless steels (AISI 304) which are different in grain size are chosen as the workpieces in experiments. It is verified by both theory models and experimental results that the smaller the grain size, the higher the material removal rate, under the same discharge conditions. Both thermal conductivity and melting point of the grain boundary are lower than those of the grain because of the grain boundary segregation. The effective thermal conductivity and local effective melting point of polycrystalline materials vary with their grain sizes since the grain boundary volume fractions change. As a consequence, the material removal rate of micro electrical discharge machining has direct relationship with grain size of the workpiece.


2012 ◽  
Vol 500 ◽  
pp. 259-265 ◽  
Author(s):  
Faizul Ezmat Abdul Hamid ◽  
Mohd Amri Lajis

In this paper an attempt has been made to investigate the performance of an electrode made through powder metallurgy (PM) of copper tungsten during electrical discharge machining (EDM). Experimental results are presented on electrical discharge machining of AISI D2 hardened steel in kerosene with a copper tungsten (Cu35% - W65%) tool electrode made through PM method with a constant duty factor of 80%. In term of high performance EDM process, higher peak current (>20A) and pulse duration (>400µs) with a high machining efficiency were used. Experimental results have shown that machining at a peak current of 40A and pulse duration of 400µs yields the highest material removal rate (MRR) whereas machining at a peak current of 20A and pulse duration of 400µs yields the lowest tool wear rate (TWR). The lowest surface roughness appears at the lowest material removal rate which is at a peak current of 20A and pulse duration of 600µs. The optimum machining performance can be performed by the combination of pulse duration and peak current at 600µs and 40A respectively.


Author(s):  
Gurpreet Singh ◽  
DR Prajapati ◽  
PS Satsangi

The micro-electrical discharge machining process is hindered by low material removal rate and low surface quality, which bound its capability. The assistance of ultrasonic vibration and magnetic pulling force in micro-electrical discharge machining helps to overcome this limitation and increase the stability of the machining process. In the present research, an attempt has been made on Taguchi based GRA optimization for µEDM assisted with ultrasonic vibration and magnetic pulling force while µEDM of SKD-5 die steel with the tubular copper electrode. The process parameters such as ultrasonic vibration, magnetic pulling force, tool rotation, energy and feed rate have been chosen as process variables. Material removal rate and taper of the feature have been selected as response measures. From the experimental study, it has been found that response output measures have been significantly improved by 18% as compared to non assisted µEDM. The best optimal combination of input parameters for improved performance measures were recorded as machining with ultrasonic vibration (U1), 0.25 kgf of magnetic pulling force (M1), 600 rpm of tool rotation (R2), 3.38 mJ of energy (E3) and 1.5 mm/min of Tool feed rate (F3). The confirmation trail was also carried out for the validation of the results attained by Grey Relational Analysis and confirmed that there is a substantial improvement with both assistance applied simultaneously.


Manufacturing ◽  
2003 ◽  
Author(s):  
Scott F. Miller ◽  
Albert J. Shih

The development of new, advanced engineering materials and the needs for precise and flexible prototype and low-volume production have made wire electrical discharge machining (EDM) an important manufacturing process to meet such demand. This research investigates the effect of spark on-time duration and spark on-time ratio, two important EDM process parameters, on the material removal rate (MRR) and surface integrity of four types of advanced material: porous metal foams, metal bond diamond grinding wheels, sintered Nd-Fe-B magnets, and carbon-carbon bipolar plates. An experimental procedure was developed. During the wire EDM, five types of constraints on the MRR due to short circuit, wire breakage, machine slide speed limit, and spark on-time upper and lower limits have been identified. An envelope of feasible EDM process parameters is created and compared across different work-materials. Applications of such process envelope to select process parameters for maximum MRR and for machining of micro features are presented.


2020 ◽  
Vol 10 (1) ◽  
pp. 401-407
Author(s):  
Yanuar Rohmat Aji Pradana ◽  
Aldi Ferara ◽  
Aminnudin Aminnudin ◽  
Wahono Wahono ◽  
Jason Shian-Ching Jang

AbstractThe machinability information of Zr-based bulk metallic glasses (BMGs) are recently limited but essential to provide technological recommendation for the fabrication of the medical devices due to the material’s metastable nature. This study aims to investigate the material removal rate (MRR) and surface roughness under different current and pulse-on time of newly developed Ni- and Cu-free Zr-based BMG using sinking-electrical discharge machining (EDM). By using weightloss calculation, surface roughness test and scanning electron microscopy (SEM) observation on the workpiece after machining, both MRR and surface roughness were obtained to be increased up to 0.594 mm3/min and 5.50 μm, respectively, when the higher current was applied. On the other hand, the longer pulse-on time shifted the Ra into the higher value but lower the MRR value to only 0.183 mm3/min at 150 μs. Contrary, the surface hardness value was enhanced by both higher current and pulse-on time applied during machining indicating different level of structural change after high-temperature spark exposure on the BMG surface. These phenomena are strongly related to the surface evaporation which characterize the formation of crater and recast layer in various thicknesses and morphologies as well as the crystallization under the different discharge energy and exposure time.


Author(s):  
Sagil James ◽  
Sharadkumar Kakadiya

Shape Memory Alloys are smart materials that tend to remember and return to its original shape when subjected to deformation. These materials find numerous applications in robotics, automotive and biomedical industries. Micromachining of SMAs is often a considerable challenge using conventional machining processes. Micro-Electrical Discharge Machining is a combination of thermal and electrical processes, which can machine any electrically conductive material at micron scale independent of its hardness. It employs dielectric medium such as hydrocarbon oils, deionized water, and kerosene. Using liquid dielectrics has adverse effects on the machined surface causing cracking, white layer deposition, and irregular surface finish. These limitations can be minimized by using a dry dielectric medium such as air or nitrogen gas. This research involves the experimental study of micromachining of Shape Memory Alloys using dry Micro-Electrical Discharge Machining process. The study considers the effect of critical process parameters including discharge voltage and discharge current on the material removal rate and the tool wear rate. A comparison study is performed between the Micro-Electrical Discharge Machining process with using the liquid as well as air as the dielectric medium. In this study, microcavities are successfully machined on shape memory alloys using dry Micro-Electrical Discharge Machining process. The study found that the dry Micro-Electrical Discharge Machining produces a comparatively better surface finish, has lower tool wear and lesser material removal rate compared to the process using the liquid as the dielectric medium. The results of this research could extend the industrial applications of Micro Electrical Discharge Machining processes.


2015 ◽  
Vol 656-657 ◽  
pp. 335-340 ◽  
Author(s):  
Fang Pin Chuang ◽  
Yan Cherng Lin ◽  
Hsin Min Lee ◽  
Han Ming Chow ◽  
A. Cheng Wang

The environment issue and green machining technique have been induced intensive attention in recent years. It is urgently need to develop a new kind dielectric to meet the requirements for industrial applications. The aim of this study is to develop a novel dielectric using gas media immersed in deionized water for electrical discharge machining (EDM). The developed machining medium for EDM can fulfill the environmentally friendly issue and satisfy the demand of high machining performance. The experiments were conducted by this developed medium to investigate the effects of machining parameters on machining characteristics in terms of material removal rate (MRR) and surface roughness. The developed EDM medium revealed the potential to obtain a stabilizing progress with excellent machining performance and environmentally friendly feature.


2016 ◽  
Vol 40 (3) ◽  
pp. 331-349 ◽  
Author(s):  
S. Sivasankar ◽  
R. Jeyapaul

This research work concentrates on Electrical Discharge Machining (EDM) performance evaluation of ZrB2- SiC ceramic matrix composites with different tool materials at various machining parameters. Monolithic ZrB2 possesses lower relative density (98.72%) than composites. ZrB2 with 20 Vol.% of SiC possesses 99.74% of the relative density with improved hardness values. Bend strength and Young’s modulus increase with SiC addition until it reaches 20 Vol% and then decreasing. EDM performance on tool materials of tungsten, niobium, tantalum, graphite and titanium at various levels of pulse on time and pulse off time are analyzed. Graphite produces the best Material removal rate (MRR) for all the workpieces. Tool wear rate decreases with melting point and thermal conductivity of the tool material.


2021 ◽  
Author(s):  
Dragan Rodic ◽  
Marin Gostimirovic ◽  
Milenko Sekulic ◽  
Borislav Savkovic ◽  
Branko Strbac

Abstract It is well known that electrical discharge machining can be used in the processing of nonconductive materials. In order to improve the efficiency of machining modern engineering materials, existing electrical discharge machines are constantly being researched and improved or developed. The current machining of non-conductive materials is limited due to the relatively low material removal rate and high surface roughness. A possible technological improvement of electrical discharge machining can be achieved by innovations of existing processes. In this paper, a new approach for machining zirconium oxide is presented. It combines electrical discharge machining with assisting electrode and powder-mixed dielectric. The assisting electrode is used to enable electrical discharge machining of nonconductive material, while the powder-mixed dielectric is used to increase the material removal rate, reduce surface roughness, and decrease relative tool wear. The response surface method was used to generate classical mathematical models, analyzing the output performances of surface roughness, material removal rate and relative tool wear. Verification of the obtained models was performed based on a set of new experimental data. By combining these latest techniques, positive effects on machining performances are obtained. It was found that the surface roughness was reduced by 18%, the metal removal rate was increased by about 12% and the relative tool wear was reduced by up to 6% compared to electrical discharge machining with supported electrode without powder.