scholarly journals Effects of Monomer Composition of Urethane Methacrylate Based Resins on the C=C Degree of Conversion, Residual Monomer Content and Mechanical Properties

Polymers ◽  
2021 ◽  
Vol 13 (24) ◽  
pp. 4415
Author(s):  
Codruta Sarosi ◽  
Marioara Moldovan ◽  
Andrada Soanca ◽  
Alexandra Roman ◽  
Timea Gherman ◽  
...  

(1) Background: This study investigated the influence of Bis-GMA, TEGDMA, UDMA, and two different polyethylene glycol (PEG)-containing, UDMO-based co-monomers on the Young’s modulus and flexural strength, degree of methacrylate C=C double bond conversion and residual monomer elution of experimental dental resins. (2) Methods: Urethane methacrylate-based monomer was synthesised via a radical chain growth polymerization mechanism using PEG in order to improve the mechanical properties. Dental resins were formulated using Bis-GMA, UDMA, or UDMO as base monomers combined with TEGDMA as a dilution monomer and DMAEM + CQ as the photo-initiator system. Degree of conversion (DC), mechanical properties, and residual monomer content of light-activated methacrylate resin formulations were evaluated and statistically analysed by ANOVA and a Tukey’s test. (3) Results: PEG-containing UDMO resins had lower Young’s modulus and elastic strength than UDMA-derived resin for all irradiation times. The highest DC (67,418%) was observed for the PEG-containing UDMO-based resin formulation when light cured for 40 s. For all samples, DC increased with the photo-polymerization time. The amount of residual monomer decreased after increasing the light-curing period from 20 to 40 s, resin with UDMO content 0.01 mol of PEG having the smallest amount of free eluted monomer. (4) Conclusions: A strong structure–property relationship exists in photo-cured dimethacrylate-based dental resins. The time and quantity of the photochemical initiation system can influence the physical–mechanical properties of the resins but also the monomers in their composition.

2017 ◽  
Vol 752 ◽  
pp. 3-10
Author(s):  
Timea Gherman ◽  
Marioara Moldovan ◽  
Miuţa Filip ◽  
Trifoi Ancuța ◽  
Maria Râpă ◽  
...  

In this study urethane dimethacrylate (UDMA) based dental resin materials were synthesized. Urethane methacrylate oligomers (UDMO) were synthesized via a radical chain growth polymerization mechanism using polyethylene glycol (PEG) in order to improve the mechanical properties, without adding a solvent in the reaction medium. The structure of the new monomer and oligomer were confirmed by FT-IR and 1H-NMR spectra. The results of FT-IR analysis indicated that the addition of PEG as plasticizer in the urethane methacrylate dental material in the adequate molar ratio (isophorone diisocyanate : HEM (2-hydroxyethyl methacrylate) : PEG = 2:2:1) improve the isocyanate double bond consumption. The Elastic strength (MPa) and Young’s Modulus of bending (MPa) were measured using a three-point bending set up. Urethane dimethacrylate monomer without PEG was used as control group. The results showed that PEG containing UDMO resins had lower Young’s Modulus: 2984 MPa and 2537 MPa (for 40s irradiation time) and Elastic strenght: 77 MPa and 51 MPa than UDMA derived resin: 3270 MPa respectively 90 MPa for all irradiation times (20 and 40 seconds).


2009 ◽  
Vol 3 (1) ◽  
pp. 202-207 ◽  
Author(s):  
N Emami ◽  
KJ Söderholm

Objectives: To evaluate Young's modulus and degree of conversion of several combinations of bisGMA, UEDMA, TEGDMA light-cure dental resin. Methods: Young's modulus and DC% were studied for 21 different resin combinations of bisGMA, TEGDMA and UEDMA. Small universal testing machine and photo-calorimetry were used for the tests. The results were evaluated using ANOVA and Duncan's multiple range tests and regular t-test. Results: Young's modulus varied between 2.37±0.2 GPa (100% TEGDMA) and 4.15±0.2 GPa (100% bisGMA). By adding TEGDMA to bisGMA or UEDMA, the Young's modulus decreased significantly (p<0.05). Degree of conversion was significantly (p<0.05) higher when the wt% of TEGDMA was high in the mixtures than for highly concentrated bis-GMA (resin mixtures with TEGDMA in comparison to mixture with bisGMA had higher degree of conversion). DC% was significantly higher (p<0.05) for binary mixtures of UEDMA and TEGDMA, and significantly lower for 100 wt% bis-GMA (p<0.05). The DC% values were between 53.1%±0.9% (100% bisGMA) and 85.6%±1% (80% UEDMA-20% TEGDMA). The concentration of bisGMA, in the monomer mixture, affected DC% and Young's modulus oppositely. Conclusions: The differences in the values for DC% were mostly justified by the differences in the molecular structures of the different monomers. It was also revealed that higher DC% does not always result in a higher Young's modulus, because molecular and network structural parameters play major roles in the final physical properties of the mixtures.


2019 ◽  
Vol 107 (2) ◽  
pp. 207 ◽  
Author(s):  
Jaroslav Čech ◽  
Petr Haušild ◽  
Miroslav Karlík ◽  
Veronika Kadlecová ◽  
Jiří Čapek ◽  
...  

FeAl20Si20 (wt.%) powders prepared by mechanical alloying from different initial feedstock materials (Fe, Al, Si, FeAl27) were investigated in this study. Scanning electron microscopy, X-ray diffraction and nanoindentation techniques were used to analyze microstructure, phase composition and mechanical properties (hardness and Young’s modulus). Finite element model was developed to account for the decrease in measured values of mechanical properties of powder particles with increasing penetration depth caused by surrounding soft resin used for embedding powder particles. Progressive homogenization of the powders’ microstructure and an increase of hardness and Young’s modulus with milling time were observed and the time for complete homogenization was estimated.


Polymers ◽  
2021 ◽  
Vol 13 (11) ◽  
pp. 1872
Author(s):  
James Anthony Dicks ◽  
Chris Woolard

The environmental issues of petroleum-derived polymeric foams have necessitated seeking renewable alternatives. This work aims to prepare renewable free-radically polymerized polymeric foams with the ability to biodegrade. Furthermore, this work attempted to incorporate a bio-based reactive diluent, which has not been reported in the literature. The synthesis of maleated castor oil glycerides was performed with products analyzed by Fourier transform infrared spectrometry using attenuated total reflection (ATR-FTIR) and 1H nuclear magnetic resonance (1H NMR) spectroscopy. Polymeric foams were prepared using maleated castor oil glycerides via free radical copolymerization with styrene and isobornyl methacrylate as reactive diluents. Scanning electron microscopy (SEM) was used to determine anisotropic macrocellular morphology, with log-normal cell diameter distributions. The compressive mechanical and energy absorption properties were investigated; the polymeric foams displayed Young’s modulus up to 26.85 ± 1.07 MPa and strength up to 1.11 ± 0.021 MPa using styrene as the reactive diluent, and Young’s modulus up to 1.38 ± 0.055 MPa and strength up to 0.088 MPa when incorporating isobornyl methacrylate. Furthermore, a thorough analysis of the cellular structure–property relationships was performed, indicating relationships to cell diameter, cell wall thickness and apparent density. The polymeric foams displayed rapid mass loss in an aerobic soil environment with multiple erosion sites revealed by SEM. In conclusion, renewable polymeric foams with excellent compressive properties were achieved using styrene as reactive diluent, but the incorporation of isobornyl methacrylate decreased strength-related properties.


2021 ◽  
Vol 11 (1) ◽  
Author(s):  
R. Salloom ◽  
S. A. Mantri ◽  
R. Banerjee ◽  
S. G. Srinivasan

AbstractFor decades the poor mechanical properties of Ti alloys were attributed to the intrinsic brittleness of the hexagonal ω-phase that has fewer than 5-independent slip systems. We contradict this conventional wisdom by coupling first-principles and cluster expansion calculations with experiments. We show that the elastic properties of the ω-phase can be systematically varied as a function of its composition to enhance both the ductility and strength of the Ti-alloy. Studies with five prototypical β-stabilizer solutes (Nb, Ta, V, Mo, and W) show that increasing β-stabilizer concentration destabilizes the ω-phase, in agreement with experiments. The Young’s modulus of ω-phase also decreased at larger concentration of β-stabilizers. Within the region of ω-phase stability, addition of Nb, Ta, and V (Group-V elements) decreased Young’s modulus more steeply compared to Mo and W (Group-VI elements) additions. The higher values of Young’s modulus of Ti–W and Ti–Mo binaries is related to the stronger stabilization of ω-phase due to the higher number of valence electrons. Density of states (DOS) calculations also revealed a stronger covalent bonding in the ω-phase compared to a metallic bonding in β-phase, and indicate that alloying is a promising route to enhance the ω-phase’s ductility. Overall, the mechanical properties of ω-phase predicted by our calculations agree well with the available experiments. Importantly, our study reveals that ω precipitates are not intrinsically embrittling and detrimental, and that we can create Ti-alloys with both good ductility and strength by tailoring ω precipitates' composition instead of completely eliminating them.


Materials ◽  
2021 ◽  
Vol 14 (13) ◽  
pp. 3467
Author(s):  
Anna Nocivin ◽  
Doina Raducanu ◽  
Bogdan Vasile ◽  
Corneliu Trisca-Rusu ◽  
Elisabeta Mirela Cojocaru ◽  
...  

The present paper analyzed the microstructural characteristics and the mechanical properties of a Ti–Nb–Zr–Fe–O alloy of β-Ti type obtained by combining severe plastic deformation (SPD), for which the total reduction was of etot = 90%, with two variants of super-transus solution treatment (ST). The objective was to obtain a low Young’s modulus with sufficient high strength in purpose to use the alloy as a biomaterial for orthopedic implants. The microstructure analysis was conducted through X-ray diffraction (XRD), scanning electron microscopy (SEM), and high-resolution transmission electron microscopy (HRTEM) investigations. The analyzed mechanical properties reveal promising values for yield strength (YS) and ultimate tensile strength (UTS) of about 770 and 1100 MPa, respectively, with a low value of Young’s modulus of about 48–49 GPa. The conclusion is that satisfactory mechanical properties for this type of alloy can be obtained if considering a proper combination of SPD + ST parameters and a suitable content of β-stabilizing alloying elements, especially the Zr/Nb ratio.


Metals ◽  
2021 ◽  
Vol 11 (3) ◽  
pp. 461
Author(s):  
Konrad Kosiba ◽  
Konda Gokuldoss Prashanth ◽  
Sergio Scudino

The phase and microstructure formation as well as mechanical properties of the rapidly solidified Mg67Ag33 (at. %) alloy were investigated. Owing to kinetic constraints effective during rapid cooling, the formation of equilibrium phases is suppressed. Instead, the microstructure is mainly composed of oversaturated hexagonal closest packed Mg-based dendrites surrounded by a mixture of phases, as probed by X-ray diffraction, electron microscopy and energy dispersive X-ray spectroscopy. A possible non-equilibrium phase diagram is suggested. Mainly because of the fine-grained dendritic and interdendritic microstructure, the material shows appreciable mechanical properties, such as a compressive yield strength and Young’s modulus of 245 ± 5 MPa and 63 ± 2 GPa, respectively. Due to this low Young’s modulus, the Mg67Ag33 alloy has potential for usage as biomaterial and challenges ahead, such as biomechanical compatibility, biodegradability and antibacterial properties are outlined.


Micromachines ◽  
2021 ◽  
Vol 12 (5) ◽  
pp. 529
Author(s):  
Chunzhi Du ◽  
Zhifan Li ◽  
Bingfei Liu

Nanoporous Shape Memory Alloys (SMA) are widely used in aerospace, military industry, medical and health and other fields. More and more attention has been paid to its mechanical properties. In particular, when the size of the pores is reduced to the nanometer level, the effect of the surface effect of the nanoporous material on the mechanical properties of the SMA will increase sharply, and the residual strain of the SMA material will change with the nanoporosity. In this work, the expression of Young’s modulus of nanopore SMA considering surface effects is first derived, which is a function of nanoporosity and nanopore size. Based on the obtained Young’s modulus, a constitutive model of nanoporous SMA considering residual strain is established. Then, the stress–strain curve of dense SMA based on the new constitutive model is drawn by numerical method. The results are in good agreement with the simulation results in the published literature. Finally, the stress-strain curves of SMA with different nanoporosities are drawn, and it is concluded that the Young’s modulus and strength limit decrease with the increase of nanoporosity.


2012 ◽  
Vol 3 (1) ◽  
pp. 13-26
Author(s):  
Myrtha Karina ◽  
Lucia Indrarti ◽  
Rike Yudianti ◽  
Indriyati

The effect of castor oil on the physical and mechanical properties of bacterial cellulose is described. Bacterial cellulose (BC) was impregnated with 0.5–2% (w/v) castor oil (CO) in acetone–water, providing BCCO films. Scanning electron micrographs revealed that the castor oil penetrated the pores of the bacterial cellulose, resulting in a smoother morphology and enhanced hydrophilicity. Castor oil caused a slight change in crystallinity indices and resulted in reduced tensile strength and Young's modulus but increased elongation at break. A significant reduction in tensile strength and Young's modulus was achieved in BCCO films with 2% castor oil, and there was an improvement in elongation at break and hydrophilicity. Impregnation with castor oil, a biodegradable and safe plasticiser, resulted in less rigid and more ductile composites.


1993 ◽  
Vol 308 ◽  
Author(s):  
Sandrine Bec ◽  
André Tonck ◽  
Jean-Luc Loubet

ABSTRACTPyrolysis of polymer precursors (polysilazane) is a technologically and economically interesting way to produce thin ceramic coatings. However, many cracks appear and decohesion occurs during pyrolysis when the ceramic coatings (SiOCN) are thicker than 0.5 micrometers. In order to understand these cracking phenomena, the coatings are mechanically characterized by nanoindentation at different stages of the pyrolysis heat treatment.During pyrolysis, the cracking temperature is detected by in-situ optical observation. The thickness of the coatings varies during pyrolysis from 3 micrometers at the polymeric state to 1 micrometer at the ceramic state. The coatings' properties, hardness and Young's modulus are evaluated after heat treatment, taking into account the substrate's influence. A large variation of these properties occurs at the cracking temperature. Both the hardness and the Young's modulus are multiplied by a factor of 10. By analysing these results, we show that cracking is correlated with the evolution of the coatings' mechanical properties during the transformation.