scholarly journals Effect of Silica Fume and Synthetic Fibre towards the Compressive Strength of Modified Crumb Rubber Cement Mortar

2021 ◽  
Vol 411 ◽  
pp. 135-142
Author(s):  
Mohamad Raduan Bin Kabit ◽  
Syed Syabil Rahmat Syed Sarkawi ◽  
MD Abdul Mannan ◽  
Johnson Olufemi Adebayo

Cracking is very common problem in cement mortar. Many past research has explored the prospect of using crumb rubber (CR) to overcome this issue. Different sizes of CR have been tested to measure its effect on the pore structure and mechanical strengths of cement mortar. Hence, this study has further modified the crumb rubber mortar mix by adding silica fume and synthetic fiber to improve its mechanical properties. The experimental results suggested that the optimum silica fume replacement of cement content was 5%. Hence, for the subsequent experiment with a fixed 5%silica fume replacement, the highest compressive strength of 26 MPa was achieved with 5% crumb rubber replacement. Finally, additional 0.1% of synthetic fiber added the modified crumb rubber mix to reduce the mix brittleness has produced a desirable compressive strength close to the control specimen which was significantly higher than the minimum threshold required by the standard. However, the water content ratio for the modified mortar mix should be further investigated as the present modified crumb rubber mix has lower workability. It is envisaged that the modified crumb rubber mortar mix has a sound potential to mitigate shrinkage cracking in cement mortar.

2017 ◽  
Vol 2017 ◽  
pp. 1-6 ◽  
Author(s):  
Gang Xue ◽  
Mei-ling Cao

The crumb rubber cement mortar is prepared by the crumb rubber aggregates in 60 mesh which are modified by 1% polyvinyl alcohol (PVA) solution. Some mechanical properties of cement mortar with different crumb rubber aggregate amounts are researched including compressive strength, flexural strength, the ratio of compressive strength to flexural strength, impact resistance, and dry contraction percentage. In our tests, we consider six kinds of the rubber contents, 0%, 7.5%, 15%, 19%, 22.5%, and 30%, respectively. The optimal mixing amount of crumb rubber is determined by measuring three indices, the ratio of compressive strength to flexural strength, impact resistance, and dry contraction percentage. It is shown by test that the ratio of compressive strength to flexural strength is the smallest when the mixing amount of rubber is 19%; meanwhile high impact resistance and rational drying shrinkage are observed. The optimal mixing amount of the rubber particles is 19% determined by this test.


Materials ◽  
2020 ◽  
Vol 13 (8) ◽  
pp. 1821 ◽  
Author(s):  
Robert Bušić ◽  
Mirta Benšić ◽  
Ivana Miličević ◽  
Kristina Strukar

The paper aims to investigate the influence of waste tire rubber and silica fume on the fresh and hardened properties of self-compacting concrete (SCC) and to design multivariate regression models for the prediction of the mechanical properties of self-compacting rubberized concrete (SCRC). For this purpose, 21 concrete mixtures were designed. Crumb rubber derived from end-of-life tires (grain size 0.5–3.5 mm) was replaced fine aggregate by 0%, 5%, 10%, 15%, 20%, 25%, and 30% of total aggregate volume. Silica fume was replaced cement by 0%, 5%, and 10% of the total cement mass. The optimal replacement level of both materials was investigated in relation to the values of the fresh properties and mechanical properties of self-compacting concrete. Tests on fresh and hardened self-compacting concrete were performed according to the relevant European standards. Furthermore, models for predicting the values of the compressive strength, modulus of elasticity, and flexural strength of SCRC were designed and verified with the experimental results of 12 other studies. According to the obtained results, mixtures with up to 15% of recycled rubber and 5% of silica fume, with 28 days compressive strength above 30 MPa, were found to be optimal mixtures for the potential future investigation of reinforced self-compacting rubberized concrete structural elements.


2019 ◽  
Vol 9 (9) ◽  
pp. 1049-1054
Author(s):  
Yunxia Lun ◽  
Fangfang Zheng

This study is aimed at exploring the effect of steel slag powder (SSP), fly ash (FA), and silica fume (SF) on the mechanical properties and durability of cement mortar. SSP, SF, and FA were used as partial replacement of the Ordinary Portland cement (OPC). It was showed that the compressive and bending strength of steel slag powder were slightly lower than that of OPC. An increase in the SSP content caused a decrease in strength. However, the growth rate of compressive strength of SSP2 (20% replacement by the weight of OPC) at the curing ages of 90 days was about 8% higher than that of OPC, and the durability of SSP2 was better than that of OPC. The combination of mineral admixtures improved the later strength, water impermeability, and sulfate resistance compared with OPC and SSP2. The compressive strength of SSPFA (SSP and SF) at 90 days reached 70.3 MPa. The results of X-ray diffraction patterns and scanning electron microscopy indicated that SSP played a synergistic role with FA or SF to improve the performance of cement mortar.


Materials ◽  
2021 ◽  
Vol 14 (21) ◽  
pp. 6654
Author(s):  
Jakub Popławski ◽  
Małgorzata Lelusz

Biomass combustion is a significant new source of green energy in the European Union. The adequate utilization of byproducts created during that process is a growing challenge for the energy industry. Biomass fly ash could be used in cement composite production after appropriate activation of that material. This study had been conducted to assess the usefulness of mechanical and physical activation methods (grinding and sieving), as well as activation through the addition of active silica in the form of silica fume, as potential methods with which to activate biomass fly ash. Setting time, compressive strength, water absorption and bulk density tests were performed on fresh and hardened mortar. While all activation methods influenced the compressive strength development of cement mortar with fly ash, sieving of the biomass fly ash enhanced the early compressive strength of cement mortar. The use of active silica in the form of silica fume ensured higher compressive strength results than those of control specimens throughout the entire measurement period.


2011 ◽  
Vol 284-286 ◽  
pp. 310-313
Author(s):  
Zhi Gang Liu ◽  
Li Rong Yang ◽  
Jun Cong Wei ◽  
Bao Hui Zhao ◽  
Xiao Xin Feng

The compressive strength and piezoresistive property of cement mortar with low adding level of multi-walled carbon nanotubes (MWCNTs) were investigated. Experimental results showed that the compressive strength of the MWCNTs/cement mortars increased with the adding amount of MWCNTs content for all the curing ages. Silica fume promoted the compressive strength development by well bonding with MWCNTs and filling effect. The electrical resistance changed synchronously with the compressive strength and the amount of the changes varied with the stress and MWCNTs addition levels. Higher MWCNTs doping level improved the piezoresistive sensitivity of the mortar. The mortar with silica fume (5-10% by weight of cement) exhibited better piezoresistive response than that without silica fume at the same MWCNTs doping levels.


2012 ◽  
Vol 253-255 ◽  
pp. 482-488
Author(s):  
Hai Bo Zhang ◽  
Xue Mao Guan ◽  
Hai Tao Shang

This paper examined the mechanical property of rubber mortars with different amount of rubber granules addition and the influence of fly ash, slag and silica fume. The increase of rubber granules results in the decrease in compressive and flexural strength of rubber mortar, but increases the ratio of flexural to compressive strength. The fly ash, slag and silica fume are useful for improving the mechanical property of mortar. The examined contact angle of water against rubber is 99.5°, which suggests the rubber surface is hydrophobic, and the hydrophobic surface interprets the weak interface between rubber and cement matrix.


2020 ◽  
Vol 870 ◽  
pp. 3-9
Author(s):  
Nahla N. Hilal ◽  
Mohammed T. Nawar ◽  
Abdulkader I. Al-Hadithi

In the present work, the properties of Polyethylene Waste cement mortar containing Polyethylene Waste treated by a reactive material are tested and compared with normal Polyethylene Waste and normal cement mortar. The Polyethylene, which is cured by a different reactive material such as: (cement, a fly ash and silica fume) is used as fine as aggregate a volumetric fractional replacing of the sand in a cement mortar. The percent of replacement was 10% by volume, density, compressive strength, modulus of rupture, and absorption are tested for all mixes at variable ages. The current results display that the cure of Polyethylene by cement were significantly improves the characteristics of Polyethylene cement mortar. Moreover, the results show that all treatment improved properties of cement mortar as a compared with Polyethylene without treatment.


2014 ◽  
Vol 875-877 ◽  
pp. 383-387 ◽  
Author(s):  
Teuku Ferdiansyah ◽  
Hashim Abdul Razak

The purpose of this paper is to discuss the influence of mineral additives i.e. metakaolin, silica fume, rice ash and fly ash incorporating with nanocarbontubes mortar composites. The effects on compressive strength at 28 days were also discussed and presented. Cement content of 500 kg/m3, water/cement ratio of 0.6 and aggregate/cement ratio of 2.75 were adopted for the mix propotion. 1%, 3% and 5% of nanocarbontubes in mortar were combined with 15% of mineral additives. The results show that mixtures of nanocarbontubes with 15% of metakaolin produce better strength compared to normal mortar. Meanwhile with addition of fly ash and rice husk ash the strength were decreased. The electrical resistance for all mixes at 28 days were also discussed and presented. The higher percentages of nanocarbon with addition of all mineral additives resulted in lower electrical resistance properties