Photocatalytic degradation of methylene blue using undoped and Ag-doped TiO2 thin films deposited by a sol–gel process: Effect of the ageing time of the starting solution and the film thickness

2010 ◽  
Vol 174 (1-3) ◽  
pp. 84-87 ◽  
Author(s):  
A. Guillén-Santiago ◽  
S.A. Mayén ◽  
G. Torres-Delgado ◽  
R. Castanedo-Pérez ◽  
A. Maldonado ◽  
...  
2013 ◽  
Vol 581 ◽  
pp. 318-323 ◽  
Author(s):  
Jianjun Tian ◽  
Huiping Gao ◽  
Hongmei Deng ◽  
Lin Sun ◽  
Hui Kong ◽  
...  

2005 ◽  
Vol 486-487 ◽  
pp. 65-68 ◽  
Author(s):  
Sang Wook Lee ◽  
Hyun Suk Jung ◽  
Dong Wook Kim ◽  
Kug Sun Hong

5, 10, and 30 nm thickness of transparent TiO2 thin films were fabricated using sol-gel process, and the influence of film thickness on the photocatalytic property was investigated. The increase in film thickness was found to enhance the photocatalytic property of the films. Photocatalytic properties of each film were estimated by decomposition of stearic acid. The amount of decomposed stearic acid increased with film thickness (5 - 30 nm). For the case of 30 nm thickness film, the stearic acid was decomposed perfectly in twelve minutes. UV-vis spectra and photocurrents of each film clearly showed that the photoactivities of TiO2 films were related to the amount of absorbed UV light and band gap shift.


2019 ◽  
Vol 6 (10) ◽  
pp. 106435 ◽  
Author(s):  
Muhammad Kamran Tariq ◽  
Adeel Riaz ◽  
Ramsha Khan ◽  
Ahsan Wajid ◽  
Hamza-ul Haq ◽  
...  

2007 ◽  
Vol 280-283 ◽  
pp. 805-808
Author(s):  
Feng Zhou ◽  
Kai Ming Liang ◽  
Hua Shao ◽  
An Min Hu

LiNO3-doped TiO2 thin films on glass-ceramics were prepared by sol-gel dip coating. The influence of LiNO3 addition on the phase transformation temperature was studied. The transformation temperatures of non-crystalline to anatase and anatase to rutile are originally 520°C and 880°C without the addition of LiNO3. By adding 5%LiNO3 the two transformation temperatures decrease to 440°C and 580°C, respectively. The average size of the particles was found to be around 40nm for the LiNO3- doped TiO2 film annealed at 600°C.


2018 ◽  
Vol 18 (3) ◽  
pp. 81-91 ◽  
Author(s):  
C. Lalhriatpuia

Nanopillars-TiO2 thin films was obtained on a borosilicate glass substrate with (S1) and without (S2) polyethylene glycol as template. The photocatalytic behaviour of S1 and S2 thin films was assessed inthe degradation of methylene blue (MB) dye from aqueous solution under batch reactor operations. The thin films were characterized by the SEM, XRD, FTIR and AFM analytical methods. BET specific surface area and pore sizes were also obtained. The XRD data confirmed that the TiO2 particles are in its anatase mineral phase. The SEM and AFM images indicated the catalyst is composed with nanosized pillars of TiO2, evenly distributed on the surface of the substrate. The BET specific surface area and pore sizes of S1 and S2 catalyst were found to be 5.217 and 1.420 m2/g and 7.77 and 4.16 nm respectively. The photocatalytic degradation of MB was well studied at wide range of physico-chemical parameters. The effect of solution pH (pH 4.0 to 10.0) and MB initial concentration (1.0 to 10.0 mg/L) was extensively studied and the effect of several interfering ions, i.e., cadmium nitrate, copper sulfate, zinc chloride, sodium chloride, sodium nitrate, sodium nitrite, glycine, oxalic acid and EDTA in the photocatalytic degradation of MB was demonstrated. The maximum percent removal of MB was observed at pH 8.0 beyond which it started decreasing and a low initial concentration of the pollutant highly favoured the photocatalytic degradation using thin films and the presence of several interfering ions diminished the photocatalytic activity of thin films to some extent. The overall photocatalytic activity was in the order: S2 > S1 > UV. The photocatalytic degradation of MB was followed the pseudo-first-order rate kinetics. The mineralization of MB was studied with total organic carbon measurement using the TOC (total organic carbon) analysis.


2001 ◽  
Vol 77 (1-2) ◽  
pp. 484-490 ◽  
Author(s):  
Serge Zhuiykov ◽  
Wojtek Wlodarski ◽  
Yongxiang Li

2010 ◽  
Vol 150-151 ◽  
pp. 112-117 ◽  
Author(s):  
Min Xian Shi ◽  
Wei Mao ◽  
Yan Qin ◽  
Zhi Xiong Huang ◽  
Dong Yun Guo

Pb(Zr0.53Ti0.47)O3 thin films with thickness of 120nm, 190nm, 310nm, 440nm and 630nm were deposited on Pt/Ti/SiO2/Si substrates by sol-gel process through repeating spining process 2 times, 4 times, 6 times, 8 times and 10 times respectively. The structures of PZT films were investigated by SEM and XRD analysis. The ferroelectric hysteresis loops were recorded by Radiant Precision Workstation and dielectric properties were measured using an Agilent HP4294A impedance analyzer. X-ray diffraction indicated that with the film thickness increasing, the diffraction intensity increased. The thickness of PZT film had great effect on ferroelectric and dielectric properties. Conclusively when the film thickness was about 310nm, the PZT thin films possessed better ferroelectric and dielectric properties.