Real-Time Investigations on the Formation of Cu(In,Ga)Se2 While Annealing Precursors Produced with a Combination of Sputtering and Thermal Evaporation

2007 ◽  
Vol 1012 ◽  
Author(s):  
Stefan Jost ◽  
Frank Hergert ◽  
Rainer Hock ◽  
Michael Purwins

AbstractWe have investigated the formation of Cu(In,Ga)Se2 thin films by real-time X-ray diffraction (XRD) experiments while annealing differently deposited and composed stacked elemental layer (SEL) precursors.The in-situ measurements during the selenization of bi-layered Cu/In precursors reveal, that the semiconductor formation process is similar for precursors with thermally evaporated or sputtered indium. In both cases, the formation of binary copper and indium selenides is observed at temperatures around the melting point of selenium. After subsequent selenium transfer reactions, the chalcopyrite CuInSe2 is formed from the educt phases Cu2-xSe and InSe.The addition of gallium leads to the formation of the intermetallic precursor phase Cu9Ga4, which reduces the overall amount of copper and gallium selenides at process temperatures above 500 K. This causes an ongoing selenization in the indium selenium subsystem, which results in the formation of CuInSe2 from the educt phases Cu2-xSe and the selenium richest indium selenide g-In2Se3.

2000 ◽  
Vol 15 (12) ◽  
pp. 2606-2611 ◽  
Author(s):  
Hsin-Yi Lee ◽  
K. S. Liang ◽  
Chih-Hao Lee ◽  
Tai-Bor Wu

Real-time x-ray reflectivity and diffraction measurements under in situ sputtering conditions were employed to study the growth behavior of LaNiO3 thin films on a Si substrate. Our results clearly show there is a transition layer of 60 Å, which grew in the first 6 min of deposition. The in situ x-ray-diffraction patterns indicated that this transition layer is amorphous. Subsequently, a polycrystalline overlayer grew as observed from the in situ x-ray reflectivity curves and diffraction patterns. Nucleation and growth took place on this transition layer with random orientation and then the polycrystalline columnar textures of (100) and (110) grew on the top of this random orientation layer. By comparing the integrated intensities of two Bragg peaks in the plane normal of x-ray diffraction, it was found that a crossover of the growth orientation from the ⟨110⟩ to the ⟨100ߩ direction occurred and the ability of (100) texturization enhanced with increasing film thickness beyond a certain critical value.


2016 ◽  
Vol 12 (3) ◽  
pp. 4394-4399
Author(s):  
Sura Ali Noaman ◽  
Rashid Owaid Kadhim ◽  
Saleem Azara Hussain

Tin Oxide and Indium doped Tin Oxide (SnO2:In) thin films were deposited on glass and Silicon  substrates  by  thermal evaporation technique.  X-ray diffraction pattern of  pure SnO2 and SnO2:In thin films annealed at 650oC and the results showed  that the structure have tetragonal phase with preferred orientation in (110) plane. AFM studies showed an inhibition of grain growth with increase in indium concentration. SEM studies of pure  SnO2 and  Indium doped tin oxide (SnO2:In) ) thin films showed that the films with regular distribution of particles and they have spherical shape.  Optical properties such as  Transmission , optical band-gap have been measured and calculated.


2019 ◽  
Vol 15 (34) ◽  
pp. 1-14
Author(s):  
Bushra A. Hasan

Lead selenide PbSe thin films of different thicknesses (300, 500, and 700 nm) were deposited under vacuum using thermal evaporation method on glass substrates. X-ray diffraction measurements showed that increasing of thickness lead to well crystallize the prepared samples, such that the crystallite size increases while the dislocation density decreases with thickness increasing. A.C conductivity, dielectric constants, and loss tangent are studied as function to thickness, frequency (10kHz-10MHz) and temperatures (293K-493K). The conductivity measurements confirm confirmed that hopping is the mechanism responsible for the conduction process. Increasing of thickness decreases the thermal activation energy estimated from Arhinus equation is found to decrease with thickness increasing. The increase of thickness lead to reduce the polarizability α while the increasing of temperature lead to increase α.


2017 ◽  
Vol 111 (8) ◽  
pp. 082907 ◽  
Author(s):  
Seiji Nakashima ◽  
Osami Sakata ◽  
Hiroshi Funakubo ◽  
Takao Shimizu ◽  
Daichi Ichinose ◽  
...  

2018 ◽  
Vol 9 (23) ◽  
pp. 6750-6754 ◽  
Author(s):  
Alessandro Greco ◽  
Alexander Hinderhofer ◽  
M. Ibrahim Dar ◽  
Neha Arora ◽  
Jan Hagenlocher ◽  
...  

2018 ◽  
Vol 6 (24) ◽  
pp. 11496-11506 ◽  
Author(s):  
Paul Pistor ◽  
Thomas Burwig ◽  
Carlo Brzuska ◽  
Björn Weber ◽  
Wolfgang Fränzel

We present the identification of crystalline phases by in situ X-ray diffraction during growth and monitor the phase evolution during subsequent thermal treatment of CH3NH3PbX3 (X = I, Br, Cl) perovskite thin films.


2015 ◽  
Vol 3 (43) ◽  
pp. 11357-11365 ◽  
Author(s):  
Geert Rampelberg ◽  
Bob De Schutter ◽  
Wouter Devulder ◽  
Koen Martens ◽  
Iuliana Radu ◽  
...  

VO2 and V2O3 thin films were prepared during in situ XRD investigation by oxidation and reduction of V and V2O5. Films show up to 5 orders of magnitude resistance switching.