scholarly journals Morphologies Tuning of Polypyrrole and Thermoelectric Properties of Polypyrrole Nanowire/Graphene Composites

Polymers ◽  
2018 ◽  
Vol 10 (10) ◽  
pp. 1143 ◽  
Author(s):  
Yong Du ◽  
Hao Niu ◽  
Jun Li ◽  
Yunchen Dou ◽  
Shirley Shen ◽  
...  

Polypyrrole (PPy) with different morphologies (e.g., particles, nanotubes, and nanowires) were successfully prepared by adding or without adding different kinds of surfactants through a chemical oxidative polymerization method, respectively. The results show that the morphologies of PPy can be effectively controlled and have a significantly effects on their thermoelectric properties. The PPy nanowires exhibit the highest electrical conductivity and Seebeck coefficient among the various PPy morphologies, such as particles, nanotubes, and nanowires, so PPy nanowires were chosen to prepare PPy nanowire/graphene thermoelectric composites via a soft template polymerization method using cetyltrimethyl ammonium bromide as the template. Both electrical conductivity and Seebeck coefficient of the PPy nanowire/graphene composites increased as the content of graphene increases from 0 to 20 wt %, and as the measured temperature increases from 300 K to 380 K, which leds to the same trend for the power factor. A highest power factor of 1.01 μWm−1K−2 at ~380 K was obtained for the PPy nanowire/graphene composites with 20 wt % PPy nanowire, which is about 3.3 times higher than that of the pure PPy nanowire.

Energies ◽  
2018 ◽  
Vol 11 (10) ◽  
pp. 2849 ◽  
Author(s):  
Yong Du ◽  
Haixia Li ◽  
Xuechen Jia ◽  
Yunchen Dou ◽  
Jiayue Xu ◽  
...  

Graphite/poly(3,4-ethyenedioxythiophene) (PEDOT) nanocomposites were prepared by an in-situ oxidative polymerization process. The electrical conductivity and Seebeck coefficient of the graphite/PEDOT nanocomposites with different content of graphite were measured in the temperature range from 300 K to 380 K. The results show that as the content of graphite increased from 0 to 37.2 wt %, the electrical conductivity of the nanocomposites increased sharply from 3.6 S/cm to 80.1 S/cm, while the Seebeck coefficient kept almost the same value (in the range between 12.0 μV/K to 15.1 μV/K) at 300 K, which lead to an increased power factor. The Seebeck coefficient of the nanocomposites increased from 300 K to 380 K, while the electrical conductivity did not substantially depend on the measurement temperature. As a result, a power factor of 3.2 μWm−1 K−2 at 380 K was obtained for the nanocomposites with 37.2 wt % graphite.


2007 ◽  
Vol 539-543 ◽  
pp. 2329-2332 ◽  
Author(s):  
Yoshikazu Shinohara ◽  
Yoshio Imai ◽  
Yukihiro Isoda ◽  
Kentaro Hiraishi ◽  
Hachiro Nakanishi

Typical conductive polymers of poly(3-alkylthiophenes) were synthesized by oxidative polymerization. Polythiophene with no side chain was also electrolyticaly polymerized. Alkyl side chains were CnH2n+1 with n=4, 6, 8, 12. The regioregularity with the HT linkage was larger than 99% based on NMR analysis. We have evaluated the effect of side chain size on the thermoelectric properties of Seebeck coefficient and electrical conductivity. The results were as follows: 1) Seebeck coefficient decreased with an increasing electrical conductivity. 2) High Seebeck coefficient >1mV/K was observed at low electrical conductivity <10-2S/cm. 3) Small side chains, especially no side chain caused higher thermoelectric properties of polythiophene series.


2008 ◽  
Vol 368-372 ◽  
pp. 559-561 ◽  
Author(s):  
Hao Ming Hu ◽  
Yuan Deng ◽  
Jian Li ◽  
Guang Sheng Wang

The precursor of (Ca1-x-yKxBiy)3Co4O9 was synthesized by sol-gel method using nitrate salts as raw materials and citrate acid as agent. The final product was obtained after the precursor was calcined at 800°C for 4 h. The polycrystalline bulk samples were fabricated by a conventional sintering process at 900°C for 12 h. XRD and SEM were used to characterize the microstructures and the composition of the samples. The transport properties of the samples at room temperature were determined by measuring electrical conductivity and Seebeck coefficient. The Bi and K-doped samples show an excellent transport properties even at room temperature. The value of power factor of (Ca0.90K0.075Bi0.025)3Co4O9 reaches 1.42×10-4Wm-1K-2 at 293K, close to the performance of pure Ca3Co4O9 at 1000K.


2020 ◽  
Vol 1 (9) ◽  
pp. 3233-3242
Author(s):  
Temesgen Atnafu Yemata ◽  
Yun Zheng ◽  
Aung Ko Ko Kyaw ◽  
Xizu Wang ◽  
Jing Song ◽  
...  

Binary post-treatment of thermoelectric PEDOT:PSS films with nitric acid and imidazolium-based ionic liquids significantly improves the electrical conductivity and Seebeck coefficient, leading to a power factor of 152 μW m−1 K−2.


2006 ◽  
Vol 510-511 ◽  
pp. 1086-1089 ◽  
Author(s):  
Wang Kee Min ◽  
Chang Ho Lee ◽  
Yong Ho Park ◽  
Ik Min Park

We investigated the effects of Fe3O4 (0~0.1 wt.%) on the thermoelectric properties of Bi1Sb4Te7.5 alloy prepared by mechanical alloying process. The Seebeck coefficient increased with Fe3O4 content, but the power factor decreased with Fe3O4 content because of the decreased electrical conductivity. The thermal conductivity decreased with Fe3O4. The carrier concentration measured by the Hall effect measurement decreased with Fe3O4. The thermal conductivity of 0.1 wt.% Fe3O4 alloy was 0.814 W/Km, 20%lower than that of Fe3O4 free alloy. As a result, the small addition of Fe3O4 improved the Z value owing to the decreased thermal conductivity by adding Fe3O4. The Z value of 0.01 wt.% Bi1Sb4Te7.5 alloy was 3.1×10-3 /K, the highest value among the prepared alloys.


2005 ◽  
Vol 492-493 ◽  
pp. 141-144 ◽  
Author(s):  
Yoshikazu Shinohara ◽  
K. Ohara ◽  
Hachiro Nakanishi ◽  
Yoshio Imai ◽  
Yukihiro Isoda

Typical conductive polymers of poly(3-alkylthiophenes) were synthesized by oxidative polymerization. Alkyl side chains were CnH2n+1 with n=4, 6, 8, 12. The regioregularity with the HT linkage was larger than 99% based on NMR analysis. Completely regioregular head-to-tail (HT) poly(3-alkylthiophenes) were obtained. We have evaluated the effect of side chain size on the thermoelectric properties of Seebeck coefficient and electrical conductivity. The results were as follows: 1) Seebeck coefficient decreased with an increasing electrical conductivity. 2) High Seebeck coefficient >1mV/K was observed at low electrical conductivity <10-2S/cm. 3) The small side chain caused the higher electrical conductivity in the range of electrical conductivity <10- 1S/cm.


Polymers ◽  
2020 ◽  
Vol 12 (3) ◽  
pp. 559
Author(s):  
Jonathan Atoyo ◽  
Matthew R. Burton ◽  
James McGettrick ◽  
Matthew J. Carnie

A two-step approach of improving the thermoelectric properties of Poly(3,4-ethylenedioxythiophene)poly(4-styrenesulfonate) (PEDOT:PSS) via the addition of the ionic liquid, 1-Ethyl-3-methylimidazolium bis(trifluoromethylsulfonyl)imide (EMIM:TFSI) and subsequent reduction with NaBH4 is presented. The addition of 2.5 v/v% of EMIM:TFSI to PEDOT:PSS increases the electrical conductivity from 3 S·cm−1 to 1439 S·cm−1 at 40 °C. An additional post treatment using the reducing agent, NaBH4, increases the Seebeck coefficient of the film from 11 µV·K−1 to 30 µV·K−1 at 40 °C. The combined treatment gives an overall improvement in power factor increase from 0.04 µW·m−1·K−2 to 33 µW·m−1·K−2 below 140 °C. Raman and XPS measurements show that the increase in PEDOT:PSS conductivity is due to PSS separation from PEDOT and a conformational change of the PEDOT chains from the benzoid to quinoid molecular orientation. The improved Seebeck coefficient is due to a reduction of charge carriers which is evidenced from the UV–VIS depicting the emergence of polarons.


2012 ◽  
Vol 465 ◽  
pp. 292-295 ◽  
Author(s):  
Wei Wei Sun ◽  
Wen Hao Fan ◽  
Shao Ping Chen ◽  
Yi Yun Li ◽  
Qing Sen Meng

Abstract. Ca3CO4O9/x wt.%SiO2 composites were prepared by using field-activated pressure-assisted synthesis(FAPAS) process. The effects of nano-SiO2 addition on the microstructure and thermoelectric properties of the Ca3CO4O9 were investigated. With an increasing of the of SiO2 content, the size of Ca3Co4O9 particles decreased. The Seebeck coefficient decreased after the doping of nano-SiO2. The electrical conductivity firstly increased and then decreased with increasing amount of nano-SiO2 and the highest value belong to the Ca3CO4O9/0.5 wt.% SiO2 - sample. With the highest electric conductivity and slightly decreased Seebeck coefficient, the Ca3CO4O9/0.5 wt.%SiO2-sample achieved the highest power factor of 0.349 mw/mk2 at 800 °C, which is 8% higher than the value of pure Ca3CO4O9 reported in the literature.


2021 ◽  
pp. 2150290
Author(s):  
Nasir Shehzad ◽  
Lixin Zhang ◽  
Shahzad Saeed ◽  
Anwar Ali

Using first-principles calculations, we studied the electronic, structural and thermoelectric properties of two-dimensional (2D) MXenes [Formula: see text] ([Formula: see text] = Ti, Zr and Hf, [Formula: see text], 2 and 3). The calculations are carried out within the generalized gradient approximation (GGA). We have calculated the Boltzmann transport equation for finding the thermoelectric properties such as power factor, Seebeck coefficient and electrical conductivity. For [Formula: see text], these materials behave as semiconductors having an indirect bandgap nature. In contrast, for [Formula: see text] these materials show metallic behavior. Out of these MXenes, we found that Ti2CO2 has a high Seebeck coefficient value, whereas the electrical conductivity of Ti4C3O2 is exceptionally high. While among all these compounds, Ti2CO2 and Hf4C3O2 have a high power factor in the 300–1200-K temperature range.


2020 ◽  
Vol 23 (4) ◽  
pp. 788-794
Author(s):  
Dai Cao Truong ◽  
Anh Tuan Thanh Pham ◽  
Oanh Kieu Truong Le ◽  
Dung Van Hoang ◽  
Truong Huu Nguyen ◽  
...  

Introduction: Zinc oxide (ZnO) is well-known as a promising thermoelectric material owing to its safety, inexpensiveness, and thermal stability. This research provides an overview of thermoelectric potentials, including structure, electrical conductivity, Seebeck coefficient, and power factor of pure ZnO semiconductor synthesized in bulk and thin-film forms. Methods: The ZnO bulk was synthesized by solid-state reaction at high temperature, while the thin film was prepared by d.c. magnetron sputtering technique. The temperature-dependent thermoelectric properties of all the samples were measured by the Seebeck LSR-3 system. The crystallographic and surface morphological information of the samples were obtained by using X-ray diffraction (XRD) and field-emission scanning electron microscopy (FESEM), respectively. Results: The XRD results confirm that both the bulk and thin-film have polycrystalline structure and characteristics of hexagonal-wurtzite ZnO. Through the FESEM observation, the bulk is well densified under high-temperature condition, while the thin-film achieve good orientation and close-packed grains. At 573 K, the obtained thermoelectric properties (electrical conductivity, Seebeck coefficient, and power factor) are respectively 352.4 S/cm, -89.5 µV/K and 282.5 µW/mK2 for the ZnO bulk; and 289 S/cm, -113.8 µV/K and 374.3 µW/mK2 for the ZnO film. Conclusion: The comparative study shows the good thermoelectric potential of ZnO material in both forms of bulk and thin film. Among them, the thin film has better results, especially in the Seebeck coefficient and power factor than one.