A New Challenge of Polymer Thermoelectric Materials as Ecomaterials

2007 ◽  
Vol 539-543 ◽  
pp. 2329-2332 ◽  
Author(s):  
Yoshikazu Shinohara ◽  
Yoshio Imai ◽  
Yukihiro Isoda ◽  
Kentaro Hiraishi ◽  
Hachiro Nakanishi

Typical conductive polymers of poly(3-alkylthiophenes) were synthesized by oxidative polymerization. Polythiophene with no side chain was also electrolyticaly polymerized. Alkyl side chains were CnH2n+1 with n=4, 6, 8, 12. The regioregularity with the HT linkage was larger than 99% based on NMR analysis. We have evaluated the effect of side chain size on the thermoelectric properties of Seebeck coefficient and electrical conductivity. The results were as follows: 1) Seebeck coefficient decreased with an increasing electrical conductivity. 2) High Seebeck coefficient >1mV/K was observed at low electrical conductivity <10-2S/cm. 3) Small side chains, especially no side chain caused higher thermoelectric properties of polythiophene series.

2005 ◽  
Vol 492-493 ◽  
pp. 141-144 ◽  
Author(s):  
Yoshikazu Shinohara ◽  
K. Ohara ◽  
Hachiro Nakanishi ◽  
Yoshio Imai ◽  
Yukihiro Isoda

Typical conductive polymers of poly(3-alkylthiophenes) were synthesized by oxidative polymerization. Alkyl side chains were CnH2n+1 with n=4, 6, 8, 12. The regioregularity with the HT linkage was larger than 99% based on NMR analysis. Completely regioregular head-to-tail (HT) poly(3-alkylthiophenes) were obtained. We have evaluated the effect of side chain size on the thermoelectric properties of Seebeck coefficient and electrical conductivity. The results were as follows: 1) Seebeck coefficient decreased with an increasing electrical conductivity. 2) High Seebeck coefficient >1mV/K was observed at low electrical conductivity <10-2S/cm. 3) The small side chain caused the higher electrical conductivity in the range of electrical conductivity <10- 1S/cm.


Energies ◽  
2018 ◽  
Vol 11 (10) ◽  
pp. 2849 ◽  
Author(s):  
Yong Du ◽  
Haixia Li ◽  
Xuechen Jia ◽  
Yunchen Dou ◽  
Jiayue Xu ◽  
...  

Graphite/poly(3,4-ethyenedioxythiophene) (PEDOT) nanocomposites were prepared by an in-situ oxidative polymerization process. The electrical conductivity and Seebeck coefficient of the graphite/PEDOT nanocomposites with different content of graphite were measured in the temperature range from 300 K to 380 K. The results show that as the content of graphite increased from 0 to 37.2 wt %, the electrical conductivity of the nanocomposites increased sharply from 3.6 S/cm to 80.1 S/cm, while the Seebeck coefficient kept almost the same value (in the range between 12.0 μV/K to 15.1 μV/K) at 300 K, which lead to an increased power factor. The Seebeck coefficient of the nanocomposites increased from 300 K to 380 K, while the electrical conductivity did not substantially depend on the measurement temperature. As a result, a power factor of 3.2 μWm−1 K−2 at 380 K was obtained for the nanocomposites with 37.2 wt % graphite.


Polymers ◽  
2018 ◽  
Vol 10 (10) ◽  
pp. 1143 ◽  
Author(s):  
Yong Du ◽  
Hao Niu ◽  
Jun Li ◽  
Yunchen Dou ◽  
Shirley Shen ◽  
...  

Polypyrrole (PPy) with different morphologies (e.g., particles, nanotubes, and nanowires) were successfully prepared by adding or without adding different kinds of surfactants through a chemical oxidative polymerization method, respectively. The results show that the morphologies of PPy can be effectively controlled and have a significantly effects on their thermoelectric properties. The PPy nanowires exhibit the highest electrical conductivity and Seebeck coefficient among the various PPy morphologies, such as particles, nanotubes, and nanowires, so PPy nanowires were chosen to prepare PPy nanowire/graphene thermoelectric composites via a soft template polymerization method using cetyltrimethyl ammonium bromide as the template. Both electrical conductivity and Seebeck coefficient of the PPy nanowire/graphene composites increased as the content of graphene increases from 0 to 20 wt %, and as the measured temperature increases from 300 K to 380 K, which leds to the same trend for the power factor. A highest power factor of 1.01 μWm−1K−2 at ~380 K was obtained for the PPy nanowire/graphene composites with 20 wt % PPy nanowire, which is about 3.3 times higher than that of the pure PPy nanowire.


2021 ◽  
pp. 2150290
Author(s):  
Nasir Shehzad ◽  
Lixin Zhang ◽  
Shahzad Saeed ◽  
Anwar Ali

Using first-principles calculations, we studied the electronic, structural and thermoelectric properties of two-dimensional (2D) MXenes [Formula: see text] ([Formula: see text] = Ti, Zr and Hf, [Formula: see text], 2 and 3). The calculations are carried out within the generalized gradient approximation (GGA). We have calculated the Boltzmann transport equation for finding the thermoelectric properties such as power factor, Seebeck coefficient and electrical conductivity. For [Formula: see text], these materials behave as semiconductors having an indirect bandgap nature. In contrast, for [Formula: see text] these materials show metallic behavior. Out of these MXenes, we found that Ti2CO2 has a high Seebeck coefficient value, whereas the electrical conductivity of Ti4C3O2 is exceptionally high. While among all these compounds, Ti2CO2 and Hf4C3O2 have a high power factor in the 300–1200-K temperature range.


2021 ◽  
Vol 7 (8) ◽  
pp. 110
Author(s):  
Songjie Yang ◽  
Matteo Zecchini ◽  
Andrew Brooks ◽  
Sara Krivickas ◽  
Desiree Dalligos ◽  
...  

The syntheses of new BEDT-TTF derivatives are described. These comprise BEDT-TTF with one ethynyl group (HC≡C-), with two (n-heptyl) or four (n-butyl) alkyl side chains, with two trans acetal (-CH(OMe)2) groups, with two trans aminomethyl (-CH2NH2) groups, and with an iminodiacetate (-CH2N(CH2CO2−)2 side chain. Three transition metal salts have been prepared from the latter donor, and their magnetic properties are reported. Three tris-donor systems are reported bearing three BEDT-TTF derivatives with ester links to a core derived from benzene-1,3,5-tricarboxylic acid. The stereochemistry and molecular structure of the donors are discussed. X-ray crystal structures of two BEDT-TTF donors are reported: one with two CH(OMe)2 groups and with one a -CH2N(CH2CO2Me)2 side chain.


1998 ◽  
Vol 545 ◽  
Author(s):  
Ke-Feng Cai ◽  
Ce-Wen Nan ◽  
Xin-Min Min

AbstractB4C ceramics doped with various content of Si (0 to 2.03 at%) are prepared via hot pressing. The composition and microstructure of the ceramics are characterized by means of XRD and EPMA. Their electrical conductivity and Seebeck coefficient of the samples are measured from room temperature up to 1500K. The electrical conductivity increases with temperature, and more rapidly after 1300K; the Seebeck coefficient of the ceramics also increases with temperature and rises to a value of about 320μVK−1. The value of the figure of merit of Si-doped B4C rises to about 4 × 10−4K−1 at 1500K.


2021 ◽  
Vol 317 ◽  
pp. 28-34
Author(s):  
Joon Hoong Lim

Thermoelectric materials has made a great potential in sustainable energy industries, which enable the energy conversion from heat to electricity. The band structure and thermoelectric properties of Ni(x)Zn(1-x)Fe2O4 have been investigated. The bulk pellets were prepared from analytical grade ZnO, NiO and Fe2O3 powder using solid-state method. It was possible to obtain high thermoelectric properties of Ni(x)Zn(1-x)Fe2O4 by controlling the ratios of dopants and the sintering temperature. XRD analysis showed that the fabricated samples have a single phase formation of cubic spinel structure. The thermoelectric properties of Ni(x)Zn(1-x)Fe2O4 pellets improved with increasing Ni. The electrical conductivity of Ni(x)Zn(1-x)Fe2O4 pellets decreased with increasing Ni content. The electrical conductivity of Ni(x)Zn(1-x)Fe2O4 (x = 0.0) is (0.515 x10-3 Scm-1). The band structure shows that ZnxCu1-xFe2O4 is an indirect band gap material with the valence band maximum (VBM) at M and conduction band minimum (CBM) at A. The band gap of Ni(x)Zn(1-x)Fe2O4 increased with increasing Ni content. The increasing band gap correlated with the lower electrical conductivity. The thermal conductivity of Ni(x)Zn(1-x)Fe2O4 pellets decreased with increasing Ni content. The presence of Ni served to decrease thermal conductivity by 8 Wm-1K-1 over pure samples. The magnitude of the Seebeck coefficient for Ni(x)Zn(1-x)Fe2O4 pellets increased with increasing amounts of Ni. The figure of merit for Ni(x)Zn(1-x)Fe2O4 pellets and thin films was improved by increasing Ni due to its high Seebeck coefficient and low thermal conductivity.


2021 ◽  
Author(s):  
Bo Feng

Abstract The effect of Ti doped at Cu site on the thermoelectric properties of BiCuSeO was studied by experimental method and first principles calculation. The results show that Ti doping can cause the lattice contraction and decrease the lattice constant. Ti doping can increase the band gap and lengthen the Cu/Ti-Se bond, resulting in the decrease of carrier concentration. Ti doping can reduce the effective mass and the Bi-Se bond length, correspondingly improve the carrier mobility. Ti doping can decrease the density of states of Cu-3d and Se-4p orbitals at the top of valence band, but Ti-4p orbitals can obviously increase the density of states at the top of valence band and finally increase the electrical conductivity in the whole temperature range. With the decrease of effective mass, Ti doping would reduce the Seebeck coefficient, but the gain effect caused by the increase of electrical conductivity is more than the benefit reduction effect caused by the decrease of Seebeck coefficient, and the power factor shows an upward trend. Ti doping can reduce Young's modulus, lead to the increase of defect scattering and strain field, correspondingly reduce the lattice thermal conductivity and total thermal conductivity. It is greatly increased for the ZT values in the middle and high temperature range, with the highest value of 1.04 at 873 K.


2008 ◽  
Vol 368-372 ◽  
pp. 547-549
Author(s):  
Jun Jiang ◽  
Ya Li Li ◽  
Gao Jie Xu ◽  
Ping Cui ◽  
Li Dong Chen

In the present study, n-type (Bi2Se3)x(Bi2Te3)1-x crystals with various chemical compositions were fabricated by the zone melting method. Thermoelectric properties, including Seebeck coefficient (α), electrical conductivity (σ) and thermal conductivity (κ), were measured in the temperature range of 300-500 K. The influence of the variations of Bi2Te3 and Bi2Se3 content on thermoelectric properties was studied. The increase of Bi2Se3 content (x) caused an increase in carrier concentration and thus an increase of σ and a decrease of α. The maximum figure of merit (ZT = α2σT/κ) of 0.87 was obtained at about 325 K for the composition of 93%Bi2Te3-7%Bi2Se3 with doping TeI4.


2014 ◽  
Vol 604 ◽  
pp. 249-253 ◽  
Author(s):  
Agnese Pura ◽  
Janis Locs ◽  
Liga Berzina-Cimdina

TiO2samples were obtained by extrusion process, sintered in air at 1000 °C, 1100 °C, 1200°C and 1300 °C and, afterwards, thermally treated under vacuum conditions at 1250 °C for 1 hour applying two different heating/cooling rates (2 °C/min and 5 °C/min). It was found that thermal treatment conditions substantially affected thermoelectric properties of the samples. Increasing sintering temperature, during the sample thermal treatment in air, the electrical conductivity of the specimens increased, while Seebeck coefficient decreased. With an increase in the heating rate during the vacuum heat treatment of the samples, the electrical conductivity of the samples decreased, while Seebeck coefficient increased.