Physical Properties of Composite Membrane Containing Apatite and Poly-Lactic Acid /Poly-Glycolic Acid Copolymer In Vitro

2005 ◽  
Vol 284-286 ◽  
pp. 749-752
Author(s):  
T. Watanabe ◽  
Seiji Ban ◽  
Toshiki Itoh ◽  
Shozo Tsuruta ◽  
Takahiro Kawai ◽  
...  

The purpose of this study was to evaluate the physical properties of the composite membrane before and after soaking in simulated body fluid (SBF) and discuss both degradation and maintenance of their properties. Before and after soaking in SBF, some deposits were found on the preexisted apatite crystals, and Ca and P were mainly detected by energy dispersive X-ray analyzer (EDX). Our results suggest that the composite membrane consisting of apatite and the biodegradable PLGA copolymer would have excellent biocompatibility and maintain adequate physical properties for in vivo use.

2018 ◽  
Vol 15 (3) ◽  
pp. 253-261
Author(s):  
Baghdad Science Journal

Commercially pure titanium (cpTi) is widely used as dental implant material although it was found that titanium exhibited high modulus of elasticity and the lower corrosion tendency in oral environment. Niobium(Nb) was chosen for this study as an alternative to cpTi implant material due to its bioinert behavior and good elastic modulus and moderate cost in addition to corrosion resistance. This study was done to evaluate the effect of biomimetic coating on the surface properties of the commercially pure titanium and niobium implants by in vitro and in vivo experiments. The in vitro study was involved etching the samples of each material in HCl then soaking in 10M NaOH aqueous solution. These samples were then immersed in a 5 times concentrated simulated body fluid for 14 days. Scanning Electron Microscope, Energy Dispersive X-ray, and X-Ray Diffraction tests were done to analyze surface changes. The in vivo study was done by the implantation of screw-shaped implants (two from each material, uncoated and the other was biomimetically coated) in the tibias of New Zealand rabbits. After 2 and 4 weeks of healing period, 20 rabbits were sacrificed for each period. A removal torque was done for ten animals in each group, whereas the other ten were used for histological testing and histomorphometric analysis with optical microscope.The in vitro experiments showed that the use of 14 days immersion in a concentrated simulated body fluid produced a layer of calcium phosphate on metal surfaces. The removal torque values and new bone formation were increased significantly in Nb than Ti, in coated than uncoated screws, and in 4 weeks than 2 weeks healing periods. The Nb implants had better biomechanical and biological properties than the commercially pure titanium implants and can be used as an alternative dental implant.


Author(s):  
N.K.R. Smith ◽  
K.E. Hunter ◽  
P. Mobley ◽  
L.P. Felpel

Electron probe energy dispersive x-ray microanalysis (XRMA) offers a powerful tool for the determination of intracellular elemental content of biological tissue. However, preparation of the tissue specimen , particularly excitable central nervous system (CNS) tissue , for XRMA is rather difficult, as dissection of a sample from the intact organism frequently results in artefacts in elemental distribution. To circumvent the problems inherent in the in vivo preparation, we turned to an in vitro preparation of astrocytes grown in tissue culture. However, preparations of in vitro samples offer a new and unique set of problems. Generally, cultured cells, growing in monolayer, must be harvested by either mechanical or enzymatic procedures, resulting in variable degrees of damage to the cells and compromised intracel1ular elemental distribution. The ultimate objective is to process and analyze unperturbed cells. With the objective of sparing others from some of the same efforts, we are reporting the considerable difficulties we have encountered in attempting to prepare astrocytes for XRMA.Tissue cultures of astrocytes from newborn C57 mice or Sprague Dawley rats were prepared and cultured by standard techniques, usually in T25 flasks, except as noted differently on Cytodex beads or on gelatin. After different preparative procedures, all samples were frozen on brass pins in liquid propane, stored in liquid nitrogen, cryosectioned (0.1 μm), freeze dried, and microanalyzed as previously reported.


1994 ◽  
Vol 71 (04) ◽  
pp. 499-506 ◽  
Author(s):  
Mark W C Hatton ◽  
Bonnie Ross-Ouellet

SummaryThe behavior of 125I-labeled recombinant hirudin towards the uninjured and de-endothelialized rabbit aorta wall has been studied in vitro and in vivo to determine its usefulness as an indicator of thrombin activity associated with the aorta wall. Thrombin adsorbed to either sulfopropyl-Sephadex or heparin-Sepharose bound >95% of 125I-r-hirudin and the complex remained bound to the matrix. Binding of 125I-r-hirudin to the exposed aorta subendothelium (intima-media) in vitro was increased substantially if the tissue was pre-treated with thrombin; the quantity of l25I-r-hirudin bound to the de-endothelialized intima-media (i.e. balloon-injured in vitro) correlated positively with the quantity of bound 131I-thrombin (p <0.01). Aortas balloon-injured in vivo were measured for thrombin release from, and binding of 125I-r-hirudin to, the de-endothelialized intimal surface in vitro; 125I-r-hirudin binding correlated with the amount of active thrombin released (p <0.001). Uptake of 125I-r-hirudin by the aorta wall in vivo was proportional to the uptake of 131I-fibrinogen (as an indicator of thrombin activity) before and after balloon injury. After 30 min in the circulation, specific 125I-r-hirudin binding to the uninjured and de-endo- thelialized (at 1.5 h after injury) aorta wall was equivalent to 3.4 (± 2.5) and 25.6 (±18.1) fmol of thrombin/cm2 of intima-media, respectively. Possibly, only hirudin-accessible, glycosaminoglycan-bound thrombin is measured in this way.


2021 ◽  
pp. 088532822110309
Author(s):  
Jinhua Hu ◽  
Bin Ai ◽  
Shibo Zhu ◽  
Zhen Wang ◽  
Huimin Xia ◽  
...  

To investigate the biocompatibility of polylactic acid-glycolic acid copolymer (PLGA) and PLGA/gelatin scaffolds and their suitability for tubular urethral replacement in a canine model. PLGA and PLGA/gelatin scaffolds was constructed by electrospinning. Microstructural differences between the scaffolds was examined by Scanning electron microscopy (SEM) followed by mechanical properties testing. Biocompatibility of the material was evaluated using SEM 4, 8, 12 and 72 h after PLGA and PLGA/gelatin scaffolds co-culture with urothelial cells. And confocal analysis was also used to showed the cell adhesive and growth at 12 h. Approximately 2 cm of the anterior urethra of twelve dogs were removed and replaced with a scaffold. After the surgery for 1 month performed urethrography and for 3 month perform hematoxylin–eosin (H&E) and Masson. The results indicated that PLGA and PLGA/gelatin scaffolds had a void microfilament structure, similar to that of normal acellular matrix tissue. And the tensile strength was decreased whereas the tensile deformation and suture retention strength was increased in PLGA/gelatin scaffolds compared to that in PLGA scaffolds Urothelial cells grew well on both scaffolds. Postoperatively, animals recovered well and urinated spontaneously. However, urethrography showed varying degrees of urethral strictures in the reconstructed urethras. H&E and Masson showed that multilayer urothelial cells were formed in both the proximal and distal segments of the reconstructed urethras but without continuity. There was a small amount of smooth muscle and blood vessels under the epithelium, but regenerative urothelial cells at the midpoint of the reconstructed segment did not continue. Lots of lymphocyte infiltration was observed under the epithelium, some collagen tissue was deposited under the neo-urethral epithelium were observed. In conclusion, PLGA and PLGA/gelatin scaffolds are not suitable for tubularized urethral replacement in the canine model.


Polymers ◽  
2020 ◽  
Vol 13 (1) ◽  
pp. 29
Author(s):  
Seung Kyun Yoon ◽  
Jin Ho Yang ◽  
Hyun Tae Lim ◽  
Young-Wook Chang ◽  
Muhammad Ayyoob ◽  
...  

Herein, spinal fixation implants were constructed using degradable polymeric materials such as PGA–PLA block copolymers (poly(glycolic acid-b-lactic acid)). These materials were reinforced by blending with HA-g-PLA (hydroxyapatite-graft-poly lactic acid) and PGA fiber before being tested to confirm its biocompatibility via in vitro (MTT assay) and in vivo animal experiments (i.e., skin sensitization, intradermal intracutaneous reaction, and in vivo degradation tests). Every specimen exhibited suitable biocompatibility and biodegradability for use as resorbable spinal fixation materials.


Cartilage ◽  
2021 ◽  
pp. 194760352110235
Author(s):  
Hongjun Zhang ◽  
Wendi Zheng ◽  
Du Li ◽  
Jia Zheng

Objective miR-146a-5p was found to be significantly upregulated in cartilage tissue of patients with osteoarthritis (OA). NUMB was shown to be involved in the autophagy regulation process of cells. We aimed to learn whether NUMB was involved in the apoptosis or autophagy process of chondrocytes in OA and related with miR-146a-5p. Methods QRT-PCR was used to detect miR-146a-5p level in 22 OA cartilage tissues and 22 controls. The targets of miR-146a-5p were analyzed using software and the luciferase reporter experiment. The apoptosis and autophagy, and related proteins were detected in chondrocytes treated with miR-146a-5p mimic/inhibitor or pcDNA3.1-NUMB/si-NUMB and IL-1β, respectively. In vivo experiment, intra-articular injection of miR-146a-5p antagomir/NC was administered at the knee of OA male mice before and after model construction. Chondrocyte apoptosis and the expression of apoptosis and autophagy-related proteins were also detected. Results miR-146a-5p was highly expressed in knee cartilage tissue of patients with OA, while NUMB was lowly expressed and negatively regulated by miR-146a-5p. Upregulation of miR-146a-5p can promote cell apoptosis and reduce autophagy of human and mouse chondrocytes by modulating the levels of cleaved caspase-3, cleaved PARP, Bax, Beclin 1, ATG5, p62, LC3-I, and LC3-II. Increasing the low level of NUMB reversed the effects of miR-146a-5p on chondrocyte apoptosis and autophagy. Intra-articular injection of miR-146a-5p antagomir can also reverse the effects of miR-146a-5p on the apoptosis and autophagy of knee joint chondrocytes in OA mice. Conclusion Downregulation of miR-146a-5p suppresses the apoptosis and promotes autophagy of chondrocytes by targeting NUMB in vivo and in vitro.


Sensors ◽  
2021 ◽  
Vol 21 (13) ◽  
pp. 4554
Author(s):  
Ralph-Alexandru Erdelyi ◽  
Virgil-Florin Duma ◽  
Cosmin Sinescu ◽  
George Mihai Dobre ◽  
Adrian Bradu ◽  
...  

The most common imaging technique for dental diagnoses and treatment monitoring is X-ray imaging, which evolved from the first intraoral radiographs to high-quality three-dimensional (3D) Cone Beam Computed Tomography (CBCT). Other imaging techniques have shown potential, such as Optical Coherence Tomography (OCT). We have recently reported on the boundaries of these two types of techniques, regarding. the dental fields where each one is more appropriate or where they should be both used. The aim of the present study is to explore the unique capabilities of the OCT technique to optimize X-ray units imaging (i.e., in terms of image resolution, radiation dose, or contrast). Two types of commercially available and widely used X-ray units are considered. To adjust their parameters, a protocol is developed to employ OCT images of dental conditions that are documented on high (i.e., less than 10 μm) resolution OCT images (both B-scans/cross sections and 3D reconstructions) but are hardly identified on the 200 to 75 μm resolution panoramic or CBCT radiographs. The optimized calibration of the X-ray unit includes choosing appropriate values for the anode voltage and current intensity of the X-ray tube, as well as the patient’s positioning, in order to reach the highest possible X-rays resolution at a radiation dose that is safe for the patient. The optimization protocol is developed in vitro on OCT images of extracted teeth and is further applied in vivo for each type of dental investigation. Optimized radiographic results are compared with un-optimized previously performed radiographs. Also, we show that OCT can permit a rigorous comparison between two (types of) X-ray units. In conclusion, high-quality dental images are possible using low radiation doses if an optimized protocol, developed using OCT, is applied for each type of dental investigation. Also, there are situations when the X-ray technology has drawbacks for dental diagnosis or treatment assessment. In such situations, OCT proves capable to provide qualitative images.


Author(s):  
Erdoğan Karip ◽  
Mehtap Muratoğlu

People are exposed to different kinds of diseases or various accidents in life. Hydroxyapatite (HA) has been widely employed for bone treatment applications. In this study, HA was extracted from sheep bones. Bio-composites were doped with 1, 5, and 10 wt.% of expanded perlite and 5 wt.% of ZrO2–MgO-P2O5. The bio-composites were prepared by the cold isostatic pressing method (250 MPa) and sintered at 900°C for 1 h. In order to evaluate the characteristics of the bio-composites, microhardness, density, X-ray diffraction (XRD), Fourier transform infra-red spectroscopy (FT-IR), scanning electron microscopy (SEM), and energy dispersive spectroscopy (EDS) analyses were carried out on them. Additionally, the specimens whose characteristics were determined were kept in synthetic body fluid (SBF), and their in vitro behavior was examined. As a result, it was observed that microhardness increased as both the weight and the grain size of the expanded perlite were increased. Calcium silicate, tri-calcium phosphate, and hydroxyapatite were observed in the XRD analysis of all samples, and the formation of apatite structures was increased by addition of ZrO2–MgO–P2O5.


Sign in / Sign up

Export Citation Format

Share Document