scholarly journals The effectiveness of waste oyster shells (WOS) as major fine aggregate replacement in concrete

2021 ◽  
Vol 261 ◽  
pp. 02014
Author(s):  
Xinglu Cai ◽  
Ruiwen Liu ◽  
Junhao Fan ◽  
Yingdi Liao

Over-exploitation of natural river sand and waste oyster shells (WOS) dumped randomly will cause serious environmental issues. Thus, a drive to using crushed WOS as fine aggregates to substitute river sand in concrete production has been initiated. This paper conducted experimental research to study the possibility of employing the crushed WOS as 100% fine aggregates in concrete. The workability, compressive strength and its size-effect, and sustainability performance of the concrete mixtures were investigated. The results indicated that, under the same water-cement ratio, the WOS concrete showed a great improvement in strength properties while a decline was found in slump tests, compared to the control concrete. Besides, the use of the crushed WOS in concrete production resulted in a modification in both eco-efficiency and cost-efficiency.

2021 ◽  
Vol 47 (3) ◽  
pp. 906-916
Author(s):  
Simon O. Olawale ◽  
Mutiu A. Kareem ◽  
Habeeb T. Muritala ◽  
Abiola U. Adebanjo ◽  
Olusegun O. Alabi ◽  
...  

The use of industrial by-products in concrete production is part of concerted efforts on the reduction of environmental hazards attributed to the mining of conventional aggregates. Consideration of iron filings (IF), a by-product from steel production process, is an environmentally friendly way of its disposal which is expected to yield economic concrete production. Six self-compacting concrete (SCC) mixes were made by partially substituting river sand with IF at 5%, 10%, 15%, and 20% and the mix without IF (0% IF) served as the control. The water-binder (w/b) ratio of 0.45 was adopted for all mixes. The fresh state properties of SCC evaluated include: filling ability determined using slump flow and T500 mm slump flow tests, passing ability determined using L-box test and segregation resistance determined using V-funnel tests. The strength properties of SCC considered were compressive and tensile strengths. All the SCC mixes met the fresh properties requirements for filling capacity, passing ability, and segregation resistance. The 28-day compressive and tensile strengths of SCC increased by 3.46% and 8.08%, respectively, with IF replacement up to 15% compared to the control SCC. However, there was reduction in compressive and tensile strengths of SCC with IF replacement beyond 15%. The strength properties of SCC is considerably enhanced with the addition of up to 15% IF. Hence, the optimum content of 15% IF is considered suitable as a replacement for river sand in SCC. Keywords: Self-compacting concrete; iron filings; fine aggregates; filling ability; passing ability


2019 ◽  
Vol 23 (1) ◽  
pp. 152-167 ◽  
Author(s):  
Danguole Bisikirske ◽  
Dagnija Blumberga ◽  
Saulius Vasarevicius ◽  
Gintautas Skripkiunas

Abstract Increasing amounts of glass waste present serious challenges in waste management to avoid environmental problems that might be created if it was to be deposited in landfills. Theoretically, glass waste is fully recyclable, but, if contaminated, containing impurities, broken or mixed colour, it makes the re-melting process impractical. A great practice of using secondary recycling material was reached by the construction industry involving glass waste in concrete mixtures as fine aggregates – reuse of waste glass in concrete production not only preserves natural resources, reduces greenhouse gas emissions, saves energy, furthermore, it may improve concrete sustainability and enhance the properties of concrete when used at the optimum quantity. In this study the container glass waste evaluation was performed, as well as experimental research of mechanical properties of four types of concrete mixtures containing glass waste as fine aggregate. The best alternative of replacement of sand by glass waste scenario in concrete production was determined, employing the multicriteria decision-making method TOPSIS.


Waterway sand and pit sand are the most normally utilized fine aggregates for concrete creation in many parts of the world. Huge scale extraction of these materials presents genuine ecological risk in numerous parts of the nation. Aside from the ecological danger, there still exists the issue of intense lack in many regions. In this way, substitute material in place of river sand for concrete production should be considered. The paper means to examine the compressive and split tensile qualities of concrete produced using quarry residue, sand, and a blend of sand and quarry dust. The experimentation is absolutely research facility based. A total of 60 concrete cubes of size 150 mm x 150 mm x 150 mm, and 60 cylinders 150 mm in diameter and 300 mm deep, conforming to M50 grade were casted. All the samples were cured and tested with a steady water/concrete proportion of 0.31. Out of the 60 blocks cast, 20 each were made out of natural river sand, quarry dust and an equivalent blend of sand and quarry dust. It was discovered that the compressive strength and split tensile strength of concrete produced using the blend of quarry residue and sand was higher than the compressive qualities of concrete produced using 100% sand and 100% quarry dust.


This paper presents an experimental investigation on the properties of concrete in which like cement is partially replacing by used nano silica and is partially replacing by used waste foundry sand. Because now a day the world wide consumption of sand as cement and as fine aggregate in concrete production is very high. Nano silica and waste foundry sand are major by product of casting industry and create land pollution. The cement will be replaced with nano silica and the river sand will be replaced with waste foundry sand (0%, 5%, 10%, 15%, 20%). This experimental investigation was done and found out that with the increase in the nano silica and waste foundry sand ratio. Compression test has been done to find out the compressive strength of concrete at the age of 7, 14, 21, and 28. Test result indicates in increasing compressive strength of plain concrete by inclusion of nano silica as a partial replacement of cement and waste foundry sand as a partial replacement of fine aggregate.


2019 ◽  
Vol 11 (17) ◽  
pp. 4647 ◽  
Author(s):  
Warati ◽  
Darwish ◽  
Feyessa ◽  
Ghebrab

The increase in the demand for concrete production for the development of infrastructures in developing countries like Ethiopia leads to the depletion of virgin aggregates and high cement demand, which imposes negative environmental impacts. In sustainable development, there is a need for construction materials to focus on the economy, efficient energy utilization, and environmental protections. One of the strategies in green concrete production is the use of locally available construction materials. Scoria is widely available around the central towns of Ethiopia, especially around the rift valley regions where huge construction activities are taking place. The aim of this paper is therefore to analyze the suitability of scoria as a fine aggregate for concrete production and its effect on the properties of concrete. A differing ratio of scoria was considered as a partial replacement of fine aggregate with river sand after analyzing its engineering properties, and its effect on the mechanical properties of concrete were examined. The test results on the engineering properties of scoria revealed that the material is suitable to be used as a fine aggregate in concrete production. The replacement of scoria with river sand also enhanced the mechanical strength of the concrete. Generally, the findings of the experimental study showed that scoria could replace river sand by up to 50% for conventional concrete production.


2015 ◽  
Vol 2015 ◽  
pp. 1-11 ◽  
Author(s):  
G. Ganesh Prabhu ◽  
Jin Wook Bang ◽  
Byung Jae Lee ◽  
Jung Hwan Hyun ◽  
Yun Yong Kim

In recent years, the construction industry has been faced with a decline in the availability of natural sand due to the growth of the industry. On the other hand, the metal casting industries are being forced to find ways to safely dispose of waste foundry sand (FS). With the aim of resolving both of these issues, an investigation was carried out on the reuse of waste FS as an alternative material to natural sand in concrete production, satisfied with relevant international standards. The physical and chemical properties of the FS were addressed. The influence of FS on the behaviour of concrete was evaluated through strength and durability properties. The test results revealed that compared to the concrete mixtures with a substitution rate of 30%, the control mixture had a strength value that was only 6.3% higher, and this enhancement is not particularly high. In a similar manner, the durability properties of the concrete mixtures containing FS up to 30% were relatively close to those of control mixture. From the test results, it is suggested that FS with a substitution rate of up to 30% can be effectively used in concrete production without affecting the strength and durability properties of the concrete.


Conventionally used cement –a primary binder also a necessitate element in producing concrete rates first in the construction industry. Production of conventional cement requires a greater skill and is energy intensive. The usage of waste materials in the production of concrete and reduction in cement content was only the possible alternative in the past decade. Associated risks with the production of Ordinary Portland Cement are well known. A greener aided with a natural friendly claim can be made only with the usage of the waste materials and reduction in evolving respiration gas to the atmosphere. Almost all works are carried out using source material fly ash, with fine aggregate and coarse aggregate. Concrete plays a vital role in the construction industry and on the other hand, river sand; one of the essential material has become very expensive which is a scarce material. Depletion of sand is a hectic issue due to increased usage of sand in construction. No other replacement materials such as quarry rock dust is not concentrated in casting geopolymer specimens. Even though in some research papers the replacement materials are added only in partial replacement without aiming on 100% replacement. Many researches mainly focus towards test results of GPC specimens using steel fibers, glass fibers. But the study related to natural fibers and hybrid fibers are found scarce. The main part of this work aimed at characterizing the engineering strength properties of geopolymer concrete by 100% replacement of fine aggregate with quarry rock dust. Hence, combination of flyash and quarry rock dust in GPC have been considered for evaluating the mechanical properties of geopolymer concrete. Also, investigation focuses on incorporation of three different fibers namely polypropylene fibers(PF), coir fibers(CF) and hybrid fibers(HF) in different percentage of proportions such as 0.5%,1%,and 1.5% to determine the maximum strength properties of GPC.


2019 ◽  
Vol 8 (3) ◽  
pp. 1982-1988

Use of agro and industrial wastes in concrete production will cause sustainable concrete era and greener habitat. In this study an endeavor has been made to discover the propriety of Sugarcane Bagasse Ash (SCBA) and Granite Waste (GW) as partial replacement for traditional river sand. The percentage substitute is calculated based on the particle packing approach. The properties such as compressive, splitting tensile, flexural strengths and modulus of elasticity, water absorption, sorptivity and rapid chloride penetration test of the concrete with bagasse ash and granite waste as a partial replacement for river sand and to evaluate them with those of conventional concrete made with river sand fine aggregate are investigated. The test results show that the strength aspects of bagasse ash-granite waste concrete are higher than those of the conventional concrete. Moreover, they suggest that the bagasse ash-granite waste concrete has higher strength characteristics and remains in the lower permeability level shows improvement in overall durability of concrete than the conventional concrete.


In recent days, there is an intense need for an alternate cost effective and sustainable raw material for concrete which does not make the structure inferior in strength. An experimental study on the utilization of the waste plastic and M-sand in the place of river sand and aggregate partially was performed in paper. In the scenario of scarcity of river sand due to the territorial government action and restriction of usage because of the eco and environmental consideration, M-Sand is found to be an effective replacement and cost effective material. Concrete specimens were casted with combination of M-sand and plastic waste with 5%, 10%, 15%, 20% and 25% and compared against control mix. Cube test for compressive strength study, cylinder test for split tensile strength study and prism test for flexural strength study were done with the proposed concert mixture. All the specimens and tests were done for different curing period of 7, 14 and 28 days. The results obtained from the proposed mix of concrete are compared with the conventional concrete mix specimen respectively. The replacement of fine aggregates reduces the quantity of river sand to be used in concrete and also plastic fibres are proved to be more economical. Positive performance of the concrete with waste plastic and M-Sand as partial replacement of river sand was observed on all the experiments and found optimal in sustainable and economical performance.


Aggregates used in concrete are fast depleting natural resource and the quarrying of which is causing environmental issues. Hence, the use of aggregate from alternate sources such as from waste discarded glass, from foundry sand discarded after metal casting process and sea shells is investigated. Compressive strength of concrete with glass powder, foundry sand and sea shell is studied individually. Concrete is cast with glass powder and foundry sand as 5%, 10%, 15% and 20% replacement of fine aggregate and with sea shell as 5%, 10%, 15% and 20% replacement of coarse aggregate individually. It is observed that compressive strength of concrete decreases with glass powder, foundry sand, and sea shell. Fine aggregate replaced by 10% glass powder, 10%, foundry sand and coarse aggregate replaced by 10% sea shell have the least decrease in strength when compared to control concrete mix.