Modeling the Creep Deformation, Damage, and Rupture of Hastelloy X Using MPC Omega, Theta, and Sin-Hyperbolic Models

Author(s):  
Mohammad Shafinul Haque ◽  
Calvin M. Stewart

Combined cycle power plants components such as steam pipe work, pressure vessels, boilers, heat exchangers, and gas turbine disks, etc. are exposed to elevated temperature and pressure operation conditions for longer durations. Components may fail within the elastic limit due to a time dependent deformation and damage mechanism called creep. Creep prediction models are used to determine the state of these components and to schedule optimum inspection, maintenance, and replacement intervals. In this study, the deformation, damage, and life of Hastelloy X is characterized using three recently developed models; the Omega, Theta projection, and Sin-hyperbolic models. An analysis is performed to compare the models in terms of accuracy, assumptions, constant identification techniques, flexibility in use, and limitations. The influence that final creep strain has on Theta and Omega model is discussed. Sixteen tests were performed at four different configurations of stress (2.1–36.5 ksi) and temperature (1200–1800°F). In the experimental data, Hastelloy X does not exhibit the primary stage. In this study, the secondary and tertiary creep stages are modeled. Creep deformation and rupture life data is used to optimize the constants for the three models. Predictions using these models are compared with experimental data. It is found that the novel Sin-hyperbolic model better fits the experimental data, and is easier to apply. The Omega model predicts longer life than the Sinh and the Theta Projection model. The rupture life prediction of the Theta projection model is the worst due to dependence on the critical creep strain rate. It is observed that the Hastelloy X final creep strain depends on stress and temperature; this leads to a less accurate critical creep strain rate prediction resulting in inaccurate rupture life predictions for the Theta projection model. The analytical damage of the Omega model exhibits a linear evolution with time while the Sinh model show a more realistic elliptical creep damage evolution with time. A process to determine the constants of all the models is clearly described. The dependence of the trajectory of the creep curves with respect to the constants is discussed in detail. An analytical derivation of each model is provided. Predictions of these three models show that the Sinh model produces a better creep deformation curve by normalizing the experimental creep strain rate data. It is found that overall the Sinh model offers more flexibility, prediction accuracy, and is easier to apply.

Author(s):  
Ricardo Vega ◽  
Jaime A. Cano ◽  
Calvin M. Stewart

Abstract The objective of this study is to introduce a method for creating “material specific” creep continuum damage mechanics-based constitutive models. Herein, material specific is defined as a constitutive model based on the mechanism-informed minimum creep strain rate (MCSR) equations found in deformation mechanism maps and calibrated to available material data. The material specific models are created by finding the best MCSR model for a dataset. Once the best MCSR model is found, the Monkman Grant inverse relationship between the MCSR and rupture time is employed to derive a rupture equation. The equations are substituted into continuum damage mechanics-based creep strain rate and damage evolution equations to furnish predictions of creep deformation and damage. Material specific modeling allows for the derivation of creep constitutive models that can better the material behavior specific to the available data of a material. The material specific framework is also advantageous since it has a systematic framework that moves from finding the best MCSR model, to rupture time, to damage evolution and, creep strain rate. Data for Alloy P91 was evaluated and a material specific constitutive model derived. The material specific model was able to accurately predict the MCSR, creep deformation, damage, and rupture of alloy P91.


Author(s):  
Md Abir Hossain ◽  
Calvin Maurice Stewart

Abstract Typically continuum damage mechanics (CDM) based constitutive models are applied deterministically where the uncertainty of experiments is not considered. This is also true for the Sine-hyperbolic (Sinh) CDM-based constitutive model where the model is calibrated to represent 50% reliability of creep data. There is a need to implement Sinh in a more stochastic manner. The objectives of this study is to incorporate the probabilistic feature in the Sinh creep damage model to reliably predict the minimum-creep-strain-rate, creep-rupture and creep deformation. This will be achieved using Monte-Carlo methods. Creep deformation data for 304 Stainless Steel is collected from literature consisting of tests conducted at 300 and 320 MPa at 600°C with five replicates. The replicate tests exhibited substantial scatter in the minimum-creep-strain-rate, stress-rupture, and overall creep deformation. Subsequently, upon calibration using the Sinh model, the material constants among the replicates varied. The trends of uncertainty carried by each material constant are studied. The interdependence of the material constants is evaluated to determine if the uncertainty carried by each material constant can be regressed using a co-dependence function. The Monte Carlo method was applied to determine the extent that the creep deformation curve varies taking into consideration the variability of the material constants. Monte Carlo simulations show that the predicted creep deformation persists within the bounds of the experimental data. A large number of Monte Carlo simulations using the Sinh model enabled the creation of credible reliability bands for the minimum-creep-strain-rate, stress-rupture, and creep deformation of 304 Stainless Steel. In future work, this statistical method will be applied to the variability of service conditions, pre-existing defects, and material constants to quantitatively establish the reliability of the Sinh model in simulating component-level creep deformation to rupture.


2000 ◽  
Vol 646 ◽  
Author(s):  
Haruyuki Inui ◽  
Koji Ishikawa ◽  
Masaharu Yamaguchi

ABSTRACTEffects of ternary additions on the deformation behavior of single crystals of MoSi2 with the hard [001] and soft [0 15 1] orientations have been investigated in compression and compression creep. The alloying elements studied include V, Cr, Nb and Al that form a C40 disilicide with Si and W and Re that form a C11b disilicide with Si. The addition of Al is found to decrease the yield strength of MoSi2 at all temperatures while the additions of V, Cr and Nb are found to decrease the yield strength at low temperatures and to increase the yield strength at high temperatures. In contrast, the additions of W and Re are found to increase the yield strength at all temperatures. The creep strain rate for the [001] orientation is significantly lower than that for the [0 15 1] orientation. The creep strain rate for both orientations is significantly improved by alloying with ternary elements such as Re and Nb.


Geofluids ◽  
2018 ◽  
Vol 2018 ◽  
pp. 1-10
Author(s):  
Fan Zhang ◽  
Jianjian Zhao ◽  
Dawei Hu ◽  
Qian Sheng ◽  
Jianfu Shao

Fluid flow and fluid-rock interaction mainly take place in fracture network, consequently resulting in deformation and permeability variation of rock and deterioration of the wellbore performance. Mechanical-reactive flow coupling creep tests are performed on cracked granite under various confining pressures and acid and alkaline solution flows. The testing results show that the confining pressure and solution pH significantly influence the creep deformation, creep strain rate, and permeability. A primary creep stage and secondary creep stage are observed in all creep tests in this study; notably, the sample under a confining pressure of 10 MPa and acid solution injection undergoes creep failure for over 2700 hours. The acid solution has a more obvious influence on the creep behavior than that of the alkaline solution. With an increase in confining pressure, the total creep strain and creep strain rate in the samples gradually decrease during the injection of either solution. The permeability of the samples injected with either solution gradually deceases during the testing process, and this deceasing rate increases with the confining pressure. The scanning electron microscopy observations on the crack surfaces after the creep tests show that the surfaces of the fractures injected with the acid solution are smooth due to the dissolution of the matrix, while those injected with the alkaline solution include voids due to the dissolution of quartz. These experimental results could improve the understanding of the long-term transport and mechanical behaviors of wellbore.


Author(s):  
Takashi Ogata

Grade 91 is widely used for steam pipes and tubes in high temperature boilers of ultra-super critical power plants in Japan. It was reported that creep damage may initiate at the fine grain region within the heat affected zone (HAZ) in welded joints prior to the base metal, so called “Type IV” damage, which causes steam leakage in existing power plants. Therefore, development of creep damage assessment methods is not only an important but also an urgent subject to maintain operation reliability. In order to evaluate creep damage of welded joints based on finite element analyses, creep deformation properties of a base metal, a weld metal and a HAZ have to be obtained from creep tests. However, it is difficult to cut a standard size creep specimen from the HAZ region. Only a miniature size specimen is available from the narrow HAZ region. Therefore, development of creep testing and evaluation technique for miniature size specimens is highly expected. In this study, a miniature tensile type solid bar specimen with 1mm diameter was machined from a base metal, a weld metal and a HAZ of a new and a used Grade 91 welded joints, and creep tests of these miniature specimens were conducted by using a special developed creep testing machine. It was found that creep deformation property is almost identical between the base metal and weld metal, and creep strain rate of the HAZ is much faster than that of these metals in the new welded joint. Relationships between stress and creep strain rates of the base metal and the HAZ in the used welded joint are within scatter bands of those in the new material. On the other hand, creep strain rate of the weld metal in the used welded joint became much faster than that in the new one. Then both the standard size and the miniature size cross weld specimens were machined from the new and the used welded joints and were tested under the same temperature and stress conditions. Rupture time of the miniature cross weld specimen is much shorter than that of the standard size cross weld specimen. The finite element creep analysis of the specimens indicates that higher triaxiality stress yields within the HAZ of the standard size specimen than that of the miniature specimen causing faster creep strain rate in the HAZ of the miniature cross weld specimen.


2010 ◽  
Vol 24 (01n02) ◽  
pp. 267-275 ◽  
Author(s):  
Y. D. HAN ◽  
H. Y. JING ◽  
S. M. L. NAI ◽  
L. Y. XU ◽  
C. M. TAN ◽  
...  

In the present study, nanoindentation studies of the 95.8 Sn -3.5 Ag -0.7 Cu lead-free solder were conducted over a range of maximum loads from 20 mN to 100 mN, under a constant ramp rate of 0.05 s-1. The indentation scale dependence of creep behavior was investigated. The results revealed that the creep rate, creep strain rate and indentation stress are all dependent on the indentation depth. As the maximum load increased, an increasing trend in the creep rate was observed, while a decreasing trend in creep strain rate and indentation stress were observed. On the contrary, for the case of stress exponent value, no trend was observed and the values were found to range from 6.16 to 7.38. Furthermore, the experimental results also showed that the creep mechanism of the lead-free solder is dominated by dislocation climb.


2016 ◽  
Vol 35 (3) ◽  
pp. 243-252
Author(s):  
Balhassn S. M. Ali ◽  
Tom H. Hyde ◽  
Wei Sun

AbstractCommonly used small creep specimen types, such as ring and impression creep specimens, are capable of providing minimum creep strain rate data from small volumes of material. However, these test types are unable to provide the creep rupture data. In this paper the recently developed two-bar specimen type, which can be used to obtain minimum creep strain rate and creep rupture creep data from small volumes of material, is described. Conversion relationships are used to convert (i) the applied load to the equivalent uniaxial stress, and (ii) the load line deformation rate to the equivalent uniaxial creep strain rate. The effects of the specimen dimension ratios on the conversion factors are also discussed in this paper. This paper also shows comparisons between two-bar specimen creep test data and the corresponding uniaxial creep test data, for grade P91 steel at 650°C.