Effects of the Stacking Sequence, Material Nature and Addition of an Adhesive Film on the Delamination Resistance of Woven Composite Laminates in Mode I and II

2015 ◽  
Vol 24 (1) ◽  
pp. 096369351502400
Author(s):  
P. Navarro ◽  
J. Aubry ◽  
F. Pascal ◽  
S. Marguet ◽  
J.F. Ferrero ◽  
...  

Woven composites are well-known for their good transverse properties and for their high fracture toughness. The damage mechanisms leading to delamination in woven composites are identified in mode I and II and are compared with those occurring in unidirectional laminates. The influence of several parameters, including the draping sequence and the fibre / matrix interface on the fracture toughness of woven composite laminates is studied. Pure Mode I and Mode II tests are carried out on several carbon/epoxy and glass/epoxy woven composites configurations and the differences observed are discussed from a fractographic point of view. The study illustrates the high fracture toughness of the composites made of woven fabrics as well the influence of the orientation of the plies, the nature of the fibres and the addition of an adhesive film.

2018 ◽  
Vol 50 (1) ◽  
pp. 23-45 ◽  
Author(s):  
Amna Siddique ◽  
Baozhong Sun ◽  
Bohong Gu

This paper reports the mode I interlaminar fracture toughness and fracture mechanisms of two-dimensional (2D) plain woven composite and three-dimensional (3D) angle-interlock woven composite. The fracture toughness behaviors were tested with double cantilever beam method at the different loading rates from 0.5 to 100 mm/min. Critical strain energy release rate was calculated to compare the difference between the 2D and the 3D woven composites. The fractographs were photographed with scanned electronic microscopy and optical microscopy to show the fracture morphologies. We found that the 3D angle-interlock woven composite has high fracture toughness than that of 2D woven composite. The binder yarns resist the crack initiation and propagation to increase the fracture toughness. While the lower in-plane stiffness of the 3D woven composites should be considered fully for designing the 3D woven composites.


Alloy Digest ◽  
2000 ◽  
Vol 49 (1) ◽  

Abstract Kaiser Aluminum Alloy 7050 has very high mechanical properties including tensile strength, high fracture toughness, and a high resistance to exfoliation and stress-corrosion cracking. The alloy is typically used in aircraft structural parts. This datasheet provides information on composition, physical properties, hardness, tensile properties, and shear strength as well as fracture toughness and fatigue. It also includes information on forming, heat treating, machining, and joining. Filing Code: AL-366. Producer or source: Tennalum, A Division of Kaiser Aluminum.


Alloy Digest ◽  
2018 ◽  
Vol 67 (9) ◽  

Abstract Ferrium M54 was designed to create a cost-effective, ultra high-strength, high-fracture toughness material with a high resistance to stress-corrosion cracking for use in structural applications. This datasheet provides information on composition, hardness, and tensile properties as well asfatigue. Filing Code: SA-822. Producer or source: QuesTek Innovations, LLC.


2015 ◽  
Vol 83 (3) ◽  
Author(s):  
Zhuo Ma ◽  
Xiangchao Feng ◽  
Wei Hong

Consisting of stretchable and flexible cell walls or ligaments, soft elastic foams exhibit extremely high fracture toughness. Using the analogy between the cellular structure and the network structure of rubbery polymers, this paper proposes a scaling law for the fracture energy of soft elastic foam. To verify the scaling law, a phase-field model for the fracture processes in soft elastic structures is developed. The numerical simulations in two-dimensional foam structures of various unit-cell geometries have all achieved good agreement with the scaling law. In addition, the dependences of the macroscopic fracture energy on geometric parameters such as the network connectivity and spatial orientation have also been revealed by the numerical results. To further enhance the fracture toughness, a type of soft foam structures with nonstraight ligaments or folded cell walls has been proposed and its performance studied numerically. Simulations have shown that an effective fracture energy one order of magnitude higher than the base material can be reached by using the soft foam structure.


2021 ◽  
Vol 11 (1) ◽  
Author(s):  
Erik Poloni ◽  
Florian Bouville ◽  
Christopher H. Dreimol ◽  
Tobias P. Niebel ◽  
Thomas Weber ◽  
...  

AbstractThe brick-and-mortar architecture of biological nacre has inspired the development of synthetic composites with enhanced fracture toughness and multiple functionalities. While the use of metals as the “mortar” phase is an attractive option to maximize fracture toughness of bulk composites, non-mechanical functionalities potentially enabled by the presence of a metal in the structure remain relatively limited and unexplored. Using iron as the mortar phase, we develop and investigate nacre-like composites with high fracture toughness and stiffness combined with unique magnetic, electrical and thermal functionalities. Such metal-ceramic composites are prepared through the sol–gel deposition of iron-based coatings on alumina platelets and the magnetically-driven assembly of the pre-coated platelets into nacre-like architectures, followed by pressure-assisted densification at 1450 °C. With the help of state-of-the-art characterization techniques, we show that this processing route leads to lightweight inorganic structures that display outstanding fracture resistance, show noticeable magnetization and are amenable to fast induction heating. Materials with this set of properties might find use in transport, aerospace and robotic applications that require weight minimization combined with magnetic, electrical or thermal functionalities.


Crystals ◽  
2021 ◽  
Vol 11 (4) ◽  
pp. 393
Author(s):  
Kei Maeda ◽  
Kosho Akatsuka ◽  
Gaku Okuma ◽  
Atsuo Yasumori

Fracture behavior via a flexural test for a newly found CaO–Al2O3–SiO2 (CAS) glass-ceramic (GC) was compared with that of enstatite GC and mica GC, which are well-known GCs with high-fracture toughness and machinability, respectively. By focusing on the nonelastic load–displacement curves, CAS GC was characterized as a less brittle material similar to machinable mica GC, compared with enstatite GC, which showed higher fracture toughness, KIC. The microcrack toughening mechanism in CAS GC was supported by the nondestructive observation of microcracks around the Vickers indentation using the X-ray microcomputed tomography technique. The CAS GC also showed higher transparency than mica GC due to its low crystallinity. Moreover, the precursor glass had easy formability due to its low-liquidus temperature.


Sign in / Sign up

Export Citation Format

Share Document