The kinetics of thermal degradation of polyphenolic compounds from elderberry (Sambucus nigra L.) extract

2018 ◽  
Vol 24 (4) ◽  
pp. 361-369 ◽  
Author(s):  
Ana-Maria Oancea ◽  
Cristina Onofrei ◽  
Mihaela Turturică ◽  
Gabriela Bahrim ◽  
Gabriela Râpeanu ◽  
...  

This main focus of this study was to evaluate the thermal degradation kinetics and the phytochemical characterization of the elderberries extract. Pelargonidin-3-sophoroside and delphinidin-3-glucoside were identified as the major anthocyanin compounds and catechin hydrate as the major flavonoid compound. In order to further understand the action of the heat treatment on the bioactive compounds from elderberry extract, fluorescence studies were also carried out. In general, heating at temperatures ranging from 100 to 150 ℃ for up to 90 min caused a decrease in fluorescence intensity, simultaneously with significant redshifts in λmax suggesting important molecular changes inside the anthocyanins structure, affecting the antioxidant activity. Increasing the heating time up to 120 min, the elderberry extract peaked at about 88 nm shifted toward higher wavelengths with respect to that of untreated solutions (peak at 442 nm). The kinetics studies of anthocyanins, fluorescence intensity, and antioxidant activity evidenced a decrease of the degradation rate constants with increased temperature while the activation energies for heat-induced fluorescence intensity, monomeric anthocyanins, and antioxidant activity were 39.62 ± 9.60, 49.97 ± 5.61, and 31.04 ± 19.92 kJ/mol, respectively. Our results can be valuable in terms of establishing the appropriate processing and formulation protocols that could lead to a more efficient utilization of these pigments in actual food products and/or nutraceuticals.

Foods ◽  
2020 ◽  
Vol 9 (11) ◽  
pp. 1593
Author(s):  
Mioara Slavu (Ursu) ◽  
Iuliana Aprodu ◽  
Ștefania Adelina Milea ◽  
Elena Enachi ◽  
Gabriela Râpeanu ◽  
...  

The thermal degradation of the anthocyanins and antioxidant activity in purple maize extracts was determined between 80 and 180 °C. The anthocyanins were found to be thermostable in the temperature range of 80 to 120 °C, whereas at higher temperatures the thermal degradation of both anthocyanins and antioxidant activity followed a first-order kinetic model. The z-values started from 61.72 ± 2.28 °C for anthocyanins and 75.75 ± 2.87 °C for antioxidant activity. The conformational space of pairs of model anthocyanin molecules at 25 and 180 °C was explored through a molecular dynamics test, and results indicated the occurrence of intermolecular self-association reactions and intramolecular co-pigmentation events, which might help explaining the findings of the degradation kinetics. The relationship between thermal degradation of anthocyanins and antioxidant activity and the in vitro release was further studied. The unheated extracts showed a high stability under gastric environment, whereas after heating at 180 °C, the digestion ended quickly after 60 min. After simulated intestinal digestion, the anthocyanins were slowly decreased to a maximum of 12% for the unheated extracts, whereas an 83% decrease was found after preliminary heating at 180 °C. The thermal degradation of anthocyanins was positively correlated with the in vitro decrease of antioxidant activity.


2021 ◽  
pp. 002199832110082
Author(s):  
Azzeddine Gharsallah ◽  
Abdelheq Layachi ◽  
Ali Louaer ◽  
Hamid Satha

This paper reports the effect of lignocellulosic flour and talc powder on the thermal degradation behavior of poly (lactic acid) (PLA) by thermogravimetric analysis (TGA). Lignocellulosic flour was obtained by grinding Opuntia Ficus Indica cladodes. PLA/talc/ Opuntia Ficus Indica flour (OFI-F) biocomposites were prepared by melt processing and characterized using Wide-angle X-ray scattering (WAXS) and Scanning Electron Microscope (SEM). The thermal degradation of neat PLA and its biocomposites can be identified quantitatively by solid-state kinetics models. Thermal degradation results on biocomposites compared to neat PLA show that talc particles at 10 wt % into the PLA matrix have a minor impact on the thermal stability of biocomposites. Loading OFI-F and Talc/OFI-F mixture into the PLA matrix results in a decrease in the maximum degradation temperature, which means that the biocomposites have lower thermal stability. The activation energies (Ea) calculated by the Flynn Wall Ozawa (FWO) and Kissinger Akahira Sunose (KAS) model-free approaches and by model-fitting (Kissinger method and Coats-Redfern method) are in good agreement with one another. In addition, in this work, the degradation mechanism of biocomposites is proposed using Coats-Redfern and Criado methods.


Molecules ◽  
2021 ◽  
Vol 26 (6) ◽  
pp. 1597
Author(s):  
Iman Jafari ◽  
Mohamadreza Shakiba ◽  
Fatemeh Khosravi ◽  
Seeram Ramakrishna ◽  
Ehsan Abasi ◽  
...  

The incorporation of nanofillers such as graphene into polymers has shown significant improvements in mechanical characteristics, thermal stability, and conductivity of resulting polymeric nanocomposites. To this aim, the influence of incorporation of graphene nanosheets into ultra-high molecular weight polyethylene (UHMWPE) on the thermal behavior and degradation kinetics of UHMWPE/graphene nanocomposites was investigated. Scanning electron microscopy (SEM) analysis revealed that graphene nanosheets were uniformly spread throughout the UHMWPE’s molecular chains. X-Ray Diffraction (XRD) data posited that the morphology of dispersed graphene sheets in UHMWPE was exfoliated. Non-isothermal differential scanning calorimetry (DSC) studies identified a more pronounced increase in melting temperatures and latent heat of fusions in nanocomposites compared to UHMWPE at lower concentrations of graphene. Thermogravimetric analysis (TGA) and derivative thermogravimetric (DTG) revealed that UHMWPE’s thermal stability has been improved via incorporating graphene nanosheets. Further, degradation kinetics of neat polymer and nanocomposites have been modeled using equations such as Friedman, Ozawa–Flynn–Wall (OFW), Kissinger, and Augis and Bennett’s. The "Model-Fitting Method” showed that the auto-catalytic nth-order mechanism provided a highly consistent and appropriate fit to describe the degradation mechanism of UHMWPE and its graphene nanocomposites. In addition, the calculated activation energy (Ea) of thermal degradation was enhanced by an increase in graphene concentration up to 2.1 wt.%, followed by a decrease in higher graphene content.


Materials ◽  
2017 ◽  
Vol 10 (11) ◽  
pp. 1246 ◽  
Author(s):  
Samson M. Mohomane ◽  
Tshwafo E. Motaung ◽  
Neerish Revaprasadu