scholarly journals The Statistical Analysis of Relation between Compressive and Tensile/Flexural Strength of High Performance Concrete

2016 ◽  
Vol 62 (4) ◽  
pp. 95-108 ◽  
Author(s):  
M. Kępniak ◽  
P. Woyciechowski

AbstractThis paper addresses the tensile and flexural strength of HPC (high performance concrete). The aim of the paper is to analyse the efficiency of models proposed in different codes. In particular, three design procedures from: the ACI 318 [1], Eurocode 2 [2] and the Model Code 2010 [3] are considered. The associations between design tensile strength of concrete obtained from these three codes and compressive strength are compared with experimental results of tensile strength and flexural strength by statistical tools. Experimental results of tensile strength were obtained in the splitting test. Based on this comparison, conclusions are drawn according to the fit between the design methods and the test data. The comparison shows that tensile strength and flexural strength of HPC depend on more influential factors and not only compressive strength.

2014 ◽  
Vol 670-671 ◽  
pp. 437-440 ◽  
Author(s):  
Fan Wang ◽  
Shan Suo Zheng ◽  
Xiao Fei Wang

With the improvement of concrete materials and the emergence of new materials, adding silica fume to high-performance concrete (HPC) has been one of the important ways in concrete technology. In this paper, through experimental study on the mechanical performance of HPC with 5%, 10%, 15% and 20% silica fume replacing cement for different water-binder ratio, along with polycarboxylates high performance water-reducing admixture, silica fume has large effects on 28d compressive strength, split tensile strength and flexural strength of the HPC. Meanwhile, due to the different level of water-binder ratio, the relationship between split tensile strength, flexural strength and compressive strength is also obvious linear.


2015 ◽  
Vol 773-774 ◽  
pp. 949-953 ◽  
Author(s):  
Izni Syahrizal Ibrahim ◽  
Wan Amizah Wan Jusoh ◽  
Abdul Rahman Mohd Sam ◽  
Nur Ain Mustapa ◽  
Sk Muiz Sk Abdul Razak

This paper discusses the experimental results on the mechanical properties of hybrid fibre reinforced composite concrete (HyFRCC) containing different proportions of steel fibre (SF) and polypropylene fibre (PPF). The mechanical properties include compressive strength, tensile strength, and flexural strength. SF is known to enhance the flexural and tensile strengths, and at the same time is able to resist the formation of macro cracking. Meanwhile, PPF contributes to the tensile strain capacity and compressive strength, and also delay the formation of micro cracks. Hooked-end deformed type SF fibre with 60 mm length and fibrillated virgin type PPF fibre with 19 mm length are used in this study. Meanwhile, the concrete strength is maintained for grade C30. The percentage proportion of SF-PPF fibres are varied in the range of 100-0%, 75-25%, 50-50%, 25-75% and 0-100% of which the total fibre volume fraction (Vf) is fixed at 0.5%. The experimental results reveal that the percentage proportion of SF-PPF fibres with 75-25% produced the maximum performance of flexural strength, tensile strength and flexural toughness. Meanwhile, the percentage proportion of SF-PPF fibres with 100-0% contributes to the improvement of the compressive strength compared to that of plain concrete.


2017 ◽  
Vol 8 (4) ◽  
pp. 392-401 ◽  
Author(s):  
Hassan A.M. Mhamoud ◽  
Jia Yanmin

Purpose This study aims to focus on the resistance to elevated temperatures of up to 700ºC of high-performance concrete (HPC) compared to ordinary Portland concrete (OPC) with regards to mass loss and residual compressive and flexural strength. Design/methodology/approach Two mixtures were developed to test. The first mixture, OPC, was used as the control, and the second mixture was HPC. After 28 days under water (per Chinese standard), the samples were tested for compressive strength and residual strength. Findings The test results showed that at elevated temperatures of up to 500ºC, each mixture experienced mass loss. Below this temperature, the strength and the mass loss did not differ greatly. Originality/value When adding a 10 per cent silica fume, 25 per cent fly, 25 per cent slag to HPC, the compressive strength increased by 17 per cent and enhanced the residual compressive strength. A sharp decrease was observed in the residual flexural strength of HPC when compared to OPC after exposure to temperatures of 700ºC.


2013 ◽  
Vol 634-638 ◽  
pp. 2716-2719
Author(s):  
Wan Shin Park ◽  
Sung Ho Cho ◽  
Song Hui Yun ◽  
Jeong Eun Kim ◽  
Do Gyeum Kim ◽  
...  

The characteristics of the compressive strength and splitting tensile strength according to replacement ratio of the blast furnace slag were found in this study. The blast furnace slag was utilizes as the concrete mix-material and then, these results were compared with the basis presented in the international standards. In this study, cylinder made of concrete with water/binder ratio 0.34 and blast furnace slag replacement rate of 10%, 30%, 50%, and 70% were prepared to measure the compressive strength and spiting tensile strength. Test results indicate that The 28 days and 91 days compressive strength is affected by blast furnace slag replacement except specimen BS30 and the splitting tensile strength in specimen BS series is slightly larger than that of OPC except specimen BS 30.


2013 ◽  
Vol 859 ◽  
pp. 52-55 ◽  
Author(s):  
Yong Qiang Ma

A great deal of experiments have been carried out in this study to reveal the effect of the water-binder ratio and fly ash content on the workability and strengths of GHPC (green high performance concrete). The workability of GHPC was evaluated by slump and slump flow. The strengths include compressive strength and splitting tensile strength. The results indicate that the increase of water-binder ratio can improve the workability of GHPC, however the strengths of GHPC were decreased with the increase of water-binder ratio. When the fly ash content is lower than 40%, the increase in fly ash content has positive effect on workability of GHPC, while the workability begins to decrease after the fly ash content is more than 40%. The addition of fly ash in GHPC has adverse effect on the strengths, and there is a tendency of decrease in the compressive strength and splitting tensile strength of GHPC with the increase of fly ash content.


Author(s):  
Faiq M. Al-Zwainy ◽  
Hussam k. Risan ◽  
Rana I. K. Zaki

The purpose of this study was to conduct a meta-analysis that shows the influence of fiber on ultimate compressive strength and tensile strength of ultra-high performance concrete. The internet scholarly search engines and ScienceDirect article references were used to illustrate the papers concerning the experimental investigations of mechanical properties of ultra-high strength concrete with and without fiber with clearly, completely and comparative raw data. The normal concrete test results were dismissed from this search. Seven trials were identified based on the adopted inclusion and exclusion criteria above. The meta-analysis based on standardized mean difference was carried out on the basis of a fixed-effects model for the major outcomes of the ultimate compressive and tensile properties of ultra-high performance concrete. A total of 888 test specimens were enrolled in these seven trials. The combined analysis yielded a sign of a significant improvement in ultimate compressive strength and tensile strength of ultra-high strength concrete with fiber addition of 2% by concrete volume. The summary effect size of ultimate compressive strength was 2.34 while a more improvement in term of tensile strength with effect size of 2.64. By addition fiber of 2% provides a significant benefit in mechanical properties of ultra-high performance concrete.


2018 ◽  
Vol 15 ◽  
pp. 1-5
Author(s):  
Tomáš Blažek ◽  
Jakub Řepka ◽  
Tomáš Vlach

This article deals with the test of selected adhesives for glued connection of high performance concrete and steel plates with various surface treatments. Results of this experiment can be used as a basis for the possible anchoring of concrete facade elements to the steel grate, the possible bonding of steel anchors on the surface of concrete facade elements. High performance concrete is a concrete that exceeds the compressive strength 100 MPa after 28 days. The second adherent is the uncoated steel and the steel with zinc coating as a second variant. Samples were tested in two different ways. The first experiment verified the single tensile strength of bond connection. The second test verified the shear strength, which is very important for connection designing.


2013 ◽  
Vol 372 ◽  
pp. 231-234
Author(s):  
Jeong Eun Kim ◽  
Wan Shin Park ◽  
Nam Yong Eom ◽  
Sun Woong Kim ◽  
Do Gyeum Kim ◽  
...  

In this study, some experimental investigations on the development of mechanical properties with age of high performance concrete (HPC) incorporated with blast furnace slag with fly ash or silica fume have been reported. Four different blended HPC were prepared in 0.40 water-binder ratio. At every four mixtures, the compressive strength, splitting tensile strength and modulus of elasticity at 7 and 28 days have been observed for HPC developments. Consequently, only replacement of silica fume significantly increases the mechanical properties in terms of compressive strength, splitting tensile strength and modulus of elasticity.


2014 ◽  
Vol 584-586 ◽  
pp. 1509-1513
Author(s):  
Nan Zhang ◽  
Juan Liao ◽  
Tao Zhang ◽  
Wen Zhan Ji ◽  
Bao Hua Wang ◽  
...  

The effect of very low temperature on high performance concrete (HPC) mechanical properties is studied by using a reasonable testing method. The results show that the compressive strengths of concrete are increasing with lower temperatures. Fly ash (FA), compared to ground granulated blast-furnace slag (GGBFS), is positive to the compressive strength increasing at low temperature. The splitting tensile strengths of concrete appear a maximum at-40°C~-80°C. The compound replacement by GGBFS and FA makes the splitting tensile strength present the extreme value at higher temperature. At very low temperature, the single or compound replacement by mineral admixtures can result in the difference of the relationship between compressive strength and splitting tensile strength, and the degradation of concrete subjected to cold-thermal shocks.


2013 ◽  
Vol 2013 ◽  
pp. 1-7 ◽  
Author(s):  
Huai-Shuai Shang ◽  
Ting-Hua Yi

For use in fire resistance calculations, the relevant thermal properties of high-performance concrete (HPC) with fly ash were determined through an experimental study. These properties included compressive strength, cubic compressive strength, cleavage strength, flexural strength, and the ultrasonic velocity at various temperatures (20, 100, 200, 300, 400 and 500∘C) for high-performance concrete. The effect of temperature on compressive strength, cubic compressive strength, cleavage strength, flexural strength, and the ultrasonic velocity of the high-performance concrete with fly ash was discussed according to the experimental results. The change of surface characteristics with the temperature was observed. It can serve as a reference for the maintenance, design, and the life prediction of high-performance concrete engineering, such as high-rise building, subjected to elevated temperatures.