Formation of Sub-100 NM GE Wires on Si by E-Beam Evaporation/Lithography

1995 ◽  
Vol 380 ◽  
Author(s):  
C. Deng ◽  
J. C. Wu ◽  
C. J. Barbero ◽  
T. W. Sigmon ◽  
M. N. Wybourne

ABSTRACTA fabrication process for sub-100 nm Ge wires on Si substrates is reported for the first time. Wires with a cross section of 6 × 57 nm2 are demonstrated. The wire structures are analyzed by atomic force (AFM), scanning electron (SEM), and transmission electron microscopy (TEM). Sample preparation for TEM is performed using a novel technique using both pre and in situ deposition of multiple protection layers using a Focused Ion Beam (FIB) micromachining system.

Author(s):  
H. J. Bender ◽  
R. A. Donaton

Abstract The characteristics of an organic low-k dielectric during investigation by focused ion beam (FIB) are discussed for the different FIB application modes: cross-section imaging, specimen preparation for transmission electron microscopy, and via milling for device modification. It is shown that the material is more stable under the ion beam than under the electron beam in the scanning electron microscope (SEM) or in the transmission electron microscope (TEM). The milling of the material by H2O vapor assistance is strongly enhanced. Also by applying XeF2 etching an enhanced milling rate can be obtained so that both the polymer layer and the intermediate oxides can be etched in a single step.


Author(s):  
Chih-Chung Chang ◽  
Jian-Chang Lin ◽  
Wen-Sheng Wu ◽  
Chih-Ying Tasi ◽  
Ching-Lin Chang

Abstract A dual beam FIB (Focused Ion Beam) system which provides the ion beam (i-beam) and electron beam (e-beam) function are widely used in semiconductor manufacture for construction analysis and failure cause identification. Although FIB is useful for defect or structure inspection, sometimes, it is still difficult to diagnose the root cause via FIB e-beam image due to resolution limitation especially in products using nano meter scale processes. This restriction will deeply impact the FA analysts for worst site or real failure site judgment. The insufficient e-beam resolution can be overcome by advanced TEM (Transmission Electron Microscope) technology, but how can we know if this suspected failure site is a real killer or not when looking at the insufficient e-beam images inside a dual beam tool? Therefore, a novel technique of device measurement by using C-AFM (Conductive Atomic Force Microscope) or Nano-Probing system after cross-sectional (X-S) FIB inspection has been developed based on this requirement. This newly developed technology provides a good chance for the FA analysts to have a device characteristic study before TEM sample preparation. If there is any device characteristic shift by electrical measurement, the following TEM image should show a solid process abnormality with very high confidence. Oppositely, if no device characteristic shift can be measured, FIB milling is suggested to find the real fail site instead of trying TEM inspection directly.


Nanophotonics ◽  
2017 ◽  
Vol 6 (5) ◽  
pp. 923-941 ◽  
Author(s):  
Gediminas Seniutinas ◽  
Armandas Balčytis ◽  
Ignas Reklaitis ◽  
Feng Chen ◽  
Jeffrey Davis ◽  
...  

AbstractThe evolution of optical microscopy from an imaging technique into a tool for materials modification and fabrication is now being repeated with other characterization techniques, including scanning electron microscopy (SEM), focused ion beam (FIB) milling/imaging, and atomic force microscopy (AFM). Fabrication and in situ imaging of materials undergoing a three-dimensional (3D) nano-structuring within a 1−100 nm resolution window is required for future manufacturing of devices. This level of precision is critically in enabling the cross-over between different device platforms (e.g. from electronics to micro-/nano-fluidics and/or photonics) within future devices that will be interfacing with biological and molecular systems in a 3D fashion. Prospective trends in electron, ion, and nano-tip based fabrication techniques are presented.


Author(s):  
Jian-Shing Luo ◽  
Hsiu Ting Lee

Abstract Several methods are used to invert samples 180 deg in a dual beam focused ion beam (FIB) system for backside milling by a specific in-situ lift out system or stages. However, most of those methods occupied too much time on FIB systems or requires a specific in-situ lift out system. This paper provides a novel transmission electron microscopy (TEM) sample preparation method to eliminate the curtain effect completely by a combination of backside milling and sample dicing with low cost and less FIB time. The procedures of the TEM pre-thinned sample preparation method using a combination of sample dicing and backside milling are described step by step. From the analysis results, the method has applied successfully to eliminate the curtain effect of dual beam FIB TEM samples for both random and site specific addresses.


Author(s):  
J. Douglass ◽  
T. D. Myers ◽  
F. Tsai ◽  
R. Ketcheson ◽  
J. Errett

Abstract This paper describes how the authors used a combination of focused ion beam (FIB) microprobing, transmission electron microscopy (TEM), and data and process analysis to determine that localized water residue was causing a 6% yield loss at die sort.


Author(s):  
Dirk Doyle ◽  
Lawrence Benedict ◽  
Fritz Christian Awitan

Abstract Novel techniques to expose substrate-level defects are presented in this paper. New techniques such as inter-layer dielectric (ILD) thinning, high keV imaging, and XeF2 poly etch overflow are introduced. We describe these techniques as applied to two different defects types at FEOL. In the first case, by using ILD thinning and high keV imaging, coupled with focused ion beam (FIB) cross section and scanning transmission electron microscopy (STEM,) we were able to judge where to sample for TEM from a top down perspective while simultaneously providing the top down images giving both perspectives on the same sample. In the second case we show retention of the poly Si short after removal of CoSi2 formation on poly. Removal of the CoSi2 exposes the poly Si such that we can utilize XeF2 to remove poly without damaging gate oxide to reveal pinhole defects in the gate oxide. Overall, using these techniques have led to 1) increased chances of successfully finding the defects, 2) better characterization of the defects by having a planar view perspective and 3) reduced time in localizing defects compared to performing cross section alone.


Author(s):  
X. Yang ◽  
X. Song

Abstract Novel Focused Ion Beam (FIB) voltage-contrast technique combined with TEM has been used in this study to identify a certain subtle defect mechanism that caused reliability stress failures of a new product. The suspected defect was first isolated to a unique via along the row through electrical testing and layout analysis. Static voltage contrast of FIB cross-section was used to confirm the suspected open defect at the via. Precision Transmission Electron Microscope (TEM) was then used to reveal the detail of the defect. Based on the result, proper process changes were implemented. The failure mode was successfully eliminated and the reliability of the product was greatly improved.


2019 ◽  
Author(s):  
Genevieve Buckley ◽  
Gediminas Gervinskas ◽  
Cyntia Taveneau ◽  
Hari Venugopal ◽  
James C. Whisstock ◽  
...  

AbstractCryo-transmission electron tomography (cryo-ET) in association with cryo-focused ion beam (cryo-FIB) milling enables structural biology studies to be performed directly within the cellular environment. Cryo-preserved cells are milled and a lamella with a thickness of 200-300 nm provides an electron transparent window suitable for cryo-ET imaging. Cryo-FIB milling is an effective method, but it is a tedious and time-consuming process, which typically results in ~10 lamellae per day. Here, we introduce an automated method to reproducibly prepare cryo-lamellae on a grid and reduce the amount of human supervision. We tested the routine on cryo-preserved Saccharomyces cerevisiae and demonstrate that this method allows an increased throughput, achieving a rate of 5 lamellae/hour without the need to supervise the FIB milling. We demonstrate that the quality of the lamellae is consistent throughout the preparation and their compatibility with cryo-ET analyses.


2011 ◽  
Vol 17 (6) ◽  
pp. 889-895 ◽  
Author(s):  
Lynne M. Gignac ◽  
Surbhi Mittal ◽  
Sarunya Bangsaruntip ◽  
Guy M. Cohen ◽  
Jeffrey W. Sleight

AbstractThe ability to prepare multiple cross-section transmission electron microscope (XTEM) samples from one XTEM sample of specific sub-10 nm features was demonstrated. Sub-10 nm diameter Si nanowire (NW) devices were initially cross-sectioned using a dual-beam focused ion beam system in a direction running parallel to the device channel. From this XTEM sample, both low- and high-resolution transmission electron microscope (TEM) images were obtained from six separate, specific site Si NW devices. The XTEM sample was then re-sectioned in four separate locations in a direction perpendicular to the device channel: 90° from the original XTEM sample direction. Three of the four XTEM samples were successfully sectioned in the gate region of the device. From these three samples, low- and high-resolution TEM images of the Si NW were taken and measurements of the NW diameters were obtained. This technique demonstrated the ability to obtain high-resolution TEM images in directions 90° from one another of multiple, specific sub-10 nm features that were spaced 1.1 μm apart.