scholarly journals INCREASING IN IMPACT VISCOSITY OF FIBER-ASH-CONCRETE

2021 ◽  
Vol 3 (6) ◽  
pp. 5-16
Author(s):  
R. Fedyuk ◽  
Yu. Liseycev ◽  
A. Taskin ◽  
R. Timohin ◽  
Sergey Klyuev ◽  
...  

The trend in building materials science is to replace the different proportions of Portland cement in the binder. Therefore, the paper proposes the principles of controlling the static and dynamic strength of fiber-reinforced concrete, consisting in the complex effect of the hydro-removed ash and slag mix and basalt fiber on the processes of structure formation of the cement composite. A four-stage purification system for the hydro-removed ash and slag mixture has been developed, including disintegration, flotation and two-stage magnetic separation. It was found that the density of the fresh mix from the dose behaves naturally, and the density of solid samples at low doses slightly decreases. High early strength of the developed composites is noted, in particular, for specimens with ASM, one and a half increase in compressive strength is traced in comparison with non-additive specimens. Combinations of "fiber + ASM" with a quadrupling of strength have a significant effect on bending strength. Successful approximations of the compressive strength and bending strength on the ASM dose for different ages (1, 7, 28 days) are traced with the regular behavior of the coefficients in the power dependences. Revealed a multiple increase in the impact strength of the developed compositions. The use of the results will lead to the possibility of designing high-strength concretes, including for special structures.

2021 ◽  
Vol 887 ◽  
pp. 415-421
Author(s):  
V. Ezerskiy ◽  
N.V. Kuznetsova ◽  
A.D. Seleznev

The object of study is a cement composite material with powdered utilized optical discs. The objective is to establish the dependences of the main strength characteristics – com-pressive strength, bending strength, and density – on the amount of waste added into the mix-ture and the water-cement ratio.The compositions of the mixtures for the production of the cement composite material samples consisted of the following components: cement, sand, powdered waste in the form of utilized optical discs and water.Based on the results of testing the samples, mathematical models have been developed which describe the dependences of the physical and mechanical properties of the cement com-posite material samples on the fraction of waste and water-cement ratio. It was found that with an increase in the amount of powdered waste added into the mixture, it reduces the compressive strength, bending strength, and density of the samples under study, however, the optimization of the water-cement ratio makes it possible to obtain equal strength compositions with a differ-ent fraction of waste.Component compositions of cement composite material mixtures with the addition of powdered utilized optical discs in the amount of 10 to 25 % of the total filler mass, which can provide construction products with a compressive strength class B20, are presented.


2020 ◽  
Vol 91 (5) ◽  
pp. 125-132
Author(s):  
A.D. SELEZNEV ◽  
◽  
N.V. KUZNETSOVA ◽  
V.A. EZERSKIY ◽  
◽  
...  

The object of study is a cement composite material with powdered utilized optical discs. The objective is to establish the dependences of the main strength characteristics – compressive strength, bending strength, and density – on the amount of waste added into the mixture and the water-cement ratio. The compositions of the mixtures for the production of the cement composite material samples consisted of the following components: cement, sand, powdered waste in the form of utilized optical discs and water. Based on the results of testing the samples, mathematical models have been developed which describe the dependences of the physical and mechanical properties of the cement composite material samples on the fraction of waste and water-cement ratio. It was found that with an increase in the amount of powdered waste added into the mixture, it reduces the compressive strength, bending strength, and density of the samples under study, however, the optimization of the water-cement ratio makes it possible to obtain equal strength compositions with a different fraction of waste. Component compositions of cement composite material mixtures with the addition of powdered utilized optical discs in the amount of 10 to 25 % of the total filler mass, which can provide construction products with a compressive strength class B20, are presented.


2020 ◽  
Vol 14 (2) ◽  
pp. 6734-6742
Author(s):  
A. Syamsir ◽  
S. M. Mubin ◽  
N. M. Nor ◽  
V. Anggraini ◽  
S. Nagappan ◽  
...  

This study investigated the combine effect of 0.2 % drink cans and steel fibers with volume fractions of 0%, 0.5%, 1%, 1.5%, 2%, 2.5% and 3% to the mechanical properties and impact resistance of concrete. Hooked-end steel fiber with 30 mm and 0.75 mm length and diameter, respectively was selected for this study.  The drinks cans fiber were twisted manually in order to increase friction between fiber and concrete. The results of the experiment showed that the combination of steel fibers and drink cans fibers improved the strength performance of concrete, especially the compressive strength, flexural strength and indirect tensile strength. The results of the experiment showed that the combination of steel fibers and drink cans fibers improved the compressive strength, flexural strength and indirect tensile strength by 2.3, 7, and 2 times as compare to batch 1, respectively. Moreover, the impact resistance of fiber reinforced concrete has increase by 7 times as compared to non-fiber concretes. Moreover, the impact resistance of fiber reinforced concrete consistently gave better results as compared to non-fiber concretes. The fiber reinforced concrete turned more ductile as the dosage of fibers was increased and ductility started to decrease slightly after optimum fiber dosage was reached. It was found that concrete with combination of 2% steel and 0.2% drink cans fibers showed the highest compressive, split tensile, flexural as well as impact strength.    


Buildings ◽  
2021 ◽  
Vol 11 (3) ◽  
pp. 82
Author(s):  
Salmabanu Luhar ◽  
Demetris Nicolaides ◽  
Ismail Luhar

Even though, an innovative inorganic family of geopolymer concretes are eye-catching potential building materials, it is quite essential to comprehend the fire and thermal resistance of these structural materials at a very high temperature and also when experiencing fire with a view to make certain not only the safety and security of lives and properties but also to establish them as more sustainable edifice materials for future. The experimental and field observations of degree of cracking, spalling and loss of strength within the geopolymer concretes subsequent to exposure at elevated temperature and incidences of occurrences of disastrous fires extend an indication of their resistance against such severely catastrophic conditions. The impact of heat and fire on mechanical attributes viz., mechanical-compressive strength, flexural behavior, elastic modulus; durability—thermal shrinkage; chemical stability; the impact of thermal creep on compressive strength; and microstructure properties—XRD, FTIR, NMR, SEM as well as physico-chemical modifications of geopolymer composites subsequent to their exposures at elevated temperatures is reviewed in depth. The present scientific state-of-the-art review manuscript aimed to assess the fire and thermal resistance of geopolymer concrete along with its thermo-chemistry at a towering temperature in order to introduce this novel, most modern, user and eco-benign construction materials as potentially promising, sustainable, durable, thermal and fire-resistant building materials promoting their optimal and apposite applications for construction and infrastructure industries.


2014 ◽  
Vol 567 ◽  
pp. 381-386 ◽  
Author(s):  
Nasir Shafiq ◽  
Muhd Fadhil Nuruddin ◽  
Ali Elheber Ahmed Elshekh ◽  
Ahmed Fathi Mohamed Salih

In order to improve the mechanical properties of high strength concrete, HSC, several studies have been conducted using fly ash, FA. Researchers have made it possible to achieve 100-150MPa high strength concrete. Despite the popularity of this FAHSC, there is a major shortcoming in that it becomes more brittle, resulting in less than 0.1% tensile strain. The main objective of this work was to evaluate the fresh and hardened properties of FAHSC utilizing chopped basalt fiber stands, CBFS, as an internal strengthening addition material. This was achieved through a series of experimental works using a 20% replacement of cement by FA together with various contents of CBFS. Test results of concrete mixes in the fresh state showed no segregation, homogeneousness during the mixing period and workability ranging from 60 to 110 mm. Early and long terms of compressive strength did not show any improvement by using CBFS; in fact, it decreased. This was partially substituted by the effect of FA. Whereas, the split and flexural strengths of FASHC were significantly improved with increasing the content of CBFS as well as the percentage of the split and flexural tensile strength to the compressive strength. Also, test results showed a progressive increase in the areas under the stress-strain curves of the FAHSC strains after the CBFS addition. Therefore, the brittleness and toughness of the FAHSC were enhanced and the pattern of failure moved from brittle failure to ductile collapse using CBFS. It can be considered that the CBFS is a suitable strengthening material to produce ductile FAHSC.


Author(s):  
Vera V. Galishnikova ◽  
Alireza Heidari ◽  
Paschal C. Chiadighikaobi ◽  
Adegoke Adedapo Muritala ◽  
Dafe Aniekan Emiri

Relevance. The load on a reinforced concrete slab with high strength lightweight aggregate concrete leads to increased brittleness and contributes to large deflection or flexure of slabs. The addition of fibers to the concrete mix can improve its mechanical properties including flexure, deformation, toughness, ductility, and cracks. The aims of this work are to investigate the flexure and ductility of lightweight expanded clay concrete slabs reinforced with basalt fiber polymers, and to check the effects of basalt fiber mesh on the ductility and flexure. Methods. The ductility and flexural/deflection tests were done on nine engineered cementitious composite (expanded clay concrete) slabs with dimensions length 1500 mm, width 500 mm, thickness 65 mm. These nine slabs are divided in three reinforcement methods types: three lightweight expanded clay concrete slab reinforced with basalt rebars 10 mm (first slab type); three lightweight expanded clay concrete slab reinforced with basalt rebars 10 mm plus dispersed chopped basalt fiber plus basalt fiber polymer (mesh) of cells 2525 mm (second slab type); three lightweight expanded clay concrete slab reinforced with basalt rebars 10 mm plus dispersed basalt fiber of length 20 mm, diameter 15 m (third slab type). The results obtained showed physical deflection of the three types of slab with cracks. The maximum flexural load for first slab type is 16.2 KN with 8,075 mm deflection, second slab type is 24.7 KN with 17,26 mm deflection and third slab type 3 is 32 KN with 15,29 mm deflection. The ductility of the concrete slab improved with the addition of dispersed chopped basalt fiber and basalt mesh.


Author(s):  
V. Nelyubova ◽  
V. Babaev ◽  
Nataliya Alfimova ◽  
S. Usikov ◽  
O. Masanin

fiber concrete is one of the types of effective building materials that ensure the operational reliability of structures due to a set of unique properties. However, the maximum physicomechanical characteristics of this type of products are achieved only if the fiber is evenly distributed in the concrete matrix and the optimum ratio of raw materials is reached. In this connection, the aim of the work was to increase the production efficiency of fiber-reinforced concrete by optimizing the formulation and technological parameters of its manufacture. The optimal method of introducing the fiber into the concrete mix and the type of superplasticizer were previously determined, which allowed ensuring the maximum physicomechanical characteristics of the products. Optimization of prescription parameters was carried out using the method of mathematical planning of the experiment, where the amount of cement, superplasticizer and basalt fiber were varied. After processing the results, the dependences of the compressive strength on variable factors were obtained, which would allow to select the optimal dosages of raw materials for given mechanical characteristics of the products.


2020 ◽  
Vol 2020 ◽  
pp. 1-16
Author(s):  
Zhishu Yao ◽  
Yu Fang ◽  
Weihao Kong ◽  
Xianwen Huang ◽  
Xuesong Wang

In order to study the static and dynamic mechanical characteristics of the coal gangue concrete used in the mine support structure, the compressive strength test, the drop weight impact test, and the Split Hopkinson Pressure Bar (SHPB) test were conducted. The compressive strength, initial and final impacting energy, dynamic strength, and failure characteristic of concrete were obtained of the concrete single-doped with coal gangue coarse aggregate, single-doped with coal gangue fine aggregate, and codoped with coal gangue coarse and fine aggregates. The results show that (1) it is feasible that employing coal gangue to replace natural coarse and fine aggregates in concrete can prepare C30 and C40 concrete; (2) the addition of coal gangue fine aggregate has a positive effect on the impact energy of the initial and final cracks of concrete, while the addition of coal gangue coarse aggregate has a negative effect on it; (3) compared with the static strength, the dynamic strength of concrete is improved no matter whether coal gangue is added to concrete; (4) the incorporation of coal gangue coarse aggregate will make the concrete shear surface smooth; (5) at the given impacting pressure, the concrete with coal gangue coarse aggregate has greater particle breakage and those with coal gangue fine aggregate has less. The research of this study can be a reference for the application of gangue concrete in mine support structures.