ABSTRACTThis manuscript discusses the morphological instability observed when multilayered samples with alternating layers of Γ-Ni(Al)/γ-Ni3Al are exposed to 800C for approximately 100 hours. Samples with 20nm/20nm or 120nm/120nm layer thickness and <001> or <Ill> crystal orientation to the interface normal were tested. Pinching off of layers is strongly affected by crystal orientation and layer thickness. Corresponding modeling suggests that the stability of this system is sensitive to fluctuations in the volume fraction of the two phases, the aspect ratio of columnar grains in the layers, and whether coherent or semi-coherent interfaces are present.

Author(s):  
H. Kung ◽  
A.J. Griffin ◽  
Y.C. Lu ◽  
K.E. Sickafus ◽  
T.E. Mitchell ◽  
...  

Materials with compositionally modulated structures have gained much attention recently due to potential improvement in electrical, magnetic and mechanical properties. Specifically, Cu-Nb laminate systems have been extensively studied mainly due to the combination of high strength, and superior thermal and electrical conductivity that can be obtained and optimized for the different applications. The effect of layer thickness on the hardness, residual stress and electrical resistivity has been investigated. In general, increases in hardness and electrical resistivity have been observed with decreasing layer thickness. In addition, reduction in structural scale has caused the formation of a metastable structure which exhibits uniquely different properties. In this study, we report the formation of b.c.c. Cu in highly textured Cu/Nb nanolayers. A series of Cu/Nb nanolayered films, with alternating Cu and Nb layers, were prepared by dc magnetron sputtering onto Si {100} wafers. The nominal total thickness of each layered film was 1 μm. The layer thickness was varied between 1 nm and 500 nm with the volume fraction of the two phases kept constant at 50%. The deposition rates and film densities were determined through a combination of profilometry and ion beam analysis techniques. Cross-sectional transmission electron microscopy (XTEM) was used to examine the structure, phase and grain size distribution of the as-sputtered films. A JEOL 3000F high resolution TEM was used to characterize the microstructure.


2015 ◽  
Vol 83 (3) ◽  
Author(s):  
Zhiling Bai ◽  
Yewang Su ◽  
Baohua Ji

The nanostructure of biological materials is built with hard mineral crystals embedded in soft protein matrix in a staggered manner. The staggered arrangement of the crystals is assumed to be critically important for the stability of the nanostructure. But the mechanism is not fully understood. In this paper, a mechanical model, considering the effects of overlapping ratio between the crystals, i.e., the staggering position, is developed for analyzing the buckling behaviors of the nanostructure. It is found that the buckling strength increases with the overlapping ratio λ in the range of 0–1/2 and reaches a peak value at λ = 1/2 that is generally adopted by nature's design of the biological materials. The effect of aspect ratio and volume fraction of mineral crystals are further analyzed at various overlapping ratios, and the results are in general consistent with previous studies for the case of λ = 1/2. In addition, the lower and upper limits of the buckling strength are obtained. Finally, we show that the contact between mineral tips can significantly enhance the buckling strength of the nanostructure when the aspect ratio of minerals is small.


Author(s):  
H. Q. Ye ◽  
T.S. Xie ◽  
D. Li

The Ti3Al intermetallic compound has long been recognized as potentially useful structural materials. It offers attractive strength to weight and elastic modulus to weight ratios. Recent work has established that the addition of Nb to Ti3Al ductilized this compound. In this work the fundamental problem of this alloy, i.e. order-disorder and antiphase domain structures was investigated at the atomic scale.The Ti3Al+10at%Nb alloys used in this study were treated at 1060°C and then aged at 700°C for 2 hours. The specimens suitable for TEM were prepared by standard jet electrolytic-polishing technique. A JEM-200CX electron microscope with an interpretable resolution of about 0.25 nm was used for HREM.The [100] and [001] projections of the α2 phase were shown in Fig.l.The alloy obtained consist of at least two phases-α2(Ti3Al) and β0 structures. Moreover, a disorder α phase with small volume fraction was also observed. Fig.2 gives [100] and [001] diffraction patterns of the α2 phase. Since lattice parameters of the ordered α2 (a=0.579, c=0.466 nm) and disorder α phase (a0=0.294≈a/2, c0=0.468 nm) are almost the same, their diffraction patterns are difficult to be distinguished when they are overlapped with epitaxial orientation relationships.


2021 ◽  
Vol 13 (9) ◽  
pp. 5086
Author(s):  
Fatih Selimefendigil ◽  
Hakan F. Oztop ◽  
Ali J. Chamkha

Single and double impinging jets heat transfer of non-Newtonian power law nanofluid on a partly curved surface under the inclined magnetic field effects is analyzed with finite element method. The numerical work is performed for various values of Reynolds number (Re, between 100 and 300), Hartmann number (Ha, between 0 and 10), magnetic field inclination (γ, between 0 and 90), curved wall aspect ratio (AR, between 01. and 1.2), power law index (n, between 0.8 and 1.2), nanoparticle volume fraction (ϕ, between 0 and 0.04) and particle size in nm (dp, between 20 and 80). The amount of rise in average Nusselt (Nu) number with Re number depends upon the power law index while the discrepancy between the Newtonian fluid case becomes higher with higher values of power law indices. As compared to case with n = 1, discrepancy in the average Nu number are obtained as −38% and 71.5% for cases with n = 0.8 and n = 1.2. The magnetic field strength and inclination can be used to control the size and number or vortices. As magnetic field is imposed at the higher strength, the average Nu reduces by about 26.6% and 7.5% for single and double jets with n greater than 1 while it increases by about 4.78% and 12.58% with n less than 1. The inclination of magnetic field also plays an important role on the amount of enhancement in the average Nu number for different n values. The aspect ratio of the curved wall affects the flow field slightly while the average Nu variation becomes 5%. Average Nu number increases with higher solid particle volume fraction and with smaller particle size. At the highest particle size, it is increased by about 14%. There is 7% variation in the average Nu number when cases with lowest and highest particle size are compared. Finally, convective heat transfer performance modeling with four inputs and one output is successfully obtained by using Adaptive Neuro-Fuzzy Interface System (ANFIS) which provides fast and accurate prediction results.


Membranes ◽  
2021 ◽  
Vol 11 (1) ◽  
pp. 58
Author(s):  
Ali Zamani ◽  
F. Handan Tezel ◽  
Jules Thibault

Membrane-based processes are considered a promising separation method for many chemical and environmental applications such as pervaporation and gas separation. Numerous polymeric membranes have been used for these processes due to their good transport properties, ease of fabrication, and relatively low fabrication cost per unit membrane area. However, these types of membranes are suffering from the trade-off between permeability and selectivity. Mixed-matrix membranes, comprising a filler phase embedded into a polymer matrix, have emerged in an attempt to partly overcome some of the limitations of conventional polymer and inorganic membranes. Among them, membranes incorporating tubular fillers are new nanomaterials having the potential to transcend Robeson’s upper bound. Aligning nanotubes in the host polymer matrix in the permeation direction could lead to a significant improvement in membrane permeability. However, although much effort has been devoted to experimentally evaluating nanotube mixed-matrix membranes, their modelling is mostly based on early theories for mass transport in composite membranes. In this study, the effective permeability of mixed-matrix membranes with tubular fillers was estimated from the steady-state concentration profile within the membrane, calculated by solving the Fick diffusion equation numerically. Using this approach, the effects of various structural parameters, including the tubular filler volume fraction, orientation, length-to-diameter aspect ratio, and permeability ratio were assessed. Enhanced relative permeability was obtained with vertically aligned nanotubes. The relative permeability increased with the filler-polymer permeability ratio, filler volume fraction, and the length-to-diameter aspect ratio. For water-butanol separation, mixed-matrix membranes using polydimethylsiloxane with nanotubes did not lead to performance enhancement in terms of permeability and selectivity. The results were then compared with analytical prediction models such as the Maxwell, Hamilton-Crosser and Kang-Jones-Nair (KJN) models. Overall, this work presents a useful tool for understanding and designing mixed-matrix membranes with tubular fillers.


2015 ◽  
Vol 11 (1) ◽  
pp. 105-113 ◽  
Author(s):  
Maher Trigui ◽  
Karim Gabsi ◽  
Walid Zneti ◽  
Suzelle Barrington ◽  
Ahmed Noureddine Helal

Abstract In this study, Bioconversion process of glucose to fructose from date syrup using Escherichia coli K12 is modeled using a commercial computational fluids dynamics (CFD) code fluent FLUENT 6.3.23 [8] which we implemented a user-defined functions (UDF) to simulate the interrelationships at play between various phases. A two phases CFD model was developed using an Eulerian – Eulerian approach to calculate the fructose volume fraction produced during time. The bioconversion process was studied as function of three initial concentration of glucose (0.14, 0.242 and 0.463gL–1), three induction time (60, 120 and 180 mn) and three inoculum volume (100, 120 and 150mL). The numerical results are compared with experimental data for bioconversion rate and show good agreement (R2= 0.894). The optimal condition of diffusion was obtained by applying an initial concentration of glucose less than 0.2gL–1 and induction time great than 100 minutes.


1995 ◽  
Vol 4 (1) ◽  
pp. 096369359500400
Author(s):  
T.D. Papathanasiou

The predictions of the Halpin equation concerning the effect of fibre volume fraction and fibre aspect ratio on the effective tensile modulus of uniaxially aligned short-fibre composites are compared with computational experiments on three-dimensional, multiparticle composite samples. The method of boundary elements is used to model the mechanical behaviour of composite specimens consisting of up to 40 discrete aligned fibres randomly dispersed in an elastic matrix. Statistical averages of computational results relating the effective tensile modulus to the aspect ratio and volume fraction of the fibres are found to agree very well with the predictions of the Halpin equation for fibre aspect ratio up to 10 and fibre volume fractions up to 20%. Computational results seem to indicate that the predictions of the Halpin equation fall bellow those of micro-mechanical models at higher volume fractions.


1994 ◽  
Vol 343 ◽  
Author(s):  
C. M. Scanlan ◽  
M. D. Wiggins ◽  
M. Gajdardziska-Josifovska ◽  
C. R. Aita

ABSTRACTThe mechanical properties of zirconia are known to be a function of phase composition. We show here that a nanolaminate geometry can be used to control the phase composition of zirconia films. The experiment consisted of growth of nanoscale multilayer films (nanolaminates) of polycrystalline zirconia and amorphous alumina by reactive sputter deposition on Si (111) and fused silica substrates. The films were characterized using x-ray diffraction and high resolution electron microscopy. The results show that both monoclinic (m) and tetragonal (t) zirconia polymorphs were formed in the zirconia layers. Most crystallites are oriented with either close-packed {111}-t or {111}-m planes parallel to the substrate. The volume fraction of tetragonal zirconia, the desired phase for transformation-toughening behavior, increases with decreasing zirconia layer thickness. Nanolaminates with a volume fraction of tetragonal zirconia exceeding 0.8 were produced without the addition of a stabilizing dopant, and independent of the kinetic factors that limit tetragonal zirconia growth in pure zirconia films.