Phase, microstructure, and wear behavior of Al2O3-reinforced Fe–Si alloy-based metal matrix nanocomposites

Author(s):  
Akash Saxena ◽  
Neera Singh ◽  
Bhupendra Singh ◽  
Devendra Kumar ◽  
Kishor Kumar Sadasivuni ◽  
...  

In the present work, phase, microstructure, and wear properties of Al2O3-reinforced Fe–Si alloy-based metal matrix nanocomposites have been studied. Composites using 2 wt.% and 5 wt.% of Si and rest Fe powder mix were synthesized via powder metallurgy and sintered at different temperature schedules. Iron–silicon alloy specimens were found to have high hardness and high wear resistance in comparison to pure iron specimens. Addition of 5 wt.% and 10 wt.% alumina reinforcement in Fe–Si alloy composition helped in developing iron aluminate (FeAl2O4) phase in composites which further improved the mechanical properties i.e. high hardness and wear resistance. Formation of iron aluminate phase occurs due to reactive sintering between Fe and Al2O3 particles. It is expected that the improved behavior of prepared nanocomposites as compared to conventional metals will be helpful in finding their use for wide industrial applications.

2021 ◽  
Vol 118 (6) ◽  
pp. 614
Author(s):  
Chellamuthu Ramesh Kumar ◽  
Subramanian Baskar ◽  
Ganesan Ramesh ◽  
Pathinettampadian Gurusamy ◽  
Thirupathy Maridurai

In this research, investigations were carried out on Al6061 base alloy with the changing weight percentage of silicon carbide (SiC) and boron carbide (B4C) with keeping the amount of talc constant. The main objective of this present study was to improve the wear resistance of aluminum alloy using SiC/B4C/talc ceramic particles using stir-casting technique and how the eco-friendly talc content influencing the solid lubricity during the abrasion process. The experiments were conducted via orthogonal array of L27 using Taguchi’s method. The optimum value along with the coefficient of friction was obtained on the basis of grey relational equations and ANOVA, which helped in analysis of most influential input parameters such as applied load, sliding speed, sliding distance and percentage of reinforcement. Conformation tests were performed for the purpose of validation of the experimental results. The specimens were analyzed using scanning electron microscope (SEM) with EDX for micro structural studies. The SiC, B4C and talc presence in the composite helped to improve the mechanical properties, according to the results. The presence of solid lubricant talc as reinforcement to the aluminum hybrid composite reduced the wear properties and decreased the co-efficient friction. These wear resistance improved aluminum metal matrix composites could be used in automobile, defense and domestic applications where high strength and wear resistance required with lesser specific weight.


Author(s):  
Quinton Porter ◽  
Zhijian Pei ◽  
Chao Ma

Abstract The ability to produce a dense part of Al-based metal matrix nanocomposites using binder jetting followed by infiltration was investigated. A green density above 1.58 g/cm3 was determined to be necessary for spontaneous direct liquid infiltration to commence, and a press-compaction-assisted binder jetting process is needed to achieve this benchmark. A green density of 1.64±0.02 g/cm3 only resulted in a density of 1.65±0.03 g/cm3 by sintering at 1050 °C, which showed that densification is not possible with sintering alone. However, infiltration with Al-6061 produced specimens with a density of 2.74±0.04 g/cm3, which corresponded to a density improvement of 65%. Moreover, the infiltrated specimens had a low open porosity of 2.71±0.95% and a high hardness of 54 HRA. This study suggests that it is feasible to manufacture parts with complex shapes and superior mechanical properties using binder Jetting followed by infiltration.


2018 ◽  
Vol 220 ◽  
pp. 441-448 ◽  
Author(s):  
Pallav Gupta ◽  
Devendra Kumar ◽  
Om Parkash ◽  
A.K. Jha ◽  
Kishor Kumar Sadasivuni

2014 ◽  
Vol 2014 ◽  
pp. 1-10 ◽  
Author(s):  
Pallav Gupta ◽  
Devendra Kumar ◽  
Om Parkash ◽  
A. K. Jha

The present paper reports the investigations on sintering and hardness behavior of Fe-Al2O3 Metal Matrix Nanocomposites (MMNCs) prepared by Powder Metallurgy (P/M) route with varying concentration of Al2O3 (5–30 wt%). The MMNC specimens for the present investigations were synthesized by ball milling, followed by compaction and sintering in an inert atmosphere in the temperature range of 900–1100°C for 1–3 hours using Powder Metallurgy route. Phase and microstructures of the specimens were characterized by XRD and SEM. Reactive sintering takes place in these materials. During sintering nano iron aluminate (FeAl2O4) phase forms. Characterization was done by measuring density and hardness. Results have been discussed critically to illustrate the effect of various processing parameters on sintering and mechanical behavior. It is expected that the results of these investigations will be useful in developing Metal Matrix Nanocomposites (MMNCs) for typical industrial applications.


Metals ◽  
2021 ◽  
Vol 11 (1) ◽  
pp. 125
Author(s):  
Seyed Kiomars Moheimani ◽  
Mehran Dadkhah ◽  
Mohammad Hossein Mosallanejad ◽  
Abdollah Saboori

Metal matrix nanocomposites (MMNCs) with high specific strength have been of interest for numerous researchers. In the current study, Mg matrix nanocomposites reinforced with AlN nanoparticles were produced using the mechanical stirring-assisted casting method. Microstructure, hardness, physical, thermal and electrical properties of the produced composites were characterized in this work. According to the microstructural evaluations, the ceramic nanoparticles were uniformly dispersed within the matrix by applying a mechanical stirring. At higher AlN contents, however, some agglomerates were observed as a consequence of a particle-pushing mechanism during the solidification. Microhardness results showed a slight improvement in the mechanical strength of the nanocomposites following the addition of AlN nanoparticles. Interestingly, nanocomposite samples were featured with higher electrical and thermal conductivities, which can be attributed to the structural effect of nanoparticles within the matrix. Moreover, thermal expansion analysis of the nanocomposites indicated that the presence of nanoparticles lowered the Coefficient of Thermal Expansion (CTE) in the case of nanocomposites. All in all, this combination of properties, including high mechanical strength, thermal and electrical conductivity, together with low CTE, make these new nanocomposites very promising materials for electro packaging applications.


Metals ◽  
2021 ◽  
Vol 11 (7) ◽  
pp. 1034
Author(s):  
Massoud Malaki ◽  
Alireza Fadaei Tehrani ◽  
Behzad Niroumand ◽  
Manoj Gupta

Metal matrix composites (MMCs) have been developed in response to the enormous demand for special industrial materials and structures for automotive and aerospace applications, wherein both high-strength and light weight are simultaneously required. The most common, inexpensive route to fabricate MMCs or metal matrix nanocomposites (MMNCs) is based on casting, wherein reinforcements like nanoceramics, -carbides, -nitrides, elements or carbon allotropes are added to molten metal matrices; however, most of the mentioned reinforcements, especially those with nanosized reinforcing particles, have usually poor wettability with serious drawbacks like particle agglomerations and therefore diminished mechanical strength is almost always expected. Many research efforts have been made to enhance the affinity between the mating surfaces. The aim in this paper is to critically review and comprehensively discuss those approaches/routes commonly employed to boost wetting conditions at reinforcement-matrix interfaces. Particular attention is paid to aluminum matrix composites owing to the interest in lightweight materials and the need to enhance the mechanical properties like strength, wear, or creep resistance. It is believed that effective treatment(s) may enormously affect the wetting and interfacial strength.