scholarly journals Development of seaweed-based bamboo microcrystalline cellulose films intended for sustainable food packaging applications

BioResources ◽  
2019 ◽  
Vol 14 (2) ◽  
pp. 3389-3410 ◽  
Author(s):  
D. Hermawan ◽  
Tze Kiat Lai ◽  
Shima Jafarzadeh ◽  
Deepu A. Gopakumar ◽  
Hasan M. ◽  
...  

Seaweed bio-composite films with different proportion of Lemang and Semantan bamboo microcrystalline cellulose (MCC) were fabricated via solvent casting. The seaweed/MCC composite films were flexible, transparent, and slightly yellow. The MCC particles further enhanced mechanical properties and opacity of films. The thermal stability of seaweed films was moderately improved upon addition of bamboo MCC particles. Bamboo MCC was found to be comparable to commercial MCC in reducing the water vapor permeability (WVP), water solubility (WS), and moisture absorption capacity (MSC) of seaweed films. The tensile strength (TS) of seaweed films was increased by 20 to 23% with addition of up to 5% MCC particles. In addition, bamboo MCC efficiently reduced the WVP of seaweed films comparable to commercial MCC particles. The WS of seaweed films was decreased by 10 to 19% with addition of 1% MCC particles loading. Lemang bamboo MCC (SB-MCC) was remarkably reduced the moisture absorption capacity (MAC) of films up to 25% with inclusion of only 1% MCC. Morphological analysis via Scanning Electron Microscopy (SEM) confirmed that there was homogeneous dispersion of MCC particles in the films. MCC particles improved the mechanical, thermal, and optical properties of seaweed films making them more suitable for food packaging applications.

Molecules ◽  
2021 ◽  
Vol 26 (9) ◽  
pp. 2569
Author(s):  
Mia Kurek ◽  
Nasreddine Benbettaieb ◽  
Mario Ščetar ◽  
Eliot Chaudy ◽  
Maja Repajić ◽  
...  

Chitosan and pectin films were enriched with blackcurrant pomace powder (10 and 20% (w/w)), as bio-based material, to minimize food production losses and to increase the functional properties of produced films aimed at food coatings and wrappers. Water vapor permeability of active films increased up to 25%, moisture content for 27% in pectin-based ones, but water solubility was not significantly modified. Mechanical properties (tensile strength, elongation at break and Young’s modulus) were mainly decreased due to the residual insoluble particles present in blackcurrant waste. FTIR analysis showed no significant changes between the film samples. The degradation temperatures, determined by DSC, were reduced by 18 °C for chitosan-based samples and of 32 °C lower for the pectin-based samples with blackcurrant powder, indicating a disturbance in polymer stability. The antioxidant activity of active films was increased up to 30-fold. Lightness and redness of dry films significantly changed depending on the polymer type. Significant color changes, especially in chitosan film formulations, were observed after exposure to different pH buffers. This effect is further explored in formulations that were used as color change indicators for intelligent biopackaging.


2013 ◽  
Vol 469 ◽  
pp. 156-161 ◽  
Author(s):  
Hong Pan ◽  
Dan Xu ◽  
Qin Liu ◽  
Hui Qing Ren ◽  
Min Zhou

Starch-based nanocomposite films were fabricated by the incorporation of different amounts of nanodiamond (ND) particles. These films were characterized by SEM, FT-IR, TGA, tensile testing and water vapor permeability measurement. It was observed that at low loadings, ND dispersed well in starch matrix. However, as the loading amount increased, aggregates as large as several micrometers appeared. The physical blending of ND with starch didnt change the thermal degradation mechanisms of starch films, only increased the char residues. As the ND loading increased, the tensile strength of composite films increased but the elongation at break decreased. However, the water vapor permeability increased as the loading of ND increased due to the increased microspores in films. With further modifications, ND may be considered as a novel of biocompatible nanofillers for reinforcement of biopolymers for food packaging applications.


Polymers ◽  
2021 ◽  
Vol 13 (24) ◽  
pp. 4406
Author(s):  
Anita Kwaśniewska ◽  
Michał Świetlicki ◽  
Adam Prószyński ◽  
Grzegorz Gładyszewski

In the present study, starch/powdered activated carbon composite films were prepared by incorporating various amounts of powdered activated carbon (PAC)—1–5, 10, and 15 %—into a starch matrix, using the solvent casting method. The effect of PAC addition on the biopolymer film was investigated. The mechanical properties were examined by ultra-nanoindentation, nanoscratch, and micro-tensile tests. Since the mechanical properties of biopolymer films are correlated with their structure, the effect of PAC addition was tested using X-ray diffraction. The surface parameters morphology and wettability were analyzed by atomic force microscopy (AFM) and contact angle measurements. The barrier properties were examined by determining water vapor permeability and the water solubility index. The obtained results did not show a monotonic dependence of the mechanical parameters on PAC content, with the exception of the maximum strain, which decreased as the amount of the additive increased. The visible effect of PAC addition was manifested in changes in the adhesive force value and in water vapor permeability (WVP). The barrier properties decreased with the increase of the filler content.


Marine Drugs ◽  
2019 ◽  
Vol 17 (12) ◽  
pp. 662
Author(s):  
Yongliang Zhuang ◽  
Shiyan Ruan ◽  
Hanghang Yao ◽  
Yun Sun

Different composite films composed of tilapia skin collagen (TSC) with Pachyrhizus starch (PS) or rambutan peel phenolics (RPP) were prepared, and the physical properties of these films were determined. The effects of PS and RPP on TSC films were investigated, and our results indicated that PS and RPP could improve the physical properties of TSC films. Opacity and film thickness showed an enhanced trend with increasing PS and RPP contents in TSC films, whereas solubility in water, elongation-at-break (EAB), and water vapor permeability (WVP) showed declining trends. TSC film with 10% PS and 0.5% RPP had the highest tensile strength, and the tensile strength dropped drastically when the content of PS and RPP increased. The light transmittances of the films could decrease with the incorporation of PS and RPP. Differential scanning calorimetry (DSC) demonstrated that the addition of PS and RPP improved the thermal stability of TSC films. In addition, X-ray diffraction indicated that the crystallinity of the films decreased and the amorphous structure of the films tended to become more complex with the addition of PS and RPP. As shown by fourier transform infrared spectroscopy (FTIR) analysis, PS and RPP can strongly interact with TSC, resulting in a modification of its structure. Scanning electron microscope (SEM) analysis showed that there was a good compatibility between TSC, PS, and RPP. The results indicated that TSC film incorporated with 10% PS and 0.5% RPP was an effective method for improve the physical properties of the film. TSC–PS–RPP composite films can be used not only in biomedical applications, but also as active food packaging materials.


Coatings ◽  
2021 ◽  
Vol 11 (2) ◽  
pp. 219
Author(s):  
Yining Wang ◽  
Jinhui Li ◽  
Xin Guo ◽  
Haisong Wang ◽  
Fang Qian ◽  
...  

Poor water-vapor barriers and mechanical properties are common problems of biobased films. To maintain food quality, the barrier and its strength performance need to be improved. Tea polyphenols (TP) are a natural active substance, and their benzene ring structure provides a barrier for them as a film material. Films that incorporate TP also have enriched functionalities, e.g., as antioxidants. Here, active poly (vinyl alcohol) (PVA)-hemicellulose (HC)/TP films with good moisture resistance and antioxidant capacity were prepared via ultrasound assistance. The effects of TP incorporation and ultrasonication on the physical, antioxidant, and micromorphological properties of the films were investigated. Results showed that the addition of TP improved the thermal stability and water-vapor permeability (WVP) of the composite films. When a PVA-HC/TP composite film with a PVA-HC to TP mass ratio of 100:10 was treated with ultrasonication for 45 min, tensile strength was 25.61 Mpa, which was increased by 54% from the film without any treatment, and water-vapor permeability (WVP) value declined from 49% to 4.29 × 10−12 g·cm/cm2·s·Pa. More importantly, the films’ DPPH scavenging activity increased to the maximal levels of 85.45%. In short, these observations create a feasible strategy for preparing high-performance biodegradable active-packaging films.


2021 ◽  
Vol 20 (2) ◽  
pp. 133-147
Author(s):  
Sajad Pirsa ◽  
Behzad Mohammadi

In this study, chitosan-polyaniline nanocomposite film was prepared in combination with different concentrations of polyaniline at various synthesis times. Surface morphology, antioxidant properties, water solubility, water vapor permeability (WVP), color properties and light transparency properties of the films were investigated. The size, shape and morphology of the synthesized particles were examined with scanning electron microscopy (SEM) technique. The results indicated that the synthesized polyaniline particles were spherical and in the range of 45–70 nm. The results obtained from the study of the effect of polyaniline on the physical properties of the chitosan film showed that increasing polyaniline concentration and synthesis time causes a decrease in the rate of the water solubility and water vapor permeability. This is an important factor in expanding its use in food packaging. The results of the colorimetric studies showed that the polyaniline sharply changed the surface color of the film. Polyaniline also increased antioxidant properties of composite film. Investigating the light transmission and transparency of the films showed that the polyaniline reduced the transparency and transmission of light, which could be used to package products that are susceptible to oxidation in the light.


Polymers ◽  
2018 ◽  
Vol 11 (1) ◽  
pp. 6 ◽  
Author(s):  
Rongfei Zhang ◽  
Xiangyou Wang ◽  
Juan Wang ◽  
Meng Cheng

In this study, the konjac glucomannan (KGM)/carrageenan (KC)/nano-silica film was prepared and characterized by scanning electron microscopy (SEM), Fourier-transform infrared spectroscopy (FTIR), and X-ray diffraction (XRD). The preservation quality of white mushrooms (Agaricus bisporus) packed using the films was also determined. The nano-silica dosage was found to affect the properties of the nanocomposite KGM/KC films. The results indicated that the properties of the films were significantly improved with the addition of nano-silica. The water vapor permeability, water solubility, moisture absorption, and light transmittance of KGM/KC/nano-silica films were significantly affected by the nano-silica dosage. In this study, the optimal nano-silica dosage to incorporate into the film in order to achieve excellent performance was 0.3%. Strong intermolecular hydrogen bonds were also observed between KGM/KC and nano-silica in the KGM/KC/nano-silica film by FTIR. In addition, the KGM/KC/nano-silica film markedly reduced the browning index, delayed the weight loss and softening, and extended the shelf life of mushrooms during storage at 4 °C. The KGM/KC film modified using nano-silica can provide a potential method for improving the preservation quality of white mushrooms during storage.


Coatings ◽  
2019 ◽  
Vol 9 (8) ◽  
pp. 525 ◽  
Author(s):  
Shiyi Feng ◽  
Feng Zhang ◽  
Saeed Ahmed ◽  
Yaowen Liu

In this study, PLA/TiO2 composites materials were prepared via electrospinning and solution casting processes. By testing the mechanical properties, water contact angle, water vapor permeability, and solubility of the composite nanofibers and films, the comprehensive performances of the two types of nanocomposites were analyzed. The results show that maximum tensile strengths of 2.71 ± 0.11 MPa and 14.49 ± 0.13 MPa were achieved for the nanofibers and films at a TiO2 content of 0.75 wt.%. Moreover, the addition of TiO2 significantly cut down the water vapor transmittance rate of the nanofibers and films while significantly improving the water solubility. Further, the antibacterial activity increased under UV-A irradiation for a TiO2 nanoparticle content of 0.75 wt.%, and the nanofiber and films exhibited inhibition zones of 4.86 ± 0.50 and 3.69 ± 0.40 mm for E. coli, and 5.98 ± 0.77 and 4.63 ± 0.45 mm for S. aureus, respectively. Overall, the performance of the nanofiber was better than that of the film. Nevertheless, both the nanocomposite membranes satisfied the requirements of food packaging materials.