The Dependence of Dielectric Properties on Composition Variation in Ba0.6Sr0.4(YTa)yTi1-2yO3

2002 ◽  
Vol 720 ◽  
Author(s):  
Daniel Potrepka ◽  
Steven Tidrow ◽  
Arthur Tauber ◽  
Kevin Kirchner ◽  
Matthew Ervin ◽  
...  

AbstractBa0.6Sr0.4(YTa)yTi1-2yO3 has been shown to have properties which are promising for tunable applications requiring low dielectric constant [1]. Ba0.6Sr0.4(YTa)yTi1-2yO3 with y ≤ 0.10 has been synthesized and well-characterized using x-ray diffraction, EDAX, and Raman Spectroscopy. The dependence of the dielectric properties on concentration, y, of Y and Ta are discussed along with implications for improved performance in device applications.

2021 ◽  
Vol 8 (7) ◽  
pp. 202365
Author(s):  
Andrea Nesterović ◽  
Jelena Vukmirović ◽  
Ivan Stijepović ◽  
Marija Milanović ◽  
Branimir Bajac ◽  
...  

The influence of different processing parameters and various Ba 2+ addition (up to 10 mol%) on the structure and dielectric properties of Bi 0.5 Na 0.5 TiO 3 -BaTiO 3 (BNT-BT) ceramics was investigated. The powders were hydrothermally synthesized in the alkaline environment at 180°C for different time periods. X-ray diffraction confirmed the presence of dominant rhombohedral Bi 0.5 Na 0.5 TiO 3 phase and a small amount of secondary pyrochlore Bi 2 Ti 2 O 7 phase in the pure BNT powders. In addition, one-dimensional Na 2 Ti 2 O 7 structure was also observed in the powder hydrothermally treated for a long time (i.e. 48 h). The amount of secondary pyrochlore phase in the BNT-BT powders increases with the increase of Ba 2+ content. The synthesized powders were pressed into pellets and finally sintered at various temperatures up to 1150°C. High density (more than 90%TD) was obtained in all BNT-BT sintered samples. Optimal sintering parameters were chosen in order to obtain dense ceramics with the optimal phase composition. The temperature dependence of dielectric properties for the BNT-BT ceramics was also studied. Relaxor behaviour of BNT-based ceramics and broad transition peaks are evident in all samples. Dielectric constant up to 400 as well as an acceptable low dielectric loss at temperatures lower than 200°C were obtained in BNT-BT ceramics.


RSC Advances ◽  
2016 ◽  
Vol 6 (26) ◽  
pp. 21662-21671 ◽  
Author(s):  
Weibing Dong ◽  
Yue Guan ◽  
Dejing Shang

To acquire low dielectric constant polyimide films with good mechanical and thermal properties and low CTE applied in microelectronic fields, three novel polyimides containing pyridine and –C(CF3)2– groups were firstly designed and synthesized.


2012 ◽  
Vol 512-515 ◽  
pp. 828-831 ◽  
Author(s):  
Wei Dong ◽  
Chang An Wang ◽  
Lei Yu ◽  
Shi Xi Ouyang

Porous Si3N4/SiO2/BN composite ceramics with high strength and low dielectric constant were prepared by dry-pressing process and pressureless sintering at 1750°C for 1.5 h in flow nitrogen. The influences of BN content on microstructure, porosity, mechanical and dielectric properties of the porous Si3N4/SiO2/BN composite ceramics were discussed. The results showed that the porous Si3N4/SiO2/BN composite ceramics with porosity ranging from 29% to 48% were fabricated by adjusting the content of BN. The flexural strength of the porous Si3N4/SiO2/BN composite ceramics was 78215 MPa. The dielectric constant of the porous Si3N4/SiO2/BN composite ceramics was 3.9~5 at 1 MHz.


2011 ◽  
Vol 700 ◽  
pp. 58-62
Author(s):  
Rachanusorn Roongtao ◽  
Supagorn Rugmai ◽  
Wanwilai C. Vittayakorn

The 0.98BaTiO3-0.02Ba (Mg1/3Nb2/3) O3ceramics has been synthesized through a conventional mixed-oxide by using BT nanopowder and BMN micropowder. The phase purity of the powders and the ceramics was examined using X-ray diffraction (XRD). The 0.98BT-0.02BMN powders were sintered to 92% of the theoretical density at a temperature of 1300 °C for 2 h. The microstructure of the sintered surface was investigated using scanning electron microscopy (SEM). The dielectric constant (εr) and loss factor (tanδ) of the sintered pellets at Curie temperture were 3000 and 0.015, respectively.


2018 ◽  
Vol 2018 (1) ◽  
pp. 000476-000482 ◽  
Author(s):  
Masao Tomikawa ◽  
Hitoshi Araki ◽  
Yohei Kiuchi ◽  
Akira Shimada

Abstract Progress of 5G telecommunication and mm radar for autopilot, high frequency operation is required. Insulator materials having low loss at high frequency is desired for the applications. We designed the low dielectric constant, and low dielectric loss materials examined molecular structure of the polyimide and found that permittivity 2.6 at 20GHz, dielectric loss 0.002. Furthermore, in consideration of mechanical properties such as the toughness and adhesion to copper from a point of practical use. Dielectric properties largely turned worse when giving photosensitivity. To overcome the poor dielectric properties, we designed the photosensitive system. After all, we successfully obtained 3.5 of dielectric constant and 0.004 of dielectric loss, and 100% of elongation at break. In addition, we offered a B stage sheet as well as varnish. These materials are applicable to re-distribution layer of FO-WLP, Interposer and other RF applications for microelectronics.


2011 ◽  
Vol 324 ◽  
pp. 298-301 ◽  
Author(s):  
Roy Jean Roukos ◽  
Olivier Bidault ◽  
Julien Pansiot ◽  
Ludivine Minier ◽  
Lucien Saviot

Lead free Na0.5Bi0.5TiO3 (NBT) and (Na0.5Bi0.5TiO3)1-x(CaTiO3)x (NBT-CT) piezoelectric ceramics with the perovskite structure were studied. The NBT and NBT-CT samples were synthesized using a solid-state reaction method and characterized with X-ray diffraction (XRD), Raman spectroscopy and dielectric measurements for several compositions (x = 0, 0.07, 0.15) at room temperature. The XRD analysis showed a stabilization of a rhombohedral phase at a low concentration of Ca (0 < x <0.15), whereas Raman spectra reveal a strong modification for the sample with x = 0.15. The dielectric properties of these ceramics were studied by measuring impedance in the 79-451K temperature range for unpoled and field cooling with an electric field (FC) conditions.


2013 ◽  
Vol 760-762 ◽  
pp. 705-708
Author(s):  
La Chen ◽  
Wei Li ◽  
Zhao Xian Xiong ◽  
Chun Xiao Song ◽  
Hong Qiu

Ceramics of (1-x)CaCu3Ti4O12-xBi2/3Cu3Ti4O12, i.e., CCTO-BCTO, with x=0, 0.01, 0.1 and 0.25, respectively, were prepared via the conventional solid-state reaction. The phase structure of the ceramics was identified by X-ray diffraction. The microstructure of the sample was observed with scanning electron microscopy. Dielectric properties and impedance spectroscopy were measured using a LCR Meter, in which 0.9CCTO-0.1BCTO displayed highest dielectric constant (584108) and lowest dielectric loss (0.42) at 1kHz among the four kinds of specimens. Based on series of experimental results, an optimum amount of x was able to improve the dielectric properties of CCTO-BCTO, through adjusting the impedance characteristics of the grain and grain boundary.


2013 ◽  
Vol 03 (04) ◽  
pp. 1350028 ◽  
Author(s):  
P. Thomas ◽  
K. B. R. Varma

CaCu 3 Ti 4 O 12 (CCTO) ceramics which has perovskite structure gained considerable attention due to its giant permittivity. But it has high tan δ (0.1 at 1 kHz) at room temperature, which needs to be minimized to the level of practical applications. Hence, TeO 2 which is a good glass former has been deliberately added to CCTO nanoceramic (derived from the oxalate precursor route) to explore the possibility of reducing the dielectric loss while maintaining the high permittivity. The structural, morphological and dielectric properties of the pure CCTO and TeO 2 added ceramics were studied using X-ray diffraction, Scanning Electron Microscope along with Energy Dispersive X-ray Analysis (EDX), spectroscopy and Impedance analyzer. For the 2.0 wt.% TeO 2 added ceramics, there is a remarkable difference in the microstructural features as compared to that of pure CCTO ceramics. This sample exhibited permittivity values as high as 7387 at 10 KHz and low dielectric loss value of 0.037 at 10 kHz, which can be exploited for the high frequency capacitors application.


1986 ◽  
Vol 72 ◽  
Author(s):  
G. V. Chandrashekhar ◽  
M. W. Shafer

AbstractDielectric properties have been measured for a series of porous and fully densified silica glasses, prepared by the sol-gel technique starting from Si-methoxide or Si-fume. The results for the partially densified glasses do not show any preferred orientation for porosity. When fully densified (˜2.25 gms/cc) without any prior treatment of the gels, they have dielectric constants of ≥ 6.5 and loss factors of 0.002 at 1 MHz, compared to values of 3.8 and <0.001 for commercial fused silica. There is no corresponding anomaly in the d.c. resistivity. Elemental carbon present to the extent of 400–500 ppm is likely to be the main cause for this enhanced dielectric constant. Extensive cleaning of the gels prior to densification to remove this carbon were not completely successful pointing to the difficulty in preparing high purity, low dielectric constant glasses via the organic sol-gel route at least in the bulk form.


Sign in / Sign up

Export Citation Format

Share Document