scholarly journals SINTESIS ESTER SELULOSA STEARAT SEBAGAI WET STRENGTH AGENT UNTUK PAPERBAG DARI TANDAN KOSONG SAWIT (TKS)

2021 ◽  
Vol 1 (3) ◽  
pp. 63
Author(s):  
Angga Tri Agusna PA ◽  
Zainuddin Ginting ◽  
Azhari Azhari ◽  
Rozanna Dewi ◽  
Zulnazri Zulnazri
Keyword(s):  

Tandan kosong kelapa sawit (TKS) adalah salah satu produk samping (by-product) berupa padatan dari industri pengolahan kelapa sawit. Kandungan selulosa yang cukup tinggi yaitu sebesar 40% menjadikan Tandan Kosong Sawit sebagai alternatif lain untuk dimanfaatkan Selulosa sebagai bahan baku pembuatan Ester Selulosa stearat. Ester Selulosa Stearat disintesa melalui reaksi transesterifikasi antara α-Selulosa hasil isolasi dari Tandan Kosong Sawit (TKS) dengan metil stearat. Sintesa Metil stearat dilakukan dengan mereaksikan metanol dan asam stearat dengan bantuan katalis H2SO4(p). Sintesis Ester selulosa stearat dilakukan dengan cara refluks selama 2 jam menggunakan pelarut metanol dengan variasi katalis Na2CO3 5, 10, 15, 20 mg dan dengan variasi volume metil stearat 5, 10, 15. Dan diambil variasi terbaik ditentukan berdasarkan uji derajat substitusi yaitu dengan variasi katalis Na2CO3 20 mg dan volume metil Stearat 15 ml, sebesar 1,95. Hasil sintesis yaitu selulosa stearat diuji gugus fungsi dengan spektroskopi FT-IR dan morfologi permukaan menggunakan SEM. Terbentuknya selulosa stearat didukung oleh spektrum FT-IR pada daerah bilangan gelombang 3468,01 cm-1 menunjukkan gugus O-H, 3062,96 cm-1 menunjukkan gugus C-H streching, 1695,43 cm-1 menunjukkan gugus C=O, cm-1 menunjukkan gugus C-H bending, 1095,57cm-1 menunjukkan gugus C-O-C, 609,51cm-menunjukkan gugus (CH2)n>4. Hasil analisis morfologi permukaan menggunakan SEM menunjukkan bahwa permukaan selulosa stearat tampak homogen, lebih teratur dan memiliki rongga-rongga yang lebih rapat daripada α-Selulosa.

Author(s):  
Eddy Kurniawan ◽  
Rizka Mulyawan ◽  
Angga Tri Agusna PA ◽  
Wika Armadani ◽  
Zainuddin Ginting

Biodegradable polybags are an alternative to overcome the weakness of synthetic polybags because of their degradation properties. Oil palm empty fruit bunches contain a lot of cellulose so that they can be used as a biodegradable polybag. Wet Strength serves to increase the physical strength of bio-polybags when exposed to water (in wet conditions) so that water content stability is required. In this study, Cellulose Stearate Esters were synthesized in an effort to increase the stability of the water content in bio-polybags. Cellulose Stearate Esters are synthesized through a transesterification reaction between -Cellulose isolated from Oil Palm Empty Fruit Bunches (EFB) with methyl stearate. The synthesis of cellulose stearate esters was carried out by refluxing for 2 hours using methanol solvent with various catalysts Na2CO3 5, 10, 15, 20 mg and with volume variations of methyl stearate 5, 10, 15. And the best variation was determined based on the degree of substitution test, namely with variations Na2CO3 catalyst 20 mg and volume of methyl Stearate 15 ml, amounting to 1.95. The result of the synthesis, namely cellulose stearate, was tested for functional groups by FT-IR spectroscopy and surface morphology using SEM. The formation of cellulose stearate is supported by the FT-IR spectrum in the wavenumber region of 3468.01 cm-1 indicating an OH group, 3062.96 cm-1 indicating a CH stretching group, 1695.43 cm-1 indicating a C=O group, cm-1 indicating a CH bending group, 1095.57cm-1 indicates a COC group, 609.51cm-1 indicates a (CH2)n>4 group. The results of surface morphology analysis using SEM showed that the surface of cellulose stearate looked homogeneous, more regular and had denser cavities than -Cellulose


Author(s):  
Steven M. Le Vine ◽  
David L. Wetzel

In situ FT-IR microspectroscopy has allowed spatially resolved interrogation of different parts of brain tissue. In previous work the spectrrscopic features of normal barin tissue were characterized. The white matter, gray matter and basal ganglia were mapped from appropriate peak area measurements from spectra obtained in a grid pattern. Bands prevalent in white matter were mostly associated with the lipid. These included 2927 and 1469 cm-1 due to CH2 as well as carbonyl at 1740 cm-1. Also 1235 and 1085 cm-1 due to phospholipid and galactocerebroside, respectively (Figs 1and2). Localized chemical changes in the white matter as a result of white matter diseases have been studied. This involved the documentation of localized chemical evidence of demyelination in shiverer mice in which the spectra of white matter lacked the marked contrast between it and gray matter exhibited in the white matter of normal mice (Fig. 3).The twitcher mouse, a model of Krabbe’s desease, was also studied. The purpose in this case was to look for a localized build-up of psychosine in the white matter caused by deficiencies in the enzyme responsible for its breakdown under normal conditions.


Author(s):  
David L. Wetzel ◽  
John A. Reffner ◽  
Gwyn P. Williams

Synchrotron radiation is 100 to 1000 times brighter than a thermal source such as a globar. It is not accompanied with thermal noise and it is highly directional and nondivergent. For these reasons, it is well suited for ultra-spatially resolved FT-IR microspectroscopy. In efforts to attain good spatial resolution in FT-IR microspectroscopy with a thermal source, a considerable fraction of the infrared beam focused onto the specimen is lost when projected remote apertures are used to achieve a small spot size. This is the case because of divergence in the beam from that source. Also the brightness is limited and it is necessary to compromise on the signal-to-noise or to expect a long acquisition time from coadding many scans. A synchrotron powered FT-IR Microspectrometer does not suffer from this effect. Since most of the unaperatured beam’s energy makes it through even a 12 × 12 μm aperture, that is a starting place for aperture dimension reduction.


Author(s):  
John A. Reffner ◽  
William T. Wihlborg

The IRμs™ is the first fully integrated system for Fourier transform infrared (FT-IR) microscopy. FT-IR microscopy combines light microscopy for morphological examination with infrared spectroscopy for chemical identification of microscopic samples or domains. Because the IRμs system is a new tool for molecular microanalysis, its optical, mechanical and system design are described to illustrate the state of development of molecular microanalysis. Applications of infrared microspectroscopy are reviewed by Messerschmidt and Harthcock.Infrared spectral analysis of microscopic samples is not a new idea, it dates back to 1949, with the first commercial instrument being offered by Perkin-Elmer Co. Inc. in 1953. These early efforts showed promise but failed the test of practically. It was not until the advances in computer science were applied did infrared microspectroscopy emerge as a useful technique. Microscopes designed as accessories for Fourier transform infrared spectrometers have been commercially available since 1983. These accessory microscopes provide the best means for analytical spectroscopists to analyze microscopic samples, while not interfering with the FT-IR spectrometer’s normal functions.


Author(s):  
Liling Cho ◽  
David L. Wetzel

Polarized infrared microscopy has been used for forensic purposes to differentiate among polymer fibers. Dichroism can be used to compare and discriminate between different polyester fibers, including those composed of polyethylene terephthalate that are frequently encountered during criminal casework. In the fiber manufacturering process, fibers are drawn to develop molecular orientation and crystallinity. Macromolecular chains are oriented with respect to the long axis of the fiber. It is desirable to determine the relationship between the molecular orientation and stretching properties. This is particularly useful on a single fiber basis. Polarized spectroscopic differences observed from a single fiber are proposed to reveal the extent of molecular orientation within that single fiber. In the work presented, we compared the dichroic ratio between unstretched and stretched polyester fibers, and the transition point between the two forms of the same fiber. These techniques were applied to different polyester fibers. A fiber stretching device was fabricated for use on the instrument (IRμs, Spectra-Tech) stage. Tension was applied with a micrometer screw until a “neck” was produced in the stretched fiber. Spectra were obtained from an area of 24×48 μm. A wire-grid polarizer was used between the source and the sample.


Author(s):  
Rahmiana Zein ◽  
Mutia Khuratul Aini ◽  
Hermansyah Aziz

Biosorpsi zat warna Rhodamine B menggunakan cangkang Pensi (Corbicula moltkiana) telah dikaji. Percobaan dilakukan dengan system batch guna memperoleh kondisi optimum biosorspi zat warna. Kapasitas biosorpsi zat warna pada pH 2 adalah 0.9958 mg/g, dengan konsentrasi larutan mula-mula 150 mg/L waktu kontak 105 menit, massa biosorben 0.1 g, ukuran partikel 32 µm dan temperature pengeringan biosorben pada 75oC. Model isotherm Langmuir menunjukkan bahwa proses penyerapan berlangsung secara kimia dan biosorpsi homogeny dari adsorbat (Rhodamine B) pada permukaan biosorben membentuk lapisan tunggal dengan nilai R2 0.9966. Analisis XRF menunjukkan bahwa penurunan kadar unsur logam pada cangkang Pensi membuktikan bahwa proses biosorpsi berlangsung dengan pertukaran kation. Hasil analisis spektrum FT-IR membuktikan adanya interaksi antaramolekul Rhodamin B dengan gugus fungsi pada cangkang Pensi. Analisis dengan SEM memperlihatkan bahwa pori-pori cangkang Pensi telah terisi penuh oleh molekul Rhodamin B. Kondisi optimum biosorpsi telah diaplikasikan pada limbah kerupuk merah dengan kapasitas penyerapan sebesar 0,2835 mg/g.   The biosorption of Rhodamine B dyes by Pensi (Corbicula moltkiana) shell has been investigated. The experiment was conducted in batch sistem in order to obtain the optimum conditions of dye biosorption. Biosorption capacity of dye was 0.9958 mg/g at pH 2, initial concentration 150 mg/L, contact time 105 minutes, biosorbent mass 0.1 gram, particle size 32 µ m and biosorbent drying temperature was at 75oC. The Langmuir Isotherm model showed chemisorption and homogeneous biosorption process of adsorbates onto the biosorbent surface formed monolayer dye molecules on the biosorbent surface with R2 value was 0.9966. XRF analysis showed that reduction of metals unsure quantity of pensi shell indicated biosorption process was occupied through cationic exchange. The result of FTIR spectra analysis indicated an interaction between Rhodamin B molecules and functional group of pensi shell. SEM analysis showed that the pensi shell pores were completely filled by Rhodamine B molecules. The optimum condition of biosorption has been aplicated in red chips wastewater industry with biosorption capacity was 0.2835 mg/g.


TAPPI Journal ◽  
2018 ◽  
Vol 17 (09) ◽  
pp. 519-532 ◽  
Author(s):  
Mark Crisp ◽  
Richard Riehle

Polyaminopolyamide-epichlorohydrin (PAE) resins are the predominant commercial products used to manufacture wet-strengthened paper products for grades requiring wet-strength permanence. Since their development in the late 1950s, the first generation (G1) resins have proven to be one of the most cost-effective technologies available to provide wet strength to paper. Throughout the past three decades, regulatory directives and sustainability initiatives from various organizations have driven the development of cleaner and safer PAE resins and paper products. Early efforts in this area focused on improving worker safety and reducing the impact of PAE resins on the environment. These efforts led to the development of resins containing significantly reduced levels of 1,3-dichloro-2-propanol (1,3-DCP) and 3-monochloropropane-1,2-diol (3-MCPD), potentially carcinogenic byproducts formed during the manufacturing process of PAE resins. As the levels of these byproducts decreased, the environmental, health, and safety (EH&S) profile of PAE resins and paper products improved. Recent initiatives from major retailers are focusing on product ingredient transparency and quality, thus encouraging the development of safer product formulations while maintaining performance. PAE resin research over the past 20 years has been directed toward regulatory requirements to improve consumer safety and minimize exposure to potentially carcinogenic materials found in various paper products. One of the best known regulatory requirements is the recommendations of the German Federal Institute for Risk Assessment (BfR), which defines the levels of 1,3-DCP and 3-MCPD that can be extracted by water from various food contact grades of paper. These criteria led to the development of third generation (G3) products that contain very low levels of 1,3-DCP (typically <10 parts per million in the as-received/delivered resin). This paper outlines the PAE resin chemical contributors to adsorbable organic halogens and 3-MCPD in paper and provides recommendations for the use of each PAE resin product generation (G1, G1.5, G2, G2.5, and G3).


TAPPI Journal ◽  
2018 ◽  
Vol 17 (09) ◽  
pp. 507-515 ◽  
Author(s):  
David Skuse ◽  
Mark Windebank ◽  
Tafadzwa Motsi ◽  
Guillaume Tellier

When pulp and minerals are co-processed in aqueous suspension, the mineral acts as a grinding aid, facilitating the cost-effective production of fibrils. Furthermore, this processing allows the utilization of robust industrial milling equipment. There are 40000 dry metric tons of mineral/microfbrillated (MFC) cellulose composite production capacity in operation across three continents. These mineral/MFC products have been cleared by the FDA for use as a dry and wet strength agent in coated and uncoated food contact paper and paperboard applications. We have previously reported that use of these mineral/MFC composite materials in fiber-based applications allows generally improved wet and dry mechanical properties with concomitant opportunities for cost savings, property improvements, or grade developments and that the materials can be prepared using a range of fibers and minerals. Here, we: (1) report the development of new products that offer improved performance, (2) compare the performance of these new materials with that of a range of other nanocellulosic material types, (3) illustrate the performance of these new materials in reinforcement (paper and board) and viscosification applications, and (4) discuss product form requirements for different applications.


Sign in / Sign up

Export Citation Format

Share Document