Properties of slag geopolymer concrete modified with fly ash and silica fume

Author(s):  
Hafez Elsayed Elyamany ◽  
Abd Elmoaty Mohamed Abd Elmoaty ◽  
Abdul Rahman Ahmed Diab

This research focused on the role of fly ash and silica fume on slag geopolymer concrete through investigating workability (slump, and slump loss), initial setting time, final setting time, and mechanical properties of slag geopolymer concrete, S-GPC, (compressive strength, splitting tensile strength, modulus of elasticity) in addition to SEM (Scanning electron microscope), and X-Ray analysis. The considered variables included, fly ash (FA) content as a replacement of ground granulated blast furnace slag (GS) (0, 10, 20, 30, and 40 %), presence of silica fume (SF) as a replacement of slag, concentration of sodium hydroxide, NaOH, (molarity: 10M, 16M, and 18M), additional water content (7.5,11,14, and 20 %), and curing type (thermal, air, and water curing). S-GPC yielded rapid stiffening and high slump loss with high mechanical properties. The use of silica fume or fly ash or a mix of them enhanced workability, decreased rate of slump loss, and delayed setting time. ACI 318 equation over estimates splitting tensile strength of FS-GPC.

2014 ◽  
Vol 548-549 ◽  
pp. 12-15 ◽  
Author(s):  
Meng Jie Lu ◽  
Ming Fang Ba ◽  
Dan Yi Man ◽  
Si Yuan Ma ◽  
Jie Yang ◽  
...  

In order to save the costs of the rapid hardening and repair sulphoaluminate cement and improve its working performance, the effects of slag, fly ash, silica fume in different contents and different adding ways on the initial setting time and working performance of sulphoaluminate cement are studied. The results show that the initial setting time of single-doped slag and fly ash both meet the requirements of repair materials, but silica fume significantly cuts the cement’s initial setting time short, which does not meet the construction conditions for rapid hardening and repair. Ultimately it is determined that the mechanical properties of sulphoaluminate cement are the best when slag and fly ash are compound added by the content of 30% at 4:1 mass ratio and simultaneously the initial setting time meets the conditions for rapid hardening and repair.


2021 ◽  
Vol 30 (3) ◽  
pp. 464-476
Author(s):  
Haider Owaid ◽  
Haider Al-Baghdadi ◽  
Muna Al-Rubaye

Large quantities of paper and wood waste are generated every day, the disposal of these waste products is a problem because it requires huge space for their disposal. The possibility of using these wastes can mitigate the environmental problems related to them. This study presents an investigation on the feasibility of inclusion of waste paper ash (WPA) or wood ash (WA) as replacement materials for fly ash (FA) class F in preparation geopolymer concrete (GC). The developed geopolymer concretes for this study were prepared at replacement ratios of FA by WPA or WA of 25, 50, 75 and 100% in addition to a control mix containing 100% of FA. Sodium hydroxide (NaOH) solutions and sodium silicate (Na2SiO3) are used as alkaline activators with 1M and 10M of sodium hydroxide solution.The geopolymer concretes have been evaluated with respect to the workability, the compressive strength, splitting tensile strength and flexural strength. The results indicated that there were no significant differences in the workability of the control GC mix and the developed GC mixes incorporating WPA or WA. Also, the results showed that, by incorporating of 25–50% PWA or 25% WA, the mechanical properties (compressive strength, splitting tensile strength and flexural strength) of GC mixes slightly decreased. While replacement with 75–100% WPA or with 50–100% WA has reduced these mechanical properties of GC mixes. As a result, there is a feasibility of partial replacement of FA by up to 50% WPA or 25% WA in preparation of the geopolymer concrete.


2015 ◽  
Vol 754-755 ◽  
pp. 406-412 ◽  
Author(s):  
Puput Risdanareni ◽  
Januarti Jaya Ekaputri ◽  
Mohd Mustafa Al Bakri Abdullah

This paper describes the effect of alkaline activator ratio (Na2SiO3/NaOH) to mechanical properties of geopolymer concrete. The mechanical properties of geopolymer concrete were assessed by setting time, split tensile strength and porosity. Fly ash was used as a cement substitute, and trass used as filler. While, Natrium hydroxide (NaOH) and Sodium Silicate (Na2SiO3) was applied as alkaline activator. In this study, NaOH concentration eight and ten molar with an alkaline activator ratio Na2SiO3/ NaOH by mass: 0.5, 1, 1.5, 2 and 2.5 were used. The test result showed that setting time, porosity and split tensile strength of geopolymer concrete were hardly influenced by NaOH concentration and the alkaline activator ratio. The alkaline activator ratio of Na2SiO3/NaOH has an optimum value at 2 and 2.5. Test result showed that the fastest setting time was 25 minute, the highest amount of closed porosity was 9.035 % and the highest split tensile strength was 2.86 MPa.


Polymers ◽  
2021 ◽  
Vol 13 (6) ◽  
pp. 875
Author(s):  
Chenchen Luan ◽  
Qingyuan Wang ◽  
Fuhua Yang ◽  
Kuanyu Zhang ◽  
Nodir Utashev ◽  
...  

There have been a few attempts to develop prediction models of splitting tensile strength and reinforcement-concrete bond strength of FAGC (low-calcium fly ash geopolymer concrete), however, no model can be used as a design equation. Therefore, this paper aimed to provide practical prediction models. Using 115 test results for splitting tensile strength and 147 test results for bond strength from experiments and previous literature, considering the effect of size and shape on strength and structural factors on bond strength, this paper developed and verified updated prediction models and the 90% prediction intervals by regression analysis. The models can be used as design equations and applied for estimating the cracking behaviors and calculating the design anchorage length of reinforced FAGC beams. The strength models of PCC (Portland cement concrete) overestimate the splitting tensile strength and reinforcement-concrete bond strength of FAGC, so PCC’s models are not recommended as the design equations.


2013 ◽  
Vol 12 (3) ◽  
pp. 215-222
Author(s):  
Katarzyna Synowiec

The paper presents the tests results of the properties of non - standard fly ash - slag cements composition. Both natural (unprocessed) and activated by grinding calcareous fly ash was used. It was found that the calcareous fly ash next to the granulated blast furnace slag may be a component of low - clinker cements (ca. 40%). Those cements are characterized by low heat of hydration and overdue of initial setting time in comparison with Ordinary Portland Cement, moreover they have an unfavorable effect on consistency and its upkeep in time. Production of fly ash - slag cements is possible for strength class 32,5 N when the component of cement is raw fly ash, and for strength classes 32,5 N, 32,5 R and 42,5 N when ground fly ash was used. Fly ash activated by grinding was characterized by higher activity.


Fibers ◽  
2019 ◽  
Vol 7 (4) ◽  
pp. 36 ◽  
Author(s):  
Hisham Alabduljabbar ◽  
Rayed Alyousef ◽  
Fahed Alrshoudi ◽  
Abdulaziz Alaskar ◽  
Ahmed Fathi ◽  
...  

The behaviors of the fresh and mechanical properties of self-compacting concrete (SCC) are different from those of normal concrete mix. Previous research has investigated the benefits of this concrete mix by incorporating different constituent materials. The current research aims to develop a steel fiber reinforcement (SFR)‒SCC mixture and to study the effectiveness of different cement replacement materials (CRMs) on the fresh and mechanical properties of the SFR‒SCC mixtures. CRMs have been used to replace cement content, and the use of different water/cement ratios may lower the cost of CRMs, which include microwave-incinerated rice husk ash, silica fume, and fly ash. Fresh behavior, such as flow and filling ability and capacity segregation, was examined by a special test in SCC on the basis of their specifications. Moreover, compressive and splitting tensile strength tests were determined to simulate the hardened behavior for the concrete specimens. Experimental findings showed that, the V-funnel and L-box were within the accepted range for SCC. Tensile and flexural strength increases upon the use of 10% silica fume were found when compared with other groups; the ideal percentage of steel fiber that should be combined in this hybrid was 2% of the total weight of the binder. Overall, steel fibers generated a heightened compressive and splitting tensile strength in the self-compacting concrete mixes.


2020 ◽  
Vol 2020 ◽  
pp. 1-12
Author(s):  
E. Rabiaa ◽  
R. A. S. Mohamed ◽  
W. H. Sofi ◽  
Taher A. Tawfik

This research investigates the simultaneous impact of two different types of steel fibers, nanometakaolin, and nanosilica on the mechanical properties of geopolymer concrete (GPC) mixes. To achieve this aim, different geopolymer concrete mixes were prepared. Firstly, with and without nanomaterials (nanosilica and nanometakaolin) of 0, 2%, 4%, 6%, and 8% from ground granulated blast furnace slag (GGBFS) were used. Secondly, steel fiber (hooked end and crimped) content of (0, 0.5%, 1, and 1.5%) was used. Thirdly, optimum values of nanomaterials with the optimum values of steel fiber were used. Crimped and hooked-end steel fibers were utilized with an aspect ratio of 60 and a length of 30 mm. Geopolymer mixes were manufactured by using a constant percentage of alkaline activator to binder proportion equal to 0.45 with GGBFS cured at ambient conditions. For alkaline activator, sodium hydroxide molar (NaOH) and sodium hydroxide solution (NaOH) were used according to a proportion (Na2SiO3/NaOH) of 2.33. The hardened concrete tests were performed through the usage of splitting tensile strength, flexural, and compressive experiments to determine the impact of steel fibers, nanometakaolin, and nanosilica individually and combined on performance of GPC specimens. The results illustrated that using a mix composed of the optimum steel fibers (1% content) accompanied by an optimum percentage of 6% nanometakaolin or 4% nanosilica demonstrated a significant enhancement in the mechanical properties of GPC specimens compared to all other mixtures. Besides, the impact of using nanomaterials individually was found to be predominant on compressive strength on GPC specimens especially with the usage of the optimum values. However, using nanomaterials individually compared to using the steel fibers individually was found to have approximately the same splitting tensile strength and flexural performance.


2020 ◽  
Vol 1005 ◽  
pp. 76-81
Author(s):  
Ghawsaddin Nazari ◽  
Shunya Yamanaka ◽  
Shigeyuki Date

Usage of mineral admixture and chemical admixture in concrete or mortar is a usual solution to reach full compaction, particularly where reinforcement blockage and lack of skilled labor happen. In this paper effect of mineral admixtures (Carbon-free fly ash, hereafter CfFA, and normal fly ash) on fresh properties and rheology of mortar have been investigated. As a result, it was confirmed that CfFA increased significantly the fluidity and air content of mortar in comparison to normal fly ash, both in 15% and 30% replacement; however, the flow loss and air stability within one hour were almost equal. In addition, the initial setting time has also been affected by variation of materials. The two mixing of 30% and 15% of CfFA had a shorter setting time in comparison to the mortar with normal fly ash. Furthermore, CfFA based mortar had a great influence on rheology of mortar. Compared to normal fly ash, CfFA Considerably decreased the plastic Viscosity and increased the productivity of the mortar, both in non-vibrated and vibrated condition, particularly those with 30% replacement.


2016 ◽  
Vol 841 ◽  
pp. 1-6 ◽  
Author(s):  
Puput Risdanareni ◽  
Adjib Karjanto ◽  
Febriano Khakim

This paper describes the result of investigating volcanic ash of Mount Kelud as fly ash substitute material to produce geopolymer concrete. The test was held on geopolymer concrete blended with 0%, 25%, 50% and 100% fly ash replacement with volcanic ash. Natrium Hidroxide (NaOH) with concentration of 12 molar and Natrium Silicate (Na2SiO3) were used as alkaline activator. While alkali-activator ratio of 2 was used in this research. The physical properties was tested by porosity and setting time test, while split tensile strength presented to measure brittle caracteristic of geopolymer concrete. The result shown that increasing volcanic ash content in the mixture will increase setting time of geopolymer paste. On the other hand increasing volcanic ash content will reduce split tensile strength and porosity of geopolymer concrete. After all replacing fly ash with volcanic ash was suitable from 25% to 50% due to its optimum physical and mechanical properties.


2013 ◽  
Vol 357-360 ◽  
pp. 1062-1065 ◽  
Author(s):  
Jeong Eun Kim ◽  
Wan Shin Park ◽  
Song Hui Yun ◽  
Do Gyeum Kim ◽  
Jea Myoung Noh

This paper presents the results of an experimental study on the compressive strength, splitting tensile strength and modulus of elasticity characteristics of high performance concrete. These tests were carried out to evaluate the mechanical properties of HPC for up to 7 and 28 days. Mixtures were prepared with water to binder ratio of 0.40. Two mixtures were containing fly ash at 25%, silica fume at 5% cement replacement, respectively. Another mixture was contains blast furnace slag and fly ash at 25%. Three standard 100¥a200 cylinder specimens were prepared. HPC showed improvement in the compressive strength and splitting tensile strength when ordinary Portland cement was replaced with silica fume. Compare with specimens FA25 and BS25FA25, specimen SF5 showed much more modulus of elasticity. It shows that the use of the blast furnace slag of 25% and fly ash of 25% cement replacement has caused a small increase in compressive strength and splitting tensile strength and modulus of elasticity compared to the only use of fly ash of 25% at 28days. The results indicated that the use of blast furnace slag or silica fume provided the good performance compare to fly ash when the mechanical properties of the high performance concretes were taken into account.