The present study aims to investigate the impact of thermal energy storage aggregate (TESA) and nano-titanium (NT) on properties of structural concrete. TESA was made of scoria encapsulated with phase change materials (PCMs). Coarse aggregates were replaced by TESA at 100% by volume of aggregate and NT was added at 5% by weight of cement. Compressive strength, probability of corrosion, thermal performance, and microstructure properties were studied. The results indicated that the presence of TESA reduced the compressive strength of concrete, although the strength was still high enough to be used as structural concrete. The use of TESA significantly improved the thermal performance of concrete, and slightly improved the resistance of corrosion in concrete. The thermal test results showed that TESA concrete reduces the peak temperature by 2 °C compared to the control. The addition of NT changed the microstructure of concrete, which resulted in higher compressive strength. Additionally, the use of NT further enhanced the thermal performance of TESA concrete by reducing the probability of corrosion remarkably. These results confirmed the crucial role of NT in improving the permeability and the thermal conductivity of mixtures containing PCM. In other words, the charging and discharging of TESA was enhanced with the presence of NT in the mixture.

2019 ◽  
Vol 46 (7) ◽  
pp. 643-656 ◽  
Author(s):  
Amin Moshtaghi Jafarabad ◽  
Morteza Madhkhan ◽  
Naser P. Sharifi

Improving the thermal performance of concrete, as an important construction and pavement material, by incorporating phase change materials (PCMs) has been the topic of much research. Also, various carrier agents such as lightweight aggregate (LWA) have been introduced to incorporate PCMs into concrete. However, incorporation of PCM-impregnated LWA reduces the compressive strength of concrete. In this study, the application of silica fume to improve the compressive strength of PCM-incorporated concrete is investigated. Two types of PCMs, salt hydrate PCM and polyethylene glycol PCM, were incorporated into concrete via scoria LWA, and different physical and mechanical characteristics of the concrete were studied when silica fume was incorporated into the mix. The results show that incorporation of silica fume increases the compressive strength of PCM-incorporated concrete, and at the same time does not diminish the thermal performance of the incorporated PCM. Therefore, incorporation of silica fume was found to be a promising strategy to improve the compressive strength of PCM-incorporated concrete.


2019 ◽  
Vol 16 (1) ◽  
pp. 52
Author(s):  
Jeriscot H. Quayson ◽  
Zakari Mustapha

Over one-third of the volume of concrete is occupied by coarse aggregate and any changes in coarse aggregate type can affect its strength and fracture properties. The paper examined the impact of coarse aggregates on compressive strength of concrete. Slump and compaction factor tests were conducted on the mixture of quartzite and crushed granite course aggregates, and quarry dust (fine aggregate). Nominal mix (1:2:3) was adopted and mix compositions were calculated by absolute weight method. Twelve (12) cubes (150x150mm) of each type of coarse aggregate were cast for 7, 14, 21, and 28 days to determine their compressive strengths. Quartzite was found to have the highest average compressive strength of 24.48N/mm2 with an average density of 2160kg/m3 , while compressive strength of crushed granite was 22.01N/mm2 with an average density of 2300kg/m3 on the 28 day of testing. Concrete made from granite had the highest workability, while concrete made from quartzite aggregate had the highest compressive strength. Densities and compressive strengths of the individual aggregates accounted for the variation in strengths of the concrete, due to differences in properties and strengths. In conclusion, the effect of any type of coarse aggregate on the compressive strength of concrete will be known and also enable contractors to determine the type of aggregate to be selected for a particular work. Keywords: Compaction factor test; slump test; strength; workability.


2020 ◽  
Vol 6 (11) ◽  
pp. 2143-2158
Author(s):  
Abbas A. Allawi ◽  
Safaa I. Ali

In this study, the effect of glass fiber reinforced polymer (GFRP) section and compressive strength of concrete in composite beams under static and low velocity impact loads was examined. Modeling was performed and the obtained results were compared with the test results and their compatibility was evaluated.‎ Experimental tests of four composite beams were carried out, where two of them are control specimen with 20 MPa compressive strength of concrete deck slab and 50 MPa for other. Bending characteristics were affected by the strength of concrete under impact loading case, as it increased maximum impact force and damping time at a ratio of 59% and reduced the damping ratio by 47% compared to the reference hybrid beam. Under static loading, there was an increase in all the parameters, including the maximum load, ductility, and stiffness. Mid-span deflection was reduced by 25% under static and impact loads. A finite element analysis was performed by using the ABAQUS software. The midspan deflection value was greater than the experimental values by 6% and 3% for impact and static loads, respectively, and all other results showed a high rate of agreement with the obtained test results. The agreement between the numerical and experimental results indicates that the developed numerical model is capable of analyzing the impact and static behavior of such hybrid GFRP-concrete system. Doi: 10.28991/cej-2020-03091608 Full Text: PDF


2018 ◽  
Vol 9 (2) ◽  
pp. 67-73
Author(s):  
M Zainul Arifin

This research was conducted to determine the value of the highest compressive strength from the ratio of normal concrete to normal concrete plus additive types of Sika Cim with a composition variation of 0.25%, 0.50%, 0.75%, 1.00%, 1.25%, 1 , 50% and 1.75% of the weight of cement besides that in this study also aims to find the highest tensile strength from the ratio of normal concrete to normal concrete in the mixture of sika cim composition at the highest compressive strength above and after that added fiber wire with a size diameter of 1 mm in length 100 mm with a ratio of 1% of material weight. The concrete mix plan was calculated using the ASTM method, the matrial composition of the normal concrete mixture as follows, 314 kg / m3 cement, 789 kg / m3 sand, 1125 kg / m3 gravel and 189 liters / m3 of water at 10 cm slump, then normal concrete added variations of the composition of sika cim 0.25%, 0.50%, 0.75%, 1.00%, 1.25%, 1.5%, 1.75% by weight of cement and fiber, the tests carried out were compressive strength of concrete and tensile strength of concrete, normal maintenance is soaked in fresh water for 28 days at 30oC. From the test results it was found that the normal concrete compressive strength at the age of 28 days was fc1 30 Mpa, the variation in the addition of the sika cim additive type mineral was achieved in composition 0.75% of the cement weight of fc1 40.2 Mpa 30C. Besides that the tensile strength test results were 28 days old with the addition of 1% fiber wire mineral to the weight of the material at a curing temperature of 30oC of 7.5%.


2021 ◽  
Vol 13 (4) ◽  
pp. 2073 ◽  
Author(s):  
Hossein Mohammadhosseini ◽  
Rayed Alyousef ◽  
Mahmood Md. Tahir

Recycling of waste plastics is an essential phase towards cleaner production and circular economy. Plastics in different forms, which are non-biodegradable polymers, have become an indispensable ingredient of human life. The rapid growth of the world population has led to increased demand for commodity plastics such as food packaging. Therefore, to avert environment pollution with plastic wastes, sufficient management to recycle this waste is vital. In this study, experimental investigations and statistical analysis were conducted to assess the feasibility of polypropylene type of waste plastic food tray (WPFT) as fibrous materials on the mechanical and impact resistance of concrete composites. The WPFT fibres with a length of 20 mm were used at dosages of 0–1% in two groups of concrete with 100% ordinary Portland cement (OPC) and 30% palm oil fuel ash (POFA) as partial cement replacement. The results revealed that WPFT fibres had an adverse effect on the workability and compressive strength of concrete mixes. Despite a slight reduction in compressive strength of concrete mixtures, tensile and flexural strengths significantly enhanced up to 25% with the addition of WPFT fibres. The impact resistance and energy absorption values of concrete specimens reinforced with 1% WPFT fibres were found to be about 7.5 times higher than those of plain concrete mix. The utilisation of waste plastic food trays in the production of concrete makes it low-cost and aids in decreasing waste discarding harms. The development of new construction materials using WPFT is significant to the environment and construction industry.


Author(s):  
Harish R ◽  
Ramesh S ◽  
Tharani A ◽  
Mageshkumar P

This paper presents the results of an experimental investigation of the compressive strength of concrete cubes containing termite mound soil. The specimens were cast using M20 grade of concrete. Two mix ratios for replacement of sand and cement are of 1:1.7:2.7 and 1:1.5:2.5 (cement: sand: aggregate) with water- cement ratio of 0.45 and varying combination of termite mound soil in equal amount ranging from 30% and 40% replacing fine aggregate (sand) and cement from 10%,15%,20% were used. A total of 27 cubes, 18 cylinders and 6 beams were cast by replacing fine aggregate, specimens were cured in water for 7,14 and 28 days. The test results showed that the compressive strength of the concrete cubes increases with age and decreases with increasing percentage replacement of cement and increases with increasing the replacement of sand with termite mound soil cured in water. The study concluded that termite mound cement concrete is adequate to use for construction purposes in natural environment.


2018 ◽  
Vol 22 (2) ◽  
pp. 427-443 ◽  
Author(s):  
Jiepeng Liu ◽  
Hua Song ◽  
Yuanlong Yang

A total of 11 L-shaped multi-cell concrete-filled steel tubular stub columns were fabricated and researched in axial compression test. The key factors of width-to-thickness ratio D/ t of steel plates in column limb and prism compressive strength of concrete fck were investigated to obtain influence on failure mode, bearing capacity, and ductility of the specimens. The test results show that the constraint effect for concrete provided by multi-cell steel tube cannot be ignored. The ductility decreases with the increase of width-to-thickness ratio D/ t of steel plates in column limb. The bearing capacity increases and the ductility decreases with the increase in prism compressive strength of concrete fck. A finite element program to calculate concentric load–displacement curves of L-shaped multi-cell concrete-filled steel tubular stub columns was proposed and verified by the test results. A parametric analysis with the finite element program was carried out to study the influence of the steel ratio α, steel yield strength fy, prism compressive strength of concrete fck, and width-to-thickness ratio D/ t of steel plates in column limb on the stiffness, bearing capacity and ductility. Furthermore, the design method of bearing capacity was determined based on mainstream concrete-filled steel tubular codes.


2020 ◽  
Vol 2 (1) ◽  
pp. 31-57
Author(s):  
Ni Ketut Sri Astati Sukawati

Concrete with various variants is a basic requirement in building a building. The concrete mixture is diverse depending on the planning made beforehand. The cement mixture is usually in the form of a mixture of artificial stone, cement, water and fine aggregates and coarse aggregates. Aggregates (fine aggregates and coarse aggregates) function as fillers in concrete mixtures. (Subakti, A., 1994). However, in building construction, additives are often added, but there is still a sense of uncertainty at the time of dismantling the mold and the reference before the concrete reaches sufficient strength to carry its own weight and the carrying loads acting on it. To overcome the time of carrying out work related to concrete, it is necessary to find an alternative solution, for example by looking for alternative ingredients of concrete mixture on the basis of consideration without reducing the quality of the concrete. From the results of previous studies it was stated that due to the partial replacement of cement with Fly Ash, the strength of the pressure and tensile strength of the concrete had increased (Budhi Saputro, A., 2008). Based on the description above, the author seeks to examine how the compressive strength of concrete characteristics that occur by adding additives Addition H.E in the concrete mixture and is there any additive Additon H.E effect on the increase in the compressive strength characteristic of the concrete. From the results of the study, it was found that the compressive strength of the concrete with the addition of additives HE was that after the compressive strength test of the concrete cube was carried out and the analysis of concrete compressive strength of 10 specimens, in each experiment a cube specimen was made with the addition of additons. HE with a dose of 80 cc, 120 cc, and 200 cc can accelerate and increase the compressive strength of concrete characteristics.


2021 ◽  
Author(s):  
Omar Siddiqui

The applicability of utilizing a variety of thermal mass including phase change materials with commonly used building materials is investigated through the use of simulations and physical testing. The thermal performance and occupant comfort potential of a novel solid-solid phase change material, known as Dal HSM, is compared and contrasted to commonly available forms of thermal mass. Detailed experimentation is conducted to successfully integrate Dal HSM with gypsum and concrete. The measurement of physical characteristics such as compressive strength and modulus of rupture is conducted to ensure that the PCM-composite compound retains the structural integrity to be utilized in a typical building. The use of thermal mass in the Toronto Net Zero house was found to contribute to energy savings of 10-15% when different types of thermal mass were used. The comfort level of the indoor occupants was also found to increase. The performance of Dal HSM was found to be comparable to a commercially available PCM known as Micronal in the heating mode. The cooling mode revealed that Dal HSM provided slightly lower energy savings when compared to Micronal due to a lower phase transition temperature and latent heat. The performance of physical test revealed a decrease in the compressive strength as the concentration of Dal HSM was increased in the PCM-gypsum specimens. Tests were also performed to analyze the impact of increasing the PCM concentration on the flexural strength of PCM-gypsum composite.


2010 ◽  
Vol 152-153 ◽  
pp. 1176-1179 ◽  
Author(s):  
Feng Lan Li ◽  
Qian Zhu

To improve the application of the new proto-machine-made sand in structural engineering, tests are carried out to study the drying shrinkage of concrete affected by stone powder in proto- machine-made sand. The target cubic compressive strength of concrete is 55 MPa, the main factor varied in mix proportion of concrete is the contents of stone powder by mass of proto-machine-made sand from 3 % to 16 %. The drying shrinkage strains of concrete are measured by the standard method at the ages of 1 d, 3 d, 7 d, 14 d, 28 d, 60 d, 90 d, 120 d, 150 d and 180 d. Based on test results, the drying shrinkage of concrete affected by the contents of stone powder in proto-machine-made sand is analyzed and compared with that of similar test of concrete with traditional machine-made sand, which shows that there is the optimum content of stone powder resulting in the lower drying shrinkage of concrete. The formula for predicting drying shrinkage strain of concrete is proposed.


Sign in / Sign up

Export Citation Format

Share Document